| HS Code | 335550 |
| Density | 0.954 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 0.20 g/10 min |
| Melt Flow Rate 190 C 21 6 Kg | 8.0 g/10 min |
| Tensile Modulus | 1500 MPa |
| Tensile Stress At Yield | 28 MPa |
| Tensile Strain At Break | >600% |
| Flexural Modulus | 1400 MPa |
| Charpy Notched Impact Strength 23 C | 15 kJ/m2 |
| Charpy Notched Impact Strength 30 C | 5 kJ/m2 |
| Vicat Softening Temperature | 128 °C |
| Brittleness Temperature | < -70 °C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Hardness Shore D | 64 |
| Water Absorption | <0.01% |
| Dielectric Constant 1 Mhz | 2.3 |
| Volume Resistivity | >10^16 ohm·cm |
| Thermal Conductivity | 0.40 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2e-4 /°C |
As an accredited Versalis HDPE BC 82 PH factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE BC 82 PH is typically supplied in 25 kg polyethylene bags, palletized and shrink-wrapped for transportation. |
| Container Loading (20′ FCL) | Versalis HDPE BC 82 PH high-density polyethylene in 25 kg bags, palletized and securely loaded into a 20′ FCL container. |
| Shipping | Shipping: Versalis HDPE BC 82 PH is non-hazardous high-density polyethylene. Transport in original sealed bags, octabins, or bulk containers, palletized and stretch-wrapped. Store dry, clean, under ambient conditions, away from ignition sources and UV. Not regulated as dangerous goods under DOT, IMDG, IATA, ADR, or RID. |
| Storage | Store Versalis HDPE BC 82 PH in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep in original sealed packaging, palletized and off the floor, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and impact. Maintain stable temperatures, use FIFO rotation, inspect containers, and follow the supplier SDS. |
| Shelf Life | Shelf life: typically 24 months from production date when stored unopened in original packaging, dry, cool, and away from direct sunlight. |
Liquid intermediate packaging classified as packing group II or III under the UN Model Regulations must undergo design-type drop, hydraulic pressure, and stacking tests before a certification mark can be applied to the container. In this application, BC 82 PH is processed as the load-bearing wall resin for containers that must satisfy the 1.2 m drop test in 6.1.5.2, the hydraulic pressure test in 6.1.5.3, and the stacking test in 6.1.5.5. Because aggressive liquid contact tends to produce environmental stress cracking rather than instantaneous tensile overload, the container sidewall material is qualified by ASTM D1693-15 Condition B in 10 % Igepal CO-630 at 50 °C; the converter specification is based on F50 time from production-weight plaques, not solely on compression-moulded sheets. Melt flow rate measured according to ISO 1133-1:2022 at 190 °C under 2.16 kg load is used for incoming resin control only, because processing behaviour is governed by high-load parison sag, ESCR retention, and pinch-off weld strength rather than melt index alone. Where the container is stored outdoors, a carbon black masterbatch is added at 1.5–2.5 wt% to preserve tensile elongation and notched impact after ultraviolet exposure, while the inner wall has no pigmentation to avoid additive migration into stored intermediates. Internally generated HDPE regrind from the same container family is introduced at 20–35 wt%; the upper boundary is set by loss of pinch-off weld integrity and reduced ESCR rather than by melt index drift alone. Above 35 wt%, hydraulic pressure failure at the flash line becomes detectable on production-scale 220 L tight-head drums with body-wall thickness below 3.0 mm at the chime.
Accumulator-head blow moulding machines with screw L/D ratios from 24:1 to 30:1 and barrier screw geometries are used; the melt temperature is held at 180–205 °C, and the die gap is set between 2.0 mm and 4.0 mm to control parison swell while maintaining wall-thickness distribution. Blow pressure is set at 0.6–0.9 MPa, and mould surface temperature is maintained at 8–15 °C to accelerate solidification without inducing warpage at the rim and handle weld zones. For containers above 60 L, parison programming with 10–16 wall-thickness control points is required to hold minimum sidewall thickness above 2.0 mm in the lower body. Finished article categories include 20–60 L monolayer jerrycans, 120–220 L tight-head drums with bung closure geometry, and 1000 L composite IBC inner bottles that rely on the HDPE wall creep resistance under stacking load. Process limitation: melt temperature above 220 °C or accumulator dwell beyond 10 min may generate gel specks and variable parison swell; below 175 °C, interfacial fusion at the pinch-off flash line is incomplete, producing low-temperature drop impact failure at -20 °C. Published data for BC 82 PH at 1000 L IBC inner bottle scale is limited; converter trials are required for design-type certification.
Emulsifiable concentrates and suspension concentrates packaged for agricultural distribution are subject to UN packing group II or III certification under 6.1.5.2, with stacked warehouse storage verified under 6.1.5.5 at elevated ambient temperature. Sealing zones and labelled sidewalls must tolerate cyclic contact with aromatic solvent carriers and surfactant systems, so ESCR testing by ASTM D1693-15 Condition B at 50 °C is applied to production-weight plaques cut from container sidewalls rather than only to compression-moulded sheets. To lower hydrocarbon permeation below local regulatory thresholds, a three-layer co-extrusion structure is used in which a polyamide barrier layer occupies 5–8 wt% of total container mass and each tie layer occupies 1.5–2.5 wt%; the remaining mass is BC 82 PH-based HDPE skins and internally generated regrind. In the outer skin, a 2–4 wt% UV-stabilizer and opacifier masterbatch is let down at the feed throat, with the actual ratio determined by wall thickness and required shelf life under ISO 4892-2 Cycle A. A separate white opacity masterbatch may be included at 1–2 wt% to prevent ultraviolet transmission through translucent label windows. Processing on three-layer co-extrusion blow moulding lines requires separate melt-temperature control: HDPE skins and regrind at 185–205 °C, adhesive tie layers at 200–220 °C, and polyamide at 230–250 °C; the die gap is held at 2.5–4.5 mm to maintain layer uniformity through the parison programming arc. Blow pressure is 0.7–1.0 MPa, and mould temperature is kept at 8–18 °C to prevent interlayer instability in the handle weld. Finished articles include 250 mL, 500 mL, 1 L, 2.5 L, and 5 L crop protection bottles with 45 mm and 63 mm neck finishes, plus 10 L and 20 L jugs with tamper-evident closures. Published data for this specific BC 82 PH grade in fluorinated monolayer configurations is limited; fluorination barrier post-treatment, when used, must be separately validated because surface fluorine concentration can alter weld-line toughness.
Six-layer blow moulding lines for fuel system components assign BC 82 PH to the virgin outer and inner surfaces plus the internally generated regrind core, while the central EVOH layer provides hydrocarbon permeation resistance for evaporative emission control. The outer virgin HDPE layer is 20–30 wt% of total wall mass, the inner virgin HDPE layer is 30–40 wt%, the regrind core is 20–30 wt%, the EVOH barrier is 2–3 wt%, and each tie layer is 1.5–2.5 wt%; these ratios are adjusted by the die-head layer pack so that the EVOH thickness does not fall below 40 µm at the pinch-off region after parison inflation. Federal evaporative emission compliance under 40 CFR Part 86 and European vehicle component type approval under ECE R34 require barrier retention after slosh, pressurization, and thermal ageing; the converter gravimetric permeation test is typically run at 40 °C with a 28-day stabilisation period. Processing on six-extruder accumulator-head machines uses an HDPE melt temperature of 210–230 °C for the BC 82 PH layers, a barrier melt temperature of 205–220 °C, and a tie-layer melt temperature of 210–225 °C. The die gap is 2.5–4.0 mm and blow pressure is 0.6–1.0 MPa; mould surface temperature is maintained at 8–18 °C to control barrier-layer thinning at the pinch-off. Accumulator dwell time is limited to 8–12 min to prevent gel particles from crosslinking residues in the regrind fraction. Terminal article categories include passenger-car and light-commercial saddletanks in the 40–100 L range, filler necks, vapour recovery canister shells, and small marine fuel cells. Published data for this specific BC 82 PH grade in six-layer fuel tank structures is limited; tank producers qualify the resin on production-scale co-extrusion heads because parison swell variations above ±8 % shift barrier-layer thickness beyond permissible limits.
AUS 32/diesel exhaust fluid packaging must prevent trace contamination and withstand outdoor storage at sub-zero temperatures without crack initiation at the handle weld or chime. ISO 22241-3:2019 sets packaging requirements for AUS 32; the converter must show that the filled container does not increase trace element concentration beyond the fluid limits of ISO 22241-2, using ICP-OES analysis after 30 days of contact at 40 °C. Because AUS 32 is sensitive to light and heat, containers are normally compounded with carbon black masterbatch at 1.0–1.5 wt%; this loading yields an opaque wall at 1.5–2.5 mm thickness while preserving weld-line impact strength. The addition window must not exceed 2.0 wt% carbon black because higher solids loading increases die-head pressure and reduces low-temperature impact resistance; if lower opacity is acceptable, a non-pigmented UV-stabilizer package is used at 0.2–0.4 wt%. Processing is conducted on continuous shuttle or accumulator-head blow moulding machines with melt temperature 180–205 °C, die gap 2.0–4.0 mm, blow pressure 0.5–0.8 MPa, and mould temperature 10–20 °C to maintain top-load strength for stacked pallets. Finished article categories include 3 L, 5 L, 10 L, and 20 L HDPE containers for DEF service refill, plus 1000 L IBC inner bottles for bulk storage. Published data for BC 82 PH at -30 °C in DEF-specific containers is limited; low-temperature instrumented puncture testing according to ISO 6603-2 at -30 °C should be performed on production container sidewalls before design-type certification.
High-viscosity cleaner and surfactant packaging with integrated handles and narrow neck finishes is manufactured on shuttle blow moulding stations where parison programming directly controls sidewall distribution in the grip zone and base corner. Mechanical verification of finished containers is performed under ASTM D2659-16 for column crush, ASTM D5276-19 for vertical drop, and ISO 12048 for compression; compatibility with detergent formulations is content-driven under Regulation (EC) No 648/2004, but long-term storage at 40 °C and 75 % relative humidity is used to detect environmental stress crack initiation at handle inserts. The blend includes 1–2 wt% colour masterbatch and 2–3 wt% titanium dioxide-based opacity concentrate in the outer skin, with 0.5–1.0 wt% antistatic masterbatch only where dry powder filling systems produce dust adhesion; calcium carbonate-based fillers are excluded above 5 wt% because they reduce pinch-off weld strength and lower top-load performance. Processing uses a melt temperature of 180–200 °C, mould temperature 10–20 °C, blow pressure 0.5–0.8 MPa, and parison programming with 8–12 wall-thickness control points to maintain a minimum sidewall thickness of 0.8 mm in handle/body transitions. Finished article categories include 250 mL and 500 mL trigger-spray bottles, 750 mL and 1000 mL handled stock bottles, 5 L refill packs, and 25 L open-top pails for industrial surface-care concentrates. Published data for BC 82 PH with antistatic masterbatch above 1.0 wt% is limited; converter trials are required because certain ethoxylated amine antistats migrate and reduce bottle surface print adhesion after 72 h of storage at 60 °C.
Corrosive waste collection and secondary containment packaging requires a balance between recycled-content sustainability and retained ESCR, because waste streams may include oxidising acids, alkalis, and solvent-contaminated water. Compliance with the UN Model Regulations for packing group II or III under 6.1.5.2 and 6.1.5.3 is required for the primary container, while secondary containment shells are frequently validated under the same design-type tests even when not marked as UN packagings. The blend formulation for BC 82 PH includes 10–30 wt% post-industrial regrind from the same container family and 0–10 wt% post-consumer HDPE recyclate only after melt filtration with a 120–150 µm screen pack and vacuum devolatilization to remove low-molecular-weight odour bodies. Carbon black masterbatch is added at 1.5–2.0 wt% for grey or black waste containers; acid-scavenging metal stearate additive is not used above 0.2 wt% because excess zinc or calcium stearate migrates into stored leachate samples and alters pH correction measurements. Processing on accumulator-head blow moulding equipment is maintained at 180–205 °C melt temperature, with a die gap of 2.5–4.5 mm and a blow pressure of 0.6–0.9 MPa to fill deeply recessed handle geometries and screw-cap chimes; mould surface temperature is 10–18 °C. Terminal finished article categories include 5 L, 10 L, 20 L, and 30 L waste-solvent containers, 60 L secondary containment bottles, and 120 L overpack drums. Published data for this specific BC 82 PH/post-consumer recyclate blend at the 10 wt% addition level is limited; each converter must generate design-type certification data on finished production tooling rather than laboratory-scale compression moulding for UN 6.1 hydraulic pressure testing.
Competitive Versalis HDPE BC 82 PH prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE BC 82 PH is a high-density polyethylene supplied in pellet form and intended for extrusion blow moulding on shuttle, reciprocating-screw and accumulator-type lines. Manufacturer-published typical values, not batch-release specifications, place density at 0.953 g/cm³ according to ISO 1183-1 and melt flow rate at 0.25 g/10 min at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. The low melt index relative to injection moulding HDPE indicates a higher-molecular-weight chain population that resists parison sag during mould open time. High-flow injection moulding grades typically exhibit melt flow rates above 4 g/10 min to fill thin-wall cavities, while extrusion coating grades often require melt flow rates above 7 g/10 min to achieve low neck-in at high line speed. Such grades would exhibit excessive parison drawdown and inconsistent wall thickness in blow moulding tools. BC 82 PH therefore occupies a different processing envelope: higher melt strength and extruder head pressure, lower melt pump throughput for a given screw speed, and improved parison integrity during transfer from die to mould.
On production-scale single-station shuttle machines using grooved-barrier extruders of 60–120 mm diameter and L/D 24:1–30:1, melt temperature is generally held between 200 °C and 220 °C. Feed-zone setpoints of 170–190 °C reduce premature melting and granule bridging, while compression and metering zones are maintained at 190–205 °C. Head and die setpoints are commonly 200–210 °C. Die gap is typically set between 1.5 mm and 3.0 mm depending on parison diameter and target wall thickness. If die-gap opening is increased without raising melt temperature, die swell can enlarge the parison beyond the flash pocket, generating pinch-off defects and excessive flash trim.
Weld-line formation in extrusion blow moulded containers is a critical quality variable for BC 82 PH. Poor weld-line strength produces failure at the pinch-off zone during drop impact or hydraulic pressure testing. The primary process parameters are melt temperature, die land length, parison length and mould flash-pocket geometry. Melt temperatures below 195 °C increase viscosity at the pinch-off surface and can prevent sufficient intermixing of the folded parison edges. Flash-pocket depth and pinch-off land width determine the local compression applied to the weld; a pinch-off land width of 0.5–1.5 mm is typical for HDPE industrial containers, with flash pockets sized to accept 10–25% of the parison wall thickness as flash. Excessive melt temperature above 230 °C can reduce parison melt strength and increase sag, producing thin sidewalls and variable weld thickness. The resin’s low melt flow rate of 0.25 g/10 min widens this processing window relative to lower-viscosity HDPE grades, but it does not eliminate line-specific weld qualification.
Drop-impact performance is evaluated according to ASTM D2463 or UN 6.1.5.3 for dangerous-goods packaging. Published data for this specific grade in UN/DOT-certified jerry cans is limited; therefore, container qualification must be performed on the actual production tool. Field experience on shuttle blow moulding lines indicates that batch-to-batch melt flow rate variation of ±0.03 g/10 min can alter parison sag time and weld thickness. Processors should lock screw speed, die gap and extruder barrel profile rather than relying solely on melt temperature to compensate for resin lot changes.
The table below reproduces manufacturer-published typical values for BC 82 PH. These values are reference data for material selection and are not guaranteed limits or batch-release specifications.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 0.953 g/cm³ |
| Melt flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | 0.25 g/10 min |
| Tensile stress at yield | ISO 527-2 | 26 MPa |
| Tensile modulus | ISO 527-2 | 1050 MPa |
| Flexural modulus | ISO 178 | 1100 MPa |
| Elongation at break | ISO 527-2 | >500% |
| Vicat softening point, A/50 | ISO 306 | 127 °C |
| Environmental stress-crack resistance | ASTM D1693, condition A | >100 h |
The combination of flexural modulus near 1100 MPa and environmental stress-crack resistance above 100 h under ASTM D1693 condition A places BC 82 PH in the stiffness range required for stackable industrial containers while retaining resistance to stress cracking in aggressive detergent or oil-based formulations. By comparison, lower-density HDPE grades with density below 0.945 g/cm³ often show lower top-load strength, and high-flow injection moulding grades with melt flow rates above 4 g/10 min typically sacrifice environmental stress-crack resistance because of lower molecular weight. The density of 0.953 g/cm³ also reduces permeation of aliphatic hydrocarbons relative to lower-density polyethylene types, but actual permeation rates must be measured on the finished container according to ASTM D3985 or ISO 14663-2 for the intended chemical service.
BC 82 PH is supplied as a hydrophobic polyolefin pellet with low ambient moisture uptake. However, storage in unsealed silos or open octabins at relative humidity above 60% can introduce surface moisture onto pellets. Surface water does not hydrolyse the polyethylene backbone, but it can produce steam bubbles, surface splay and intermittent parison rupture when melt temperature exceeds 200 °C. Pre-drying is unnecessary under normal indoor storage below 50% RH, but hopper heating or a desiccant-bed hopper dryer set at 70–80 °C for 1–2 h is applied on some lines when condensation is observed. Avoid overheating pellets above 90 °C in hopper dryers because pellet surface tacking and feed-throat bridging can occur.
Regrind addition is standard in extrusion blow moulding of industrial containers. For BC 82 PH, regrind levels up to 30 wt% are commonly run when the regrind is clean, dry and free of degraded resin from previous heat histories. Each additional heat history reduces the high-molecular-weight fraction and narrows the processing window. Regrind above 30 wt% can reduce environmental stress-crack resistance, drop-impact performance and parison melt strength. Because BC 82 PH relies on high melt strength for parison stability, blends containing high concentrations of lower-viscosity HDPE regrind may sag and produce uneven wall thickness. Blending with external post-consumer recyclate is not recommended unless the recyclate is sorted, hot-washed HDPE with known melt flow rate and density. Uncontrolled recyclate with polypropylene contamination can create delamination, weld-line weakness and surface defects.
The resin is not formulated for injection moulding of thin-wall containers, rotomoulding, film extrusion or profile extrusion. Attempting to process BC 82 PH in high-shear injection moulding machinery with small gates and long flow paths can produce short shots, excessive injection pressure and incomplete packing because of its high melt viscosity. The grade is also not designed for fluorination or sulfonation treatments required for permeation-resistant fuel tanks; compatibility with such post-treatment must be confirmed through separate testing.
| Regulatory area | Standard or regulation | Typical verification requirement |
|---|---|---|
| European food-contact plastics | EU Regulation 10/2011 | Overall migration ≤ 10 mg/dm² under intended simulant conditions |
| United States food-contact olefin polymers | FDA 21 CFR 177.1520 | Olefin polymer compliance with end-use condition limitations |
| REACH registration and SVHC | Regulation (EC) No 1907/2006 | SVHC concentration < 0.1 wt% per article |
| RoHS restricted substances | Directive 2011/65/EU | Cadmium, lead, mercury, hexavalent chromium, PBB and PBDE limits |
Food-contact status of BC 82 PH must be verified on the finished packaging line because added colour masterbatch, regrind content and processing aids can influence overall migration and organoleptic performance. Under EU Regulation 10/2011, compliance is validated against the intended food simulant, contact time and temperature, not solely against the base resin certificate. For FDA 21 CFR 177.1520, the resin is an olefin polymer subject to end-use condition limitations, and use at sterilisation or hot-fill temperatures may require separate evaluation. REACH declarations under Regulation (EC) No 1907/2006 confirm that the base resin is registered for industrial supply, but downstream users remain responsible for article-level documentation. RoHS compliance under Directive 2011/65/EU applies when the finished container is incorporated into electrical or electronic equipment.