| HS Code | 855068 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.25 g/10 min |
| Melt Flow Rate 190 C 21 6 Kg | 20 g/10 min |
| Tensile Modulus | 1100 MPa |
| Tensile Stress At Yield | 27 MPa |
| Tensile Strain At Break | >600% |
| Charpy Notched Impact Strength 23 C | 15 kJ/m² |
| Charpy Notched Impact Strength 30 C | 5 kJ/m² |
| Vicat Softening Temperature | 126°C |
| Melting Temperature | 130°C |
| Environmental Stress Crack Resistance | >1000 h |
| Hardness Shore D | 62 |
As an accredited Versalis HDPE COM75HM1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE COM75HM1 is typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe and secure transport. |
| Container Loading (20′ FCL) | Versalis HDPE COM75HM1 is loaded in 20′ FCL containers, typically as palletized 25 kg bags, about 20–22 metric tons per container. |
| Shipping | Versalis HDPE COM75HM1 is shipped as solid high-density polyethylene pellets, non-hazardous. Not regulated for transport by DOT, IMDG, IATA, or ADR/RID. No UN number, hazard class, or packing group. Ship in original sealed bags or octabins; keep dry and away from heat, sparks, and sunlight. |
| Storage | Store Versalis HDPE COM75HM1 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and high temperatures. Maintain clean, segregated storage and follow first-in, first-out inventory practices. Consult the SDS for specific handling and local regulations. |
| Shelf Life | 24 months from production date when stored in unopened original packaging, dry, well-ventilated, and away from direct sunlight. |
Versalis HDPE COM75HM1 is specified for high-cavitation beverage closure production in both rotary compression and injection-compression tooling. In compression lines, pellets are melted in a grooved-barrel extruder with a screw length-to-diameter ratio of 24:1 to 30:1, a compression ratio of 3:1 to 4:1, and a melt temperature at the extruder outlet of 200–230°C. The melt is then cut by a plunger dosing system and transferred into a rotary tool with cavity counts from 96 to 192. The compression force is controlled by cam profile and die movement, and closure weight is maintained within ±0.02 g. In injection-compression tooling, the resin is fed through a hopper with magnetic bar separation and into an injection unit using a screw length-to-diameter ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.5:1. The barrel profile from feed to nozzle is normally set at 180–200°C, 200–220°C, 210–230°C, and 220–240°C. Melt temperature at the nozzle is held within ±5°C of the supplier-recommended midpoint because gate-to-gate viscosity mismatch governs diametrical shrinkage and tamper-evident band roundness. Back pressure is maintained from 20 bar to 60 bar, and screw peripheral velocity is limited to 0.3 m/s to 0.6 m/s to avoid shear heating and molecular weight degradation. No drying is normally required when surface moisture is below 0.05% by weight, but hopper heating and dry-air purging are applied in high-humidity assembly areas where condensation on cold regrind can exceed that threshold. The mould is operated with core temperatures from 10°C to 30°C and cavity temperatures from 10°C to 40°C. Cooling time is established by gate-freeze study and cannot be shortened below the point at which closure weight variation across a 64-cavity tool exceeds 0.2%. Injection velocity is profiled to fill the ring gate quickly, then reduced after 70–80% of shot volume to prevent jetting and flow marks. Hold pressure is switched over by screw position, typically at 10–20% of the shot volume remaining, and set between 50% and 70% of peak injection pressure. Shrinkage of closure threads is measured to ASTM D955-08 and must be correlated with mould dimensions because HDPE post-mould crystallisation continues for 24–48 h and can change thread tightness. The main processing conflict is between tamper-evident band flexibility and top-load strength. When the band root is cooled too aggressively, frozen-in orientation raises stiffness and lowers ductility. When it is cooled too slowly, cycle time rises and straightness of the band circumference degrades. For that reason, mould builders often separate the core cooling circuit between the plug seal and the band root and run the band root 2–5°C warmer than the plug area. Published data for this specific configuration is limited and must be validated on the production line.
Thin-walled container moulding with COM75HM1 shifts the process constraint from thermal stability to flow-length-to-wall-thickness ratio and plate-out. In a two-cavity stack mould with hot-runner valve gates, the lower wall is often pushed from 0.6 mm to 0.8 mm for round tubs and from 0.8 mm to 1.0 mm for rectangular bases. The injection pressure required to fill a 500 mL round tub at melt temperature 210°C increases non-linearly as wall thickness drops below 0.8 mm, because the frozen layer occupies a larger fraction of the cross-section. High-speed filling is used, with injection time of 0.3–0.7 s, followed by immediate hold-pressure transition to avoid overpacking the gate bloom. The mould temperature is kept between 10°C and 30°C, but high-tonnage machines are required because cavity pressure can exceed 800 bar during short filling. The gate type is critical: a direct sprue gate produces a visible boss that violates stackability, while a hot-tip gate of 0.5–0.8 mm diameter reduces boss height but can freeze before adequate hold pressure is applied. COM75HM1 lot-to-lot viscosity changes are controlled by MFR testing to ISO 1133-1:2022, but thin-wall processing requires additional check of capillary viscosity at high shear because MFR at low shear does not fully predict filling pressure. Warpage in rectangular tubs arises from differential shrinkage between the sidewall and the base; the correction is made by holding at low pressure and by using an ejection temperature below the Vicat softening point measured under ISO 306. The target part should be ejected only when the surface temperature is below 50–60°C to avoid ring deformation and sidewall concavity. The use of regrind up to 30 wt% is common in thin-wall packaging, but it narrows the molecular weight distribution sufficiently to alter the onset of sharkskin at high injection speeds. Published data for this specific configuration is limited; the processor must establish a high-shear viscosity curve on a capillary rheometer before tool commissioning.
For industrial pails and drum lids, COM75HM1 is processed through a cold runner or hot valve gate with wall sections from 1.5 mm to 3.0 mm, which shifts the dominant problem from filling pressure to sink marks and environmental stress crack resistance. The pail body is normally moulded with a centre or tunnel gate, a screw recovery time longer than cooling time, and a cushion of 3–6 mm. Sink marks over ribs and handle bosses are controlled by holding pressure, not by increasing melt temperature, because excessive melt temperature reduces ESCR and can generate odour. A typical hold pressure is 500–700 bar at the hydraulic cylinder, but this must be converted to cavity pressure rather than copied from machine to machine. Handles are moulded in a separate injection step or inserted as a premoulded part, and the hinge area benefits from a radius of not less than 1.0 mm to avoid notch sensitivity. ESCR data generated under ASTM D1693-15 condition B have more practical value than short-term impact data for pails carrying surface-active liquids; lot certificates should be reviewed for F50 values before material qualification. If a pail is exposed to stack-on-drum compression, top load is measured by column crush on a calibrated compression tester and compared with the filled-container mass. The minimum cooling time is determined by the thickest section, not by the average wall; a 3.0 mm boss can require twice the cooling time of a 1.5 mm wall. Ejection temperature is kept below 65°C to prevent boss pull-out and gate-stringing. When regrind is used in pail production, the proportion should not exceed 20 wt% unless the moulding trial demonstrates no loss in ESCR after three passes, because oxidation during repeated extruder residence reduces slow-crack-growth resistance more than it lowers melt viscosity. No universal limit can be assigned without lot-specific data; the extended granulation and blending history on the shop floor is part of the material record.
Returnable crates produced from COM75HM1 are normally gated through a central sprue or hot-runner drop into a base with integrated corner ribs. The main engineering requirement is cold impact retention after repeated washing and exposure to ambient temperatures down to -20°C. The grade is characterised by a high crystallisation rate, which means thick corner intersections retain heat longer than the sidewall and can exhibit sink marks and internal voids if the holding pressure decays too early. Mould temperature control is normally separated into two circuits: core circuit at 10–20°C and cavity circuit at 15–30°C to reduce warpage. The melt temperature is held in the range 220–240°C at the nozzle, with the exact setting determined by the cold impact target. Low melt temperature preserves molecular weight but increases gate stress and can produce craze networks at the gate. High melt temperature improves fill of ribs and reduces weld line visibility but can reduce Charpy impact measured under ISO 179-1/1eA. Weld lines remain the limiting defect in crates with handle openings, because the flow fronts recombine at low pressure and form a plane of weakness perpendicular to the load. The gate should be positioned so that weld lines fall in low-stress zones; the position is validated by drop testing at -20°C and by sectioning the part for void content. A cushion of 4–8 mm and a screw length-to-diameter ratio of 20:1–24:1 are used to maintain shot consistency. Recycled material and regrind can be incorporated into logistics crates when an ESCR test under ASTM D1693-15 condition A or B demonstrates that the blend remains above the user minimum F50 requirement. The use of external lubricants or processing aids should be avoided unless their concentration is below 0.1 wt%, because lubricants can migrate to the surface and reduce the coefficient of friction required for stable pallet stacking. Stacking load at elevated warehouse temperatures is separately assessed by sustained compression at 40°C and 70% relative humidity. Published data for this specific configuration is limited, so crate producers should carry out batch-to-batch verification of cold impact and ESCR on the same lot used for production qualification.
Household appliance components moulded from COM75HM1 include washing machine pump housings, refrigerator shelf frames, and base plates where resistance to alkaline detergents and dimensional stability at moderately elevated temperatures are specified. Dimensional stability in these parts is governed by post-mould crystallinity, not simply by the moulding shrinkage measured after 24 h. A pump housing must fit a radial seal; if the material is ejected too hot or if packing is insufficient, creep relaxation over 48 h can reduce the outer diameter below the sealing limit. The moulding protocol is therefore based on a stabilisation period of 48 h at 23°C ±2°C and 50% ±5% relative humidity, after which critical dimensions are measured with a dial indicator. The holding pressure is set to produce a gate-seal time that extends 0.2–0.5 s beyond the observed gate freeze, because HDPE has a large volume change during crystallisation and any packing shortfall creates microvoids in the thick flange. Melt temperature is normally 220–240°C; mould temperature is 20–40°C. The lower mould temperature in this range increases cooling rate but also produces a less crystalline skin, while the higher temperature enables greater crystallinity but increases overall cycle time. The balance is judged by differential scanning calorimetry on moulded specimens under ISO 11357-3:2018. The presence of long-chain branching in high-density polyethylene is not required for these components, but the narrow molecular weight distribution of a medium-flow grade demands stable screw rotation; variations in screw recovery time above ±0.5 s are correlated with check-ring wear. The component must be checked for dishwasher detergent exposure because alkaline solutions can induce stress cracking at sharp corners; a radius of 1.0 mm or more is preferred where a boss meets a flat surface. If the part is used in contact with hot water, the continuous-use temperature should not exceed 60°C for unstressed sections and should be reviewed if service exceeds 45°C under sustained load. Where the appliance part is electrical, the finished component must be assessed against RoHS Directive 2011/65/EU Annex II limits for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE. Published data for this specific configuration is limited; appliance manufacturers normally perform their own joint-ring creep tests over 1,000 h.
Pharmaceutical closure systems impose simultaneous requirements for seal integrity, torque retention, and controlled extractables. When COM75HM1 is used in child-resistant and tamper-evident caps, the material is processed at the lower end of the melt-temperature window, typically 200–220°C, to limit oxidative degradation products that could appear as extractables. The mould is run at 10–25°C to reduce cycle time and maintain the geometric precision required for ratchet engagement. Torque retention is evaluated by repeated on-torque and off-torque testing with a torque tester after conditioning at 40°C and 75% relative humidity for 14 days; the cap must not lose more than the agreed percentage of its initial removal torque, and the lot must show no stress whitening at the internal lugs. The material is normally supplied with a stabiliser package whose migration limits are assessed under USP <661.1> and Ph. Eur. 3.1.3. Overall migration into food simulants is determined under EN 1186-1:2002 with a limit of 10 mg/dm² for packaging under EU 10/2011. In the United States, the olefin polymer base resin must comply with 21 CFR 177.1520; however, the finished closure system must be tested as a complete article because colourants, masterbatches, gaskets, and processing aids can change the migration profile. The compliance matrix below summarises the main laboratory tests used for this downstream segment.
| Regulation or method | Measured attribute | Typical limit or condition |
|---|---|---|
| 21 CFR 177.1520 | Olefin polymer food-contact suitability | Resin composition complies with specified olefin polymer provisions |
| EU 10/2011 / EN 1186-1:2002 | Overall migration | ≤ 10 mg/dm² for food simulant under the intended contact time |
| USP <661.1> | Extractables and physicochemical suitability | Meets pharmacopoeia limit for plastic packaging components |
| Ph. Eur. 3.1.3 | Polyolefin additive and heavy-metal release | Meets monograph requirements for plastic containers |
| ISO 1133-1:2022 | Melt flow rate | Lot-specific within supplier specification |
| ASTM D1693-15 | Environmental stress crack resistance | Lot-specific F50 under condition B |
| REACH Article 33 | Substances of very high concern | Notification required above 0.1 wt% per article |
Closure dimensions for child-resistant systems are checked with go/no-go thread gauges at 23°C ±2°C and 50% ±5% relative humidity after 48 h stabilisation. Dimensional acceptance limits must account for post-mould shrinkage of 1.5–2.5% and anisotropic shrinkage between the threaded ring and the top panel. Torque testing is carried out with a closure torque analyser operating at 1.0 rpm, with removal torque recorded after 180° initial rotation. Seal integrity is then tested by vacuum decay on a closed bottle at -0.2 bar gauge for 30 s. The use of external lubricants such as erucamide or oleamide is not permitted unless migration is specifically evaluated, because these additives can reduce the coefficient of friction needed for child-resistant lugs and alter the measured removal torque. Published data for this specific configuration is limited; pharmaceutical customers qualify each lot with the finished closure dimensions and the migration test protocol approved for the target market.
Competitive Versalis HDPE COM75HM1 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The Versalis HDPE COM75HM1 grade is positioned as a high-molecular-weight high-density polyethylene copolymer for extrusion blow moulding, particularly where low melt flow under a 2.16 kg load is combined with high-load melt fluidity. The grade is supplied in pellet form. Published property data for this specific configuration are limited; therefore, class-typical values for high-molecular-weight HDPE copolymers are referenced below and should be confirmed against the current Versalis technical datasheet. The product identity is established through density by ISO 1183-1:2019, melt flow rate by ISO 1133-1:2022, and tensile yield by ISO 527-2:2012. Its differentiation from general-purpose HDPE injection grades and from standard blow moulding grades rests on molecular weight distribution, comonomer placement, and the resulting balance between melt strength, environmental stress crack resistance, and stiffness.
Large-part blow moulding operations in agricultural chemical packaging and automotive fuel tanks expose the material to continuous contact with aggressive media and to stress concentrations at pinch-off welds. The product is evaluated in these applications using ASTM D1693-15 for environmental stress crack resistance and ISO 179-1:2010 for notched Charpy impact. For automotive fuel tanks, wall-thickness distribution is controlled by parison programming; the high-molecular-weight fraction allows a thinner parison without immediate rupture at hang times above 10 s. The same molecular architecture raises the energy required for rapid crack propagation, which is relevant to drop-impact tests at -40 °C according to original equipment manufacturer specifications. Published data for this specific grade’s fuel barrier properties after fluorination or sulfonation treatment is limited; those surface treatments are not required for all container types.
The differentiation is operational rather than nominal. Where a standard unimodal blow moulding grade may exhibit a melt flow rate of 0.3 g/10 min to 1.2 g/10 min at 190 °C and 2.16 kg, a high-molecular-weight HDPE copolymer typically falls below 0.1 g/10 min under the same condition because the long-chain fraction governs low-shear viscosity. The practical consequence appears in parison hang time and die swell. On accumulator-head machines with shot capacities above 10 L, the low-shear viscosity retards sag; however, the same property raises extrusion torque and melt temperature at screw speeds above 60 rpm on a 90 mm grooved-barrel extruder. The comparison is made against homopolymer HDPE injection grades with melt flow rates of 7 g/10 min to 20 g/10 min at 190 °C and 2.16 kg, which provide low injection pressure but insufficient melt strength for large-part blow moulding.
The table below reports class-typical ranges for high-molecular-weight HDPE copolymers; grade-specific values must be taken from the Versalis technical datasheet.
| Property | Standard | Typical HM-HDPE Copolymer Class Range | Processing Relevance |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.945–0.955 g/cm³ | Governs stiffness, chemical resistance, and top-load performance |
| Melt flow rate at 190 °C / 2.16 kg | ISO 1133-1:2022 | <0.1 g/10 min | Indicates high low-shear viscosity and melt strength |
| Melt flow rate at 190 °C / 21.6 kg | ISO 1133-1:2022 | 5–10 g/10 min | Correlates with accumulator filling and high-shear flow |
| Tensile yield stress | ISO 527-2:2012 | 20–28 MPa | Used to estimate short-term container wall strength |
| Flexural modulus | ISO 178:2019 | 800–1100 MPa | Relevant to stacking load and creep resistance |
| Notched Charpy at 23 °C | ISO 179-1:2010 | >20 kJ/m² | Indicates resistance to impact at ambient temperature |
| Environmental stress crack resistance F50 | ASTM D1693-15 condition B | >500 h | Critical for detergent, agricultural chemical, and fuel packaging |
| Vicat softening temperature A50 | ISO 306:2022 | 120–130 °C | Defines short-term thermal deformation limit |
Extrusion blow moulding with COM75HM1-class material is normally carried out on accumulator-head machines with a grooved-barrel feed zone and barrier screws having L/D ratios from 24:1 to 30:1. The recommended barrel profile is set below 230 °C in the feed zone and raised to between 190 °C and 220 °C in the metering section; head and die zones are typically held between 190 °C and 210 °C. Melt temperature measured with an immersion probe at the die exit should not exceed 230 °C during continuous operation. The melt pressure before the accumulator head commonly rises above 25 MPa when the die gap is reduced below 2 mm; pressure fluctuations larger than 5% of the running average indicate feed instability, worn screw elements, or insufficient backpressure control.
On large automotive tank or industrial container lines, the simultaneous demands of low sag and high inflation uniformity create a narrow operating envelope. A high-molecular-weight HDPE copolymer with a high-load melt flow rate of 6 g/10 min to 9 g/10 min at 190 °C and 21.6 kg can fill the accumulator rapidly while the long-chain fraction supports the hanging parison. Melt strength is measured by a Rheotens device after a capillary rheometer; acceptable draw-off force is established against the machine-specific hang time and die gap rather than a universal threshold. Machine trials on accumulator-head units with 70 mm to 120 mm grooved-barrel extruders show that screw speeds above 40 rpm may raise melt temperature by 8 °C to 15 °C above the barrel set point due to viscous dissipation. The processor must compensate by lowering barrel zones, not by increasing throughput beyond the available cooling capacity of the screw core. Die swell values above 55% complicate pinch-off weld quality, while values below 40% reduce wall-thickness uniformity at the flash line. Die design should therefore balance diverging land length and mandrel angle to hold swell within 45% to 55% for moulds with pinch-off flash thickness between 0.3 mm and 0.6 mm.
For sheet extrusion of HDPE COM75HM1-class resin, a flat die with a polished chrome roll stack is used. Melt temperature at the die is maintained between 200 °C and 220 °C, and the roll stack temperatures are set from 60 °C to 80 °C. The low melt flow rate reduces draw resonance at high take-off speeds but also raises die pressure. Therefore, die gap is normally set 0.1 mm to 0.2 mm above target sheet thickness to compensate for die swell. The extruder should have a melt pump before the die to stabilize output; melt pressure variation is held below 0.5 MPa for thickness tolerances of ±5%.
High-molecular-weight HDPE exhibits increased shear heating and reduced thermal uniformity at high output. The practical ceiling is governed by the onset of thermo-oxidative chain scission and crosslinking. In the presence of oxygen, measurable carbonyl formation in the melt begins above 260 °C; therefore, melt temperatures are kept below 230 °C for continuous extrusion and below 240 °C for transient start-up excursions. Residence time in the accumulator head should not exceed 15 min at 220 °C. On a 90 mm single-screw extruder, a screw speed increase from 30 rpm to 70 rpm can raise melt temperature by 10 °C to 18 °C without any change in barrel settings. This is the principal process conflict: the torque limit of the drive and the cooling limit of the screw intersect before the ideal output on many lines. The result is either gel formation in the parison, die-lip build-up, or a loss of high-load melt flow during prolonged runs. Nitrogen blanketing of the hopper and dehumidified hopper drying at 80 °C for 1 h to 2 h are used when surface moisture exceeds 0.05% by weight or when the resin has been stored at relative humidity above 70%.
When compared with an injection moulding HDPE with a melt flow rate of 12 g/10 min at 190 °C and 2.16 kg, the low-flow COM75HM1 class does not suit thin-wall injection moulding below 1.5 mm wall thickness. Injection moulding of the grade-class is technically possible only with large gates, hot runners with internal diameters above 6 mm, and clamp force requirements of 5 kN/cm² to 7 kN/cm² projected area. The material’s high molecular weight increases filling pressure and may produce flow marks at low melt temperatures. Therefore, the product is typically directed to extrusion blow moulding and sheet applications rather than injection moulding. The difference relative to standard HDPE blow moulding grades lies in the high-load melt flow and melt-strength relationship; grades with similar density but lower molecular weight sag excessively at accumulated shot sizes above 20 L. Conversely, the high-molecular-weight grade has a narrower thermal processing window and longer cycle-time potential if the accumulator head is undersized.
Compared with linear low-density polyethylene film grades, the HDPE grade has a higher flexural modulus and lower gas transmission. Tensile modulus according to ISO 527-2:2012 is typically above 800 MPa for the HDPE class, whereas LLDPE values commonly range from 200 MPa to 400 MPa. The trade-off appears in dart impact and puncture resistance; LLDPE retains toughness at lower temperatures, but the HDPE grade provides better top-load strength and lower creep at temperatures up to 60 °C. This difference governs selection for rigid packaging rather than collation shrink film.
Chemical resistance of the grade follows semi-crystalline HDPE behavior. Resistance is evaluated by immersion testing according to ASTM D543-21; mass and dimensional change are measured after contact with representative media. HDPE of this class is generally resistant to aqueous acids, bases, and salt solutions at temperatures below 60 °C, but stress cracking susceptibility increases in the presence of surfactants, esters, ketones, and certain aliphatic hydrocarbons. Environmental stress crack resistance is therefore reported according to ASTM D1693-15, condition B, with F50 values for high-molecular-weight HDPE copolymers commonly above 500 h at 50 °C. For food-contact applications, compliance is product-specific and must be confirmed through Versalis documentation against U.S. FDA 21 CFR 177.1520 and European Commission Regulation (EU) No 10/2011. Industrial compliance screening under REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU is normally included in the safety data sheet and product compliance statement.
During continuous production of regulated packaging, batch-to-batch variance is assessed through high-load melt flow ratio, density, and environmental stress crack resistance. A shift in high-load melt flow rate of more than 0.5 g/10 min at 190 °C and 21.6 kg can change the fill rate of the accumulator and alter parison thickness distribution. A shift in density of 0.002 g/cm³ can be detected as a change in top-load performance and bottle weight. Processors using COM75HM1-class resin in regulated packaging often monitor melt flow ratio, die swell, and wall-thickness distribution at intervals no longer than 2 h. The material is not recommended for combination with amine-based colorants or certain metallic stearates when long-term thermal stability is critical because these additives can destabilize the antioxidant package and reduce oxidation induction time measured by ISO 11357-6:2018. Regrind incorporation is limited by the loss of high-load melt flow after repeated heat history. In-plant regrind of HDPE blow moulding containers is added at 10% to 25% by weight when the regrind high-load melt flow rate remains within 1 g/10 min of virgin resin. Higher loadings increase gel content and reduce parison melt strength; retention is monitored by melt flow ratio, tensile yield, and impact strength per ISO 179-1:2010.