Versalis Hdpe Fb 506

Versalis HDPE FB 506

    • Product Name: Versalis HDPE FB 506
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 372894
    Polymer Type High-density polyethylene (HDPE)
    Density 0.953 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Stress At Yield 26 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength At 23 C 10 kJ/m²
    Notched Izod Impact Strength At 20 C 4 kJ/m²
    Shore D Hardness 62
    Vicat Softening Temperature 124 °C
    Melting Temperature 130 °C
    Environmental Stress Cracking Resistance >1000 h
    Bulk Density 0.55 g/cm³
    Water Absorption <0.01%
    Thermal Conductivity 0.35 W/m·K
    Specific Heat Capacity 1.9 kJ/kg·K
    Coefficient Of Linear Thermal Expansion 1.5×10^-4 /°C
    Dielectric Constant At 1 Mhz 2.3
    Volume Resistivity >10^16 Ω·cm

    As an accredited Versalis HDPE FB 506 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE FB 506 is supplied in 25 kg polyethylene bags, palletized and shrink-wrapped for secure transport.
    Container Loading (20′ FCL) 20′ FCL loading: Versalis HDPE FB 506 in 25 kg bags, palletized and stretch-wrapped, secured for sea transport; typical net weight 20–22 MT.
    Shipping Versalis HDPE FB 506 is shipped as non-hazardous, solid high-density polyethylene pellets in moisture-barrier bags, octabins, or bulk containers. It is not classified as dangerous goods under DOT, ADR, IMDG, or IATA regulations. Keep dry, away from ignition sources, oxidizers, UV exposure, and contamination.
    Storage Store Versalis HDPE FB 506 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep bags or containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged outdoor exposure and excessive stacking. Store at ambient temperature, preferably below 50°C, and follow the manufacturer’s SDS.
    Shelf Life Typically 24 months when stored sealed in original packaging, dry, cool, and away from direct sunlight.
    Application of Versalis HDPE FB 506

    All percentage values in the application formulas below are by total formula weight. The grade is evaluated against film extrusion conditions; injection molding and blow molding process data are not part of this section.

    When High-Stalk Film Extrusion Challenges a 12 μm Gauge Target

    HDPE FB506 at nominal density 0.950 g/cm³ and melt flow rate 0.5 g/10 min (190 °C/2.16 kg, ISO 1133-1) is processed on high-stalk blown-film lines for retail carrier bag stock. A representative monolayer formula includes HDPE FB506 82 wt%, C6-LLDPE 14 wt%, slip/antiblock masterbatch 2 wt%, and white color masterbatch 2 wt%. Reducing LLDPE below 10 wt% lowers handle-area weld-out, while exceeding 25 wt% decreases tensile modulus and increases extrusion motor load due to viscosity mismatch. The production line is specified with a barrier screw L/D of 30:1, die gap 1.0–1.2 mm, blow-up ratio 3.5:1–4.0:1, and melt temperature 200–220 °C. A high-stalk configuration with frost-line height 900–1,200 mm above the die is used because the HDPE melt requires a longer deformation path to redistribute gauge; internal bubble stabilization with closed-loop layflat correction maintains gauge variation within ±8% as verified by ASTM D6988. Finished film from this process is converted into die-cut T-shirt bags, wicket-cut produce bags, and perforated checkout roll stock. Compliance testing commonly references ASTM D882 for tensile properties, ASTM D1922 and ISO 6383-2 for Elmendorf tear, ASTM D1709 Method B for dart-drop impact, and EU 94/62/EC for packaging heavy metals with a sum limit of 100 ppm. Pre-drying of the resin is unnecessary below 60% storage relative humidity; condensation on cold granules should be avoided because localized surface moisture creates bubble pinholes at 12–15 μm gauge.

    Representative high-stalk processing window across gauge targets
    Film gaugeBlow-up ratioFrost lineDie gapMelt temperature
    12 μm3.8:11,100 mm1.0 mm210 °C
    25 μm3.2:1950 mm1.2 mm215 °C
    50 μm2.8:1800 mm1.5 mm220 °C

    In three-layer cereal-liner coextrusions, HDPE FB506 is placed in the outer skin to supply crush stiffness and moisture-vapor resistance while an LLDPE or LDPE sealant layer provides hot-tack. A representative five-layer structure uses HDPE FB506 at 52 wt%, LLDPE at 22 wt%, LDPE at 12 wt%, maleic-anhydride tie at 8 wt%, and EVOH with 32 mol% ethylene at 6 wt%. The HDPE skin is extruded through a 40 mm grooved-feed extruder with L/D 30:1 at 215–230 °C; the coex die gap is 1.2–1.8 mm, the blow-up ratio is 2.2:1–2.8:1, and the frost line is kept at 400–600 mm to limit EVOH crystallization. Post-bubble surface treatment to 38–42 mN/m is required before lamination or flexographic printing. Finished forms include cereal box liners, dry-mix pouches, and cracker sleeves. The HDPE layer qualifies under FDA 21 CFR 177.1520(c) for olefin polymers and under EU 10/2011/EC Annex I with overall migration limit 10 mg/dm² for dry food simulants; good manufacturing practice is controlled under EU 2023/2006/EC. Operational boundaries: EVOH viscosity mismatch with HDPE at melt temperatures below 215 °C creates interfacial instability, so screw speed differentials are held within 10% between the HDPE and barrier extruders.

    How Does 30% Regrind Alter Melt Filtration and Bubble Stability?

    Heavy-gauge liners produced from HDPE FB506 typically operate with in-process regrind because edge trim and start-up scrap are re-extruded on the same line. A representative formula for 80 μm drum liners includes HDPE FB506 68 wt%, clean in-house regrind 25 wt%, carbon black masterbatch 4 wt%, fluoropolymer processing aid 1 wt%, and UV-stabilizer masterbatch 2 wt%. The extruder is specified with a 75 mm barrier screw, L/D 30:1, screen pack 60/100/120 mesh, die gap 1.8–2.5 mm, and melt temperature 210–230 °C. Blow-up ratio is held between 2.0:1 and 2.8:1; wider ratios above 3.0:1 increase film curvature and complicate gusset folding. When regrind exceeds 30 wt%, screen-pack pressure rises by 15–25% over 8 h runs, and unmelted gels from oxidized trim appear as fisheyes larger than 0.4 mm; online thickness scanners respond with gauge variation above ±10%. Finished articles include FIBC inner liners, drum liners, and box liners for powder and granular chemicals. Standards applied to final liners include ASTM D5748 for puncture resistance, ASTM D882 for tensile properties, ISO 527-3 for film tensile modulus, and EU 94/62/EC heavy-metal limits. REACH SVHC screening is carried out on the commercial regrind stream before re-introduction to avoid migrating substances from print inks or adhesive labels.

    At calcium carbonate loadings above 50 wt%, the melt strength of HDPE FB506 supports microporous breathable backsheet produced by machine-direction orientation. A representative filled cast-film formula includes HDPE FB506 42 wt%, stearic-acid-coated ground calcium carbonate 50 wt%, C6-LLDPE 5 wt%, TiO₂ white masterbatch 2 wt%, and fluoropolymer processing aid 1 wt%; the calcium carbonate mean particle size is specified at 1.0–1.5 μm with top-cut below 8 μm to prevent screen blockage. The cast film line runs a 90 mm extruder with L/D 30:1, die temperature 230–250 °C, and a chill-roll temperature of 20–30 °C. The primary film is fed to an MDO unit with preheat rolls at 80–100 °C, stretching rolls at 100–120 °C, and annealing rolls at 105–115 °C; the draw ratio is limited to 2.0:1–3.0:1. Above 3.5:1, pore collapse and transverse striping reduce water-vapor transmission rate while increasing machine-direction tear weakness. Current end products are diaper backsheet, adult incontinence film, and feminine hygiene backing. The film is tested for water-vapor transmission according to ASTM E96/E96M Procedure E, tensile properties according to ASTM D882, and peel strength of any adhesive lamination according to ASTM F88; the formulation is screened against REACH SVHC and is offered in grades meeting OEKO-TEX Standard 100 Product Class I for finished hygiene articles.

    Frozen Food Film Structures at Low-Temperature Impact Thresholds

    For frozen-vegetable and IQF liners, HDPE FB506 is blended with LLDPE to reduce brittle failure at storage temperatures of −25 °C to −18 °C. A representative formula has HDPE FB506 60 wt%, C6-LLDPE 25 wt%, LDPE 10 wt%, slip/antiblock masterbatch 3 wt%, and green color masterbatch 2 wt%. Blown-film processing uses a die gap of 1.0–1.8 mm, a blow-up ratio of 2.5:1–3.5:1, a frost line of 500–800 mm, and melt temperature 200–225 °C. The film is run to 35–60 μm; below 25 μm, the HDPE-rich structure exhibits brittle puncture at freezer temperatures unless LLDPE content is raised above 35 wt%. Increasing LLDPE content above 20 wt% improves dart-drop impact and machine-direction Elmendorf tear values, but final values must be established on the production line because gauge, frost line, and die gap shift the result by more than 20%. End products include frozen vegetable bags, IQF fruit pouches, and shrink-free carton liners. Compliance references FDA 21 CFR 177.1520(c) for food contact, EU 10/2011/EC Annex I overall migration 10 mg/dm², and EU 2023/2006/EC for GMP. Because the film is not retorted, migration testing is limited to freezing and room-temperature simulants rather than hot-fill simulants.

    Permeance Testing Separates Under-Slab Film from Packaging Film

    HDPE FB506 is used in construction vapor-retarder sheet at thicknesses of 150–250 μm. A representative formulation includes HDPE FB506 86 wt%, C4-LLDPE 10 wt%, and carbon black masterbatch 4 wt%; no slip or antiblock is added because the film is not wound for high-speed converting. Blown-film lines run with a die gap of 2.0–2.5 mm, blow-up ratio 1.8:1–2.4:1, melt temperature 200–220 °C, and internal bubble cooling. The low blow-up ratio increases machine-direction orientation and lowers water-vapor permeance; finished film is tested according to ASTM E96/E96M Procedure A at 23 °C and 50% RH. Class A vapor retarders under ASTM E1745 require permeance not exceeding 0.300 perm (17 ng/Pa·s·m²). The HDPE film must be free of pinholes; a 10 m² roll is inspected under light-box or high-voltage holiday detection. Terminal articles are under-slab vapor retarders, crawl-space liners, and temporary concrete curing covers. In addition to ASTM E1745, the sheet is screened for REACH SVHC and for recycled content claims under ISO 14021 where applicable.

    Free Quote

    Competitive Versalis HDPE FB 506 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE FB 506 is a high-density polyethylene grade positioned in the manufacturer’s extrusion blow molding portfolio for rigid containers, industrial packaging, and technical hollow parts. The model designation FB 506 identifies a medium-high-molecular-weight product with a controlled molecular weight distribution. Its nominal melt mass-flow rate is 0.30 g/10 min at 190 °C/2.16 kg according to ISO 1133-1, and its nominal density is 0.950 g/cm³ according to ISO 1183-1. These two specifications situate the grade between low-MFR large-part blow molding resins with greater parison melt strength and high-MFR injection molding resins with shorter cycle times but reduced slow crack resistance. The density value supplies top-load and hoop stiffness in stacking applications, while the MFR remains low enough to permit controlled parison sag during accumulator and shuttle press operations. On extrusion blow molding lines with 60–90 mm barrier screws, the reported melt temperature window is commonly 180–230 °C, although head pressure and melt temperature must be verified against the specific screw, die head, and shot size.

    What Separates FB 506 from a Narrow-MWD Injection Molding HDPE?

    The principal difference is molecular weight distribution and its consequences for shear flow and parison stability. FB 506 is designed for extrusion in which shear at the die lip is lower than in injection moulding and in which the parison must survive gravitational stretching before mould closing. A narrow-MWD injection moulding grade with similar density and a melt mass-flow rate of 1.0–2.5 g/10 min does not generate sufficient parison melt strength and typically shows lower notched impact resistance and lower environmental stress crack resistance. At the opposite end, a high-molecular-weight blow moulding grade with an MFR below 0.10 g/10 min provides greater sag resistance but raises extruder torque, melt pressure, and shear heating on the same screw profile. In field transfers between these product types on an 80 mm grooved-barrier extruder with L/D 32:1, die head pressures for medium-MFR blow moulding HDPE typically range from 150 bar to 300 bar, depending on parison programming, die gap, and melt temperature. Published data for this specific FB 506 configuration is limited, and line validation remains necessary.

    Specified Physical and Mechanical Properties

    The following nominal values are drawn from manufacturer technical literature for the grade family and are not batch-release limits. Current certificate of analysis data should be used for production lot acceptance.

    Property Test method Unit Nominal value
    Melt mass-flow rate, 190 °C/2.16 kg ISO 1133-1 g/10 min 0.30
    Density ISO 1183-1 g/cm³ 0.950
    Tensile stress at yield ISO 527-2 MPa 28
    Elongation at break ISO 527-2 % >600
    Flexural modulus ISO 178 MPa 1050
    Charpy notched impact strength, 23 °C ISO 179-1/1eA kJ/m² 15
    Environmental stress crack resistance, 50 °C, 10 % Igepal CO-630 ASTM D1693 h >300
    Vicat softening temperature, 10 N ISO 306/A120 °C 124
    Hardness Shore D ISO 868 — 61

    For tensile yield determination under ISO 527-2, the test speed is commonly 50 mm/min; flexural modulus under ISO 178 is determined with a 2 mm/min loading rate and a 64 mm support span. The notched Charpy specimen under ISO 179-1/1eA carries a 0.25 mm notch radius. These test conditions matter when comparing values from different resin suppliers, because strain rate influences yield stress and flexural modulus in semicrystalline polyethylene.

    Container producers select FB 506 for jerrycans, stackable drums, agricultural chemical bottles, marine fluid containers, and industrial packaging where drop impact and long-term slow crack growth are specified. In blow molded jerrycans with a nominal wall thickness of 1.2–1.8 mm, burst resistance and top-load performance depend strongly on corner radius, pinch-off weld integrity, and parison programming, not only on the resin strength. For rectangular containers, parison programming is used to increase wall thickness at corners; when the die gap is increased by 10–20 % relative to a narrow-MWD grade, the resulting swell compensates for local thinning at pinch-off zones. This experience is based on shuttle blow moulding line behaviour and should be revalidated for accumulator-head machines.

    When Environmental Stress Crack Resistance Governs Container Qualification

    Environmental stress cracking in HDPE is controlled by tie-chain density, molecular weight, and density. FB 506 is evaluated under ASTM D1693 in 100 % Igepal CO-630 at 50 °C; containers exposed to surfactants, mineral-oil-based formulations, or agrochemical adjuvants use this test as a screening parameter. However, the ESCR result does not guarantee compatibility with aggressive media containing aromatic hydrocarbons, chlorinated solvents, or strong oxidising acids. For such media, full-container immersion testing according to ASTM D543 or the end-use specification is required. The grade should not be used in continuous contact with these chemical classes above ambient temperature without validation. Compared with lower-density PE grades, the density of 0.950 g/cm³ raises stiffness while retaining a slow crack resistance level appropriate for industrial containers; increasing density further would reduce ESCR, whereas lowering density would sacrifice top-load capacity. This balance is the key distinction from commodity HDPE grades used in film or injection moulding.

    Moisture management differs from polar engineering resins such as polyamide or PET. HDPE is not hygroscopic, but surface condensation on cold pellets transferred from outdoor silos into a warm indoor feed hopper can introduce 0.05–0.15 % surface moisture, which is sufficient to create parison microvoids and surface streaks. A hopper dryer at 70–80 °C for 2–4 h is applied when storage or transfer conditions exceed 60 % relative humidity. In continuous extrusion, melt residence time should be minimised. Prolonged hold-up in accumulator heads at melt temperatures above 230 °C can shift MFR upward, generate gel specks, and reduce parison melt strength due to chain scission. Start-up residence time is typically kept below 10–15 min and continuous run residence time below 5 min in production practice.

    Die Swell, Wall-Thickness Programming, and Failure Boundaries in Shuttle Lines

    On shuttle blow molding machines with one or two cavities, parison programming compensates for differential wall thinning at container corners. FB 506 produces moderate die swell due to its molecular weight distribution, which influences final wall distribution more than density alone. When transferring a mould from a conventional narrow-MWD grade, the die gap is often increased by 10–20 % and the melt temperature adjusted downward to increase melt strength without excessive shear. Melt temperatures below 180 °C can generate high backpressure and surface melt fracture in the form of shark-skin on parisons; melt temperatures above 220 °C can produce excessive sag and reduce die swell. A controlled melt temperature window of 185–215 °C is therefore typical for the grade in continuous shuttle extrusion, with actual values depending on screw design, die land length, and shot size. At die-lip shear rates in the range 100–1000 s⁻¹, medium-broad HDPE grades exhibit shear-thinning sufficient to reduce viscosity at the die lip without gross melt fracture, but line-specific validation is necessary because die land length and die gap dominate the shear history.

    Differences from other Versalis HDPE products are process-specific. A pipe grade is designed for long-term hydrostatic strength under ISO 9080 and may not survive blow molding with stable parison sag because its molecular architecture is optimised for slow crack growth under constant pressure rather than for swell and sag control. A rotational moulding HDPE powder differs in particle size distribution, stabiliser package, and zero-shear viscosity; it cannot be directly substituted on extrusion blow molding equipment. In contrast, a high-MFR injection grade at 1.0–2.5 g/10 min may be moulded in shorter cycles but fails the ESCR and drop-impact requirements of industrial container specifications. These product-family differences, rather than density alone, define why FB 506 is positioned specifically for extrusion blow molding of medium-volume containers and technical hollow parts.

    Compliance for food-contact use, where claimed, must be verified against the current Versalis product stewardship declaration. The resin can be evaluated under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 for plastic food-contact materials, but specific migration limits depend on the final article surface-to-volume ratio, wall thickness, and food simulant. For industrial containers shipped under UN dangerous goods regulations, qualification testing includes drop, leakproofness, hydraulic pressure, and stack tests on the actual container design; resin type alone does not provide UN certification. Recycled regrind addition should be controlled within the proportion specified by the end-use compliance scheme, because uncontrolled post-industrial regrind can shift MFR and ESCR outside the nominal range and invalidate dangerous goods packaging approvals.