Versalis Hdpe Com75hf2

Versalis HDPE COM75HF2

    • Product Name: Versalis HDPE COM75HF2
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 798491
    Materialtype High Density Polyethylene (HDPE)
    Density 0.975 g/cm³
    Meltflowrate 20 g/10 min (190°C/2.16 kg)
    Tensilemodulus 1400 MPa
    Tensilestressatyield 30 MPa
    Tensilestrainatbreak >500%
    Flexuralmodulus 1300 MPa
    Charpynotchedimpactstrength 4 kJ/m² (23°C)
    Ballindentationhardness 70 MPa
    Shoredhardness 65
    Vicatsofteningtemperature 125 °C
    Heatdeflectiontemperature 75 °C (0.45 MPa)
    Meltingtemperature 133 °C
    Crystallizationtemperature 115 °C
    Waterabsorption <0.01%
    Thermalconductivity 0.4 W/m·K
    Coefficientoflinearthermalexpansion 1.5E-4 /°C
    Volumeresistivity >1E15 ohm·cm
    Dielectricconstant 2.3 (1 MHz)

    As an accredited Versalis HDPE COM75HF2 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE COM75HF2 is typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure industrial handling.
    Container Loading (20′ FCL) Typical 20′ FCL loading for Versalis HDPE COM75HF2: 25 kg bags on pallets, approximately 20–25 metric tons net, subject to carrier limits.
    Shipping Versalis HDPE COM75HF2 is shipped as non-hazardous polyethylene pellets in 25 kg PE bags or octabins, palletized and stretch-wrapped. Transport in clean, dry trucks/containers; protect from moisture, sunlight, and contamination. No special hazardous-goods documentation required. Store cool, dry, ventilated; keep packaging sealed.
    Storage Store Versalis HDPE COM75HF2 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging sealed to prevent moisture, dust, and contamination. Use pallets, stack safely, and follow first-in, first-out rotation. Avoid prolonged UV exposure, outdoor storage, and temperatures that may degrade the polymer. Ensure a clean, compatible storage area; protect bags from punctures.
    Shelf Life Shelf life is typically 24 months when stored in original packaging, dry, cool, below 40°C, away from direct sunlight.
    Application of Versalis HDPE COM75HF2

    High-Cavitation Injection Moulding of Snap-On Closure Systems

    COM75HF2 is processed in multi-cavity closure tools with cavitation counts from 24 to 96. The reciprocating screw should maintain a compression ratio of 2.0:1 to 2.5:1 and an L/D ratio between 20:1 and 25:1. Nozzle melt temperature is held at 190 °C to 230 °C; the lower end is preferred where organoleptic performance is declared under EU Regulation (EU) No 10/2011. Valve-gate tip diameters from 0.6 mm to 1.2 mm prevent gate stringing and minimise closure skirt ovality. Injection speed at the screw is set between 80 mm/s and 140 mm/s, with switch-over to hold pressure at a screw position representing 96% to 98% of total shot volume. Cavity hold pressure is maintained at 45 MPa to 70 MPa for 0.8 s to 2.5 s depending on wall thickness. Mould coolant inlet temperature is held at 10 °C to 25 °C. Warpage across the tamper-evident band increases when mould surface temperature exceeds 30 °C because differential post-crystallisation occurs between the plug seal and the outer skirt. Screw recovery time should be monitored against the producer’s melt-volume-flow-rate declaration cited under ISO 1133-1:2022. A worn check ring producing shot-weight variability above 0.15% in high-cavitation tools produces inconsistent pack force and cap ovality. Slip and antiblock additive masterbatch is compounded at 1.2 wt% to 2.5 wt% in a compatible high-density or linear low-density carrier. Colour masterbatch is metered at 0.8 wt% to 1.5 wt%. Regrind from hot runners and cold sprues is reincorporated up to 15 wt% for food-contact declarations. Beyond 15 wt%, closure torque retention after 24 h and tensile snap-band fracture energy can shift outside validated limits, and organoleptic panels may report higher mineral-oil or phenolic notes. Compliance references for dairy and beverage closures include FDA 21 CFR 177.1520(c)2.1, EU Regulation (EU) No 10/2011, and GB 4806.6-2016 where applicable. Overall migration must not exceed 10 mg/dm² under EU test conditions for aqueous, acidic, and fatty-food simulants specified in Annex III and Annex V. Closure torque retention is verified according to converter standards derived from ASTM D2063/D2063M-10(2017) or the equivalent DIN 6134 test that records breakaway torque after 24 h at 23 °C and 50% RH. The terminal application is a snap-on or screw-cap tamper-evident lid for fresh dairy, dairy-alternative, and non-carbonated beverage bottles between 200 mL and 1 L. The interference bead on the inner wall is critical; its radial thickness is typically 0.8 mm to 1.4 mm and must be filled without visible sink marks. The operating boundary is the trade-off between melt fluidity and stress-crack resistance in fatty-food environments; closures frequently require liners where oil-in-water emulsions are packed.

    Thin-wall refrigerated packaging production with COM75HF2 is run on fast injection moulding machines whose clamp force is selected from 1,500 kN to 5,000 kN. The priority is consistent filling of wall sections from 0.7 mm to 1.4 mm at flow-length-to-wall-thickness ratios above 180:1. Materia melt temperature is controlled at 195 °C to 220 °C at the nozzle. Coolant temperature is set at 15 °C to 25 °C. Injection velocity is profiled from 100 mm/s to 160 mm/s during filling and reduced to 30 mm/s to 50 mm/s before final pack. A shut-off nozzle is required because decompression travel of 2 mm to 5 mm prevents drool at high melt temperatures. Hold pressure is applied at 35 MPa to 55 MPa for 0.5 s to 1.5 s. Total cycle time including demoulding is typically 8 s to 14 s for 0.9 mm walls. Nucleating masterbatch is introduced at 0.5 wt% to 1.2 wt% to reduce post-moulding shrinkage and stabilise top-load performance. Regrind is limited to 10 wt% because thin-wall parts are sensitive to melt-pressure fluctuations caused by bulk-density variation in flake regrind. A cold-runner sprue diameter below 3.0 mm can generate pressure losses exceeding 15 MPa across the runner system and must be sized against the specific tool layout. Food-contact compliance is based on FDA 21 CFR 177.1520(c)2.1 and EU Regulation (EU) No 10/2011. Migration testing is conducted using the fatty-food simulant selected under the latest consolidated Annex III at 4 °C or 20 °C depending on declared service. The terminal products are refrigerated deli containers, spread tubs, and overcaps used between 0 °C and 4 °C. Deep-drawn corners and stacking lugs demand a balance between mould release and impact resistance, and excessive hold pressure above 60 MPa can initiate stress whitening at the bottom radius of a spread tub.

    Application segmentPrimary compliance referenceTest or condition
    Dairy closure systemsFDA 21 CFR 177.1520(c)2.1; EU Regulation (EU) No 10/2011Overall migration below 10 mg/dm²; organoleptic panel per DIN 10955:2004
    Refrigerated spread tubs and deli containersFDA 21 CFR 177.1520(c)2.1; EU Regulation (EU) No 10/2011 Annex IFatty-food simulant under Annex III; refrigerated contact at 4 °C
    Returnable crates and pallet feetREACH Regulation (EC) No 1907/2006 Annex XVII; RoHS 2011/65/EUISO 8611-1:2011 rated load and corner drop
    Cold-chain diagnostic containersISO 10993-5:2009; ISO 10993-10:2010; USP <661.1>Cytotoxicity, irritancy, and extractables profile

    What Shifts When Returnable Crates and Pallet Feet Are Moulded from a High-Fluidity HDPE?

    Returnable logistics parts shift the critical material property away from high-shear melt flow and toward low-temperature impact, creep, and environmental stress-cracking resistance. COM75HF2 is processed in thick-wall tools with shot weights from 800 g to 6,000 g on accumulator-assisted injection moulding machines with clamp force from 8,000 kN to 15,000 kN. Melt temperature is maintained at 200 °C to 235 °C; coolant temperature at the mould is set from 20 °C to 45 °C. The injection fill time is intentionally extended from 3 s to 6 s to avoid jetting and flow-shadow marks across rib junctions. Hold pressure is set at 60 MPa to 80 MPa and held for 12 s to 20 s. Total cycle time for crate bodies weighing from 1.5 kg to 6.0 kg can reach 45 s to 75 s. Gate bushing diameter is 2.5 mm to 4.0 mm, sufficient to reduce shear heating and local gate fracture. Regrind is introduced at 20 wt% to 30 wt% through a gravimetric blender and must be dry-screened through a 6 mm mesh to remove granulate whiskers and longs. UV stabiliser masterbatch is dosed at 1.5 wt% to 3.0 wt% for outdoor and warehouse-to-retail pool circulation. Carbon black masterbatch, where used, is dosed at 2.0 wt% to 2.5 wt%. The operational boundary is clear: high melt-flow grades usually display lower notched impact and lower ESCR than blow-moulding or sheet-extrusion HDPE grades. Published COM75HF2-specific ESCR data as a function of regrind loading at 20 wt% to 30 wt% are limited; qualification should reference ASTM D1693-13 Condition C with 10% Igepal CO-630 at 50 °C before detergent-containing returnable service is approved. Perforated side-wall patterns and radiused rib roots with minimum radius 2.0 mm reduce stress concentrations. Pallet tests follow ISO 8611-1:2011 for rated load, corner drop, and bottom pallet deck deflection. RoHS 2011/65/EU recast (EU) 2015/863 applies to electric-wheeled container tracking tags, and REACH Regulation (EC) No 1907/2006 Annex XVII applies to articles placed on the European market. Terminal parts are returnable distribution crates, collapsible bulk containers, dairy case shells, and pallet feet. In crate service, the failure mode most often observed on production lines is side-wall crack initiation at the gate vestige due to excessive frozen-in orientation; reducing hold pressure below 80 MPa and increasing gate diameter above 3.0 mm can reduce the rejection rate.

    ParameterHigh-cavitation closuresThick-wall returnable crates
    Nozzle melt temperature190 °C – 230 °C200 °C – 235 °C
    Mould coolant temperature10 °C – 25 °C20 °C – 45 °C
    Cavity hold pressure45 MPa – 70 MPa60 MPa – 80 MPa
    Regrind ceiling15 wt% food contact20 wt% – 30 wt% non-food
    Cycle range8 s – 14 s total45 s – 75 s total

    Houseware and storage-product moulding with COM75HF2 is specified where surface gloss, dimensional stability, and mould release matter more than food-contact declarations. The injection tool is constructed with a polished core and cavity, draft angles from 0.5° to 1.0°, and wall thickness from 2.2 mm to 3.5 mm. Nozzle melt temperature is held at 190 °C to 220 °C. Mould coolant temperature is set from 30 °C to 50 °C to avoid visible flow lines and jetting on large flat surfaces. Edge gates with width 2.0 mm to 4.0 mm and land length 0.5 mm to 1.0 mm are common. Injection velocity is profiled from 70 mm/s to 100 mm/s in the first 60% of flow length and decelerates to 25 mm/s to 40 mm/s in the final pack. Hold pressure is set at 50 MPa to 65 MPa for 4 s to 8 s. Total cycle time for a 2 L storage container is 22 s to 35 s. Colour masterbatch is metered at 2.0 wt% to 3.5 wt%, and slip masterbatch at 0.3 wt% to 0.8 wt% for stackability. Regrind is allowed up to 20 wt% when the material is dry and free from dust. Contact with mineral oil or kerosene-based cleaners should be avoided because such agents can accelerate environmental stress-cracking in stressed snap-hinge regions. REACH Regulation (EC) No 1907/2006 Annex XVII restrictions for phthalates apply only where the article is a childcare article within the scope of entry 51; COM75HF2 does not require phthalate plasticisers. The terminal products are modular storage boxes, pantry organisers, waste bins, and non-food utility buckets. Mixing requires no additional compounding in this segment.

    If Cold-Chain Diagnostic Containers Require Leak Integrity After Vacuum Sealing

    Diagnostic transport containers moulded from COM75HF2 rely on precise sealing surfaces rather than transparency or breathability. The processing discipline is stricter because regrind levels are capped at 10 wt% and external lubricants are avoided. Melt temperature at the nozzle is set between 200 °C and 230 °C. Mould temperature is controlled at 15 °C to 30 °C. Injection velocity is profiled from 100 mm/s to 180 mm/s for thin lid perimeters and reduced to 30 mm/s to 45 mm/s for boss and snap-fit areas. Cavity hold pressure is maintained at 40 MPa to 60 MPa for 1.5 s to 3.0 s. Sealing rims must be held to flatness within 0.10 mm per 50 mm of rim length to avoid vacuum-seal leaks after capping. No internal solvents, slip additives, or anti-static agents are added without extractables validation. The validation chain references ISO 10993-5:2009 for cytotoxicity and ISO 10993-10:2010 for irritation when the part is declared as a diagnostic or specimen transport article. USP <661.1> is used for container extractables in pharmaceutical packaging contexts, and ICH Q3D applies to elemental impurities where a drug-contact statement is submitted. A limitation: published COM75HF2-specific gamma sterilisation compatibility data are limited; converters selecting this polymer for irradiated diagnostic products must validate post-irradiation impact retention, as high-dose gamma irradiation above 25 kGy can cause chain scission and surface discolouration in unmodified polyethylene. Ethylene oxide sterilisation at 37 °C to 55 °C is less aggressive to the polymer matrix, but residual gas retention must be tested on the sealed container geometry. In practice, mould-filling simulation with cavity pressure transducers is advisable for rim-dominated parts; short-shot sensors placed at the last sealing point reduce leak-rate variability between cavities. The terminal products are cold-chain diagnostic transport tubes, lid-sealed specimen cups, and non-invasive sampling containers used between -20 °C and 4 °C.

    Non-food industrial closures and chemical packaging apertures form a segment in which torque retention and thread stability are more demanding than in dairy closures. The grade is moulded into 28 mm and 38 mm neck closures with integral bore seals for agrochemical, home-care, and industrial fluid containers. Melt temperature is set at 195 °C to 225 °C; mould temperature is kept at 15 °C to 30 °C. Hold pressure is set at 55 MPa to 75 MPa for 1.0 s to 3.0 s to press the bore seal and thread profiles without dimensional drift. Closure liner insertion is required where aromatic or oxygenated solvents are packed. The converter should validate under the performance packaging requirements of the UN Recommendations on the Transport of Dangerous Goods or equivalent national regulation where the packed product is classified as dangerous goods. REACH Regulation (EC) No 1907/2006 Annex XVII and CLP Regulation (EC) No 1272/2008 apply to the finished article or packed chemical system. Published data on long-term chemical resistance of COM75HF2 to ketones and chlorinated solvents are limited; preliminary soak testing should follow ISO 175:2010 for 7 days at 23 °C and include visual inspection, weight change, and torque retention. Terminal products are non-food industrial closure systems, trigger-spray bottle adapters, and dispensing plugs.

    Free Quote

    Competitive Versalis HDPE COM75HF2 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE COM75HF2 is positioned within the high-density polyethylene class defined by ISO 17855-1 through a density above 0.941 g/cm³. The grade is supplied as pelleted olefinic feedstock for injection moulding, where melt front velocity, solidification rate, and demoulding release exert direct control over cycle time and dimensional yield. The product identifier is a commercial designation rather than a compositional formula; the manufacturer’s certificate of analysis carries the lot-specific melt mass-flow rate, density, tensile yield stress, and impact values produced under standardised methods. Components manufactured from this grade are commonly evaluated against ISO 527-2 for tensile behaviour, ISO 179-1 for Charpy impact, ISO 306 for thermal softening, and ASTM D1693 for environmental stress crack resistance when chemical exposure is expected. The HF segment of the designation denotes a high-flow design intended for thin-section flow lengths; the actual melt mass-flow rate and density limits must be confirmed against the current technical data sheet because these values are lot-dependent and may be revised by the manufacturer without public notice.

    Which Standardised Test Methods Govern Release Data for HDPE COM75HF2?

    Release data for HDPE COM75HF2 are generated under the methods listed in the compliance matrix below. The matrix does not state absolute specification values; it defines the measurement framework that permits valid comparison between this grade and other polyolefins. Melt mass-flow rate is determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. Density is measured on conditioned specimens under ISO 1183-1. Tensile properties are obtained at 23 °C and 50 mm/min unless otherwise noted, using Type 1A specimens per ISO 527-2. Charpy notched impact strength is tested at 23 °C on edgewise specimens according to ISO 179-1/1eA. Vicat softening temperature is measured using the A50 method under ISO 306 with a 10 N load and a 50 °C/h heating rate. Environmental stress crack resistance is assessed by bent-strip exposure under ASTM D1693; the result is a function of stress concentration and detergent formulation, not an intrinsic material constant that transfers directly to every end-use geometry.

    Verification areaReference methodPrimary unit
    Melt mass-flow rate 190 °C/2.16 kgISO 1133-1:2022g/10 min
    DensityISO 1183-1g/cm³
    Tensile yield stress and yield strainISO 527-2MPa, %
    Flexural modulusISO 178MPa
    Charpy notched impact strength 23 °CISO 179-1/1eAkJ/m²
    Vicat softening temperature A50ISO 306°C
    Environmental stress crack resistanceASTM D1693h

    Successful conversion of HDPE COM75HF2 in a reciprocating-screw injection moulding machine depends on controlling the melt condition at the nozzle, not on replicating a fixed barrel setpoint from another facility. A general-purpose polyolefin screw with an L/D ratio of 20:1 to 25:1 and a compression ratio of 2.0:1 to 3.0:1 is preferred. Melt temperature measured by a needle pyrometer should be maintained within the window supplied by the manufacturer; typical starting setpoints for high-flow HDPE injection moulding range from 200 °C to 240 °C at the nozzle. Mould temperatures between 10 °C and 40 °C are common, with lower temperatures used for thin-wall parts and higher temperatures used where surface gloss and weld-line strength are more important than cycle time. Back pressure between 0.5 MPa and 1.5 MPa is generally sufficient to maintain screw recovery consistency without excessive shear heating. Excessive melt residence time at high temperature can cause molecular weight degradation, visible as silver streaking, lower melt viscosity, and brown specks from oxidised material accumulating in the check ring. If regrind is used, the ratio should be controlled and screened to avoid contamination by paper, dust, or polypropylene closures because density and viscosity shifts create visible flow defects and inconsistent gate seal.

    When Injection Moulding Competition with Blow Moulding or Film Extrusion Is Evaluated

    HDPE COM75HF2 is not intended for extrusion blow moulding. Blow moulding grades are designed with higher melt strength and strain-hardening elasticity to support parison sag resistance. A high-flow injection moulding grade subjected to blow moulding conditions may produce a parison that draws down excessively, leading to thin top and sidewalls. Conversely, a blow moulding grade used in thin-wall injection moulding can require excessive injection pressure and produce flow marks because its higher molecular weight lowers melt front velocity at equivalent gate dimensions. These differences are measurable as melt flow rate and die swell divergence, not as a simple density difference. Similarly, cast or blown film HDPE grades are formulated for bubble stability, drawability, and film toughness; COM75HF2 is not optimised for film thickness below 100 µm because the molecular architecture that benefits injection moulding may reduce melt extension uniformity on a blown film line. Published data for this specific configuration is limited, and film trials should not proceed without first verifying bubble stability on the target extrusion line.

    Closure systems for beverages, dairy, and household products are among the most demanding applications for a grade in this class. Multi-cavity closure moulds running 24 to 96 cavities often require hot-runner temperature uniformity within ±5 °C to avoid premature gate freeze-off, because high-flow HDPE still exhibits a rapid transition from melt to solidified plug when the gate cools. Valve-gated hot-runner systems may be required for large-diameter caps to control gate vestige and to prevent drool during mould opening. Housewares and crates fabricated from COM75HF2 may show reduced impact when moulded with inadequate packing pressure. A short-shot study and gate-seal time determination are necessary before setting hold pressure. In practice, gate-seal time varies with wall thickness, melt temperature, and mould steel; published data for this specific configuration is limited.

    For applications involving aggressive detergent or solvent exposure, environmental stress crack resistance should be assessed under ASTM D1693 or the relevant UN transport standard on finished parts, because internal moulded-in stress and gate location influence performance more strongly than resin selection alone. Contact with strong oxidising agents, chlorinated solvents, and high-aromatic hydrocarbon streams should be avoided unless validated on the final article. The base resin may be suitable for food packaging under 21 CFR 177.1520, but the finished article must be evaluated for migration according to the intended food type, temperature, and contact duration. Additives or colorants may alter compliance status, and a food-contact statement specific to the final formulation should be requested from the masterbatch supplier and the resin manufacturer.

    Within the manufacturer’s high-density polyethylene portfolio, product grades are segregated primarily by melt flow rate, density, and stabilizer/additive package. Grades with lower melt flow rate are favoured for thick-walled industrial containers and sheet because higher molecular weight contributes to environmental stress crack resistance and impact. Grades with higher melt flow rate may be chosen for extremely thin-wall packaging, but at the cost of lower impact strength and lower environmental stress crack resistance. COM75HF2 occupies the high-flow injection moulding segment; for specific values, the portfolio overview and current technical data sheet should be compared. Without such verification, lot-specific performance boundaries remain unconfirmed.

    Top