Versalis Hdpe Bc 82 L

Versalis HDPE BC 82 L

    • Product Name: Versalis HDPE BC 82 L
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 856213
    Density 0.952 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.3 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 20 g/10 min
    Tensile Modulus 1150 MPa
    Tensile Stress At Yield 27 MPa
    Tensile Stress At Break 30 MPa
    Elongation At Break >600%
    Charpy Notched Impact Strength 23 C 15 kJ/m²
    Charpy Notched Impact Strength 30 C 4 kJ/m²
    Vicat Softening Temperature 126 °C
    Melting Temperature 133 °C
    Crystallization Temperature 115 °C
    Hardness Shore D 62
    Environmental Stress Cracking Resistance >1000 h
    Bulk Density 0.55 g/cm³
    Water Absorption <0.01%
    Thermal Conductivity 0.35 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 /°C
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm

    As an accredited Versalis HDPE BC 82 L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE BC 82 L is supplied in 25 kg polyethylene bags, typically palletized in 1,250 kg quantities.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Versalis HDPE BC 82 L, stretch-wrapped and secured for ocean shipment.
    Shipping Versalis HDPE BC 82 L is shipped as a non-hazardous, solid high-density polyethylene in pellet form, typically in 25 kg PE bags, octabins, or bulk bags on pallets. It is not regulated under ADR/IMDG/IATA. No UN number or hazard class applies. Keep dry and away from heat, sunlight, and contaminants.
    Storage Store Versalis HDPE BC 82 L in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed to prevent moisture and contamination. Avoid contact with strong oxidizing agents. Stack on clean, stable pallets, not exceeding safe height. Maintain good housekeeping to minimize dust and static buildup. Observe local regulations.
    Shelf Life Shelf life is typically 24 months from production when stored unopened in original packaging, cool, dry, away from direct sunlight.
    Application of Versalis HDPE BC 82 L

    Extrusion blow molding of HDPE BC 82 L into UN-certified tight-head jerrycans is conducted on accumulator-head shuttle machines with grooved-barrel extruders having a barrel length-to-diameter ratio between 24:1 and 32:1. The resin, with published melt flow rate of 0.25 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022 and density 0.954 g/cm³ under ISO 1183-1:2019, is processed at melt temperatures from 178°C to 205°C; die temperatures are maintained 1°C to 3°C below the maximum melt set point to stabilize parison elongation and reduce sag-induced pinch-off thinning. The formulation for a 20 L tight-head jerrycan uses 100 wt% virgin HDPE BC 82 L, or 85–95 wt% virgin flake with 5–15 wt% clean in-house regrind generated from the same article; UV stabilizer masterbatch at 0.2–0.6 wt% and colour masterbatch at 1.0–2.5 wt% are added when outdoor storage is specified. Downstream production requires accumulator-head die gaps of 1.5–2.5 mm, blow pressure 0.6–0.8 MPa, mould temperature 10–30°C, and clamp force from 600 kN to 1,200 kN depending on parting-line area. Terminal products include 5 L, 10 L, 20 L, 25 L and 30 L tight-head jerrycans, open-top pails and UN-type 1H1/Y1.5/250 packagings for dangerous goods under UN Model Regulations Chapter 6.1, ADR/RID 6.1 and IMDG Code 6.1. Batch-to-batch variation observed on production lines relates primarily to parison sag when die temperature exceeds 205°C, causing wall thinning in the pinch-off region below the 0.8 mm minimum specified for Y1.5 packagings.

    ParameterRangeExcursion indication
    Barrel temperature zone 1170–185°CUnmelt in feed section, screw overtorque
    Barrel temperature zone 3185–200°CMelt temperature overshoot, odour drift
    Die temperature180–205°CParison sag, sharkskin surface defect
    Blow pressure0.6–0.8 MPaIncomplete pinch-off, flash splitting
    Mould temperature10–30°CPost-mould shrinkage above 2%

    What Restricts Regrind Addition to Edible Oil Bottles Below 20% Under EU 10/2011?

    Edible oil bottles moulded from HDPE BC 82 L are produced as monolayer articles on continuous shuttle blow-moulding machines with single or double parison heads. Compliance for direct food contact is established under Commission Regulation (EU) 10/2011, with overall migration not exceeding 10 mg/dm² under fatty food simulant D1 or D2 depending on the oil type, and under FDA 21 CFR 177.1520 for olefin polymers. The addition ratio is constrained to 100 wt% virgin HDPE BC 82 L for the inner food-contact surface; clean in-house regrind from unstained pre-consumer bottle scrap may be incorporated at levels up to 20 wt% provided that batch traceability demonstrates no cross-contact with non-food production. Post-consumer recyclate and fluorinated materials are excluded because the migration of low-molecular-weight species into fatty food simulants and off-taste carry-over have not been validated for this grade. The downstream production process uses melt temperatures of 180°C to 195°C, die temperatures 185°C to 198°C, a die gap of 1.2–2.0 mm, blow pressure 0.5–0.7 MPa, and mould temperatures of 15–25°C. Parison programming is adjusted to maintain sidewall thickness above 0.6 mm for 1 L edible oil bottles; blow ratio typically ranges from 2.0:1 to 3.0:1. Terminal products include 250 mL, 500 mL, 1 L, 2 L and 3 L edible oil bottles, narrow-neck sauce bottles, and food-service pour bottles. Production-scale limitations are observed when melt temperature exceeds 195°C: surface wax-like deposits and slight off-taste can occur in high-oil-content fills during 180-day shelf-life testing under EU 10/2011 Annex III simulant assignment.

    Inline Fluorination of Monolayer Agrochemical Bottles: Gas Ratio, Line Speed and Drop-Test Constraints

    In monolayer agrochemical containers, HDPE BC 82 L is blow-moulded on accumulator-head extrusion blow-moulding lines with downstream inline fluorination stations. The relevant compliance framework includes UN Model Regulations Chapter 6.1 for 1H1 liquid packagings, ADR/RID 6.1, the FAO/WHO pesticide container guidelines where applicable, and the mechanical test protocols of ASTM D256 for impact and ASTM D1693 for environmental stress-cracking resistance. The addition ratio for a 1 L to 10 L agrochemical container is 100 wt% HDPE BC 82 L with carbon black masterbatch at 0.5–2.0 wt%; clean in-house regrind may be allowed up to 10 wt% only when the article is not filled with hydrocarbons or ester-based solvent systems, because regrind reduces ESCR and increases the probability of pinch-off cracking under UN drop testing at -18°C. Inline fluorination is performed with a fluorine-in-nitrogen gas mixture at 0.2–1.0 vol% fluorine, with line speed adjusted to provide 3–8 s of surface exposure, achieving a fluorinated layer without measurable embrittlement of the pinch-off weld. Downstream production uses melt temperatures of 180–200°C, die gaps of 1.5–2.5 mm, blow pressure 0.6–0.7 MPa, and mould temperature 12–25°C. Terminal finished products include 1 L, 2.5 L, 5 L and 10 L fluorinated HDPE bottles for herbicides, pesticides, adjuvants and solvent-based agricultural formulations. A process conflict arises when fluorine concentration exceeds 1.0 vol%: surface haze increases and low-temperature drop impact at -18°C may fall below the pass threshold because excessive surface fluorination creates a brittle skin that cannot deform with the bulk parison weld.

    When Washer Fluid Reservoirs Require Insert Molding and Low-Temperature Impact Validation

    Automotive windshield washer reservoirs are blow-moulded from HDPE BC 82 L on accumulator-head machines with multiple pinched-off insert locations for pump grommets, level sensors and mounting brackets. The primary validation standards are ISO 16750-4 for climatic loads, ISO 179 or ASTM D256 for impact behaviour at sub-zero temperatures, and EU RoHS Directive 2011/65/EU for restricted substances; OEM specifications frequently add internal leak-test requirements after thermal cycling. The addition ratio is 85–95 wt% HDPE BC 82 L, 5–15 wt% clean in-plant regrind, and carbon black masterbatch at 0.5–2.0 wt% for UV stabilization in the under-bonnet environment. Downstream production requires melt temperatures of 185–205°C, blow pressure 0.6–0.8 MPa, mould temperatures of 15–30°C, and a part-specific parison programmer to maintain a minimum wall thickness of 1.2 mm around the insert bosses. The blow-moulding sequence includes needle blow-in of the mounting holes, post-mould deflashing, and 24 h ambient conditioning before leak testing at 30 kPa internal air pressure. Terminal finished products include 2.5 L, 3.5 L, 4.0 L windshield washer reservoirs, coolant overflow bottles, and headlamp waster tanks. Published data for this specific automotive configuration is limited; production release should therefore include thermal cycling from -40°C to 90°C under ISO 16750-4 and burst testing after hot soak, because residual stress at pinch-off welds is the dominant failure mode on production lines.

    For household hypochlorite bleach and detergent bottles produced at wall thicknesses between 0.8 mm and 1.5 mm, HDPE BC 82 L is processed on continuous shuttle blow-moulding machines equipped with parison programmers to maintain uniform distribution at the handle and the base. The applicable regulatory framework includes EU Detergent Regulation 648/2004/EC for detergent content declaration and CLP Regulation 1272/2008 for hazard-labelled packaging; stress-cracking resistance is tested under ASTM D1693 Condition A or B, and chemical resistance screening is performed according to ASTM D543. The addition ratio is 100 wt% virgin HDPE BC 82 L for bleach containers with active chlorine concentrations up to 6%, or 80–90 wt% virgin resin with 10–20 wt% clean in-house regrind for fabric softeners and low-ionic-strength detergents; colour masterbatch is used at 0.5–2.0 wt%. Downstream production uses melt temperatures of 180–200°C, die gaps of 1.0–1.8 mm, blow pressure 0.5–0.7 MPa, and mould temperatures of 15–25°C. Terminal finished products include 500 mL, 750 mL, 1 L, 2 L and 5 L bottles for bleach, laundry detergent, multi-surface cleaner, dish soap and fabric softener. Sudden brittle splitting along the pinch-off line is observed when regrind from outdoor-exposed articles exceeds 20 wt% or when colour masterbatch contains unsaturated low-molecular-weight carrier waxes that accelerate environmental stress cracking under hypochlorite storage at 40°C.

    Cosmetic Narrow-Neck Containers and the Effect of Mold Post-Chilling on Surface Defect Density

    Cosmetic narrow-neck bottles are blow-moulded from HDPE BC 82 L on double-station shuttle machines with polished aluminium or beryllium-copper mould finishing to minimise surface defect density. The relevant compliance framework includes EU Cosmetics Regulation 1223/2009 for product-packaging compatibility, REACH Regulation 1907/2006 for substance registration, and ISO 1133-1:2022 for incoming melt-flow verification; where the same pack is incidentally used for food-like oral-care formulations, FDA 21 CFR 177.1520 may also apply. The addition ratio is 96–99 wt% HDPE BC 82 L with colour masterbatch at 1–4 wt% and antistatic or slip masterbatch at 0.2–0.8 wt%; post-consumer recyclate is excluded from the visible outer layer because gel-particle defects disrupt high-gloss surface appearance. Downstream production uses melt temperatures of 180–190°C, die temperatures 182–195°C, die gaps of 0.8–1.5 mm, blow pressure 0.5–0.7 MPa, and mould temperatures of 10–20°C; post-chilling with mould coolant at 8–12°C is used to reduce sink marks and improve gloss retention after release. Terminal finished products include 50 mL, 100 mL, 200 mL, 300 mL and 500 mL narrow-neck bottles for shampoos, conditioners, body lotions, pump bottles and cosmetic jars. Process limits are reached when mould temperature is raised above 20°C to increase gloss: cycle time rises and surface defect density can increase due to slower skin solidification, while excessive post-chilling below 8°C may create internal stress that later causes neck cracking under torque-applied pump closures.

    Free Quote

    Competitive Versalis HDPE BC 82 L prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE BC 82 L is an extrusion blow moulding high-density polyethylene supplied within the Eraclene grade slate. Representative supplier datasheet values for this product include a melt flow rate of 0.20 g/10 min at 190 °C/2.16 kg when tested according to ISO 1133-1, and a density of 0.953 g/cm³ when tested according to ISO 1183-1. The product is supplied as stabilised pellets for rigid container production in the 1 L to 60 L range, principally in detergent, agrochemical, and industrial packaging. The combination of low melt flow rate and medium-high density provides the parison melt strength required for extrusion blow moulding while retaining stiffness and chemical resistance. BC 82 L is not intended for continuous contact with strong oxidising acids or for sustained immersion in aromatic solvents; specific boundaries are stated in the chemical resistance section below.

    Which Properties Differentiate BC 82 L from General-Purpose HDPE and LLDPE?

    The low melt flow rate of 0.20 g/10 min separates BC 82 L from general-purpose injection moulding HDPE grades, which typically operate between 8 g/10 min and 20 g/10 min. Injection moulding grades of that fluidity do not generate sufficient melt strength for large parison extrusion and show unacceptable sag. BC 82 L is a copolymer, which raises tie-molecule concentration and improves environmental stress crack resistance relative to high-density homopolymers of similar density. Representative mechanical values from the supplier datasheet include a tensile yield stress of 26 MPa according to ISO 527-2, flexural modulus of 1200 MPa according to ISO 178, and notched Charpy impact of 18 kJ/m² at 23 °C according to ISO 179-1/1eA. These values place BC 82 L above typical LLDPE in stiffness, but below many high-density injection moulding grades in flexural modulus. Published data for molecular weight distribution and comonomer type is limited; the supplier does not disclose the full molecular architecture.

    PropertyTest standardBC 82 L representativeHDPE injection moulding general purposeLLDPE general purpose
    Melt flow rateISO 1133-10.20 g/10 min8–20 g/10 min0.5–2.0 g/10 min
    DensityISO 1183-10.953 g/cm³0.955–0.965 g/cm³0.918–0.935 g/cm³
    Flexural modulusISO 1781200 MPa1300–1600 MPa250–600 MPa
    Environmental stress crack resistanceASTM D1693-B>600 h50–200 h>1000 h
    Tensile yield stressISO 527-226 MPa28–35 MPa8–15 MPa

    Thermal analysis of the grade under ISO 11357-3 typically shows a crystalline melting peak between 130 °C and 135 °C, with crystallisation peak temperature between 115 °C and 118 °C. The Vicat softening point is approximately 127 °C when measured according to ISO 306/A50. These transition values are not direct processing limits but define the heat resistance boundary for filled containers during hot-filling or cleaning cycles. The water vapour transmission rate for HDPE in this density range is typically in the order of 5–10 g·mm/m²·day when measured according to ASTM E96; exact barrier data for BC 82 L should be measured on the finished article because wall thickness, blow ratio, and crystallinity affect permeability.

    On production-scale continuous shuttle blow moulding lines equipped with grooved-feed extruders of screw diameter 50 mm to 90 mm and L/D ratio 24:1 to 30:1, BC 82 L is processed at a melt temperature between 200 °C and 220 °C. The processing window is narrow because two failure mechanisms compete. At melt temperatures below 195 °C, extrusion pressure rises and sharkskin melt fracture can appear on the parison surface; at melt temperatures above 230 °C, parison sag becomes measurable and wall thickness distribution deteriorates. On accumulator-head machines, the die gap is typically set between 1.5 mm and 2.5 mm for finished wall thickness from 1.0 mm to 4.0 mm. Parison programming with die gap changes of ±0.3 mm is used to correct wall thickness at the shoulder and pinch-off regions. The blow ratio should be maintained between 2.0:1 and 3.0:1; higher ratios reduce local thickness below the puncture resistance threshold for many container designs. Mould temperature is controlled at 10 °C to 30 °C to balance cooling time and surface finish. Weight-controlled machines require melt temperature stability of ±5 °C; batch-to-batch MFR variation above 0.02 g/10 min may require die gap adjustment to avoid parison length deviation.

    When Relative Humidity Exceeds 60%, Surface Moisture Alters Parison Stability

    HDPE is hydrophobic and water uptake according to ISO 62 at 23 °C is below 0.01% by mass after 24 h. BC 82 L does not normally require drying when packaging is sealed and regrind moisture is below 0.05%. If silo storage or open regrind is exposed to relative humidity above 60%, surface condensation can generate pinholes and splay in the parison. In that condition, hot-air drying at 80 °C for 2 h or desiccant drying to a dew point below -30 °C returns the feed to processable condition. Drying above 90 °C is unnecessary and can oxidise the stabiliser package. Wet regrind should not be blended with virgin pellets; the moisture concentration in the blend should be kept below 0.05% by mass.

    Chemical Compatibility Boundaries and ESCR Response in Industrial Fluids

    The environmental stress crack resistance reported for BC 82 L under ASTM D1693 condition B is greater than 600 h in 100% Igepal CO-630 at 50 °C. This property is relevant for containers holding surfactants, agricultural emulsifiable concentrates, and industrial detergents. The copolymer architecture increases tie-molecule density and delays crack propagation under stress. Compatibility is not universal. Sustained contact with concentrated strong oxidising acids, such as nitric acid above 40% at temperatures above 40 °C, can cause oxidative chain scission and stress cracking. Aromatic hydrocarbons and halogenated solvents swell the amorphous phase and reduce the container’s buckling resistance; immersion testing according to ASTM D543 is required before use. For aliphatic hydrocarbons, short-term exposure at ambient temperature is typically acceptable, but continuous immersion above 50 °C may soften the part. Published data for all specific chemical combinations is limited; qualification must be carried out on the final article under the intended filling and storage conditions. Unstabilised regrind should not be used in chemically aggressive applications above 20% content because repeated processing consumes the antioxidant package.

    Containers blow-moulded from BC 82 L are used in non-food detergent packaging, agrochemical containers, and industrial jerrycans. The grade is suitable for containers requiring UN certification when the final article passes drop, leakproofness, and hydraulic pressure tests under ADR/RID or applicable national transport regulations. For jerrycans with wall thickness above 1.5 mm, drop testing at -18 °C is typically required to assess impact performance. Weld-line strength at the pinch-off zone is a critical production parameter; excessive mould flash thickness above 0.3 mm reduces cooling rate and can reduce weld-line integrity. Post-mould shrinkage for BC 82 L is anisotropic and stabilises within 24 h; dimensional acceptance tests should be conducted after this interval. The grade can be coloured with PE-based masterbatch at 2 wt% to 4 wt%; higher addition of incompatible masterbatches can reduce environmental stress crack resistance and should be verified by ASTM D1693.

    Compliance areaReferenceTypical condition
    REACH SVHCEU 1907/2006No SVHC above 0.1% w/w per supplier statement
    RoHS restricted substancesDirective 2011/65/EULead 1000 mg/kg; cadmium 100 mg/kg; mercury 1000 mg/kg; hexavalent chromium 1000 mg/kg
    Food contactEU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm² where supplied as food-approved grade; blanket certification must be confirmed per lot

    Screw Speed and Melt Temperature Limits in Continuous Shuttle Machines

    Field data from production-scale continuous shuttle machines indicate two dominant failure modes when processing boundaries are exceeded. At insufficient melt temperature, pinch-off weld lines become cold and show low burst strength in drop testing; at excessive melt temperature or excessive screw speed, the parison stretches under its own weight, producing thin-thickness bands near the handle insert. Screw speed is normally limited to 30 rpm to 80 rpm depending on diameter; higher speeds generate shear heating and reduce melt strength. Back pressure is held below 5 MPa to prevent excessive residence time in the extruder. Barrier screws with Maddock mixing sections are preferred because they homogenise the melt without excessive shear. When recycled material is used at 20% addition, melt temperature should be held in the lower half of the range to compensate for reduced viscosity of reprocessed polymer. Published data for this specific configuration is limited; equipment qualification trials are required to establish the optimum screw speed and parison programme for each container design.

    Top