| HS Code | 482541 |
| Product Name | Versalis HDPE DB 506 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 21 6 Kg | 0.25 g/10 min |
| Tensile Stress At Yield | 26 MPa |
| Tensile Strain At Yield | 9% |
| Flexural Modulus | 1200 MPa |
| Izod Notched Impact Strength At 23 C | 20 kJ/m² |
| Izod Notched Impact Strength At 30 C | 5 kJ/m² |
| Vicat Softening Temperature | 125 °C |
| Shore D Hardness | 62 |
| Melting Temperature | 130 °C |
| Environmental Stress Cracking Resistance F50 10 Igepal | >1000 h |
As an accredited Versalis HDPE DB 506 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE DB 506 is supplied in 25 kg polyethylene bags, typically palletized and stretch-wrapped for industrial transport. |
| Container Loading (20′ FCL) | Versalis HDPE DB 506 loaded in 20′ FCL: 25 kg bags, palletized and shrink-wrapped, securely stowed for sea transport. |
| Shipping | Versalis HDPE DB 506 is shipped as non-hazardous solid polyethylene pellets in 25 kg moisture-proof bags, octabins, or bulk trucks. It is not regulated for transport. Keep dry, cool, ventilated, and away from ignition sources, direct sunlight, and contamination. No special dangerous goods documentation required. |
| Storage | Store Versalis HDPE DB 506 indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers tightly closed on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and contact with strong oxidizers. Protect from physical damage. Follow the supplier’s safety data sheet. |
| Shelf Life | Recommended shelf life is typically 24 months when stored dry, in original unopened packaging, away from heat and direct sunlight. |
Extrusion blow moulding of UN-certified jerry cans in the 5 L to 30 L range from DB 506 uses accumulator-head machines with grooved-barrel extruders of 24:1 L/D to generate sufficient melt homogeneity for parison programming. Melt temperature measured at die entry is held at 185–205 °C, while mould temperature is kept between 10 °C and 16 °C to accelerate pin-off cooling without inducing internal voids. The critical failure mode in drop testing is not tensile rupture but weld-line separation at the pinch-off and handle pinch areas. Wall thickness at these nodes is controlled through parison programming with 15–20 radial points; die gap for a 20 L shot is set to 2.0–3.5 mm. Typical clamp force ranges from 350 kN to 500 kN, and blow pressure is 0.7–0.8 MPa. Production experience shows that failure at the handle pinch occurs when the parison is stretched beyond 2.5:1 draw ratio before mould closure.
Formulation for UN containers is normally virgin DB 506 combined with 20–30 wt% clean post-industrial regrind from the same container line, sieved to 2 mm and produced without mineral oil contact. Carbon black masterbatch is added at 1.5–2.5 wt% when outdoor stacking is specified. Melt flow rate of the dry blend is verified at 190 °C under 2.16 kg according to ISO 1133-1:2022; values outside 0.2–0.3 g/10 min correlate with handle-area thinning and should be rejected for this load case. Finished containers are leak-tested at 20 kPa internal air for 15 s and drop-tested according to UN Model Regulations 6.1.3. Top-load creep is not covered by drop testing and must be checked separately at 40 °C for 28 days with a fixed load of 250 N on the container closure.
In detergent and surfactant packaging, the controlling material property is environmental stress-cracking resistance under circumferential stress, not short-term burst strength. Bottles blow-moulded from DB 506 for laundry detergent, liquid dishwashing concentrate, and quaternary ammonium disinfectant formulations are processed at a melt temperature of 190–205 °C and a mould temperature of 15–20 °C. Mould temperatures below 15 °C are avoided in monolayer structures because oriented skin layers can reduce crack initiation time when the bottle is stored with 2–5% non-ionic surfactant at 40 °C. Stress-cracking resistance is measured according to ASTM D1693 condition B at 50 °C; the F50 value for this molecular-weight class is typically reported above 100 h, though published data for DB 506 under specific alcohol ethoxylate loads is limited. The dominant failure mode in field returns is not burst but pin-hole cracking 2–3 mm from the parting line, initiated by top load during capping and retained detergent film.
Formulation uses 1.0–2.0 wt% white masterbatch for opacity and, in three-layer coextruded bottles, up to 10 wt% clean regrind in the middle layer only. The outer visual layer is kept virgin to avoid surface defects that act as stress risers. Bottles are leak-tested at 20 kPa for 15 s after trimming. To reduce parting-line cracking, the pinch-off flash land is increased to 1.5–2.0 mm and line speed is reduced to maintain a weld-line temperature above 120 °C at the moment of knife trim.
Agricultural chemical packaging for emulsifiable concentrates, suspension concentrates, and oil flowables demands a separate compatibility envelope. Containers of 5–10 L based on DB 506 are produced on continuous extrusion blow moulding lines with 65–80 mm grooved-barrel extruders, melt temperature 190–205 °C, and parison programming aligned to offset neck tooling. Monolayer HDPE is not barrier-complete for emulsifiable concentrates containing xylene or aromatic hydrocarbon solvent. For those products, the blow-moulded container is fluorinated in a separate chamber with 0.1–0.5% fluorine in nitrogen for 3–10 min depending on wall thickness. Without surface fluorination, solvent uptake can reach 5–8 wt% after 28 days at 40 °C, causing panel deformation and volumetric distortion above 3%. The fluorinated layer reduces solvent permeation to less than 0.5 g/m²·day at 23 °C for the specific solvent mixture used in the commercial formulation.
Formulation for agrochemical containers includes 0.8–1.5 wt% UV stabilizer masterbatch and 1.0–2.0 wt% colour masterbatch. Regrind from fluorinated containers is excluded from the outer layer unless the fluorinated skin is mechanically removed, because retained fluorine at the surface can affect interlayer adhesion. Finished containers are qualified by performing the UN Model Regulations 6.1.3 drop test after 28-day storage with the actual formulation at 40 °C, not with water only. Closure seal integrity is monitored by weight loss after 28 days at 40 °C; the acceptance limit is 0.5% of initial package weight. This segment operates at the upper limit of monolayer HDPE capability, and containers for highly volatile solvent mixtures are shifted to coextruded barrier structures when permeation exceeds 1.0 g/m²·day.
Windshield washer reservoirs, coolant recovery bottles, and SCR feed containers for off-road vehicles place long-term thermal ageing under water–glycol mixtures on blow-moulded HDPE. Production of DB 506 automotive parts on single-head machines with suction blow moulding or 3D manipulation uses die-entry melt temperature 195–210 °C and mould temperature 12–18 °C. The pinch-off is designed with a 2–3 mm flash land to avoid delamination at the welded base during pressure testing. Long-term performance is verified by pressure cycling from 0 kPa to 120 kPa at 80 °C for 50,000 cycles, followed by burst testing above 250 kPa at 23 °C. Slow crack growth resistance is assessed by the full notch creep test per ISO 16770:2019, as automotive reservoirs fail by creep rupture at the boss weld rather than by Izod impact. Formulation uses 0.5–1.0 wt% heat stabilizer masterbatch for coolant exposure at 100 °C and 1.0–2.0 wt% carbon black in under-hood parts. Published data for DB 506 under 50% ethylene glycol at 90 °C is limited, so qualification is performed on finished parts processed from the same batch. Parts are inspected for weld-line thinning at the boss base with a minimum wall thickness acceptance of 70% of the nominal sidewall.
Multi-cavity extrusion blow moulding of small containers up to 1 L from DB 506 introduces shear-history differences between centre and edge cavities. In an eight-cavity setup on a 70 mm extruder with a side-fed die head, the cavity closest to the die pin receives a hotter, lower-viscosity parison segment. The resulting wall thickness difference across mould positions can reach 0.2–0.4 mm and can shift filled-container drop performance from pass to fail under UN Model Regulations 6.1.3. Process correction uses a three-zone die head with die land lengths of 20–25 mm and a pre-blow delay of 0.1–0.3 s. Melt temperature is reduced from 205 °C at the die entry to 190 °C in the outer head zone. This narrows intra-cavity weight variation from ±3.0% to ±1.2%; representative cavity-level data from a single-plant campaign are shown below.
| Mould position | Die land length | Pre-blow delay | Cavity weight variation | Wall thickness spread |
|---|---|---|---|---|
| Centre cavity | 20 mm | 0.1 s | ±3.0% | 0.85–1.05 mm |
| Outer edge cavity | 25 mm | 0.3 s | ±1.2% | 0.95–1.02 mm |
Formulation for this segment is virgin DB 506 with up to 15 wt% regrind from trimmed flash. The regrind is dried to <0.05 wt% moisture; humid regrind creates surface splay and weakens the weld line. End products are 500 mL to 1 L household chemical bottles. Weight distribution is checked after trimming with a check fixture; the acceptance limit for such containers is ±1.0 g. If the eight-cavity tool cannot maintain this spread, the edge cavities are blocked to restore uniform clamping and parison release.
Motor-oil and automotive aftermarket fluid bottles in the 1 L to 5 L range are blow-moulded on shuttle machines at high output, but panel deformation after filling is the primary dimensional defect. DB 506 processed at 190–205 °C with a die gap of 1.5–2.5 mm and a mould temperature of 10–15 °C produces sufficient top-load strength; however, hot filling of gear oil at 60–70 °C into a monolayer bottle can cause sidewall vacuum collapse if the closure is tightened before the headspace cools. To suppress collapse, the bottle shoulder is programmed 15–20% thicker than the sidewall and 2–4 vacuum panels are placed in the body. Dimensional stability is checked on a 24 h panel test at 23 °C after 1 h at 60 °C with the closure sealed; acceptable sidewall deflection is set at ≤1.5 mm. Compatibility with lubricant basestocks is assessed by 28-day immersion at 40 °C under ASTM D543-14; weight gain below 0.5 wt% is the typical control limit. Published data for DB 506 under specific API Group II basestocks is limited. The closure seat is flame-treated after trimming to raise surface energy above 42 mN/m for ink adhesion. Regrind from trim is added at up to 20 wt% after passing a 3 mm screen. Finished bottles are used for 1 L, 4 L, and 5 L motor-oil and hydraulic-fluid packages.
Competitive Versalis HDPE DB 506 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDB 506 is supplied as a high-molecular-weight high-density polyethylene pellet for extrusion blow moulding of rigid hollow articles in the 1–30 L range, including industrial containers, household chemical bottles, and packaging where stress-cracking resistance and drop impact are specified. The product is classified under EN ISO 1043-1:2012 as PE-HD, and the producer’s technical bulletin positions it as a broad-molar-mass-distribution blow moulding grade. Under ISO 1183-1, density is typically reported at 0.952 g/cm³; melt-mass flow rate measured at 190°C under a 5 kg load in accordance with ISO 1133-1:2022 is normally near 1.2 g/10 min, while the 21.6 kg value is typically near 9.0 g/10 min. The product therefore occupies the intermediate-viscosity region between high-flow HDPE grades for injection moulding and very low-MFR HDPE grades for 200 L drums. These values are not lot-specific guarantees; the current certificate of analysis and the grade specification govern release testing.
On shuttle blow moulding platforms with clamp forces between 20 t and 30 t, HDB 506 is processed with barrel temperature profiles from 170°C at the feed throat to 195–210°C at the adapter, while the die head is held at 190–205°C. Melt temperature at the die should remain below 220°C to limit oxidative chain scission and odour formation. Blow pressure is commonly set at 0.6–0.8 MPa, with blow ratios between 2.5:1 and 3.5:1 depending on parison length and mould geometry. The screw should provide a compression ratio of 2.5:1 to 3.5:1 and an L/D of 25:1 to 30:1. Pre-drying is not normally required for sealed packaging; however, opened containers stored at relative humidity above 60% can accumulate surface moisture, leading to parison bubbles and splay. Pellet moisture measured by Karl Fischer titration is specified below 0.05 wt% in unopened original packaging.
Regrind levels of 30–50 wt% are used on continuous lines when contamination is controlled through fine-screen packs and magnetic traps. Higher regrind loadings tend to reduce environmental stress-cracking resistance and require adjustment of the parison programmer. In continuous 24 h production, parison hang time is the primary reject criterion; hang times beyond 8 s generate visible wall thinning at the pinch-off and unacceptable top-load variation. Batch-to-batch variation in the 21.6 kg MFR is typically addressed through capillary rheometry checks rather than the 2.16 kg melt index measurement, because the 2.16 kg value approaches the lower resolution boundary of the test for this molecular weight.
The selection of HDB 506 in extrusion blow moulding is governed by melt strength, parison swell, and stress-cracking resistance rather than by tensile yield alone. A unimodal HDPE of similar density and 5 kg MFR typically exhibits lower die swell and shorter hang-time tolerance. The broad molecular weight distribution of HDB 506 gives measured die swell of 30–45% under normal die temperatures, requiring tooling with smaller die-core diameters and active parison programming to maintain wall uniformity. This behaviour is advantageous in tall containers where the parison must support its own weight for several seconds without excessive drawdown. On a single-head shuttle machine, the difference between acceptable and unacceptable pinch-off wall thickness is often less than 0.15 mm, so parison program steps are set in 10–20 ms increments.
Compared with high-flow HDPE blow moulding grades having 2.16 kg MFR values above 1.0 g/10 min, HDB 506 shows lower melt flow but greater environmental stress-cracking resistance under ASTM D1693B. Conversely, compared with drum-grade HDPE having 21.6 kg MFR values below 6.0 g/10 min, HDB 506 permits shorter cooling cycles for containers up to 30 L but does not supply sufficient parison stability for very large accumulator-head parts with shot weights above 10 kg. Published data for the exact shear-viscosity curve of HDB 506 in small-amplitude oscillatory rheometry is limited; when mould-filling simulation is required, capillary rheometry at 190°C, 210°C, and 230°C should be conducted on the actual lot.
Within rigid packaging plants running 24 h cycles, the limiting process condition is usually parison sag rather than melting rate. Melt pools in the die head are maintained between 185°C and 200°C; exceeding 210°C for extended hold times causes discoloration and lowers the melt strength that protects against drawdown. When back-pressure is increased above 20 bar to improve homogenization, screw speed must be reduced to avoid excessive shear heating. The use of grooved-feed extruders with 25:1 length-to-diameter ratio provides stable output but can raise melt temperature by 5–8°C at high screw speed, so barrel cooling zones are applied in the feed section.
In blow moulding trials, the practical lower wall thickness for HDB 506 is constrained by environmental stress-cracking performance rather than by tensile failure. For aggressive liquid formulations, a formed-container ESCR test is more informative than a plaque test because parison orientation and pinch-off welds create craze initiation sites that do not exist in compression-moulded specimens. The producer’s datasheet values should not be applied to stacked containers without verifying creep behaviour under sustained top load using ISO 12048 or ASTM D2659.
In accumulator-head machines, the parison is extruded from a ring die with die gaps typically set 30–50% larger than the intended part wall thickness. Die swell of HDB 506 at output rates between 50 kg/h and 150 kg/h depends on shear rate and die land length; longer lands of 15–25 mm reduce swell but raise head pressure. For a 1 L bottle weighing 38 g, the wall thickness distribution can shift by 0.1 mm when melt temperature changes by 5°C, so temperature control within ±3°C at the die is required to keep part weight within specification. During parison programming, the die gap is closed to 40–60% of the initial opening near the pinch-off zone to compensate for parison sag.
The table below summarizes representative datasheet property values for extrusion blow moulding grades and should not replace the current Versalis certificate of analysis.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density at 23°C | ISO 1183-1 | 0.952 | g/cm³ |
| Melt-mass flow rate, 190°C/5 kg | ISO 1133-1:2022 | 1.2 | g/10 min |
| Melt-mass flow rate, 190°C/21.6 kg | ISO 1133-1:2022 | 9.0 | g/10 min |
| Tensile yield stress | ISO 527-2 | 27 | MPa |
| Elongation at break | ISO 527-2 | 800 | % |
| Flexural modulus | ISO 178 | 1200 | MPa |
| Notched Charpy impact, 23°C | ISO 179-1 | 24 | kJ/m² |
| Notched Charpy impact, -30°C | ISO 179-1 | 5–7 | kJ/m² |
| Environmental stress cracking resistance, 100% Igepal CO-630, condition B | ASTM D1693B | >600 | h |
| Vicat softening temperature, A50 | ISO 306 | 127 | °C |
The low-temperature impact value is included because containers shipped in cold climates can fail at -30°C even when ambient impact is acceptable. The Charpy value alone does not fully define drop impact; formed-container testing at -20°C with a specified drop height is required for hauler or automotive applications.
When HDB 506 replaces a lower-ESCR incumbent material, downgauging should be validated against top-load and drop-impact requirements rather than by density alone. A wall-thickness reduction from 1.2 mm to 0.9 mm can reduce top-load capacity by approximately 30–40% because stiffness scales with the cube of wall thickness. For rectangular containers with large flat panels, the limiting criterion is often vacuum deformation or sidewall buckling, not pinch-off strength. In these cases, finite-element buckling analysis should be calibrated with physical top-load testing under ISO 12048. Blow-moulded HDB 506 surfaces may orient to different degrees depending on parison inflation rate and cooling rate; therefore, data obtained on compression-moulded plaques should not be extrapolated to corner sections without verification.
For oil-based and surfactant-based products, medium-to-high density HDPE grades such as HDB 506 offer adequate short-term hydrocarbon resistance, but adverse storage conditions can produce slow crack growth at moulded-in stresses. The relevant failure mode is often environmental stress cracking at the pinch-off weld, which is best evaluated using ASTM D1693B on specimens cut from the container, or ISO 22088-2 for comparative screening. If the product is used with concentrated nitric acid or strong oxidizing agents, published compatibility data for HDPE generally does not cover formed-container welds; specific chemical storage tests should be run at the intended temperature and stack load.
| Compliance area | Standard or regulation | Applicability |
|---|---|---|
| Material designation | EN ISO 1043-1:2012 | PE-HD |
| Melt-flow classification | ISO 17855-2 | Polyethylene moulding and extrusion material |
| Melt-mass flow rate | ISO 1133-1:2022 | Routine lot release and incoming inspection |
| Density | ISO 1183-1 | Method A, immersion at 23°C |
| Tensile and elongation | ISO 527-2 | Type 1B specimen, 50 mm/min |
| Flexural modulus | ISO 178 | Three-point bending, 2 mm/min |
| Impact resistance | ISO 179-1 | Notched Charpy, edgewise impact |
| Environmental stress cracking | ASTM D1693B or ISO 22088-2 | Bent strip under alkylphenol surfactant |
| European food-contact migration | Regulation (EU) No 10/2011, EN 1186-1 | HDPE compliance requires overmoulding or conversion testing |
| United States food-contact resin | 21 CFR 177.1520 | Olefin polymers, conditions of use by container design |
| REACH registration | Regulation (EC) No 1907/2006 | Product as imported polymer |
| RoHS restricted substances | Directive 2011/65/EU | Cadmium, lead, mercury, hexavalent chromium limits |
| Vicat softening temperature | ISO 306 | Method A50, 10 N load |
During conversion trials, the limiting process condition is often heat removal from the pinch-off and handle regions rather than melting rate. Mould cooling water at 10–30°C with high-turbulence channels is applied to keep cycle times within the productivity window; warmer mould surfaces above 40°C increase gloss but extend cooling time and can cause post-mould shrinkage. Published data for oxygen and hydrocarbon permeation of HDB 506 in formed containers under ASTM D3985 or DIN 53380-2 is limited; qualification should therefore use formed-container transmission testing rather than plaque-derived coefficients. Moisture, residence time, and regrind limitations define the operational envelope more tightly than melt temperature alone. For a candidate container, the specification should include formed-part ESCR under ASTM D1693B, cyclic top load under ISO 12048, and drop-impact testing at -20°C using a drop height and filling medium agreed with the converter.