Versalis Hdpe Fc 82

Versalis HDPE FC 82

    • Product Name: Versalis HDPE FC 82
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 795115
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.20 g/10 min
    Tensile Modulus 1300 MPa
    Tensile Stress At Yield 29 MPa
    Tensile Strain At Yield 9 %
    Tensile Strain At Break >600 %
    Flexural Modulus 1300 MPa
    Izod Notched Impact Strength At 23 C 25 kJ/m²
    Izod Notched Impact Strength At 30 C 6 kJ/m²
    Shore D Hardness 65
    Vicat Softening Temperature 128 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Cracking Resistance 10 Igepal 50 C >1000 h
    Water Absorption <0.01 %
    Thermal Conductivity 0.45 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity >1E15 ohm·cm

    As an accredited Versalis HDPE FC 82 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE FC 82 packaging: 25 kg polyethylene bags, normally stacked on pallets for bulk industrial shipment.
    Container Loading (20′ FCL) Versalis HDPE FC 82 loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, labeled, and secured for ocean freight.
    Shipping Versalis HDPE FC 82 is shipped as non-hazardous polyethylene pellets in 25 kg bags, octabins, or bulk tankers/containers. Keep dry, cool, ventilated, away from ignition, UV, and contaminants. No special transport classification; follow local regulations and maintain packaging integrity. Store under ambient conditions and protect from moisture and direct sunlight.
    Storage Store Versalis HDPE FC 82 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, and undamaged, on pallets off the floor to prevent moisture and contamination. Avoid prolonged UV exposure. Use first-in, first-out stock rotation; maintain good housekeeping. Do not store near foodstuffs or incompatible materials.
    Shelf Life Versalis HDPE FC 82 has a recommended shelf life of 24 months when stored sealed, dry, away from heat and direct sunlight.
    Application of Versalis HDPE FC 82
    Blown film conversion for T-shirt carrier bags is performed on single-screw extruders with L/D ratios between 25:1 and 30:1. The screw employs a barrier flight section and a Maddock mixing element. Melt temperature at the die exit is held between 190°C and 220°C. The die is a spiral mandrel type with an annular gap of 1.2 mm to 1.6 mm. The bubble is operated in the stalk configuration. Frost line height is maintained between 6 and 12 die diameters above the die face. Blow-up ratio is set from 3:1 to 4:1. Film thickness between 10 µm and 20 µm is achievable with Versalis HDPE FC 82. Tensile properties are measured per ASTM D882. Secant modulus at 1% strain for HDPE blown film of this density class typically exceeds 600 MPa. Elmendorf tear strength per ASTM D1922 is anisotropic in HDPE film. Machine-direction tear values are typically below 200 mN. Transverse-direction tear values exceed 800 mN. Dart impact strength per ASTM D1709 Method A for 18 µm film is above 60 g. The high modulus permits downgauging from 20 µm to 14 µm without collapse of bag opening. The bubble is collapsed through a wooden or aluminum collapsing frame. The film is gusseted on the winder. In-line punching forms the handle cut-outs. The finished T-shirt bag has a width between 300 mm and 600 mm. The film contains slip agent and antiblock masterbatch at a combined loading of 1 wt% to 3 wt%. Coefficient of friction per ASTM D1894 is maintained below 0.4. The resin is received in pellet form and is not hygroscopic. Pre-drying is not required when stored below 60% relative humidity. Published data for this specific configuration is limited. The ranges cited are typical for HDPE blown film grades of equivalent density and melt flow rate.

    What limits dart impact in thin-gauge waste sack extrusion?

    Waste bin liner production on the same blown film line introduces a different failure mode. The film gauge is increased to 15 µm to 25 µm. Dart impact resistance per ASTM D1709 Method B becomes the controlling specification. Typical HDPE blown film values fall between 80 g and 150 g at 20 µm. Environmental stress cracking resistance per ASTM D1693 condition B in 10% Igepal CO-630 is used to qualify the resin for long-term wet waste contact. The F50 value for HDPE film grades of this density class exceeds 50 hours. The film is coextruded in three layers. The core layer may contain post-consumer recycled polyethylene at 20 wt% to 40 wt%. Outer skins are virgin FC 82 to maintain tear and seal strength. Carbon black masterbatch is dosed at 2 wt% to 3 wt%. Carbon black particle size is specified between 20 nm and 50 nm. Dispersion quality is checked by film surface microscopy. Agglomerates above 50 µm cause pinholes. The bubble is run with a blow-up ratio of 2.5:1 to 3.5:1. A lower blow-up ratio increases MD tear. It also increases dart impact. The frost line is lowered to 4 to 6 die diameters. This reduces crystalline orientation. The finished sack is star-sealed at the bottom. Capacity ranges from 60 L to 120 L. The sack is tested for leak resistance per EN 13592. This standard specifies a 10 L water fill test without leakage for 2 minutes.

    Food contact status under FDA 21 CFR 177.1520(c) 2.1.

    Direct food contact film produced from Versalis HDPE FC 82 requires confirmation of the additive package against the applicable regulatory lists. The base olefin polymer is covered under FDA 21 CFR 177.1520 paragraph (c) item 2.1. This listing permits use in contact with all food types under conditions of use E through G. Condition of use E refers to room temperature filled and stored. Condition of use G covers frozen storage. The European Union framework requires compliance with Regulation (EU) No 10/2011. Overall migration limit is 10 mg/dm² of surface area. Specific migration limits for additive monomers are listed in Annex I. Verification is performed per EN 1186-1. The film is used as a monolayer bread bag liner. Gauge is 15 µm to 30 µm. Addition of food-approved slip agents is limited to 500 ppm. Antiblocking agents are dosed between 1000 ppm and 2000 ppm. Both additives must appear in the Union List of authorised substances. Printing on the film surface requires low-migration inks. Inline corona treatment raises surface energy above 38 dynes/cm per ASTM D2578. The treated film is immediately printed. The end product is a dry cereal liner. The liner is inserted into a paperboard carton. Seal strength is measured per ASTM F88. Hot-tack performance is not critical for this application.
    Standard or RegulationDesignation / ClauseApplication to FC 82 Film
    FDA 21 CFR 177.1520(c) 2.1Olefin polymers, food contactDirect food contact for dry and aqueous foods
    EU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm²EU food contact compliance
    REACH SVHCCandidate List threshold 0.1% w/wArticle notification
    RoHS 2011/65/EU Annex IIPb 1000 ppm, Hg 1000 ppm, Cd 100 ppm, Cr(VI) 1000 ppm, PBB 1000 ppm, PBDE 1000 ppmEEE component restrictions
    ASTM D4976-12aPE plastics molding and extrusion materialsMaterial specification
    ISO 1133-1:2022MFR at 190°C/2.16 kgMelt flow control
    ISO 1183-1:2019DensityDensity control
    Five-layer coextrusion barrier film for dry food and pharmaceutical packaging uses FC 82 as the structural skin layer. The layer distribution is 40 wt% HDPE skin / 5 wt% tie / 10 wt% EVOH / 5 wt% tie / 40 wt% HDPE skin. The tie resin is a maleic anhydride grafted LLDPE with a grafting level between 0.2 wt% and 0.5 wt%. The EVOH core is a 38 mol% ethylene grade. The die is a five-layer spiral mandrel die. Each extruder runs at a set point offset. HDPE skins are extruded at 200°C to 220°C. The EVOH core is extruded at 190°C to 200°C. The tie layers are extruded at 200°C to 210°C. Melt temperature differences between layers are held below 10°C to prevent interfacial shear instability. The bubble is run at a blow-up ratio of 2.5:1 to 3:1. The frost line is set at 8 to 10 die diameters. Film gauge is 30 µm to 60 µm. Oxygen transmission rate per ASTM D3985 is below 1 cm³/(m²·day·atm) at 23°C and 0% RH. Water vapour transmission rate per ASTM F1249 is below 5 g/(m²·day) at 23°C and 85% RH. The end product is a stand-up pouch for oxygen-sensitive dry powder. The pouch is sealed on a vertical form-fill-seal line. Seal strength per ASTM F88 exceeds 15 N/25 mm. The structure is not suitable for retort or hot-fill above 80°C.

    When FC 82 replaces a conventional LDPE core in heavy-duty industrial liner film

    Heavy-duty industrial liner film is extruded on large blown film lines with die diameters between 400 mm and 600 mm. The film gauge is 80 µm to 150 µm. Conventional LDPE liners at 150 µm are downgauged to 100 µm when HDPE is substituted. The stiffness gain comes from the higher secant modulus. Puncture resistance per ASTM D5748 is the primary mechanical specification. Typical values for 100 µm HDPE blown film exceed 25 N. Tensile energy to break per ASTM D882 is measured in both MD and TD. HDPE film shows lower tensile energy to break than LDPE at equal gauge. This is a known limitation. The film is less forgiving at fold lines. Crease stress whitening occurs at sharp folds. The end user must accept a stiffer, less elastic sack. The advantage is higher stacking strength and lower material consumption. The liner is used as a drum liner for chemical powders. It is also used as a rubble sack on construction sites. Carbon black masterbatch is added at 2 wt% for UV resistance. The bubble is run with a low blow-up ratio of 2:1 to 2.5:1. A low BUR biases orientation toward the machine direction. This increases MD tensile strength. The extruder output is limited by bubble cooling capacity. Internal bubble cooling is used to raise output by 20% to 30%. The film is wound on jumbo rolls. Slitting is performed offline.Adhesive lamination of HDPE blown film as a base substrate for flexible packaging is performed on solventless lamination lines. The HDPE film is first corona treated. The surface energy must exceed 38 dynes/cm per ASTM D2578. The treatment must be performed in-line within 24 hours of lamination. Surface energy decays with time. A solventless polyurethane adhesive is applied at 1.5 g/m² to 2.0 g/m². The adhesive is cured at 40°C for 24 hours. The secondary substrate is aluminium foil or polyester film. The HDPE film provides moisture barrier and heat sealability. Seal initiation temperature per ASTM F1921 is between 120°C and 130°C. Final seal strength per ASTM F88 exceeds 10 N/25 mm. The laminate is used as an outer layer for stand-up pouches. The HDPE surface is printed by flexographic or gravure process. Adhesion between the HDPE film and the adhesive must exceed 2 N/15 mm per ASTM F904. Delamination at the HDPE/adhesive interface is a known failure mode. Corona re-treatment is not recommended. The film is laminated within 12 hours of extrusion to preserve surface energy. The end product is a pet food bag. The structure is HDPE 30 µm / adhesive / PET 12 µm / adhesive / HDPE 30 µm. The lamination machine runs at 150 m/min to 250 m/min. Tension control is critical. The HDPE film modulus is higher than LDPE. This reduces stretch during lamination. Registration accuracy is improved.
    Free Quote

    Competitive Versalis HDPE FC 82 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE FC 82 is introduced as a high-density polyethylene resin positioned for blown-film extrusion in applications requiring a measurable balance of tensile stiffness, melt strength, and downgauging tolerance. The product model belongs to the film-grade subset of the Versalis HDPE range; its FC prefix indicates a film-oriented molecular architecture and additive package, while the numeric suffix separates it from adjacent film grades having different melt viscosity and mechanical response. Specifications for the grade are conventionally expressed through density, melt mass-flow rate, and ash content. The corresponding test methods are ISO 1183-1:2019 for density, ISO 1133-1:2022 for MFR at 190 °C under 2.16 kg and 5.0 kg loads, and ISO 3451-1 for ash. Because published data for this exact configuration are limited, the current technical data sheet and batch certificate should be treated as the controlling reference for numerical values.

    At incoming inspection, the ratio between high-load MFR and low-load MFR is used as an indirect index of molecular weight distribution. For film-grade HDPE, this ratio is usually higher than that of injection-molding grades but may overlap with blow-molding HDPE. The extrudate swell measured on a capillary rheometer at 190 °C and 50 s⁻¹ provides additional differentiation: film-grade HDPE typically shows lower extrudate swell than blow-molding HDPE because parison sag resistance is not required. These rheological checks are not a substitute for the full datasheet; they detect lot-to-lot drift when a converter certifies multiple suppliers against Versalis HDPE FC 82.

    Typical end-use categories for this resin class include T-shirt bags, wave-top bags, liners, and light industrial packaging produced on high-stalk or low-stalk blown-film lines. The selection of film structure and thickness is governed by the mechanical performance required in downstream bag-making operations, including tensile yield, tear resistance, and water-vapour transfer rate.

    How does the FC 82 designation separate film-grade HDPE from blow-molding and injection-molding polyethylenes?

    The separation is primarily rheological. Film-grade HDPE is formulated to maintain a stable bubble at high blow-up ratios, which requires high extensional viscosity at draw temperatures but a controlled die swell. Blow-molding HDPE shares the low MFR characteristic but is optimized for sag resistance and parison swell. Injection-molding HDPE is formulated with a higher MFR and a narrower molecular weight distribution to reduce filling pressure and cycle time. Substitution of one HDPE category for another without revalidation alters die pressure, back pressure, melt temperature, and final mechanical properties.

    Class-level differentiation of HDPE categories under ISO 1133-1 and ISO 1183-1
    HDPE category Typical MFR at 190 °C/2.16 kg (g/10 min) Typical density (g/cm³) Critical process requirement
    Film-grade HMW-HDPE 0.15–0.40 0.948–0.955 Bubble stability, low die-lip deposit
    Blow-molding HMW-HDPE 0.20–0.50 0.949–0.957 Parison sag resistance, extrudate swell
    Injection-molding HDPE 20–60 0.950–0.965 Short cycle time, low injection pressure

    The FC 82 suffix should not be interpreted as a nominal melt index. Product nomenclature can overlap with other suppliers; therefore, any incoming substitution must compare density, MFR, high-load MFR, and the relevant mechanical test values on the same film line.

    Rheological and thermal boundaries in blown-film conversion

    On blown-film lines equipped with grooved-feed extruders of L/D 25:1 to 30:1 and barrier screws, the feed zone is normally held at 180–190 °C. The compression and metering zones are operated at 210–230 °C. Melt temperature measured after the breaker plate should remain between 200 °C and 220 °C. Extended residence time above 240 °C can generate gel particles and shift the molecular weight distribution, causing off-specification die pressure and film appearance defects.

    Spiral mandrel dies with a die gap of 0.8–1.2 mm are preferred. Blow-up ratio is generally maintained between 2.5:1 and 4.0:1, and frost line height is stabilized at 6–10 die diameters. Vertical oscillation beyond ±2 die diameters can increase thickness variation and produce visible gauge bands. Internal bubble cooling, when available, stabilizes the bubble and shifts the frost line downward; without internal bubble cooling, the maximum stable take-off speed is lower and the frost line is more sensitive to room air currents.

    The critical shear rate at the die lip limits output. When high-molecular-weight film grades are extruded through narrow die gaps, sharkskin melt fracture can appear at output rates above approximately 1.5 kg/h per centimetre of die circumference, depending on die temperature and resin lot. The corrective sequence begins with raising the die temperature by 5–10 °C, widening the die gap within the specified window, and reducing screw speed. If melt fracture persists, a different resin lot or a processing aid approved for HDPE film extrusion should be evaluated.

    Dynamic melt rheology at 190 °C is often measured on a parallel-plate oscillatory rheometer according to ISO 6721-10 with strain amplitude 5% and angular frequency from 0.1 rad/s to 100 rad/s. In film-grade HMW-HDPE, the storage modulus G′ exceeds loss modulus G″ as frequency increases; the crossover point provides a comparative measure of molecular weight distribution breadth. A grade with a broader MWD shows a lower crossover frequency and a more gradual terminal slope, which correlates with enhanced shear thinning during die extrusion and better bubble stability at high output.

    Extensional viscosity at draw temperatures is not directly captured by MFR. Melt strength measured on an extensional rheometer or a haul-off strand test at 190 °C provides better differentiation among film-grade lots. High melt strength is desirable to resist bubble rupture during draw-down; however, excessive die swell impairs gauge control. Barrier screws with distributive mixing reduce melt temperature fluctuation, but high-shear dispersive mixing sections can generate local temperature spikes of 5–15 °C, which contribute to gel formation and die-lip deposit.

    HDPE is non-hygroscopic, therefore predrying is not normally required. If pellets are stored below dew point or exposed to surface condensation, a dry-air hopper at 60–70 °C for 1–2 h removes surface moisture and prevents bubble defects. Drying must remain below the pellet softening temperature to avoid bridging in the hopper.

    For high-speed bag converting, the coefficient of friction and blocking resistance of the finished film are governed by slip and antiblock additives. Slip additives reduce coefficient of friction by migrating to the film surface; the coefficient of friction is measured according to ASTM D1894, and blocking by ASTM D3354. If the base grade does not contain the required surface additives, a masterbatch is introduced at the extruder hopper. Dispersive quality of the additive masterbatch must be monitored by film optical inspection and coefficient of friction mapping across the layflat width.

    During film property evaluation, tensile yield and elongation are measured according to ISO 527-3 or ASTM D882, dart drop impact by ISO 7765-1 Method A or ASTM D1709 Method A, and Elmendorf tear resistance by ISO 6383-2 or ASTM D1922. HDPE film grades typically display higher tensile modulus and lower water-vapour transmission than linear low-density polyethylene of equivalent thickness, but lower dart impact and lower tear resistance. In downgauged structures, machine-direction tear under ISO 6383-2 can become the limiting property because of orientation effects in the blown bubble. Water-vapour transmission rate is assessed by ISO 15106-3 or ASTM F1249, and oxygen transmission rate by ASTM D3985. The exact values for Versalis HDPE FC 82 must be drawn from the current datasheet; published data for this specific configuration is limited, and lot-to-lot variability should be accounted for in specification agreements.

    Relative to low-density polyethylene, HDPE FC 82 is expected to show higher density, greater tensile yield stress, and lower water-vapour transmission rate, but lower dart drop impact and a more translucent film appearance. Relative to linear low-density polyethylene, the HDPE film shows higher modulus and lower elongation at break. These differences are measurable under ISO 527-3, ISO 7765-1, and ISO 15106-3. Product selections therefore begin with the required material handling performance, not with a simple resin substitution.

    When downgauging below 12 µm, the limiting defects appear as bubble instability and tear anisotropy

    At thickness below 12 µm, the operating window narrows. Bubble instability becomes more sensitive to melt temperature fluctuation; a variation of ±3 °C at the die can shift the frost line and produce gauge bands. Internal bubble cooling stabilizes the bubble and improves heat removal. Without internal bubble cooling, maximum stable take-off speed is reduced and gauge variation may exceed ±5%.

    Die-lip deposit formation on production lines can require cleaning every 6–12 h when the resin contains low-molecular-weight species. A polyolefin purge compound or manual die-face cleaning is used. Repeated mechanical die-lip scraping may damage chrome plating and should be minimized; ceramic-coated lips are preferred when long campaigns are planned.

    Because blown HDPE film displays anisotropic orientation, tear resistance in the machine direction is frequently the first property to fall below specification during downgauging. Converters compensate by blending with 10–20 wt% linear low-density polyethylene or by adjusting blow-up ratio. Such changes also modify tensile yield and water-vapour transmission and therefore require revalidation under the relevant mechanical and food-contact standards.

    Compliance status under food-contact and industrial chemical legislation

    For food-contact applications, HDPE resins intended for packaging must be supported by a supplier statement referencing EU Regulation No 10/2011 and FDA 21 CFR 177.1520. The food-contact status is formulation-dependent; converters must verify overall migration limits and specific migration limits for additives by the methods in EN 1186-1 and EN 13130-1. RoHS Directive 2011/65/EU applies to electrical and electronic equipment packaging only in limited contexts, but heavy-metal restrictions are commonly assessed by EN IEC 62321. REACH compliance is documented through the safety data sheet and extended SDS, including SVHC content below 0.1 wt% per article.

    Compliance checklist matrix for HDPE packaging grade evaluations
    Regulation or standard Scope Typical test method / clause
    EU Regulation No 10/2011 Plastic materials and articles intended for food contact Overall migration by EN 1186-1; specific migration by EN 13130-1
    FDA 21 CFR 177.1520 Olefin polymers in food contact End-use compliance statement; migration testing under relevant food simulants
    REACH Regulation (EC) No 1907/2006 Registration, evaluation, authorisation, and restriction of chemicals SDS and extended SDS; SVHC concentration below 0.1 wt%
    RoHS Directive 2011/65/EU Restriction of hazardous substances in electrical and electronic equipment Heavy-metal screening by EN IEC 62321 where applicable

    On high-output multi-layer blown-film lines, Versalis HDPE FC 82 is typically used as the stiffening substrate layer in structures that combine HDPE with linear low-density polyethylene or low-density polyethylene seal layers. The melt temperature of the HDPE layer is held within the range 200–220 °C, and the die gap is set according to the most shear-sensitive layer. Differences from LLDPE-rich structures appear in tensile modulus and water-vapour barrier: HDPE increases modulus and reduces moisture vapour transmission rate but lowers dart drop impact. Converters using automatic gauge control report that the HDPE layer requires more frequent thickness profile correction than LLDPE because of its higher melt elasticity at low shear. Incompatibility with amine-based additives should be avoided if prolonged high-temperature residence is anticipated; certain amine-based stabilisers can contribute to discolouration and deposition on die lips. Processing aid compatibility should be confirmed with the supplier before trial. Published data for this specific configuration is limited, and processing trials on the target line are required to establish the final operating window.

    Top