    Specifications
    HS Code 226473
    Polymer Type High Density Polyethylene (HDPE) Copolymer
    Density 0.970 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 30.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 600 %
    Flexural Modulus 1400 MPa
    Hardness Shore D 65
    Vicat Softening Point 128 °C
    Melting Point 135 °C
    Brittleness Temperature -70 °C
    Thermal Conductivity 0.400 W/m-K
    Water Absorption 0.010 %
    Environmental Stress Cracking Resistance Escr >1000 h

    As an accredited Versalis HDPE COM70HF1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE COM70HF1 is supplied in 25 kg polyethylene bags, typically palletized with 40 bags per pallet.
    Container Loading (20′ FCL) Chemical Versalis HDPE COM70HF1 in 25 kg bags, palletized, loaded into a 20′ FCL container, secured for ocean freight.
    Shipping Versalis HDPE COM70HF1 is a non-hazardous, high-density polyethylene resin shipped as solid pellets. It is not regulated as dangerous goods for transport. Typical packaging: 25 kg bags or jumbo bags, palletized and stretch-wrapped. Ship in dry containers or trucks at ambient temperature; protect from moisture and contamination.
    Storage Store Versalis HDPE COM70HF1 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Do not stack excessively; avoid damage and UV exposure. Maintain clean, segregated storage and follow FIFO. Use appropriate grounding to prevent static buildup during handling. Consult SDS for detailed precautions.
    Shelf Life Shelf life is typically 24 months from production when stored in original packaging, dry, cool, and away from direct sunlight.
    Application of Versalis HDPE COM70HF1

    Feeding HDPE COM70HF1 into a high-speed injection moulding cell for thin-wall beverage closures requires control of shear-sensitive flow behaviour at filling velocities that routinely exceed 200 mm/s in the runner system. The barrel profile is set between 180 °C at the feed throat and 230 °C at the nozzle, while the hot runner manifold is held within ±5 °C of the nozzle set point to prevent premature gate freeze. Gates are dimensioned with land lengths below 0.8 mm and are placed in sub-surface or edge configurations to limit pressure drop during the pack phase. Injection velocity is increased until the flow front fills the tamper-evident band without jetting, which on multicavity closures is normally confirmed by short-shot progression at 10% increments. Hold pressure is maintained until cavity pressure transducers show a clear decay inflection indicating gate freeze. Mould temperature is controlled at 10–30 °C with turbulent water channels and monitored at each cavity wall. Dimensional stability is assessed after 24 h ambient conditioning using ISO 294-4, with shrinkage for thin-wall HDPE closures typically in the 1.5–2.5% range. Finished closures are tested for drop impact according to ASTM D2463-15, and closure retention or strip torque is measured on application-specific capping heads. Food-contact status is verified under FDA 21 CFR 177.1520(c) and EU No 10/2011, with overall migration determined by EN 1186-1. When slip and anti-block masterbatches are used at 1–3 wt%, coefficient of friction is checked against ISO 8295 because erucamide migration can alter cap decoration and downstream capping torque.

    On production-scale closure lines, cavity-to-cavity fill imbalance exceeding 5% by shot weight has been correlated with ovality drift above the tolerance of high-speed capping equipment. Gate freeze must be confirmed by cavity pressure transducer decay rather than timer-only hold settings, because barrel lot changes can shift solidification time by more than 0.3 s on thin-wall rims. The screw should have a compression ratio of 2.5:1 to 3.0:1 and an L/D ratio of 20:1 to 25:1, with a non-return valve seal inspected at scheduled intervals to avoid shot-weight variation. Pre-drying is not normally required if sealed packaging is handled, but storage at relative humidity above 60% can introduce surface moisture sufficient to cause splay in thin sections. Material cleaned from purges should not be re-introduced into food-contact closures unless the re-grind fraction is controlled and migration re-tested under EN 1186-1.

    What Defines the Extrusion Blow Moulding Window for Small Rigid Containers?

    For small containers under 1 L, COM70HF1 can be processed on a shuttle blow moulder with a continuous extrusion head, but the operating window is narrower than for a dedicated blow-moulding HDPE because the melt flow behaviour increases parison sag. Melt temperature is held in the lower portion of the HDPE envelope, normally 180–200 °C, to preserve adequate melt strength during parison hang time. The extruder is specified with an L/D ratio of 24:1 to 30:1 and a barrier-type screw, which stabilises output against die pressure variation. Parison programming is not optional; a wall-thickness programmer is required to compensate for flare at the tail and thinning at the neck. The die gap is adjusted for a blow-up ratio that keeps container sidewall stress within measurable limits. Mould closing speed is set to avoid excessive pinch-off tailing, and the flash pocket is vented to prevent air entrapment at the parting line. Blow pressure is applied at 0.6–0.8 MPa through calibrated needle blow pins, followed by post-mould cooling in a sizing fixture for neck and handle regions. For household chemical containers, environmental stress-crack resistance is evaluated under ASTM D1693, Condition A or B, with the specific F50 acceptance criterion set by the brand owner. Grade-specific published data for COM70HF1 in extrusion blow moulding is available from the producer’s technical service, but line validation remains required because parison sag depends on melt temperature, shot size, and die gap together rather than on melt index alone.

    Thermoformed Thin-Gauge Sheet: Plug-Assist Sequencing and Cooling

    Sheet extrusion at 0.3–1.0 mm gauge demands a flat die with automatic gauge control keeping thickness within ±3% across the web. Melt temperature at the die is maintained at 200–220 °C, and the sheet is polished on a three-roll stack with roll temperatures of 60–90 °C to balance surface gloss and residual stress. The reheated sheet enters a form-cut-in-place thermoformer where the lower surface temperature is set just above the crystalline melting temperature; the grade-specific peak melting point is determined by ISO 11357-3 differential scanning calorimetry. Plug-assist speed, plug depth, and plug delay are set as a coordinated sequence to avoid base-thickness thinning below 60% of the starting sheet gauge. Plug material is syntactic foam or P20 steel with independent temperature control, and plug surface texture is specified to avoid sticking without the use of external release agents that could compromise food-contact compliance. Vacuum and air pressure are sequenced only after the plug has displaced the sheet into the cavity, preventing early cooling against the plug. Residual moisture in the sheet above 0.02% causes bubble defects during heating; pre-drying is required when storage humidity exceeds 60% RH. For fatty food applications, compliance under EU No 10/2011 requires migration testing with simulant D2 according to EN 1186-1, and the thermoformed article should be trimmed with die cutting that compensates for anisotropic sidewall shrinkage.

    In masterbatch production, HDPE COM70HF1 functions as a carrier resin for pigment and additive systems that are let down at 2–5% in the final moulding or extrusion resin. Compounding is performed on a co-rotating twin-screw extruder with an L/D ratio of 40:1 to 44:1 and screw diameters of 25–75 mm depending on line scale. Pigments and mineral additives are introduced through side feeders located after the polymer melting zone, while liquid dispersants and antioxidants are added through injection lances at 0.5–1.5 wt%. Melt temperature is controlled within 200–230 °C and monitored by an infrared melt probe, with vacuum devolatilisation applied at −0.08 MPa to strip residual moisture and low-molecular-weight volatiles. The melt strand is cooled in water at 20–40 °C and pelletised to a uniform length of 2.5–3.5 mm to prevent feeding stratification in downstream dilute-phase blenders. Dispersion quality is inspected by filter pressure rise and by optical microscopy on pressed films, because pigment agglomerates above 10 µm can create film or fibre defects at low let-down ratios. Thermal stability of the compounded carrier is checked by melt flow rate retention after multiple extrusion passes according to ISO 1133-1:2022. A masterbatch based on COM70HF1 cannot automatically inherit the food-contact status of the base resin; every additive formulation must be re-evaluated under EU No 10/2011 and FDA 21 CFR 177.1520 through migration testing of the final article.

    Regulatory verification matrix for finished articles made from HDPE COM70HF1
    JurisdictionRegulation or standardTest methodLimit or requirement
    US food contactFDA 21 CFR 177.1520(c)FDA extraction cellExtractables per food type
    EU food contactEU No 10/2011EN 1186-110 mg/dm² overall migration
    EU industrial articlesRegulation (EC) No 1907/2006Supplier SVHC declaration0.1% w/w per article
    EU electrical/electronicDirective 2011/65/EU Annex IIEN 62321-5Pb 1000 mg/kg, Cd 100 mg/kg

    When COM70HF1 Replaces Conventional HDPE in Monofilament Extrusion

    Monofilament extrusion of HDPE COM70HF1 is limited to diameters above 0.20 mm because the grade’s high-flow behaviour reduces the maximum continuous draw ratio before melt fracture or filament break-up. The line consists of a single-screw extruder with a metering section length of at least 8D, a spinning head with screen pack filtration, a water quench tank at 30–40 °C, a first godet stand, a heated drawing oven, a second godet stand, and an online diameter gauge. Melt temperature is set between 190 °C and 220 °C, and the quench bath temperature is adjusted to control crystalline orientation before drawing. The first godet speed is typically set at 10–25 m/min, while the second godet speed is adjusted to produce a draw ratio of 6:1 to 8:1; however, published data for COM70HF1 in this specific configuration is limited, and the exact draw ratio must be established by line trials. Annealing in a hot-air or water bath at 80–100 °C reduces free shrinkage and stabilises the oriented structure. Tensile strength is measured according to ISO 2062 or ASTM D2256, and knot strength is determined separately because high-flow HDPE can show lower knot efficiency than grades designed for monofilament. For netting and brush applications, elongation at break is normally maintained above 15%, but the acceptable range depends on the end-use standard and the drawing ratio selected.

    Compression Moulding Is Applied to Prototype Liners and Thick-Wall Parts

    Compression moulding is applied when short runs or thick-walled parts require low residual stress and the absence of gate or weld-line weaknesses. COM70HF1 is charged as powder or pellets into a matched metal mould mounted in a hydraulic press. Mould temperature is maintained at 170–190 °C, and clamp pressure is applied at 2–5 MPa on the projected part area. The press closes in multiple stages, with slow closing below 50 mm/s for the final 5 mm of stroke to allow trapped air to escape. Breathing cycles may be introduced at 30 s intervals to vent volatiles and reduce void formation in thick sections. Cooling under pressure is continued until the core temperature falls below 60 °C, because ejection above this temperature can cause post-mould warpage. Dimensional stability is measured after 48 h relaxation according to ISO 279, and cooling rates above 10 °C/min are avoided in sections thicker than 10 mm to minimise internal voids. This route is suitable for prototype liners, thick-walled machine guards, and moulded plates where compression moulded consistency under ISO 293 is required for material qualification. For industrial parts placed on the EU market, REACH Article 33 of Regulation (EC) No 1907/2006 requires SVHC content to remain below 0.1% w/w per article unless specific communication obligations are triggered.

    Free Quote

    Competitive Versalis HDPE COM70HF1 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE COM70HF1 is a high-density polyethylene grade supplied by Versalis for injection moulding and compression moulding operations. The product designation carries the manufacturer, polymer family, base series, and a flow-related suffix. Lot release is controlled by the certificate of analysis issued for the production batch. Where open-access technical data for the specific COM70HF1 configuration are limited, the values cited in this document are class-typical for high-flow HDPE injection moulding grades and must be checked against the supplier’s technical data sheet before process or part qualification.

    As a high-density polyethylene, the grade is classified by a density equal to or greater than 0.940 g/cm³ when tested under ISO 1183-1:2019 at 23 °C. The high-flow identifier is relevant to mould filling, screw recovery time, gate freeze, and part shrinkage. Melt mass-flow rate for high-flow HDPE grades is conventionally reported under ISO 1133-1:2022 at 190 °C and 2.16 kg; the exact COM70HF1 melt-flow specification shall be taken from the supplier-controlled datasheet because production campaigns can vary within the product specification band. The combination of density, molecular weight distribution, and comonomer placement determines short-term mechanical response, warpage behaviour, and environmental stress crack resistance in the final part.

    How Does Melt Rheology Influence Cycle Time and Gate Freeze in Thin-Wall Moulds?

    Processing conditions for the COM70HF1 class are established on conventional injection moulding machines with screw L/D ratios between 20:1 and 24:1 and compression ratios of 2.5:1 to 3.5:1. The melt temperature band for high-flow HDPE is 200 °C to 250 °C; the mould wall temperature is normally maintained between 10 °C and 40 °C for rigid packaging, closures, and thin-wall containers. At mould temperatures above 40 °C, cycle time increases and post-ejection shrinkage may produce dimensional drift. At melt temperatures below 180 °C, injection pressure rises and short shots occur in sections below 1.0 mm. At melt temperatures above 280 °C, residence time must be shortened to avoid oxidative degradation and discoloration.

    High-flow HDPE grades of this type exhibit pseudoplastic behaviour. Melt viscosity under low shear can be one to two orders of magnitude higher than under injection shear rates of 10³ s⁻¹ to 10⁴ s⁻¹. This shear-thinning characteristic supports thin-wall filling but requires balanced runner systems. In multi-cavity tools with unequal gate freeze times, cavity-to-cavity mass variation can exceed 1.5%. Gate freeze in closures with wall sections below 1.0 mm can occur within 2 s to 4 s. The resulting processing window is narrow because early switch-over causes short shots, while late switch-over increases flash and part mass variation. Velocity-to-pressure switch-over should therefore be based on cavity pressure rather than screw position alone.

    Production-scale observations on machines with clamp force from 1000 kN to 3000 kN indicate that screw recovery time can increase when pellets stored in humid ambient conditions form throat bridging. If pellet surface moisture is suspected because of storage at relative humidity above 60%, pre-drying at 60 °C to 80 °C for 1 h to 2 h in a desiccant or hot-air hopper dryer reduces splay formation and melt-pressure variability. Feed-zone temperature should remain below 50 °C to prevent pellet softening and bridging. Melt pressure fluctuation above 15% at a constant screw speed is an indicator of feed inconsistency rather than a normal melt viscosity shift.

    Mechanical properties of high-flow HDPE injection moulding resins are documented under ISO and ASTM methods. For HDPE class materials, tensile yield stress determined according to ISO 527-2:2012 is typically 22 MPa to 30 MPa, with elongation at yield of 6% to 12%. Flexural modulus under ISO 178:2019 is usually 900 MPa to 1500 MPa. Notched Charpy impact strength under ISO 179-1:2010 at 23 °C is commonly 4 kJ/m² to 8 kJ/m²; at -20 °C values may fall to 2 kJ/m² to 4 kJ/m². The exact COM70HF1 values must be read from the supplier data sheet because additive package and comonomer distribution affect impact performance. Environmental stress crack resistance under ASTM D1693-21 is sensitive to comonomer type and molecular weight; high-flow HDPE grades may show shorter ESCR than bimodal pipe grades, which is acceptable for short-lived or rigid packaging applications but must be evaluated when detergents or oils are present.

    PropertyTest methodClass-typical range for high-flow HDPECOM70HF1 confirmation
    DensityISO 1183-1:2019≥0.940 g/cm³Lot certificate
    Melt mass-flow rateISO 1133-1:2022Supplier specification bandRequired
    Tensile yield stressISO 527-2:201222–30 MPaRequired
    Flexural modulusISO 178:2019900–1500 MPaRequired
    Notched Charpy at 23 °CISO 179-1:20104–8 kJ/m²Required
    Vicat softening temperatureISO 306/A120120–130 °CRequired
    Heat deflection temperature at 0.45 MPaISO 75-2/B60–80 °CRequired

    The material is used in injection moulded closures, crates, housewares, industrial containers, and thin-wall packaging where fast cycle time and controlled shrinkage are required. In closure applications, continuous use temperature is normally limited below 70 °C under low load because creep and stress relaxation increase with temperature. Contact with aggressive hydrocarbons, surfactants, or oxidising media can accelerate environmental stress cracking; compatibility testing under the service fluid is required before production release. The grade is not intended for pressure pipe service.

    When This Polyethylene Class Is Compared With Bimodal Pipe and Blow-Moulding Resins

    The COM70HF1 high-flow class differs from blow-moulding HDPE in melt strength and flow behaviour. Blow-moulding HDPE grades are typically designed with low melt-flow rates of 0.2 g/10 min to 1.5 g/10 min at 190 °C and 2.16 kg and broad molecular weight distributions to stabilise parison formation. In contrast, high-flow injection grades flow at higher melt-flow values and have narrower molecular weight distribution. This lowers die swell and improves dimensional tolerance in injection cavities but reduces sag resistance in extrusion blow moulding. Compared with bimodal high-density polyethylene pipe resins formulated for long-term hydrostatic strength and slow crack growth resistance under ISO 9080:2012, the COM70HF1 class is not intended for pressure pipe applications where minimum required strength values of 8 MPa to 10 MPa at 20 °C and 50 years are specified.

    Compliance referenceTypical assessment for HDPE injection gradeSupplier confirmation required
    REACH Regulation 1907/2006/ECSubstance registration and safety data sheet applyYes
    RoHS Directive 2011/65/EU as amendedBase HDPE normally considered compliant; additive package must be assessedYes
    FDA 21 CFR 177.1520Olefin polymers may comply for food contact subject to conditions of useYes
    Drying thresholdSurface moisture control at relative humidity above 60%Process control
    Melt residence limitKeep below 15 min at melt temperature; avoid sustained exposure above 300 °CProcess control

    Operational boundaries include the avoidance of strong oxidising media such as concentrated nitric acid or halogens at elevated temperature. The use of regrind is permitted when melt-flow shift and impact retention are monitored; regrind addition above 20% can alter filler distribution and reduce Charpy impact unless process parameters are revalidated. The grade should not be combined with amine-based processing additives where oxidative stability is critical, because some amine chemistries can interfere with the stabiliser package and shorten thermal-oxidative lifetime. Storage should be in closed containers at ambient temperature below 40 °C and protected from direct sunlight and rain. Any lot release decision is based on the product certificate of analysis and the supplier’s current technical data sheet, not on class-typical ranges alone.