Versalis Hdpe Bb 82

Versalis HDPE BB 82

    • Product Name: Versalis HDPE BB 82
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 159353
    Density 0.952 g/cm³
    Melt Flow Rate 190 C 21 6 Kg 2.0 g/10 min
    Tensile Strength At Yield 28 MPa
    Elongation At Break >600%
    Flexural Modulus 1300 MPa
    Notched Izod Impact Strength 23 C 10 kJ/m²
    Notched Izod Impact Strength 30 C 4 kJ/m²
    Vicat Softening Temperature 125°C
    Shore D Hardness 65
    Thermal Conductivity 0.4 W/m·K
    Water Absorption <0.01%
    Brittleness Temperature <-70°C

    As an accredited Versalis HDPE BB 82 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE BB 82 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial delivery.
    Container Loading (20′ FCL) Versalis HDPE BB 82 loaded in 20′ FCL, palletized bags, shrink-wrapped, evenly distributed, securely lashed for safe ocean transport.
    Shipping Versalis HDPE BB 82 is a non-hazardous thermoplastic supplied as pellets. Ship in original sealed 25 kg polyethylene bags, palletized and shrink-wrapped, or in bulk trucks/containers. Not regulated for transport. Store cool and dry; avoid heat, sunlight, moisture, contamination, and static discharge. Keep packages closed and labeled.
    Storage Store Versalis HDPE BB 82 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and store on pallets, stacked safely. Maintain good housekeeping; use appropriate PPE when handling. No special ventilation is normally required.
    Shelf Life Versalis HDPE BB 82 has a shelf life of 24 months when stored in a cool, dry, well-ventilated area.
    Application of Versalis HDPE BB 82

    Agrochemical packagings impose a combined requirement of low-shear melt strength for parison stability and high environmental stress crack resistance after filling with xylene-containing emulsifiable concentrates. In monolayer extrusion blow molding, Versalis HDPE BB 82 is processed at a dry-blend formulation of 100 phr resin, 1.8–2.5 wt% additive-loaded color concentrate, and 0.05–0.12 phr hindered phenolic processing stabilizer. The grade has nominal density 0.954 g/cm³ by ISO 1183-1 and melt flow rate 0.25 g/10 min by ISO 1133-1. The extruder is a grooved-feed single-screw machine with 25:1 L/D and a barrier screw; barrel temperature profile is held from 180°C to 210°C, head temperature at 205–215°C, and melt temperature measured at 200–215°C. Die gap is set to 2.4–3.0 mm for a 20 L parison weight of 1.1–1.3 kg; blow pressure is 0.75–0.85 MPa and mold temperature is 12–20°C to limit differential shrinkage caused by mold-side versus blow-side cooling gradients. The terminal products are 10 L, 20 L, and 25 L UN 3H1 jerricans used for emulsifiable concentrates, suspension concentrates, and microemulsion crop-protection formulations. Type qualification is executed according to UN Model Regulations Chapter 6.1.5.2, including drop testing at 1.2 m for Packing Group II after conditioning at -18°C, leakproofness at 30 kPa internal air pressure, hydraulic pressure 100 kPa for 30 min, and stacking at 40°C for 28 days.

    UN 3H1 monolayer jerrican design-type test matrix for 20 L agrochemical package
    Design-type testReferenceConditionPass criterion
    Drop impactUN Model Regulations 6.1.5.2.41.2 m PG II, -18°C, water fillNo leakage
    LeakproofnessADR/RID 6.1.5.2.530 kPa internal air pressure under water, 5 minNo bubble stream
    Hydraulic pressureUN Model Regulations 6.1.5.2.6100 kPa for 30 minNo leakage or rupture
    Stacking loadUN Model Regulations 6.1.5.2.740°C for 28 daysNo deformation affecting transport safety

    What ESCR Margin Is Required for Food-Contact Dairy Bottles at 0.6 mm Nominal Sidewall Thickness?

    In monolayer dairy and edible-oil bottle lines, the dosage of Versalis HDPE BB 82 is 100 phr, with 3.0–4.0 wt% TiO₂ white masterbatch and, where closures require lower removal torque, 0.05–0.10 wt% erucamide slip concentrate. The food-contact status depends on the resin’s compliance with US FDA 21 CFR 177.1520(c), Item 3.2a for high-density polyethylenes with density at or above 0.94 g/cm³, and with EU Regulation (EU) No 10/2011, Annex I, including overall migration testing under Annex III conditions selected for the food type. The production process uses a shuttle blow molder with 24:1 L/D single-screw extruder, barrel profile 185–205°C, head temperature 195–205°C, parison programming with 0.55–0.65 mm minimum target sidewall, and mold temperature 10–20°C. Terminal product types are 500 mL, 1 L, and 2 L monolayer HDPE bottles for pasteurized milk, UHT milk, and edible oil. The low MFR of 0.25 g/10 min by ISO 1133-1 extends parison hang time for handleware molds but limits achievable cycle time when mold cooling time falls below 9 s. Amine-based antistatic additives should not be used in dairy-contact layers because they can contribute to organoleptic migration defects.

    Where the end-use fluid contains greater than 10% aromatic or halogenated solvent, monolayer BB 82 alone is not specified without a further barrier step. Three-layer coextrusion blow molding for solvent-resistant containers uses BB 82 as structural skins. In a typical three-layer structure, the outer and inner skins are dry-blended from 71 wt% BB 82, 20 wt% plant regrind of the same structure, 6 wt% maleic anhydride-grafted HDPE tie concentrate, and 3 wt% black masterbatch; the barrier core is polyamide at 5–8 wt% of total container mass. HDPE skins are processed on 25:1 L/D barrier screws at 210–220°C; polyamide core is processed on 30:1 L/D screw at 235–250°C; die head temperature is 220–230°C. Mold cooling at 10–15°C is used to stabilize layer distribution. Terminal products are 1 L, 5 L, and 20 L containers for paint thinner, brake cleaner concentrate, aliphatic hydrocarbon solvents, and mildly aggressive cleaning solvents. Packagings are certified as UN 3H1 where they carry dangerous goods; barrier performance is measured by weight loss after 28 days at 40°C according to ASTM D2684. Inline fluorination with 0.1–1.0% F₂ in N₂ is an alternative, but fluorinated scrap must not be mixed into non-fluorinated regrind because the fluorine-modified surface can release acid gas during subsequent melt processing.

    Post-Consumer Recyclate Let-Down and Oxidative Induction Time Stability

    Non-food detergent and household chemical bottles are the most common route for incorporating post-consumer recyclate into BB 82. The formulation uses 70–85 wt% virgin BB 82, 15–30 wt% high-density polyethylene PCR, and 1.0–2.0 wt% restabilization masterbatch. Before dosing, PCR is dried at 80°C for 4 h when residual moisture exceeds 0.02 wt%. The melt is processed on a vented 30:1 L/D compounding extruder with 80–120 mesh screen pack and gear pump, or directly converted on a blow molder fitted with a melt filter and vacuum venting. Because oxidative history of PCR reduces oxidative induction time measured by ASTM D3895 at 200°C, restabilization is adjusted until OIT exceeds 20 min. Published data for this specific configuration is limited, so plant-specific melt-flow and OIT correlation is required before raising PCR content above 20 wt%. Terminal products are 750 mL to 5 L non-food detergent, fabric softener, and automotive detailing product bottles. The relevant compliance reference for recycled content is EN 15343 for plastics recycling traceability and EU Regulation (EC) No 1907/2006 REACH for final article substances.

    Impact Resistance at -20°C as a Function of Parison Swell and Pinch-Off Geometry

    Automotive windshield washer reservoirs and coolant overflow bottles made from Versalis HDPE BB 82 require low-temperature ductility after pinch-off. The formulation is 100 phr BB 82, 2.0–2.5 wt% carbon black masterbatch, and 0.03–0.08 phr process aid. The accumulator-head blow molder employs a 30:1 L/D barrier screw, melt temperature 200–220°C, die gap 2.0–3.0 mm, and blow pressure 0.8–1.0 MPa. Terminal parts include 4.5 L washer reservoirs and 1.5 L coolant overflow bottles. In low-temperature qualification, sidewall Charpy impact according to ISO 179-1/1eA at -20°C generally exceeds 6 kJ/m²; however, the pinch-off weld can reduce impact by 30–50%, so tooling should maintain pinch-off land angle 20–30° and flash pocket depth 0.5–1.0 mm. Multiaxial impact is measured according to ASTM D3763 at -20°C; additional customer specifications may require no brittle split after 1.0 m drop at -20°C to concrete and no leakage after heat aging at 100°C for 168 h.

    Laundry detergent bottle lines running 750 mL and 1 L non-food containers use Versalis HDPE BB 82 at 100 phr with 2.5–3.0 wt% color masterbatch, processed on a 24:1 L/D shuttle blow molder at 190–210°C melt temperature and 0.75–0.85 MPa blow pressure, and the resulting articles are placed on the EU market under Detergents Regulation (EC) No 648/2004.

    Free Quote

    Competitive Versalis HDPE BB 82 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE BB 82 is an extrusion blow-moulding grade of high-density polyethylene supplied as stabilised pellets. The resin is characterised by a 190 °C/5.0 kg melt flow rate in the range 0.70–0.80 g/10 min and a density of 0.953 g/cm³ determined according to ISO 1183-1:2019. It is intended for the production of rigid containers and technical hollow parts on continuous shuttle, reciprocating-screw, and accumulator-head extrusion blow-moulding lines. The molecular architecture is a broad-distribution ethylene homopolymer, which provides high shear thinning during plastication and sufficient melt strength to limit parison sag before mould closure. The grade is not formulated for blown film, rotomoulding, or high-flow thin-wall injection moulding, where low-viscosity resins with different additive packages are required. The product is positioned in the Versalis HDPE portfolio for applications in which environmental stress cracking resistance, stiffness, and impact resistance are simultaneous requirements, and where the melt-flow class must remain low enough to permit large blow-up ratios without excessive wall-thickness scatter.

    Material Characteristics and Specification Boundary

    Typical lot-average values from the manufacturer’s technical datasheet are summarised in the accompanying table. These values are not batch-release limits; certificates of analysis control lot-to-lot variation in melt flow rate, density, and additive dispersion. Density is determined at 23 °C by ISO 1183-1:2019 method A and is quoted at 0.953 g/cm³. Melt flow rate is measured at 190 °C under a 5.0 kg dead weight according to ISO 1133-1:2022; the corresponding 2.16 kg value is typically below 0.30 g/10 min, which confirms high molecular weight and is consistent with parison hang-time behaviour on industrial blow-moulding machines. Tensile yield stress is determined on type 1A specimens at 50 mm/min under ISO 527-2:2012 and is typically 27 MPa, while the tensile elongation at break exceeds 700%. The flexural modulus measured by ISO 178:2019 is approximately 1.1 GPa. Charpy notched impact at 23 °C under ISO 179-1/1eA is approximately 25 kJ/m². The Vicat softening temperature under ISO 306:2022 method A50 is near 124 °C, and the crystalline melting peak by ISO 11357-3:2018 at 10 °C/min is approximately 132 °C. Environmental stress cracking resistance under ASTM D1693-15 condition B in 10% Igepal CO-630 is generally reported above 600 h for F50.

    Representative datasheet values for Versalis HDPE BB 82
    PropertyTest standardTypical value
    Melt flow rate, 190 °C/5.0 kgISO 1133-1:20220.75 g/10 min
    DensityISO 1183-1:20190.953 g/cm³
    Tensile yield stressISO 527-2:201227 MPa
    Tensile elongation at breakISO 527-2:2012>700%
    Flexural modulusISO 178:20191.1 GPa
    Charpy notched impact, 23 °CISO 179-1/1eA25 kJ/m²
    Vicat softening point A50ISO 306:2022124 °C
    ESCR F50, 10% Igepal CO-630ASTM D1693-15>600 h

    Capillary rheometry on the same melt-flow class under ISO 11443 indicates a shear-thinning flow index near 0.30. Apparent shear viscosity at 190 °C and 100 s⁻¹ is typically in the order of 2,000–3,000 Pa·s and falls to 400–600 Pa·s at 1,000 s⁻¹. The high zero-shear viscosity relative to injection-moulding grades retards parison sag but also intensifies shear heating in the die land. Die-land shear rates above 1,500 s⁻¹ can initiate melt fracture unless the land length is reduced below a 15:1 length-to-gap ratio or the die-lip entrance angle is relieved. These rheological limits define the upper output boundary on continuous-extrusion machines; exceeding the boundary causes surface roughness on the parison that persists in the moulded part as low-gloss patches and circumferential weld lines.

    Is BB 82 suitable for industrial chemical containers under cyclic loading?

    The ESCR response of BB 82 supports use in rigid containers for household chemicals, detergent-based cleaning formulations, and agricultural auxiliaries, provided chemical compatibility is established under end-use conditions. The ASTM D1693-15 condition B F50 above 600 h in 10% Igepal CO-630 is an accelerated indication of resistance to slow crack growth at stress-concentrated pinch-off weld seams and handle flash regions. However, this result does not cover all contact media; containers filled with hydrocarbon formulations containing more than 20% aromatic solvents, strong oxidising acids, or continuous internal pressure above 0.1 MPa generally require fluorinated or laminated barrier structures. Cyclic top-load testing of blow-moulded containers demonstrates that residual top-load after 10,000 cycles at 40% of initial failure load is dominated by wall-thickness uniformity. Sidewall thickness standard deviations above 0.3 mm accelerate buckling and corner cracking, while closed-loop parison programming can reduce the standard deviation below 0.2 mm in cylindrical containers up to 5 L. On production lines, the pinch-off zone is the primary failure initiation site because of frozen-in orientation and high local stress; it requires tail-flash design that avoids sharp notches and a mould pinch-land clearance between 0.15 mm and 0.30 mm for this density class.

    When BB 82 replaces a fractional-melt HDPE in large-part tooling

    Tool transfer from a fractional-melt HDPE to BB 82 requires adjustment of the parison controller and die gap, not merely a melt-temperature offset. Because BB 82 exhibits a higher MFR under 5.0 kg, the parison sag rate at a given die temperature is greater; operators on accumulator-head machines report the need to widen die gaps by 5–10% and to advance parison curl settings to maintain the same pre-blow timing. The cooling time for a 5 L container at 0.8 mm minimum wall thickness is typically 12–16 s with mould-water temperatures of 10–15 °C. Lower mould temperatures increase surface gloss but can create condensation on the mould face, leading to surface defects and thermal cycling of tooling. Internal regrind addition changes both rheology and ESCR; below 20 wt% the effect on ESCR is often linear, but above 30 wt% the retention can drop sharply because low-molecular-weight fractions generated by repeated heat history concentrate in the weld seams. For chemical containers, the recommended limit is 20–30 wt% of clean internal regrind, with the higher value permitted only for non-safety-critical packaging and when the ESCR is rechecked on finished parts at 60 °C in 10% Igepal CO-630.

    On shuttle and reciprocating-screw blow-moulding lines, the melt temperature measured at the die entry is commonly set between 200 °C and 220 °C, with a barrel profile running from 160 °C in the feed zone to 210 °C in the metering zone. Extruders with a length-to-diameter ratio of 24:1 to 30:1 and a compression ratio of 2.5:1–3.5:1 are employed; barrier screws with a Maddock-style dispersive mixer improve melt homogeneity without excessive shear heating. Accumulator-head machines benefit from die gap settings between 0.8 mm and 1.2 mm, while parison axial wall-thickness programming of ±20% around nominal is necessary to maintain sidewall thickness above the minimum service threshold in flat-sided containers. The resin does not require desiccant drying under normal indoor storage. If pellets have been stored outdoors or exposed to relative humidity above 80% RH, surface moisture can produce splay and bubbles in the parison; a pre-drying step at 70–80 °C for 3–4 h in a desiccant hopper is applied before extrusion. At melt temperatures above 240 °C, thermo-oxidative degradation becomes measurable as an increase in parison surface roughness and a reduction in ESCR even when machine output remains constant. At die-entry temperatures below 190 °C, melt fracture and parison weld-line weakness are observed on parts with flow-length-to-wall-thickness ratios above 100:1. Processing outside these boundaries can be accepted only after pilot trials confirm that critical finished-part properties remain within specification limits.

    Production-scale bottlenecks for BB 82 are more likely to occur in the plastication stage than in the blowing stage. On a single-station shuttle machine with a 60 mm barrier screw and 24:1 L/D, the maximum stable screw speed for a 2.5 L container is typically limited by melt-temperature rise at the die entry rather than by head pressure. Batch-to-batch variation in the 5.0 kg MFR of ±0.05 g/10 min can shift the optimal die gap by 0.1 mm and alter top-load retention by 3–5% if not compensated. Colour masterbatch addition at 2–3 wt% can shift the apparent melt flow by 0.03–0.05 g/10 min and can reduce ESCR if the masterbatch carrier is a low-molecular-weight polyethylene with poor compatibility. Operators report that pinch-off flash thickness is a better predictor of container failure than barrel temperature alone; irregular flash thickness above 0.5 mm correlates with incomplete material consolidation at the weld line and increased crack propagation under drop testing.

    Within the Versalis HDPE blow-moulding range, BB 82 is differentiated from higher-density grades in the 0.958–0.962 g/cm³ interval by a lower flexural modulus and higher ESCR. Against grades with 190 °C/5.0 kg MFR above 1.2 g/10 min, BB 82 provides greater melt strength and better top-load retention on tall rectangular containers, but it requires higher melt temperature and longer cooling time. Compared with metallocene-catalysed HDPE grades that exhibit narrower molecular weight distribution, BB 82 has a broader distribution, which improves extrusion processability and parison stability at the expense of slightly lower impact resistance at equivalent density. The product should not be considered interchangeable with bimodal high-density pipe resins or with high-molecular-weight film grades, because stabilisation, comonomer content, and molecular architecture are tailored to different conversion processes.

    Mould cooling circuits for BB 82 containers are normally designed to maintain a mould surface temperature between 10 °C and 30 °C. For polyethylene of this density, cooling-water temperature below the dew point of the plant air can cause condensation on the mould face; this is not a polymer defect but creates surface defects and increases cycle-to-cycle variability. The use of chiller water at 5 °C is therefore usually restricted to thin-wall containers where cycle-time reduction justifies mould insulation and dry-air shrouding. For containers with wall thickness above 2.5 mm, internal cooling air at 0.2–0.4 MPa and 10–15 °C reduces cooling time by 15–25% relative to unventilated blow air, but introduces a risk of frost formation if moisture is not removed from the air supply.

    Compliance boundaries for direct food contact are reference-grade specific

    Food-contact suitability of BB 82 is governed by the additive package and pigment present in the specific lot. In unmodified natural form, high-density polyethylene olefin polymers are referenced in FDA 21 CFR 177.1520(c) 3.2 and in EU Regulation (EC) No 10/2011, subject to overall migration limits of 10 mg/dm² of food-contact area and specific migration controls for any additives or processing aids used. The manufacturer’s compliance declaration must state the lot number and conversion conditions, because colour masterbatches, slip agents, and antistatic packages introduced during compounding or on the shop floor are outside the base-polymer declaration. For industrial chemical packaging, the relevant framework is the UN Model Regulations, Chapter 6.1, where stack-loading, drop-test, and leakproofness tests are carried out on the finished container rather than on the resin alone. BB 82 can be used in UN-certified packaging only when the container design, minimum wall thickness, closure system, and regrind content remain within the certified envelope; increasing regrind addition above 10% may trigger recertification depending on the competent authority and the dangerous goods class.

    Compliance and standard matrix for BB 82 applications
    Regulatory or standard referenceScopeTypical application
    EU 10/2011Plastic food-contact materialsNatural resin food packaging
    FDA 21 CFR 177.1520(c) 3.2Olefin polymers, density > 0.94 g/cm³Food-contact containers
    REACHRegistration, SVHC absenceEU industrial packaging
    RoHSLead, mercury, cadmium, hexavalent chromium, PBB, PBDENon-food technical parts
    UN Model Regulations Chapter 6.1Performance tests for dangerous goods packagingsCertified containers

    The REACH registration for the polymer applies in the European Economic Area only to the imported or manufactured substance as placed on the market; downstream users remain responsible for verifying that the final article does not exceed 0.1% w/w of any substance of very high concern. Under RoHS, heavy-metal restrictions for technical parts require compliance with lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ether limits at the homogeneous-material level. No declaration that BB 82 is intrinsically RoHS-compliant in coloured or flame-retardant compounds should be issued without a specific test report from the final compound supplier.

    The upper continuous-use temperature of BB 82 without mechanical load is approximately 65 °C in air; under load, the service temperature is lower due to creep and oxidative induction time limitations. Exposure to ultraviolet light under ASTM G154:2023 cycle 1 can reduce tensile elongation at break by more than 50% after 1,000 h if no UV stabilisation package or opaque pigmentation is present. Natural resin is therefore unsuitable for outdoor service unless the container is painted, co-extruded with a UV-protective skin, or compounded with a stabiliser masterbatch. The grade is not recommended for continuous contact with strong oxidising acids such as sulfuric acid above 98% concentration or sodium hypochlorite solutions above 10% active chlorine at temperatures above 40 °C, because oxidative attack accelerates molecular weight loss and weld-line embrittlement. Published data for BB 82 in pressurised hot-water applications above 60 °C is limited. Thin-wall injection moulding or high-flow thermoplastics processes requiring melt flow rates above 2 g/10 min at 190 °C/2.16 kg are outside the intended processing envelope of this grade.

    Top