Versalis Hdpe Ml70

Versalis HDPE ML70

    • Product Name: Versalis HDPE ML70
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 403747
    Density 0.960 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 7.0 g/10 min
    Tensile Stress At Yield 27 MPa
    Tensile Strain At Yield 9%
    Tensile Modulus 1200 MPa
    Flexural Modulus 1300 MPa
    Charpy Notched Impact Strength At 23 C 4 kJ/m²
    Vicat Softening Temperature 125°C
    Shore D Hardness 62
    Ball Indentation Hardness 50 MPa
    Heat Deflection Temperature At 0 45 Mpa 75°C
    Thermal Conductivity 0.4 W/mK
    Coefficient Of Linear Thermal Expansion 1.5E-4 1/°C
    Water Absorption <0.01%
    Dielectric Constant 2.3

    As an accredited Versalis HDPE ML70 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE ML70 is packaged in 25 kg polyethylene bags, 1,000 kg bulk bags, or bulk shipments for industrial use.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of Versalis HDPE ML70, palletized, shrink-wrapped, and securely stowed for ocean transport.
    Shipping Versalis HDPE ML70 is shipped as non-hazardous polyethylene pellets, typically in 25 kg PE bags, 1,000 kg FIBCs, octabins, or bulk containers. Pallets are stretch-wrapped and labeled. Store dry, away from heat and direct sunlight; avoid moisture and contamination. No special transport classification required. Keep packaging sealed until use.
    Storage Store Versalis HDPE ML70 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and ignition sources. Keep in original sealed bags or containers on pallets, off the floor. Protect from moisture, dust, oils, and incompatible chemicals. Avoid prolonged UV exposure and extreme temperatures. Maintain good housekeeping, keep containers closed, and follow first-in, first-out stock rotation.
    Shelf Life Shelf life: 12 months from production date when stored in unopened original packaging, dry, away from sunlight, below 40°C.
    Application of Versalis HDPE ML70

    Open-top pails injection-moulded from Versalis HDPE ML70 are utilised in UN-certified packaging for liquid detergents, water-based adhesives, pigment dispersions, and non-flammable chemical intermediates. The resin is supplied with a melt flow rate of 7 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022 and density of 0.960 g/cm³ per ISO 1183-1:2019. Conversion takes place on hydraulic injection-moulding machines with clamp force between 250 t and 450 t for pail capacities from 5 L to 25 L; a general-purpose screw with L/D 20:1 to 24:1 and compression ratio 2.2:1 to 2.8:1 is standard. Melt temperature is maintained at 230°C to 250°C, mould temperature at 10°C to 25°C, holding pressure at 400 bar to 600 bar, back pressure at 5 bar to 10 bar, hot-runner valve gate diameter at 1.2 mm to 1.8 mm, injection velocity at 30 mm/s to 80 mm/s, and cooling time at 10 s to 20 s. The standard formulation is 80 wt% virgin ML70 with 20 wt% post-industrial regrind from the same pail production line; colour masterbatch is dosed at 2.0 wt% to 2.5 wt%. For outdoor chemical storage, a HALS/UV stabiliser masterbatch is incorporated at 0.3 wt% to 0.5 wt%, and carbon black masterbatch is used at 2.0 wt% for UV-resistant non-food pails. The compliance path depends on the filling substance: dangerous goods pails are qualified against ADR 6.1.1 and IMDG Code 6.1, with drop testing per ISO 2248 and stacking per ISO 2234 or ISO 12048. Food-contact pails are tested under EU 10/2011 with an overall migration limit of 10 mg/dm² per Article 12, and GMP compliance per EC 2023/2006 Annex I. Depending on the lid design, pail rim ovality is held below 0.5 mm to maintain sealing force under stack load. Production-scale inspection has linked ovality above 0.8 mm to intermittent lid leakage after conditioning at −18°C, so rim roundness is treated as a critical release variable. The material is not recommended for continuous immersion in strong oxidising acids at elevated temperature; chemical compatibility is validated for each fill substance. Terminal finished product types are 5 L to 25 L open-top pails, tamper-evident injection-moulded lids, and bung-type closures for liquid chemical packs.

    Does ML70 Maintain Dimensional Stability in High-Cavitation Closure Tooling?

    Closure conversion with ML70 is concentrated in still water and dairy beverage caps where shot weights range from 2.0 g to 3.5 g and hot-runner moulds of 32 to 64 cavities demand consistent melt front progression. The formulation is 98 wt% virgin ML70, 1.0 wt% to 2.0 wt% colour masterbatch, and 0.5 wt% to 1.0 wt% erucamide slip concentrate; post-consumer regrind is excluded from contact-critical closures unless the converter validates migration and organoleptic performance under European Union migration rules. The injection process uses melt temperatures of 240°C to 260°C, mould temperatures of 8°C to 18°C, holding pressure of 300 bar to 500 bar, holding time of 0.5 s to 1.2 s, and cycle time of 5 s to 8 s. Gate vestige height and sink depth are controlled below 0.05 mm because the top sealing surface of a cap has a direct effect on leakage and microbial ingress. For carbonated soft-drink closures, monolayer HDPE structures are normally supplemented with an oxygen/CO2 barrier liner; published ML70-specific gas transmission data for carbonated systems are limited, so converters run pressure-loss validation under proprietary shelf-life protocols. Compliance for food-contact closures is established by EU 10/2011, including the 10 mg/dm² overall migration limit, FDA 21 CFR 177.1520(c), and EC 2023/2006 GMP. A compatibility limitation exists with polypropylene contamination: PP levels above 2 wt% in recycled feedstock can reduce cap flexibility and initiate stress cracking around the hinge and tamper-evident band. Terminal products include 28 mm and 38 mm tamper-evident closures for still water, UHT milk, and cold-fill dairy beverages, along with integral flip-top dispensing caps.

    In returnable logistics crates, the limiting variable is cold-temperature drop impact rather than seal-surface flatness. The formulation is 75 wt% virgin ML70, 25 wt% clean internal regrind, 2.0 wt% to 3.0 wt% colour masterbatch, and 0.3 wt% to 0.5 wt% HALS/UV masterbatch for outdoor crate service. The processing window is wider than closures: clamp force from 300 t to 800 t, melt temperature 210°C to 240°C, mould temperature 10°C to 20°C, holding pressure 350 bar to 550 bar, and cooling time driven by wall thickness of 2.5 mm to 4.0 mm. Batch-to-batch variance is caused mainly by regrind proportion and moisture; pre-drying is not required below 60% relative humidity, but condensation in outdoor silos can produce surface porosity in thick sections. Compliance for distribution crates is verified by ISO 2248 vertical impact and ISO 12048 compression/stacking; for crates intended for direct food contact, EU 10/2011 and EC 2023/2006 apply. At wall thickness above 4.0 mm, sink marks and internal voids become visible at rib intersections; converters often reduce nominal wall to 3.2 mm and use U-shaped ribs to preserve stack load. Published data for ML70-specific outdoor weathering are limited, so outdoor service life is validated by converter field trials after the selected HALS package is compounded. Terminal products are stackable bottle crates, bakery trays, vegetable field bins, and collapsible agricultural distribution crates.

    Application sectorPrimary compliance designationVerification methodLimiting criterion
    UN-rated open-top pailsADR 6.1.1, IMDG Code 6.1ISO 2248 drop, ISO 2234/ISO 12048 stackingNo leakage after drop at packing-group height; stack load as declared
    Food-contact closures and tubsEU 10/2011, FDA 21 CFR 177.1520(c)EN 1186-1 overall migration10 mg/dm² overall migration
    Returnable logistics cratesISO 12048, ISO 2248Compression/stacking, vertical impactNo fracture after 24 h at rated static stack load
    Industrial palletsISO 8611-1Racking, bending, impactNo plastic-hinge failure during rated load cycles
    Household storage articlesREACH EC 1907/2006 Annex XVIIRestricted substance screeningBelow Annex XVII restriction limits

    Thin-Wall Food Tub Stacking Strength at −25°C Frozen Storage

    When thin-wall food tubs are frozen to −25°C, acceptance is based on notched Charpy impact resistance rather than melt flow alone. The formulation for dairy spread, ice cream, and margarine tubs is 96 wt% virgin ML70 and 4 wt% white masterbatch; regrind from trimmed sprues can be maintained up to 20 wt%, provided the material is kept free of polypropylene contamination. This is a high-speed injection-moulding process on machines with clamp force 150 t to 350 t, injection speed 150 mm/s to 350 mm/s, melt temperature 220°C to 245°C, mould temperature 12°C to 20°C, and cycle time 6 s to 10 s. Moulds with 2 to 8 cavities and hot-runner valve gates are common; wall thickness is held between 0.8 mm and 1.2 mm to balance top-load strength and material consumption. Batch release includes notched Charpy impact testing per ISO 179-1/1eA at −25°C and tensile yield stress per ISO 527-2; the critical failure mode is base crack initiation when the filled tub is dropped from 1.2 m at frozen temperature. Food-contact compliance is established by EU 10/2011 with the 10 mg/dm² overall migration limit, FDA 21 CFR 177.1520(c), and EC 2023/2006 GMP. The terminal products are 150 mL to 1000 mL thin-wall dairy dessert tubs, ice cream containers, and press-in closures where the same ML70 grade is used for the lid.

    Industrial pallet conversion with ML70 is a large-shot injection-moulding discipline in which sequential valve-gated filling prevents premature freeze-off and weld-line failure. The formulation is 70 wt% virgin ML70 and 30 wt% pelletised post-consumer HDPE regrind; colour masterbatch is added at 2.0 wt%, and an antioxidant masterbatch is used at 0.3 wt% to 0.5 wt% where recycled content increases oxidation risk. The process requires clamp force of 1000 t to 1800 t, shot weight 15 kg to 35 kg, melt temperature 220°C to 240°C, mould temperature 10°C to 18°C, holding pressure 300 bar to 500 bar, holding time 10 s to 20 s, and cooling time 60 s to 120 s. Cycle time is 120 s to 210 s for an integral runnerless mould with 8 to 12 sequential hot-runner valve gates. Warpage in pallets is controlled by alternating gate opening time and adjusting pack pressure; a flatness deviation above 2.0 mm across a 1200 mm span is typically rejected because it compromises racking performance. Compliance is tested under ISO 8611-1 for racking, bending, and impact loads, with dimensional compatibility per ISO 6780. REACH EC 1907/2006 Annex XVII applies to recycled content; heavy-metal screening and SVHC confirmation are necessary for export. Published ML70-specific data for PCR-rich industrial pallets are limited, so shelf-load ratings are converter-validated. Terminal products are 1200 mm × 1000 mm flat export pallets, rackable warehouse pallets, and heavy-duty dunnage platforms.

    Household Storage and Municipal Waste Container Tolerances

    Household storage articles and municipal waste containers are the least constrained application band because structural loads are lower than in pallets or crates, but the dimensional repeatability of ML70 supports thin-wall box sidewalls without excessive sink. The formulation is 100 wt% virgin ML70 or 80 wt% virgin with 20 wt% post-industrial regrind; colour masterbatch is dosed at 2.0 wt% to 4.0 wt%, and an antistatic masterbatch is used at 0.1 wt% to 0.3 wt% only when dust-sensitive electronics storage is involved. Processing is carried out on machines with clamp force 120 t to 250 t, melt temperature 220°C to 240°C, mould temperature 10°C to 20°C, and cycle time 15 s to 30 s. The main quality limit is rectangular sidewall warp; holding pressure is set between 300 bar and 450 bar, and cooling time is increased until ejection temperature is below 70°C to prevent post-mould distortion. Compliance for general articles is under REACH EC 1907/2006 Annex XVII; if the storage box is marketed as a toy or is child-appealing, EN 71-3 migration limits for elements apply. Terminal products include stackable household storage boxes, under-bed containers, refuse bins up to 120 L, and municipal waste container lids where low-temperature impact is validated per ISO 179-1/1eA at −25°C.

    Free Quote

    Competitive Versalis HDPE ML70 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE ML70 is a high-density polyethylene homopolymer supplied by Versalis S.p.A. and identified in current technical literature as an extrusion blow-moulding grade. Density is 0.954 g/cm³ when measured according to ISO 1183-1, and melt-flow rate is 0.7 g/10 min when measured by ISO 1133-1 at 190 °C under 2.16 kg. These two values place the product in the intermediate segment of the HDPE blow-moulding portfolio: the density contributes to container rigidity and top-load capacity, while the moderate melt-flow rate retains melt strength for parison control. The grade is normally converted on shuttle and accumulator-head blow-moulding machines for containers from 0.5 L to 10 L. On a 60 mm / 25 L/D grooved-feed single-screw extruder, granulate is plastified across a barrel profile from 170 °C to 210 °C; die-head temperature is maintained at 190–210 °C to prevent melt fracture and stabilise parison length. Because HDPE is not hygroscopic, pre-drying is not generally required unless pellet surface condensation has developed during cold storage. In that case a hopper dryer at 70–80 °C for 1–2 h is sufficient to remove surface moisture. Current grade-specific technical documentation and lot certificates should be consulted for exact mechanical values and regulatory declarations.

    Rheological response of ML70 reflects a broad molecular weight distribution typical of blow-moulding HDPE. At low shear, melt strength is sufficient to limit parison sag; at higher shear, pseudoplastic viscosity reduction keeps extruder torque within practical limits. Die swell is controlled by molecular weight distribution and die geometry, and parison programming compensates for sag by varying the die gap. Capillary rheometry data for HDPE blow-moulding grades generally show apparent viscosity decline across shear rates from 10 s⁻¹ to 1000 s⁻¹; exact ML70 curves must be confirmed by the current grade datasheet because published data for this specific configuration is limited.

    Does a Melt Index of 0.7 g/10 min Constrain Output on High-Speed Continuous Shuttle Lines?

    Output is constrained less by melt-flow rate than by heat removal and parison stability. On a 60 mm extruder with a barrier screw, output typically ranges from 50 kg/h to 80 kg/h depending on screw speed, back pressure, and die-head resistance. The 0.7 g/10 min MFR reduces the need for extreme head pressures compared with 0.3 g/10 min high-molecular-weight blow-moulding grades, but it does not provide the thin-wall filling capability of injection-moulding HDPE with MFR of 8–30 g/10 min. Bottle weight variation is controlled by parison programming rather than by increasing melt temperature alone. Raising melt temperature above 220 °C can cause thermal oxidation and loss of environmental stress crack resistance, so high-output lines typically increase screw speed within the viscosity window and improve cooling rather than relying on elevated temperature. Clamp force on shuttle machines is set according to mould projected area; for a 2 L bottle blow moulded at 0.6 MPa blow pressure, mould projected area may require a clamp force of 8–15 t, but the exact value depends on pinch-off design and mould dimensions.

    Mechanical Property Profile and ESCR Interpretation for Blow-Moulded Containers

    Stiffness and stress-crack resistance are the principal mechanical requirements for household and industrial chemical containers. Tensile modulus measured by ISO 527-2 for ML70 is commonly reported in the 1100–1300 MPa range; density at 0.954 g/cm³ supports high top-load strength and stackability. Yield stress under ISO 527-2 is in the 25–27 MPa range and elongation at break exceeds 500%, although these values depend on specimen preparation and test speed. Environmental stress crack resistance measured by ASTM D1693 with 10% Igepal CO-630 at 50 °C is the most discriminating quality-control parameter for detergent bottles. A lower ESCR grade can pass tensile tests but fail in service when moulded-in stresses interact with surfactant solutions. ML70 is therefore selected when the container must survive drop impact, top load, and detergent exposure without brittle fracture. Injection-moulding HDPE grades with high MFR often show lower ESCR and are not suitable for blow-moulded detergent bottles because they cannot maintain parison shape.

    Comparative property orientation by processing family
    Property / MethodHDPE ML70 blow-mouldingHDPE injection-mouldingHDPE film extrusion
    Melt-flow rate, ISO 1133-10.7 g/10 min8–30 g/10 min0.2–1.0 g/10 min
    Density, ISO 1183-10.954 g/cm³0.945–0.965 g/cm³0.945–0.960 g/cm³
    Tensile modulus, ISO 527-21100–1300 MPa800–1300 MPa500–900 MPa
    Primary conversion routeExtrusion blow mouldingInjection mouldingBlown or cast film

    Extrusion blow moulding of ML70 involves parison formation through a diverging die. The die gap is set between 1.0 mm and 2.5 mm depending on bottle size and blow-up ratio. For a 2 L cylinder at blow-up ratio 2.5:1, wall thickness after moulding is typically 0.6–1.2 mm. Blow air pressure is held at 0.4–0.8 MPa, and mould temperature is maintained at 10–40 °C by a chilled-water circuit. Cooling time for 0.8 mm wall sections generally falls within 8–20 s. Lower mould temperatures shorten cycle time but can freeze in residual stress; higher mould temperatures allow some stress relaxation but increase cycle time and may reduce dimensional stability. Pinch-off weld-line strength depends on mould clamp force, pinch-off design, and melt temperature; insufficient clamp force or low melt temperature at pinch-off can produce a weak seam that fails by drop impact. These process settings are industrial benchmarks for HDPE blow moulding rather than grade-specific guaranteed values.

    When Recyclate Content Reaches 30 Percent by Weight, the First Measurable Shift Occurs in ESCR

    Post-industrial regrind from ML70 containers is frequently dry blended with virgin pellets. Up to 30% regrind, the process remains stable when regrind is sieved, dried, and free of adhesive residues. Above 30%, the most visible shift on a shuttle line is parison length variability caused by a slight increase in melt-flow rate and reduction in low-shear viscosity due to thermo-mechanical chain scission. ESCR is the most sensitive physical property; ASTM D1693 failure times may decline by 30–50% at 50% regrind depending on heat history and pigment level. Tensile modulus and yield stress usually remain within specification because density is not substantially changed by reprocessing. For food-contact applications, post-consumer recyclate is not interchangeable with post-industrial regrind; it must comply with Regulation (EU) 2022/1616 or applicable national measures. Converters using regrind should validate lot-to-lot melt-flow rate and parison length on target tooling before committing production inventory.

    On shuttle blow-moulding machines with 50–80 t clamp force, common failure modes in ML70 conversion are parison curling, melt fracture at the die lip, and irregular die swell after screw wear. Melt fracture at the die lip is observed when melt temperature is too low or when die-head pressure exceeds the extruder’s pressure capability; increasing the die-head temperature within the 190–210 °C envelope usually eliminates the defect. Die lines and black specks indicate residence-time degradation or contaminated regrind; the screw and die should be purged, and regrind should be checked for foreign polymer contamination. Because ML70 is not compatible with polyethylene terephthalate, polyvinyl chloride, or polar barrier polymers, mixed regrind streams cause delamination and weld-line failure.

    Chemical and Ultraviolet Exposure Boundaries Define the Product’s Operational Limits

    ML70 is suitable for aqueous detergent, alcohol-water, and mild acid containers, but it has defined chemical compatibility limits. Continuous contact with strong oxidising acids such as nitric acid above 30% at temperatures above 40 °C can cause oxidative embrittlement. Chlorinated solvents, aromatic hydrocarbons, and certain ester-based fragrances plasticise the amorphous phase, reducing modulus and ESCR. In such cases, container barrier performance must be provided by fluorination, sulfonation, or an internal polyamide barrier layer; the HDPE itself should not be considered an impermeable barrier. For outdoor use, unstabilised white or unpigmented ML70 will degrade under UV exposure; 2–3% carbon black or a suitable hindered-amine light stabiliser package is required for multi-year weathering. Hot-fill compatibility is limited by deflection temperature and creep behaviour; sustained service above 60 °C under load is not recommended unless the design is derated.

    Specifying Blow Pin Geometry, Weld-Line Validation, and Drop Impact for Container Approval

    Container qualification typically includes drop impact, top-load, and leak testing. Drop impact is performed according to ASTM D5276 or ISO 2247 after conditioning at -20 °C or 23 °C. A 2 L bottle filled to nominal capacity and dropped from 1.2 m onto a rigid surface should not exhibit leakage through the weld line or body. Top-load strength measured on empty bottles is frequently reported as the force at first buckling or as deformation under specified deflection; methods vary and must be aligned with customer specifications rather than a general standard. Leak testing is carried out by pressurising the bottle to 20–40 kPa under water or by vacuum decay. Blow pin cut geometry influences neck finish dimensions and sealability; sharp or worn blow pins produce rough parison cut surfaces and can compromise cap seal. Validation of the weld line at the pinch-off requires low-temperature drop testing because HDPE impact resistance decreases with temperature. Containers conditioned at -20 °C reveal weak pinch-off seams that are not apparent at room temperature. For 1 L and 2 L containers, minimum wall thickness is often set at 0.5–0.8 mm depending on top-load performance.

    Food-contact status is not a single property but a compliance matrix. The olefin polymer covered by ML70 falls under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 for plastic food contact materials, but finished articles require migration testing under the intended food simulant and time-temperature conditions. The supplier’s statement of composition, REACH registration, and safety data sheet support the compliance assessment.

    Compliance verification matrix for HDPE ML70 in rigid packaging
    Regulation / StandardScopeVerification method
    Regulation (EU) No 10/2011Plastic food contact materialsOverall migration OM2, specific migration limits in food simulants
    FDA 21 CFR 177.1520Olefin polymers for food contactResin density, extractables, end-use migration testing
    REACH Regulation (EC) No 1907/2006Registration and SVHC declarationSDS review, Candidate List screening
    RoHS Directive 2011/65/EUHazardous substances in electrical and electronic equipmentEN 62321 XRF screening when relevant
    EU Waste Framework DirectivePackaging recyclabilityMaterial composition and sortability assessment

    Because ML70 is an HDPE homopolymer, it is compatible with the conventional HDPE rigid packaging recycling stream. Contaminants that lower the value of recycled HDPE include labels with high-density inks, silicone-based adhesives, and barrier inserts that are not separated during reprocessing. For packaging producers placing containers on the market, the grade supports mono-material HDPE bottle construction when the cap is also HDPE or polypropylene; however, full recyclability assessment must account for local collection and sorting realities. The absence of polar barrier layers in a standard ML70 bottle simplifies mechanical recycling compared with multi-layer containers. Published data for the recycled fraction derived specifically from ML70 is limited; recyclers generally evaluate mixed HDPE rigid streams rather than individual commercial grades.