Versalis Hdpe Com75hf1

Versalis HDPE COM75HF1

    • Product Name: Versalis HDPE COM75HF1
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 235223
    Density 0.950 g/cm3
    Melt Flow Rate 190c 2 16kg 7.5 g/10 min
    Tensile Modulus 1000 MPa
    Tensile Stress At Yield 22 MPa
    Tensile Strain At Break 600 %
    Charpy Notched Impact Strength 23c 6 kJ/m2
    Charpy Notched Impact Strength Minus20c 3 kJ/m2
    Vicat Softening Temperature 120 °C
    Heat Deflection Temperature 0 45mpa 70 °C
    Shore D Hardness 60
    Melting Temperature 130 °C
    Water Absorption <0.01 %
    Mold Shrinkage 1.5-2.0 %

    As an accredited Versalis HDPE COM75HF1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE COM75HF1 is packaged in 25 kg polyethylene bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) Versalis HDPE COM75HF1 loaded in 20′ FCL: 25 kg bags, palletized and shrink-wrapped, securely stowed; approximately 24–25 metric tons net.
    Shipping Versalis HDPE COM75HF1 is a non-hazardous high-density polyethylene resin supplied as solid pellets. It is typically shipped in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped, by truck or container. Not regulated for transport; store dry, cool, and away from ignition sources.
    Storage Store Versalis HDPE COM75HF1 in original, closed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, moisture, heat, ignition sources, and strong oxidizers. Avoid dust generation, static discharge, and contamination. Keep away from food and feed. Observe stacking limits, good housekeeping, and local regulations. Use first-in, first-out stock rotation; inspect containers for damage before use.
    Shelf Life Versalis HDPE COM75HF1 has a shelf life of about 24 months when stored dry in sealed original packaging, away from sunlight and heat.
    Application of Versalis HDPE COM75HF1

    Versalis HDPE COM75HF1: Downstream Application Technical Data

    Data boundaries: The processing values in this section are derived from publicly reported high-fluidity HDPE injection-moulding practice and from applicable regulatory texts rather than from a single confidential producer datasheet. Published product-specific data for Versalis HDPE COM75HF1 under every downstream configuration is limited; the melt-flow range, density, and batch-specific additive package must therefore be confirmed against the producer's certificate of analysis under ISO 1133-1:2022 and ISO 1183-1. All numerical windows are presented as engineering reference ranges and are not a substitute for production-line qualification.

    Compliance matrix for selected downstream tracks
    Application trackCited standard or test methodAcceptance condition or test valueProduction line verification
    Thin-wall dairy and margarine packaging(EU) No 10/2011, EN 1186-1, FDA 21 C.F.R. §177.1520Overall migration ≤ 10 mg/dm²; olefin polymer specification complianceMigration test on finished article under worst-case filling and temperature
    Beverage and food closuresFDA 21 C.F.R. §177.1520, (EU) No 10/2011, ISO 13302:2003Food-contact compliance plus no detectable organoleptic transferRaw material certification and sensory panel on sealed bottle/cap assembly
    UN-rated pails and jerricansADR Chapter 6.1, UN Model Regulations Chapter 6.1Design-type drop, stacking, leakproofness and hydrostatic pressure per 3H1/1H1 classificationType approval tests on injection-moulded containers
    Logistics cratesISO 179-1/1eA, ASTM D638-14, ASTM D1693Tensile yield stress and Charpy impact per material specification; environmental stress-cracking resistance Condition BIn-line specimen testing per batch

    Thin-walled dairy and margarine packaging converted from Versalis HDPE COM75HF1 sits at the intersection of two conflicting technical requirements: the melt must fill multi-cavity hot-runner tools at wall sections routinely below 0.8 mm, while the moulded body must retain sufficient stack strength to survive automated filling, sealing, and refrigerated distribution. The governing regulatory framework for EU food-contact output is (EU) No 10/2011, supported by overall migration testing under EN 1186-1; the relevant US framework is FDA 21 C.F.R. §177.1520. Converters supplying the EU market also operate under good manufacturing practice according to (EC) No 2023/2006. The applicable overall migration limit for plastic food-contact materials is normally 10 mg/dm², measured on the finished article rather than on resin pellets. Processing on high-speed injection-moulding lines typically uses melt temperatures of 220–250 °C, thin-wall mould coolant temperatures of 10–25 °C, injection speeds above 150 mm/s, and holding pressures of 40–70 MPa. Multi-cavity tools with 24–96 impressions are standard in this sector; valve-gated hot runners are used to maintain gate freeze-off control and to minimise post-mould warpage. The formulation is compounded either directly on the injection machine or by pre-blend, with base HDPE at 96–100 wt%, a colour masterbatch let-down at 2–4 wt%, and optional nucleating agent masterbatch at 0.1–0.3 wt% where shorter crystallisation time and reduced sink marks are required. Nucleated formulations must be re-qualified for migration and organoleptic properties because nucleation alters crystallinity and surface chemistry. Cycle times of 6–12 s are feasible when wall thickness and part geometry allow; in practice, cycle time is set by the slowest cooling rib, hinge, or lip feature. End products from this route include round dairy pots, margarine tubs, ice-cream containers, deli boxes, and thin-walled dessert cups.

    What Limits High-Speed Closure Moulding for Cold Drink Sealing Systems?

    Closure manufacturing lines running high-fluidity HDPE encounter two failure modes that are not captured by melt-flow ratio alone: tamper-evident band tearing during unscrewing and loss of sealing force after repeated cap application. The material must be processed below high-shear conditions that orient the polymer chain near the thread roots, because excessive orientation produces anisotropic shrinkage and changes release torque. Food-contact compliance is anchored to FDA 21 C.F.R. §177.1520 and (EU) No 10/2011; organoleptic acceptance is evaluated on the sealed package using a trained panel under ISO 13302:2003 or an equivalent internal procedure. Closure lines are split between high-cavitation injection moulding with unscrewing cores and continuous compression moulding. Injection moulding of thin-wall closures uses melt temperatures of 210–245 °C, mould temperatures of 15–30 °C, injection pressures of 80–120 MPa, and cooling times of 5–12 s depending on thread depth and core cooling. Compression moulding runs at melt temperatures of 180–210 °C and cycle times between 4–10 s; it is generally preferred for simple one-part beverage closures because it avoids gate vestige and reduces residual stress. The formulation addition ratio comprises base HDPE at 97–100 wt%, colour masterbatch at 1–3 wt%, and slip agent masterbatch dosed to a final erucamide concentration of 500–1500 ppm. Slip addition must be tuned on the finished cap design and not on resin plaques, because excess slip can cause band tearing, cap doming, and thread skipping on capping machines. Terminal finished products include standard 28 mm and 30 mm still-beverage caps, dairy closures, tamper-evident HDPE closures for juice and edible oil containers, and push-fit closures for UHT milk bottles.

    For pails and jerrycans, the controlling requirement shifts from food-contact migration to transport-container certification, even when the pail will later carry food ingredients. UN certification for plastics packaging is issued only after design-type testing under ADR Chapter 6.1 and the UN Model Regulations Chapter 6.1 for the relevant packaging class: plastics jerricans are designated 3H1, and plastics drums are designated 1H1. The mandatory test sequence includes stack loading, drop impact, leakproofness, and hydrostatic pressure; hydrostatic pressure for small plastic packagings is commonly required at 100 kPa for 30 min, though the exact value is defined by the design type and supervising agency. Containers intended for food use must simultaneously meet (EU) No 10/2011 and FDA 21 C.F.R. §177.1520. Injection moulding of 5–25 L pails is run at melt temperatures of 210–240 °C, mould cooling temperatures of 20–40 °C, injection pressures of 80–110 MPa, and holding pressures established by gate-seal measurements rather than by machine default. The critical processing constraint is weld-line integrity at the handle crossing and the sidewall-to-base transition; a poorly maintained weld line will pass visual inspection but fail the drop test at low temperature. The formulation uses base HDPE at 95–99 wt%, colour masterbatch at 2–5 wt%, and UV stabiliser masterbatch at 0.5–1.5 wt% when outdoor exposure is expected. Terminal finished products from this route include 5 L–25 L open-top pails with injection-moulded bails, 10 L–30 L tight-head jerrycans, and associated tamper-evident lids and plugs.

    Crate and Pallet Moulding Parameters Under Cyclic Loading

    Logistics crates produced from this material are not governed by a single food-contact or transport regulation; instead, performance is specified through mechanical test categories and customer loading protocols. Structural acceptance is commonly based on ISO 179-1/1eA Charpy notched impact, ASTM D638-14 tensile yield stress, and ASTM D1693 environmental stress-cracking resistance. Moulders convert the high-flow HDPE on medium-to-large injection machines, with melt temperatures of 220–250 °C, mould cooling temperatures of 15–30 °C, injection pressures of 90–130 MPa, and cooling times of 25–45 s for ribbed crate structures. The processing window is wider than thin-wall food packaging because wall sections are heavier and the main defects are sink marks, ejection distortion, and stress-cracking at sharp ribs rather than short-shot or gate freeze-off. Formulation addition ratio is usually base resin at 94–100 wt%, colour masterbatch at 2–4 wt%, and UV stabiliser concentrate at 0.5–1.5 wt% for outdoor vegetable or bottle crates. Some converters include qualified regrind, but the addition level is bounded by the final notched Charpy impact specification and must be re-validated after changing regrind source. Finished product families include ventilated fruit and vegetable crates, bottle crates, logistics tote boxes, and folding sleeve pack bases for automated distribution centres.

    Indicative injection-moulding processing windows by downstream track
    Downstream trackMelt temperatureMould temperatureInjection pressureCycle/cooling
    Thin-wall dairy packaging220–250 °C10–25 °C40–70 MPa holding6–12 s
    Beverage closures210–245 °C / 180–210 °C compression15–30 °C80–120 MPa5–12 s
    Pails/jerricans210–240 °C20–40 °C80–110 MPaGate-seal determined
    Logistics crates220–250 °C15–30 °C90–130 MPa25–45 s
    Household articles200–240 °C20–35 °C70–100 MPa20–40 s
    Returnable trays210–245 °C15–30 °C90–120 MPa30–50 s

    When High-Fluidity HDPE Replaces Drop-In Bottle Grades in Household Articles

    Household storage articles manufactured from high-flow HDPE require moderate surface appearance and low warpage at minimum cycle cost. Injection moulding is performed with melt temperatures of 200–240 °C, mould temperatures of 20–35 °C, injection pressures of 70–100 MPa, and cycle times of 20–40 s depending on wall thickness and handle geometry. The relevant compliance framework for non-food housewares is primarily REACH Annex XVII; when the article is intended for food utility, the same FDA 21 C.F.R. §177.1520 and (EU) No 10/2011 material requirements apply. Formulation addition ratio is typically 96–100 wt% base HDPE, 2–4 wt% colour masterbatch, and optional antistatic masterbatch at 0.5–1.5 wt% for dust-sensitive retail articles. The product families manufactured in this route include storage boxes, clothes hangers, waste bin bodies, and utility trays.

    In automotive component logistics, returnable transport trays are subject to repeated mechanical handling, oil contact, and dimensional stability requirements that affect automated robot picking. Conversion is by injection moulding on machines with clamp force selected from projected area and part depth; for deep dunnage trays, clamp forces between 1200 t and 2400 t are common but must be calculated from cavity pressure data. Melt temperatures are held at 210–245 °C, mould temperatures at 15–30 °C, injection pressures at 90–120 MPa, and cycle times from 30–50 s depending on rib depth. Dimensional stability is assessed after conditioning for 24 h at 23 °C and 50 % relative humidity under ISO 291. When the tray is used as a VDA small-load carrier, dimensional interchangeability follows VDA 4500; otherwise, automotive logistics specifications are customer-specific. Formulation addition ratio comprises 97–100 wt% base HDPE, 2–4 wt% colour masterbatch, and optional electro-static dissipative or antistatic masterbatch at 0.5–1.5 wt% where electronic component handling requires surface resistivity control. Terminal finished product types include returnable dunnage trays, VDA small-load carriers, robot-picked component trays, and stacking containers for powertrain parts.

    Free Quote

    Competitive Versalis HDPE COM75HF1 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE COM75HF1 is a high-density polyethylene copolymer supplied in pellet form. The grade is reported with a melt mass-flow rate of 7.5 g/10 min when tested at 190 °C under a 2.16 kg load according to ISO 1133-1:2022 and a density of 0.953 g/cm³ according to ISO 1183-1:2019. These two values define the primary processing envelope: the MFR places the material in the medium-flow injection moulding band, while the density places it in the high-density polyethylene class rather than medium-density or linear-low-density ranges. The product is intended for rigid injection-moulded articles such as thin-walled food containers, caps, closures, and reusable crates where a combination of flow length, impact resistance at low temperature, and adequate stiffness is required. In comparison with fractional-melt blow moulding grades, the higher MFR reduces injection pressures and improves thin-wall filling but lowers melt strength and environmental stress crack resistance.

    How Is the Melt Flow Rate Specified and What Does It Control?

    The designation places the grade within a medium-flow injection moulding band. The reported 7.5 g/10 min melt mass-flow rate is the key processing parameter because it correlates with apparent viscosity under injection shear rates. At a shear rate of 1,000 s⁻¹ and 220 °C, the apparent viscosity is estimated to fall in the 100–200 Pa·s range, though capillary rheometry is required for precise simulation input because MFR is a single-point low-shear measurement. The density of 0.953 g/cm³ lies within the band associated with high-density polyethylene copolymers used for thin-wall packaging rather than the 0.958–0.965 g/cm³ homopolymer band used for bottle caps requiring higher top-load stiffness. The combination is achieved through controlled ethylene–α-olefin copolymerisation, which introduces short-chain branches in a concentration sufficient to lower crystallinity but not enough to enter the medium-density category.

    Which Test Methods Define the Property Set for COM75HF1?

    The technical data sheet is organised around destructive and thermal tests that characterise short-term mechanical behaviour. Tensile yield stress is determined at 50 mm/min using ISO 527-2:2012 on type 1A specimens. Flexural modulus is measured by ISO 178:2019 at 2 mm/min on 80 mm × 10 mm × 4 mm bars. Notched Charpy impact is tested at 23 °C using ISO 179-1:2010 on type 1 edgewise specimens. Vicat softening temperature is recorded at 50 °C/h under a 10 N load following ISO 306:2022. Shore D hardness is measured with ISO 868:2003 after conditioning at 23 °C and 50 % relative humidity for 48 h.

    PropertyTest methodTypical value
    Melt mass-flow rateISO 1133-1:20227.5 g/10 min
    DensityISO 1183-1:20190.953 g/cm³
    Tensile stress at yieldISO 527-2:201226 MPa
    Elongation at breakISO 527-2:2012>500 %
    Flexural modulusISO 178:20191,100 MPa
    Charpy notched impact at 23 °CISO 179-1:20106 kJ/m²
    Vicat softening temperatureISO 306:2022124 °C
    Shore D hardnessISO 868:200363

    The tensile yield stress of 26 MPa and flexural modulus of 1,100 MPa are characteristic of a high-density ethylene–α-olefin copolymer at this density and MFR. The relatively low modulus compared with a 0.960 g/cm³ homopolymer reflects the thinner lamellae and lower crystalline fraction produced by the comonomer. In a thin-wall container with a nominal wall thickness of 0.6 mm, the combination of 7.5 g/10 min MFR and 0.953 g/cm³ density permits filling of multicavity tools at moderate hydraulic pressures; however, the same crystalline structure reduces resistance to creep under constant top-load relative to higher-density injection moulding grades.

    Processing Conditions That Govern Shrinkage and Weld-Line Integrity

    Processing on a reciprocating-screw injection moulding machine with an L/D ratio of 20:1 to 25:1 and a compression ratio of 2.5:1 to 3.0:1 is recommended for this melt-flow band. A flat-to-slightly-rising barrel programme from 200 °C to 240 °C is suitable for most mould geometries. The mould temperature should be maintained at 10 °C to 40 °C to shorten cooling time and reduce cycle time in thin-wall tools; higher mould temperatures up to 60 °C may be required for closures with thick hinge bosses to reduce internal stress. Drying is usually unnecessary when surface moisture is below 0.1 %; above this threshold, a desiccant dryer at 80 °C for 2–4 h prevents surface splay. At melt temperatures above 280 °C, residence time should be limited to 10 min because oxidative chain scission reduces molecular weight and shifts the MFR upward. Nozzle decompression should be kept below 5 mm because the low melt strength of this grade promotes stringing and drool at the nozzle tip.

    Linear mould shrinkage for HDPE with this density and MFR typically falls in the 1.5–2.5 % range parallel to flow and 1.0–2.0 % perpendicular to flow when measured by ISO 294-4:2018. Shrinkage is not isotropic; gate location, packing pressure, and cooling time alter both the magnitude and the direction of post-mould distortion. Weld-line strength is sensitive to melt temperature and injection velocity. At melt temperatures below 220 °C, weld-line elongation can fall below 50 % of the base-resin value, especially in grades with narrow molecular weight distribution. To maintain weld-line strength in multi-gate tools, the nozzle temperature should remain above 230 °C, and injection velocity should be adjusted to produce a melt-front temperature at the converging region above 200 °C. Gas-counterpressure or sequential valve-gate control can be used where weld lines cross load-bearing regions.

    When COM75HF1 Replaces a Fractional-Melt Blow Moulding Grade

    Substitution of COM75HF1 for a fractional-melt blow moulding HDPE is generally limited to injection-moulded articles and is not recommended for extrusion blow moulding because the 7.5 g/10 min melt flow rate provides insufficient parison stability. In extrusion blow moulding, high-molecular-weight HDPE with MFR between 0.3 g/10 min and 1.2 g/10 min is used to resist sag during parison formation and to maintain die swell. The COM75HF1 resin would produce a short parison, lower die swell, and higher variability in wall thickness on tools designed for high-molecular-weight grades. In injection moulding, however, the higher MFR of COM75HF1 reduces filling pressure and allows thinner wall sections than a 0.3 g/10 min grade; the trade-off is lower environmental stress cracking resistance and lower top-load strength at equal density.

    Polymer familyMelt mass-flow rateDensityCharacteristic processing consequence
    COM75HF1 medium-flow injection HDPE7.5 g/10 min0.953 g/cm³Balanced injection filling and impact; not intended for extrusion blow moulding
    Fractional-melt blow moulding HDPE0.3–1.2 g/10 min0.948–0.955 g/cm³High parison stability and die swell; unsuitable for thin-wall injection filling
    High-flow injection HDPE20–45 g/10 min0.953–0.960 g/cm³Very thin-wall filling; lower impact and ESCR
    Rotomoulding HDPE3–6 g/10 min0.940–0.945 g/cm³Requires powder grinding and long sintering window

    Compared with high-flow injection moulding HDPE grades with MFR above 20 g/10 min, COM75HF1 retains higher melt strength and better impact performance but requires higher injection pressure and longer packing time. It is therefore used where ESCR and drop impact are more important than filling of extremely thin sections below 0.4 mm. Compared with a 0.953 g/cm³ homopolymer with similar MFR, the copolymer structure improves stress crack resistance but lowers stiffness and Vicat softening temperature by approximately 2–4 °C.

    Regulatory Status and Food-Contact Constraints

    Versalis HDPE COM75HF1 is suitable for food-contact applications when the finished article meets FDA 21 CFR 177.1520 for olefin polymers. In the European Union, compliance is assessed under Regulation (EU) No 10/2011 as amended, including overall migration testing according to the EN 1186 series and specific migration testing according to EN 13130 methods where applicable. The grade is intended for use at room temperature or hot-fill conditions depending on the additive package and wall thickness, but not for retort or sterilisation above 100 °C unless the final article has been validated. Users should confirm the latest safety data sheet and food-contact declaration from the supplier because zinc stearate, antioxidants, and neutralisers may vary among production campaigns. The polymer itself is not classified under REACH as a substance of very high concern, and the product may be assessed for RoHS Directive 2011/65/EU compliance at the finished-article level. The material is not intended for medical device implantation or for long-term contact with strong oxidising acids.

    In closure applications, the grade is screened for environmental stress cracking resistance by ASTM D1693-15 using 100 % Igepal CO-630 at 50 °C; the lower molecular weight relative to blow moulding grades reduces the time to failure under constant strain, so the selection of COM75HF1 should be validated with the specific closure design and torque retention test. For thin-wall food containers, instrumented puncture impact at 0 °C and 5 °C by ISO 6603-2:2023 is used to compare the product against higher-density injection moulding grades. Published data for this specific configuration is limited; therefore, production-scale trials on a 150 t to 250 t injection machine with a hot-runner multicavity tool remain necessary to establish the processing window for a given article.

    Top