Versalis Hdpe Bc 82

Versalis HDPE BC 82

    • Product Name: Versalis HDPE BC 82
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 602149
    Density 0.954 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.2 g/10 min
    Tensile Stress At Yield 30 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1400 MPa
    Charpy Notched Impact Strength 23 C 15 kJ/m2
    Charpy Notched Impact Strength 30 C 5 kJ/m2
    Vicat Softening Temperature 126°C
    Brittleness Temperature < -70°C
    Hardness Shore D 65
    Environmental Stress Cracking Resistance 10 Igepal 50 C >1000 h
    Melting Temperature 132°C

    As an accredited Versalis HDPE BC 82 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE BC 82 comes in 25 kg polyethylene bags, palletized at 55 bags per pallet, totaling 1,375 kg net.
    Container Loading (20′ FCL) Versalis HDPE BC 82, high-density polyethylene, in 25 kg bags, palletized and loaded into a 20′ FCL, approximately 18–20 MT net.
    Shipping Versalis HDPE BC 82 is a non-hazardous high-density polyethylene. It is normally shipped in 25 kg bags, jumbo bags, or bulk containers, palletized and wrapped. Transport by road, rail, or sea in dry conditions, away from direct sunlight and ignition sources. No dangerous goods documentation is required.
    Storage Store Versalis HDPE BC 82 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging sealed, on pallets, off the floor. Protect from moisture, UV exposure, dust, and mechanical damage. Avoid extreme temperatures and prolonged storage near incompatible materials. Ensure good ventilation, housekeeping, and local regulation compliance.
    Shelf Life Versalis HDPE BC 82 shelf life is typically 24 months when stored dry, cool, ventilated, and away from direct sunlight.
    Application of Versalis HDPE BC 82

    Screening of HDPE BC 82 for UN-certified jerrican production begins with lot certification of melt flow index and density; supplier-published values for this blow moulding grade place MFR at 0.25 g/10 min under ISO 1133-1 and density at 0.952 g/cm³ under ISO 1183-1, but each lot must be verified against its certificate of analysis because a deviation of 0.02 g/10 min is sufficient to alter parison sag behaviour on large accumulator-head machines. In a typical 20 L jerrican line using a 90 mm extruder with L/D 26:1 and a compression ratio of 2.5:1, the barrel temperature profile from feed to metering is set at 170°C, 185°C, 195°C, and 200°C; the melt temperature is held between 190°C and 200°C, the die head is maintained at 195°C to 205°C, and the mould is chilled to 15°C to 20°C to preserve wall thickness consistency and reduce post-mould shrinkage. The accumulator head is programmed with 20 to 100 axial wall thickness points; parison drop time above 4 s on a 1.8 mm target wall is a standard field indication of excessive sag, producing thin bottom flash and a higher risk of failure in UN drop tests. Blow air pressure of 0.6 MPa to 0.8 MPa and blow time of 18 s to 25 s are typical on single-station machines; the blown article is post-cooled in the mould for 8 s to 12 s to prevent handle-area deformation during demoulding. Formulation control for dangerous goods packaging typically uses 3.0 wt% to 5.0 wt% of a carbon black masterbatch in a PE carrier, 0.2 wt% to 0.5 wt% of a fluoroelastomer process aid when melt fracture appears at outputs above 250 kg/h, and 0.1 wt% to 0.3 wt% of an antioxidant masterbatch if closed-loop regrind exceeds 20 wt%; the use of external lubricants above 0.5 wt% is avoided because of reduced interlayer fusion in flash weld lines. The terminal products are 20 L, 25 L, 30 L, and 60 L 3H1 jerricans, and 3H2 open-head pails for solvents, acids, alkalis, oxidizers, and petroleum distillates. Compliance is governed by UN ST/SG/AC.10/11/Rev.7 Chapter 6.1, ADR 6.1.3, and the IMDG Code packaging provisions; design-type testing includes drop heights of 1.2 m for Packing Group II liquids and 0.8 m for Packing Group III liquids, as well as hydraulic pressure testing at 100 kPa for 30 min under ADR 6.1.5. HDPE BC 82 alone does not confer UN certification; the finished package must pass design-type testing, lot inspection, and be marked with the relevant UN code.

    Stress Crack Resistance in Aggressive Detergent Bottling

    The selection of HDPE BC 82 for liquid detergent bottles is controlled less by short-term tensile yield than by environmental stress cracking resistance under non-ionic surfactant load, because a bottle that withstands ASTM D638-14 tensile testing can still fail in service through slow crack growth. The high molecular weight fraction and low MFR in the 0.25 g/10 min range support an F50 value above 200 h when tested under ASTM D1693-15 Condition B at 50°C in 100% Igepal CO-630; this is the relevant control because bottle sidewall stresses concentrate at pinch-off weld lines and base corners. At mould temperatures above 20°C, slow cooling increases spherulite diameter and reduces ESCR; at mould temperatures below 8°C, frozen-in orientation increases residual stress. Continuous extrusion blow moulding on shuttle machines with 4 to 8 cavities, 65 mm screw diameter, L/D 26:1, and low-shear screws optimized for HDPE uses melt temperatures of 185°C to 195°C, die temperatures of 190°C to 200°C, and mould temperatures of 10°C to 15°C to produce wall thicknesses from 0.35 mm to 0.8 mm for bottles between 500 mL and 5 L. To prevent stress cracking in aggressive formulations, the addition ratio is normally 1.5 wt% to 3.0 wt% of titanium dioxide white masterbatch, 0.1 wt% to 0.3 wt% of antistatic masterbatch where filling lines require surface resistivity below 10^14 ohm/square, and 0.2 wt% to 0.5 wt% of a processing aid; post-consumer recycled HDPE is restricted to 10 wt% to 20 wt% in the outer layer and is not used in contact with aggressive bleach or caustic formulations unless ESCR data under ASTM D1693-15 Condition A are generated for each lot. Regulatory references for the finished packaging include Directive 94/62/EC for packaging and packaging waste, Regulation (EC) 648/2004 for detergent packaging safety, and REACH Annex XVII for restricted substances; if the package is exported as empty packaging, national food-contact certificates are not required. Terminal product types include 500 mL, 1 L, 2 L, and 5 L HDPE bottles for laundry detergents, fabric softeners, bleach, hard-surface cleaners, and industrial hand cleaners; monolayer use is acceptable when the active oxygen content of the formulation is below 5%, while higher bleach concentrations require compatibility testing under ASTM D543-21. Published data for HDPE BC 82 with specific fragrance and enzyme systems is limited; each new detergent formulation should be validated by 30-day oven aging at 50°C and visual inspection for microcracks before tooling release.

    In crop protection packaging, HDPE BC 82 is allocated as the structural layer in monolayer or three-layer coextruded bottles where the filled product contains hydrocarbon solvents, emulsifiable concentrates, or hydrolysis-prone active ingredients; the grade is processed at 195°C to 210°C on a main extruder of 60 mm to 75 mm with L/D 28:1, while a polyamide or EVOH barrier layer is run at 210°C to 220°C and a maleic anhydride grafted tie layer at 205°C to 215°C. The structure typically consists of 85 wt% to 92 wt% HDPE BC 82, 2 wt% to 5 wt% barrier resin, 1 wt% to 2 wt% tie resin, and 2 wt% to 4 wt% UV-stabilised colour masterbatch; this formulation ratio is adjusted to maintain bottle mass within ±2% of the approved UN design type. A three-layer die head with 1.2 mm outer die gap is used, and flash from the mould is recycled at 15 wt% to 25 wt% in the outer layer only, because barrier layer regrind can plate out on the screw and cause melt pressure fluctuation above 5 bar/min. The blow mould is chilled to 8°C to 12°C, colder than standard detergent bottle moulds, to stabilise wall thickness and shorten cycle time to 45 s to 70 s for a 5 L insecticide container. Compliance standards for agrochemical packaging include UN ST/SG/AC.10/11/Rev.7 for dangerous goods, EC 1272/2008 CLP for supply packaging of hazardous mixtures, and the FAO/WHO International Code of Conduct on Pesticide Management for packaging reuse and disposal; weathering of the outer layer is referenced to ISO 4892-2:2013 Cycle 1, but quantitative colour shift limits must be set by the masterbatch supplier because published data for HDPE BC 82 with specific UV packages is limited. Terminal products are 1 L, 5 L, 10 L, and 20 L containers for herbicides, insecticides, fungicides, and plant growth regulators; fluorination treatment may be required for solvent-based formulations above 70% aromatic solvent content, with barrier loss tested under a paired permeation panel before lot release.

    When HDPE BC 82 Replaces Lined Steel in Diesel Exhaust Fluid Service

    The substitution of lined steel by HDPE BC 82 in diesel exhaust fluid (DEF) packaging is governed by ISO 22241-3:2017, which requires that packaging materials do not leach calcium, magnesium, iron, or aluminium ions into the urea solution above specified limits; HDPE is the dominant monolayer material for this service, but resin choice and processing must avoid post-mould oxidation products that can raise ammonia evolution. On a shuttle blow moulding line for 2 L to 10 L DEF bottles, the melt temperature is held at 180°C to 190°C, the die head at 185°C to 195°C, and the mould at 10°C to 15°C; lower melt temperatures are used than in heavy-duty jerrican production because thin-walled bottles require higher melt strength to prevent parison drawdown. The formulation uses 1.5 wt% to 2.5 wt% of a white masterbatch formulated without heavy-metal pigments, 0.2 wt% to 0.4 wt% of a high-molecular-weight hindered amine stabilizer masterbatch for UV exposure, and 0.1 wt% to 0.3 wt% of an acid scavenger masterbatch; post-consumer recyclate is typically excluded from the internal layer because trace contamination can compromise ISO 22241-3:2017 compliance. The extruder screw should be a barrier screw with L/D 25:1 to 28:1, and the melt pressure should remain below 350 bar to avoid excessive shear heating; field experience on 65 mm shuttle machines shows that melt temperature drift above 195°C is associated with off-taste and conductivity drift in accelerated DEF storage at 40°C. Terminal products include 2 L, 5 L, and 10 L DEF containers with tamper-evident necks, and 1 L, 4 L, and 5 L engine lubricant containers; the same grade can be used for coolant bottles if the coolant concentrate is diluted with water below 50% glycol, while higher glycol concentrations require layer-specific permeability validation under ASTM D3985. Published data for HDPE BC 82 in DEF packaging with specific lot-to-lot source variation is limited; each new supplier lot should be tested for trace metal extraction and storage stability at 40°C for 12 weeks before filling-line approval.

    Compliance and processing boundary matrix for HDPE BC 82 downstream applications
    Application segmentPrimary regulatory or test referenceTypical HDPE BC 82 addition levelProduction-scale boundary
    UN-certified jerricansUN ST/SG/AC.10/11/Rev.7; ADR 6.1.3; ADR 6.1.53.0–5.0 wt% carbon black masterbatch; 0.2–0.5 wt% process aidDie head 195–205°C; parison drop <4 s at 1.8 mm wall
    Detergent bottlesASTM D1693-15; Directive 94/62/EC; Regulation (EC) 648/20041.5–3.0 wt% TiO₂ masterbatch; 0.2–0.5 wt% processing aidMelt 185–195°C; wall 0.35–0.8 mm
    Agrochemical containersUN ST/SG/AC.10/11/Rev.7; EC 1272/2008; ISO 4892-2:2013HDPE BC 82 85–92 wt%; barrier resin 2–5 wt%; tie resin 1–2 wt%Main-layer melt 195–210°C; mould 8–12°C
    DEF and lubricant containersISO 22241-3:2017; REACH Annex XVII1.5–2.5 wt% white masterbatch; 0.2–0.4 wt% HALS masterbatchMelt 180–190°C; melt pressure <350 bar
    Industrial pailsASTM D1693-15; ASTM D256; UN ST/SG/AC.10/11/Rev.72.0–4.0 wt% colour masterbatch; 20–30 wt% regrindDie gap 1.5–2.0 mm; die swell 35–45% at 50 s⁻¹
    Fuel and oil containersADR 6.1.3; ASTM D638-14; ASTM D543-212.0–3.0 wt% UV masterbatch; 0.1–0.3 wt% antioxidant masterbatchMelt 185–195°C; wall 1.2–1.5 mm for 5 L

    Pinch-Off Weld Integrity Is the Controlling Parameter in Pail Moulding

    For 5 L to 20 L open-head industrial pails, HDPE BC 82 is run on double-station accumulator-head machines with dual parison ejection; the dominant process constraint is not chemical resistance but die swell and parison sag because the parison must maintain a uniform preform before mould close. Die swell for this grade is typically 35% to 45% at shear rates around 50 s⁻¹ in capillary rheometry; grade-specific values should be confirmed under ISO 11443. Die gap settings of 1.5 mm to 2.0 mm are used with blow moulds at 15°C to 20°C and melt temperatures of 190°C to 200°C. The formulation for pails uses 2.0 wt% to 4.0 wt% carbon black or industrial colour masterbatch and permits 20 wt% to 30 wt% of closed-loop regrind from the same production lot; the regrind addition is limited to this range because higher levels reduce ESCR F50 under ASTM D1693-15 Condition A below 50 h in some pigment-rich formulations. Compliance is driven by ASTM D1693-15 for stress crack resistance, ASTM D256 for impact strength of the pail body, and UN ST/SG/AC.10/11/Rev.7 for 3H2 open-head packages when filled with hazardous solids; non-hazardous industrial paints and inks fall under Directive 94/62/EC only. Terminal products are 5 L, 10 L, 15 L, and 20 L pails for paints, inks, adhesives, powder detergents, and solid water-treatment chemicals. Because pail lids are often injection moulded from a higher-MFR HDPE, the seal interface should be validated for stack load at 40°C for 48 h under compressive creep testing rather than by short-term dimensional checks only.

    What Limits Hydrocarbon Weight Loss in Small-Scale Fuel Containers?

    For small-volume petroleum distillate containers, HDPE BC 82 is processed on single-station shuttle blow moulding machines with 50 mm to 60 mm screw diameter and L/D 24:1 to 26:1; the finished containers are used for kerosene, mineral spirits, and chain-bar oil where permeation is controlled by wall thickness rather than barrier coextrusion. The melt temperature is set at 185°C to 195°C, the mould temperature at 10°C to 15°C, and the blow pressure at 0.6 MPa to 0.75 MPa; wall thickness for a 5 L container is maintained at 1.2 mm to 1.5 mm to reduce hydrocarbon weight loss below the ADR vapour pressure threshold for dangerous goods packaging. Formulation addition is 2.0 wt% to 3.0 wt% of a UV-stabilized red or black masterbatch, 0.1 wt% to 0.3 wt% of an antioxidant masterbatch, and no external slip agent above 0.1 wt% because surface migration can interfere with cap torque retention. Compliance references are ADR 6.1.3 for packaging Group III flammables, ASTM D638-14 for weld-line tensile integrity, and ASTM D543-21 for weight change after immersion in reference fuel C; the supplier recommends immersion at 23°C for 7 days and a maximum weight gain of 3% before the container is released. Terminal products are 1 L, 2 L, 5 L, and 10 L fuel and oil containers with UN markings for Packing Group III hydrocarbon liquids; published data for HDPE BC 82 with ethanol-blended gasoline above E10 is limited, and long-term storage of fuels with oxygenates above 10% should be validated by permeation testing under 40°C.

    Free Quote

    Competitive Versalis HDPE BC 82 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE BC 82, sold under the Eraclene designation, is a high-density polyethylene blow moulding grade supplied in pellet form. The grade is intended for extrusion blow moulding of rigid hollow bodies where low melt flow rate and high melt strength are required. The two primary specification values are a density of 0.954 g/cm³ determined at 23 °C according to ISO 1183-1 and a melt flow rate of 0.25 g/10 min measured at 190 °C under a 2.16 kg load according to ISO 1133-1. These values differentiate the product from high-MFR injection moulding HDPE grades, which typically flow above 4 g/10 min, and from lower-density film grades, whose density is often below 0.945 g/cm³. The high density contributes to article stiffness, while the low melt flow rate improves parison hang time and melt stability during continuous and intermittent blow moulding.

    Published producer technical datasheet values for the grade include a tensile yield stress of 26 MPa under ISO 527-2, a flexural modulus near 1,200 MPa under ISO 178, an elongation at break above 600 %, and a notched Charpy impact strength at 23 °C of approximately 6 kJ/m² under ISO 179-1/1eA. Vicat softening temperature is reported at 126 °C under ISO 306/A50 with a 10 N load. These values are typical rather than absolute grade guarantees and should be verified against the lot certificate supplied with each production batch. Variation in comonomer distribution and stabiliser package can shift Charpy impact and environmental stress crack resistance within the producer’s specification window.

    The molecular architecture of BC 82 is characterised by a broad molar mass distribution. The high-molar-mass fraction raises zero-shear viscosity and parison strength, while the lower-molar-mass fraction provides shear thinning during die flow. This balance differentiates BC 82 from a monomodal HDPE with the same nominal melt flow rate, which may show higher die swell but lower melt strength. The distinction becomes measurable in parison draw-down before mould closure and in the wall-thickness distribution of finished articles.

    What Processing Limits Appear When BC 82 Is Melt-Processed?

    Continuous extrusion blow moulding of HDPE BC 82 is normally operated with a melt temperature at the die of 175 °C to 205 °C. Below 175 °C, the high-molecular-weight fraction increases extruder head pressure and may generate surface melt fracture on the parison, particularly when the die is fitted with a narrow land length. Above 205 °C, the parison can sag and produce wall-thickness variation in containers with a shot volume exceeding 5 L. Single-screw extruders with a 25:1 L/D ratio and a grooved feed section are commonly used because the grooved feed section suppresses pellet slip and stabilises output against die pressure fluctuations. Barrel temperature profiles are commonly set from 160 °C at the feed throat to 200 °C at the die adapter, with the die temperature kept 5 °C to 10 °C below the adapter temperature to increase melt strength. These parameters are starting points and require tool-specific adjustment.

    In accumulator-head intermittent blow moulding, the melt accumulates in the head before shot discharge. For a 10 L container with a shot weight near 350 g, melt temperatures at the accumulator are generally held between 180 °C and 195 °C. Blow air pressure on production lines is typically set between 0.6 MPa and 1.0 MPa. The low MFR of BC 82 contributes to high melt strength but also increases pressure drop through the die. On a 60 mm grooved-feed extruder, screw speed is usually limited to 30 rpm to 60 rpm to avoid overheating the melt and generating gel particles. Published line-specific pressure data for BC 82 is limited; tooling trials should be used to establish head pressure and shot-speed limits.

    Die swell in BC 82 is lower than that of a parity MFR monomodal HDPE. The reduced swell allows die bushing diameters closer to the final container diameter, but it also reduces parison wall thickness for a given die gap. For container sidewalls, a die gap setting of 1.0 mm to 1.5 mm may produce a final wall of 0.7 mm to 1.2 mm after parison inflation. These values depend on blow-up ratio and mould geometry. Cooling time in blow moulding scales approximately with the square of wall thickness. Increasing wall thickness from 1.0 mm to 2.0 mm can extend cycle time by a factor of approximately 4. Mould temperature is usually set between 10 °C and 25 °C for rapid solidification, although excessive cooling can increase surface defects and frozen-in stress.

    Drying is typically unnecessary because HDPE is hydrophobic. If regrind is stored outdoors or in high-humidity environments, surface moisture above 0.05 wt% may produce splay and blow-pin deposits. In that case, predrying at 80 °C for 2 h in a desiccant hopper is sufficient. Prolonged drying above 4 h at 80 °C is not recommended because long residence at elevated temperature can accelerate oxidation of the regrind fraction.

    Blow moulding trials on production lines equipped with accumulator-head machines have used HDPE BC 82 to form containers from 1 L to 20 L with wall thicknesses between 0.6 mm and 2.0 mm. The grade is less suited to thin-wall applications below 0.4 mm because the low melt flow rate limits draw-down and can produce frozen-in stress. Containers above 20 L may require higher melt strength or a wider molecular weight distribution than the standard BC 82 specification, depending on parison weight and machine type. Published data for this specific boundary is limited.

    Thermal, Mechanical, and Compliance Data

    Typical property set for Versalis HDPE BC 82
    PropertyTest methodTypical value
    DensityISO 1183-10.954 g/cm³
    Melt flow rateISO 1133-10.25 g/10 min
    Tensile yield stressISO 527-226 MPa
    Elongation at breakISO 527-2>600 %
    Flexural modulusISO 1781,200 MPa
    Charpy notched impact strength at 23 °CISO 179-1/1eA6 kJ/m²
    Vicat softening temperatureISO 306/A50126 °C
    Shore D hardnessISO 86862

    The tensile yield stress and flexural modulus correlate with high top-load retention in stacked bottles and jerry cans. The notched Charpy value supports impact resistance in ambient handling, but it is not a substitute for full article drop testing. For containers intended for transport of hazardous liquids, drop tests should follow ADR/RID or equivalent transport regulations, and the test should cover the lowest expected service temperature, typically -18 °C for frozen goods distribution. Impact strength decreases at lower temperatures, and a container that passes at 23 °C may fail at -20 °C.

    Food-contact compliance may be established under EU Regulation (EU) No 10/2011 for plastics intended to contact food and under FDA 21 CFR 177.1520 for olefin polymers in the United States. The resin supplier’s declaration should be reviewed for the specific monomer composition, additive package, and overall migration limit. Packaging and packaging waste compliance is typically assessed through EU Directive 94/62/EC and the corresponding heavy metal limit of 100 mg/kg for the sum of lead, cadmium, mercury, and hexavalent chromium. Compliance is use-dependent and must be confirmed by the converter on the finished article.

    Chemical resistance of HDPE BC 82 follows general HDPE behaviour. Aromatic hydrocarbons, chlorinated solvents, and strong oxidising acids are not recommended for continuous contact because they can swell or stress-crack the polymer. For household chemical containers, environmental stress crack resistance screening should be performed under ASTM D1693, condition B, or a full container test using the specific fill. Where high-temperature filling is required, the maximum continuous service temperature of the container should be derived from creep and top-load data at the filling temperature; the Vicat value of 126 °C does not alone define the hot-fill limit.

    ESCR in HDPE blow moulding grades is influenced by short-chain branching and molar mass distribution. At a density of 0.954 g/cm³, BC 82 is stiffer but may show lower ESCR than a lower-density HDPE or MDPE copolymer blow moulding grade. In applications with aggressive surfactant systems, a lower-density blow moulding grade or a bimodal MDPE may be required. For bleach and quaternary ammonium disinfectant packages, finished-container ESCR data should be generated under the intended fill concentration and closure torque.

    If HDPE BC 82 Is Compared with High-MFR HDPE Grades

    Comparison with injection-moulding HDPE grades shows that HDPE BC 82 is not a drop-in substitute for thin-wall injection moulded parts. Injection moulding HDPE grades commonly have melt flow rates between 4 g/10 min and 20 g/10 min to fill long flow paths at moderate injection pressure. At 0.25 g/10 min, BC 82 requires higher injection pressure, larger gates, and thicker wall sections. It may be processed by injection moulding only in short-flow, thick-wall parts where melt temperature is raised to 220 °C to 240 °C, mould temperature is held at 30 °C to 50 °C, and injection speed is reduced to avoid jetting. Published data for this specific injection moulding use is limited; it should be validated by mould-flow analysis and pilot tool trials.

    Compared with film-grade HDPE, BC 82 has a higher density and higher flexural modulus. Film grades are commonly designed at densities from 0.940 g/cm³ to 0.952 g/cm³ to balance tear strength and dart impact. The higher density of BC 82 increases stiffness but reduces low-temperature puncture impact and tear resistance, making it unsuitable for primary blown film applications. Blow moulding grades also contain lower levels of polymer processing aids and slip agents than many film grades, which can affect melt fracture and surface friction during parison tracking.

    Comparative typical values across polyethylene processing families
    AttributeHDPE BC 82Injection-moulding HDPE representative rangeFilm-grade HDPE representative range
    Melt flow rate0.25 g/10 min4–20 g/10 min0.1–0.5 g/10 min
    Density0.954 g/cm³0.950–0.960 g/cm³0.940–0.952 g/cm³
    Flexural modulus1,200 MPa1,000–1,400 MPa600–900 MPa
    Typical processextrusion blow mouldinginjection mouldingfilm blowing
    Parison draw-down behaviourlow sag tendencynot applicablenot applicable

    The representative ranges in the adjacent columns are drawn from public commercial datasheet ranges for general-purpose HDPE grades and are not producer specifications for BC 82. Direct substitution should be based on the complete property profile of the target grade and the fabrication line capabilities.

    Compared with a high-MFR blow moulding HDPE, BC 82 exhibits lower die swell and higher melt strength. This result is beneficial for long parisons and large bottles because it reduces draw-down before mould closure. The trade-off is higher head pressure and lower output per screw revolution. On lines with gravimetric or volumetric extruder control, the output limit may shift from screw speed to head pressure. Processors switching from a 0.6 g/10 min blow moulding HDPE may need to reduce screw speed by 10 % to 20 % and increase die gap to maintain the same shot weight and parison wall distribution. These adjustments are line-specific and should not be used as universal offsets.

    In blow moulding scrap handling, BC 82 regrind can be mixed with virgin pellets at levels up to 30 wt% in many non-food applications without visible loss of parison stability. Higher regrind fractions above 50 wt% may narrow the processing window because repeated heat history increases gel formation and reduces ESCR. The level of regrind must be validated by measuring lot melt flow rate and density after compounding. If regrind is to be used in food-contact articles, the converter must confirm that the closed-loop recycling process complies with the applicable polymer-specific regulatory provisions.

    Top