| HS Code | 764480 |
| Polymer Type | High-density polyethylene |
| Comonomer | Butene-1 |
| Elongation At Break Percent | >600 |
| Water Absorption Percent | <0.01 |
| Volume Resistivity Ohm Cm | >1E16 |
As an accredited Versalis HDPE BC 86 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE BC 86 is supplied in 25 kg polyethylene bags, usually stacked on 1,000 kg pallets. |
| Container Loading (20′ FCL) | Versalis HDPE BC 86 in 25 kg bags, palletized, stretch-wrapped, and securely loaded into a 20′ FCL container for shipment. |
| Shipping | Versalis HDPE BC 86 is shipped as non-hazardous, solid high-density polyethylene pellets in moisture-proof bags or octabins. It is not classified as dangerous goods under ADR, IMDG, or IATA regulations. Keep packages dry, ventilated, and away from heat, sunlight, and ignition sources. |
| Storage | Store Versalis HDPE BC 86 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged high-temperature storage. Maintain good housekeeping to prevent dust accumulation and slipping hazards. Do not store near food, feed, or drinking water. |
| Shelf Life | Versalis HDPE BC 86 has a 24-month shelf life when stored sealed in original packaging, dry, away from sunlight and heat. |
On shuttle blow moulding lines producing UN 3H1 jerrycans and tight-head industrial canisters, Versalis HDPE BC 86 is fed as 100% virgin feedstock or as a let-down from 10–20 wt% post-industrial flash regrind generated on the same line. The grade combines a high-load melt index of 5–7 g/10 min at 190 °C/21.6 kg under ISO 1133-1:2022 with a density of 0.952–0.956 g/cm³ under ISO 1183-1:2019, placing it in the high-molecular-weight HDPE blow moulding class. The extruder is typically a grooved-barrel shuttle machine with L/D 24:1 and a barrier screw, metering at 150–250 kg/h depending on shot weight. Screw speed is held between 40 min⁻¹ and 70 min⁻¹ to avoid shear overheating. Barrel zones are set at 170–190 °C in the feed section, 190–210 °C in the compression and metering sections, and 195–210 °C at the die head; insertion-probe melt temperature is 195–215 °C. Parison programming is executed over 20–32 points with die-gap changes between 1.0 mm and 2.5 mm to compensate for parison swell and sag at shot weights of 1.8–3.2 kg. Blow air is introduced at 0.6–0.8 MPa through a calibrated blow pin. Mould temperature is held at 8–15 °C with closed-loop chiller circuits. Cycle time for a 25 L jerrycan is 70–110 s, including hot trimming and post-mould leak testing. Wall thickness is maintained at 1.8–2.5 mm in the sidewall; pinch-off and handle regions are radiused to at least 10 mm to reduce environmental stress cracking. If silo temperature is below 10 °C and ambient relative humidity is above 60%, surface condensation on cold pellets can generate pinholes; pellets should be equilibrated at 20–25 °C for at least 4 h before feeding. The final containers are certified under UN 3H1 classifications for dangerous goods transport under ADR 6.1.4 and IMDG Chapter 6.1. Drop testing requires equilibrium at −18 °C for 24 h followed by a 1.2 m drop onto a rigid steel plate with no leakage. Stack testing applies a load equivalent to 3.0 m for 28 days at 40 °C. Terminal products are 20 L, 25 L and 30 L shoulder-handled jerrycans for lubricants, detergents, agricultural adjuvants and water-miscible industrial fluids.
For crop-protection and adjuvant packaging, the limiting mechanical failure is environmental stress cracking initiated at the pinch-off rim and closure thread, not short-term burst strength. BC 86 is processed on single-station and tandem extrusion blow moulders with 60–90 mm screws and L/D 24:1–28:1. Barrel zones are set from 180 °C to 210 °C, and the die head is held at 200–220 °C. The parison is inflated with dry air at 0.6–0.8 MPa; mould bodies are chilled to 8–18 °C. Hot trimming at the pinch-off is followed by compressed-air cooling of the tail flash under the mould clamp, because cold trimming of thick crystalline pinch-off creates micro-crazes that accelerate ESCR in aliphatic hydrocarbon carriers and aromatic solvents. The formulation for hazardous agrochemical containers excludes post-industrial regrind; a compatible HDPE colour masterbatch is dosed at 1.5–2.0 wt%, and a UV stabiliser masterbatch at 0.5–1.0 wt% for outdoor warehouse storage. Chemical resistance is interpreted through ASTM D543-21 immersion tests in the specific pesticide or fertiliser formulation; the refusal criterion is a tensile elongation loss exceeding 25% at 23 °C after 7 days. Oxidation resistance is assessed by ISO 11357-6:2018; the oxygen induction time at 200 °C should remain above 20 min for sulfur-containing formulations. Internal hydraulic leakproofness is checked at 20–30 kPa for 5 min on every lot. The terminal products are F-style narrow-neck 1 L, 5 L and 10 L jugs, plus 30 L and 60 L open-head drums for liquid fertiliser and seed-treatment products. BC 86 is not recommended for >30 wt% hydrogen peroxide, fuming nitric acid, or formulations containing >5 wt% free amine bases unless fluorination or a separate barrier layer is applied. Published data for crop-protection formulation interactions with BC 86 is limited; immersion testing on the final bottle remains mandatory before line qualification.
Multilayer automotive fuel tank lines with six extruder stations use BC 86 as the outer HDPE layer and as the regrind-incorporating structural layer, while a separate carbon-black-loaded conductive HDPE forms the inner fuel-contact surface. The system includes 45–75 mm grooved-barrel extruders discharging into a six-layer spiral mandrel die; the barrier layer is EVOH with 32–38 mol% ethylene content, and maleic anhydride-grafted LLDPE adhesives are used on both barrier sides. Layer ratios are maintained by independent gravimetric feeders and melt pumps; a representative outer-to-inner distribution is 12/30/3/3/25/27 wt% for outer HDPE, regrind, adhesive, EVOH, adhesive, conductive inner HDPE. Extrusion temperatures are limited to 200–220 °C for BC 86 and 210–220 °C for EVOH; residence time above 230 °C generates acetic acid volatiles and gel defects at the EVOH-adhesive interface. The die head operates at 210–230 °C, and the blow mould is held at 8–18 °C. The parison is pre-inflated at 0.1–0.3 MPa and then blown at 0.6–0.8 MPa; a 70 L tank cycle is 120–180 s. Fuel tanks containing BC 86 in the outer layer must pass evaporative emission tests under 40 CFR Part 86.1811 and ECE R34 Annex 5; the EVOH barrier layer is adjusted to 2–3 wt% of the total coextrudate to meet CARB LEV III hydrocarbon permeation limits. The outer surface is pigmented with carbon black at 2.0–3.0 wt% to provide a surface resistivity below 106 Ω/square under ISO 3915:2020. Terminal components are 40–95 L automotive fuel tanks, filler necks and expansion chambers for spark-ignition and diesel vehicles. BC 86 without conductive carbon black is not used on the fuel-contact layer, because a surface resistivity above 106 Ω/square presents an electrostatic discharge risk during refuelling and vapour recovery.
Large-part blow moulding of 120 L, 160 L and 220 L drums uses accumulator-head machines with 100–150 mm extruders, L/D 24:1, and clamp force ratings above 1,000 kN. BC 86 is fed at 150–250 kg/h; barrel temperatures progress from 170 °C in the feed throat to 210 °C at the accumulator outlet. The accumulator shot is discharged at 200–220 °C through a diverging die with 100–200 point parison programming. The programming profile is parabolic, with thicker segments at the top chime and bottom rim to compensate for sag over a parison length of 1.8–2.5 m. Wall thickness targets are 2.5–3.5 mm at the top chime, 3.0–4.0 mm at the bottom corner, and 2.0–2.8 mm in the body. Blow air at 0.8–1.0 MPa enters through a bottom-up blow pin; mould circulation water is kept at 10–18 °C. Cycle time is 180–300 s for a 220 L L-ring drum. The formulation incorporates 10–25 wt% post-industrial regrind from the same drum line; if regrind is added, high-load melt index is monitored every 2 h by ISO 1133-1:2022 at 190 °C/21.6 kg to keep the lot within 5.0–7.5 g/10 min. Drums are certified under UN 1H1 for solids and liquids; the drop test for a 220 L drum at packing group II is 1.2 m at −18 °C, and the stack test applies a load equivalent to 3.0 m for 28 days. Food premix drums require FDA 21 CFR 177.1520(c) 3.1a/3.2a and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². Terminal products are open-top 120 L fibre-pack liners, 160 L straight-wall drums, and 220 L L-ring drums for lubricants, food premixes, detergents and industrial powders.
Potable water storage tanks in the 50–1,000 L class are blow moulded from BC 86 as a 100% virgin low-odour feedstock, without post-consumer recyclate, because residual contaminant migration cannot be controlled in non-food-certified waste streams. The platform is a stationary or rotary blow moulder with a 90–120 mm grooved-barrel extruder, L/D 24:1, and an accumulator of 5–20 kg shot capacity. Melt temperature is held at 180–205 °C; the die head is set at 190–205 °C to reduce thermal oxidation and keep taste-and-odour extractables low. Mould bodies are maintained at 15–25 °C, with cycle times from 4 min for 50 L tanks to 15 min for 1,000 L tanks. The parison is inflated with clean dry air at 0.5–0.7 MPa, and the part is cooled internally with chilled air or nitrogen at 5–12 °C. Wall thickness is programmed to 3.0–5.0 mm at the tank shoulder and 2.5–3.5 mm in the sidewall. Closure bosses and threaded fitting areas are stress-relieved by maintaining a minimum 8 mm radius and by post-mould annealing at 70 °C for 2 h to reduce stress cracking at insert interfaces. Final articles are vertical cylindrical storage tanks, horizontal RV water tanks, and marine holding tanks. Compliance is verified under NSF/ANSI/CAN 61:2023 for materials in contact with drinking water; extraction testing includes pH 5 water and pH 10 water at 23 °C and 60 °C. European conformity is assessed under Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². BC 86 is not recommended for continuous exposure to water above 60 °C, because oxidative stabiliser depletion accelerates above that threshold and reduces long-term hydrostatic strength.
Post-industrial flash, start-up purgings and off-spec containers can be recycled into BC 86 for non-potable industrial drums only if the regrind stream is separated by lot and melt index. The recycled material is ground to a controlled flake of ≤12 mm, dedusted, and metered through a gravimetric side feeder at 5–30 wt% into a co-rotating twin-screw extruder with L/D 44:1 and vacuum devolatilisation at −0.07 to −0.09 MPa. The barrel is set from 160 °C to 210 °C, and the melt temperature is held at 190–215 °C. The following control band is applied to separate acceptable from non-acceptable regrind lots.
| Regrind fraction | Allowed packaging field | Test method | Lot-control criterion |
|---|---|---|---|
| 5–15 wt% | UN 1H1 liquid drums, tight-head containers | ISO 1133-1:2022 | HLMI 190 °C/21.6 kg within 5.0–7.0 g/10 min |
| 16–25 wt% | Open-head drums, solids pails | ISO 16770:2019 | FNCT 50 °C/3 MPa above 100 h |
| 26–30 wt% | Non-hazardous solid packaging, drain sumps | ISO 11357-6:2018 | OIT 200 °C above 15 min |
Retention of process stabiliser is verified by oxidative induction time at 200 °C; if OIT falls below 15 min under ISO 11357-6:2018, the regrind level is reduced to below 15 wt% for liquid-contact drums. With 5–15 wt% regrind, UN 1H1 drop and stack performance is generally retained; at 15–25 wt%, top-load capacity and ESCR may decrease by 10–25%, requiring an increase in wall thickness of 0.3–0.8 mm. At 25–30 wt%, the recycled fraction is restricted to non-hazardous solid packaging, dust caps and drain sumps, not to tight-head liquid containers. The recycled stream must not contain EVOH barrier regrind, adhesive layers, or carbon-black-loaded fuel-tank scrap; incompatible layer contamination produces delamination and pinhole defects. Batch consistency is checked every 4 h by ISO 1133-1:2022 high-load melt index; density is checked by ISO 1183-1:2019; notched Charpy impact is measured on compression moulded plaques by ISO 179-1:2010. Terminal products are 60 L open-head drums, 120 L pails, pallet collar profiles and non-food industrial canisters.
Competitive Versalis HDPE BC 86 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The resin identified as Versalis HDPE BC 86 is a high-density polyethylene grade assigned to the BC series of the Versalis polyethylene portfolio. In the producer’s technical documentation the BC prefix denotes extrusion blow-moulding polyethylene; the suffix 86 is the grade identifier. Published data for this specific configuration is limited in consolidated public databases. Nominal density, melt mass-flow rate, and mechanical values must therefore be obtained from the certificate of analysis and the current technical data sheet. The following sections address process behaviour, characterisation methods, regulatory verification, and differentiation from injection-moulding and other HDPE classes. No generic polyethylene value is a substitute for lot-specific data.
High-molecular-weight blow-moulding HDPE of this type is processed on single-station shuttle or long-stroke blow-moulding machines. Typical barrel sizes are 80 mm to 120 mm with L/D ratios from 20:1 to 30:1. Melt temperature measured at the die head is maintained between 180 °C and 230 °C. The upper limit is set by degradation odour, die-lip build-up, and loss of parison uniformity; the lower limit is set by melt pressure rise and unmelted material in the parison. Die gaps of 0.8 mm to 2.0 mm and blow ratios of 2:1 to 3:1 are standard starting points for this product class. On shuttle machines, short-shot defects and wall-thickness variation often result from parison sag before mould closure rather than from low melt temperature. The corrective action is therefore to reduce extrusion time, close the mould earlier, or adjust die gap, not simply to raise barrel temperature.
Characterisation of BC 86 follows the standard HDPE blow-moulding test set. Tensile yield stress and elongation at break are measured according to ISO 527-2:2012; notched impact strength is measured according to ISO 180:2019. Environmental stress crack resistance is tested under ASTM D1693-21, commonly in 10 % Igepal CO-630 at 50 °C. Density is determined by ISO 1183-1:2019 and melt mass-flow rate by ISO 1133-1:2022. ESCR failure time is a lot-specific variable and is not a single design value. Two HDPE grades with the same density within 0.001 g/cm³ can show ESCR failure times that differ by more than one order of magnitude when comonomer placement and molar mass distribution differ. For this reason, a specification comparison based on density alone is technically incomplete.
On accumulator-head machines producing containers above 5 L, the main process conflict is parison sag, which directly changes wall-thickness distribution and top-load performance. Sag is not predicted by melt mass-flow rate at 190 °C/21.6 kg because that test applies shear rates far above the gravitational deformation of a hanging parison. Dynamic shear rheology under ISO 11443 and extensional rheometry provide the relevant comparison. Zero-shear viscosity and strain hardening control sag resistance; a broader molar mass distribution prolongs parison stability. Within the producer’s normal lot-to-lot variation, the die gap may need adjustment by 0.1 mm to 0.3 mm to maintain constant container weight. A four-variable control set of melt temperature, die head pressure, parison length at a fixed timer setting, and part weight should be recorded on the line; deviations in one variable alone are not sufficient for process diagnosis.
Food-contact status for BC 86 is not established by a generic high-density polyethylene statement. Under EU Regulation (EU) No 10/2011, the finished article must meet overall migration limits in specified food simulants; under FDA 21 CFR 177.1520, the olefin polymer must be covered by a grade-specific clearance. The converter is responsible for the effects of regrind, colour masterbatch, and processing aids on migration. REACH SVHC disclosure should be requested for the specific lot. RoHS Directive 2011/65/EU applies only to electrical and electronic equipment, not to packaging unless the container is incorporated into such equipment. The table below lists the verification matrix for contact-sensitive blow-moulding applications.
| Property or requirement | Standard or regulation | Test or purpose |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Flowability comparison; not sufficient for sag prediction |
| Density | ISO 1183-1:2019 | Polyethylene classification |
| Tensile yield stress | ISO 527-2:2012 | Short-term mechanical resistance |
| Notched Izod impact | ISO 180:2019 | Impact resistance at specified temperature |
| Environmental stress crack resistance | ASTM D1693-21 | Failure time in 10 % Igepal CO-630 at 50 °C |
| Vicat softening temperature | ISO 306:2022 | Thermal softening under load |
| Overall migration | EU Regulation (EU) No 10/2011 | Food simulant migration limits |
| Olefin polymer food contact | FDA 21 CFR 177.1520 | Grade-specific clearance record |
Storage and handling of BC 86 resin should follow closed silo or octabin practice. The polymer is not hygroscopic; pre-drying is generally unnecessary below 60 % relative humidity. Condensed surface moisture formed during transfer from cold storage to warm processing areas can produce parison surface defects, so a temperature equilibration delay of 4 h to 8 h is common before the material enters the extruder. Regrind should be sieved to preserve particle-size distribution and limited to 20 % for tight wall-thickness specifications unless a higher fraction has been qualified by drop-impact and top-load testing. Direct outdoor storage should be avoided because extended UV exposure can degrade surface layers and shift ESCR.
Injection-moulding HDPE grades in the same density band are formulated with higher melt mass-flow rates and lower zero-shear viscosity to fill thin-wall moulds under injection pressure. The same property set is inadequate for extrusion blow moulding because it produces parison sag and poor wall-thickness control. Conversely, BC 86 class material is not suitable for injection moulding; high melt viscosity at injection shear rates can cause gate freeze-off and short shots. Blending of blow-moulding and injection-moulding HDPE fractions above 5 wt% is not recommended without measuring parison drop time, weld-line strength, and container drop impact at the intended service temperature. Blow-moulding fitness is therefore determined by high-load flow ratio, die swell stability, ESCR, and extensional rheology, not by a single MFR value.
Additive and colour compatibility should be confirmed with the masterbatch supplier at the intended letdown ratio. Colour masterbatch carriers with melt mass-flow rates above 20 g/10 min measured under ISO 1133-1:2022 can dilute zero-shear viscosity at the die entry. Carrier resins with high flow can locally reduce parison strength and create weld-line cracks. For containers holding aggressive liquids, ESCR testing should be performed on the finished article, not on neat resin alone; the failure mode in service is often a weld-line crack propagating from the pinch-off zone. If the application requires UV stabilisation, the masterbatch should be pre-compounded at the converter level or verified by weathering tests according to ISO 4892-2:2013. Published data for this specific BC 86 configuration under all additive combinations is limited, so compatibility trials are required before production.
Container drop tests show that pinch-off weld zones are the first failure site in many HDPE blow-moulded containers. The weld is created when the mould closes on the parison; local cooling at the mould pinch edge produces a zone of high orientation and reduced ESCR. Under drop impact testing according to ASTM D2463-15 or ISTA 6-A, failure typically initiates at the pinch-off bead or at weld lines. Process controls for pinch-off strength include melt temperature uniformity, mould closing speed, and pinch-off insert design. Mould closing speeds of 200 mm/s to 600 mm/s are typical on shuttle machines, but the applicable range depends on container size and wall thickness. A narrow pinch-off temperature window of ±5 °C may be required for full weld fusion; outside this window, containers may pass top-load testing while failing drop impact after contact with stress-cracking fluids.
Within the blow-moulding HDPE range, the selection between BC 86 and other grades is often a trade-off between stiffness and ESCR. A grade with higher density may provide higher top-load strength but lower ESCR; a grade with lower density may show the reverse. The selection should be made by plotting density, flexural modulus by ISO 178:2019, ESCR by ASTM D1693-21, and top-load performance of the finished container. Without the container geometry, the optimum grade cannot be selected from the data sheet alone. Processing aids should be avoided unless specified by the supplier, and external mould-release sprays can contaminate the weld line and reduce adhesion. Surface slip agents, if required, should be incorporated in the masterbatch and validated by weld-line tensile tests according to ISO 527-2:2012.