| HS Code | 327801 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.20 g/10 min |
| Melt Flow Rate 190 C 21 6 Kg | 6.0 g/10 min |
| Tensile Stress At Yield | 26 MPa |
| Tensile Strain At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Izod Notched Impact Strength At 23 C | 15 kJ/m² |
| Vicat Softening Temperature 10 N | 125°C |
| Hardness Shore D | 62 |
| Brittleness Temperature | < -70°C |
| Melting Temperature | 132°C |
| Thermal Conductivity | 0.45 W/m·K |
| Water Absorption | < 0.01% |
| Volume Resistivity | > 1 × 10^16 Ω·cm |
| Dielectric Constant At 1 Mhz | 2.3 |
| Environmental Stress Crack Resistance Escr | > 1000 h |
As an accredited Versalis HDPE BB 76 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE BB 76 is supplied in 25 kg polyethylene bags, typically stacked on 1,250 kg pallets. |
| Container Loading (20′ FCL) | Versalis HDPE BB 76, bagged in 25 kg PE bags, palletized and loaded into a 20-foot FCL container for shipment. |
| Shipping | Versalis HDPE BB 76 is typically shipped as non-hazardous high-density polyethylene pellets in 25 kg bags, palletized and stretch-wrapped. Transport in clean, dry, covered trucks or containers at ambient temperature. Protect from moisture, contamination, direct sunlight, and extreme heat. No UN dangerous goods classification applies. |
| Storage | Store Versalis HDPE BB 76 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and oxidizing agents. Keep original packaging sealed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking and mechanical damage. Maintain ambient conditions, use clean dry floors, follow first-in/first-out stock rotation, and comply with local regulations and the supplier’s safety data sheet. |
| Shelf Life | Typically 12 months from production when stored in original packaging, dry, ventilated, protected from direct sunlight and heat. |
Extruded parisons of high-molecular-weight HDPE based on Versalis BB 76 are processed on accumulator-head blow-moulding machines with grooved-barrel single-screw extruders at length/diameter ratios of 24:1 to 30:1. The grade is specified around a density of 0.945 g/cm³ per ISO 1183-1:2019 and a high-load melt flow rate in the 6.0 g/10 min region at 190 °C/21.6 kg per ISO 1133-1:2022, placing it in the high-sag-resistance range required for 20 L to 60 L UN-rated jerrycans and tight-head drums. Melt temperatures are held between 185 °C and 210 °C, while mould temperatures are maintained at 10 °C to 30 °C to balance surface defect rejection against cooling-cycle productivity. Parison programming with axial wall-thickness control is used to increase wall thickness at pinch-off zones and top chime areas, with post-mould dimensional checks referencing net mass and brimful capacity. In this application, the polymer’s resistance to environmental stress cracking is assessed under ASTM D1693-15 Condition B in 100% Igepal CO-630, with commercial specification values typically above 1000 h; this threshold is relevant for containers holding aggressive industrial cleaners, aliphatic hydrocarbons, and oxidising formulations. Processors report that blow-pressure settings of 0.6 MPa to 0.8 MPa and pre-blow delay times under 3 s reduce melt fracture and improve weld-line integrity at the handle and bung zones. The processing window is comparatively narrow at the lower melt-temperature end because HMW-HDPE of this viscosity class begins to exhibit reduced flow through narrow die gaps below 185 °C, while temperatures above 210 °C increase parison sag and can transfer polymer degradation products to the inner surface. Compliance for dangerous goods packaging is anchored to the UN Model Regulations Chapter 6.1 and the ADR transport provisions under 6.1.5.3, with drop, stack, leakproofness, and hydraulic pressure tests required for the finished container design. During dry-side blending, processors add 2.0–4.0 wt% colour masterbatch and 0.1–0.3 wt% hindered-amine light stabilizer concentrate, with regrind ratios limited to 30% unless UN qualification testing on first-generation regrind supports higher levels without reducing ESCR below the design minimum. Terminal products include UN-marked 3H1 jerrycans and 1H1 tight-head drums for liquid dangerous goods under Packing Groups II and III.
| Packing group | Drop height |
|---|---|
| I | 1.8 m |
| II | 1.2 m |
| III | 0.8 m |
Automotive fuel-tank tooling for HDPE BB 76 involves multilayer co-extrusion blow-moulding lines with six-layer die heads, in which the resin functions primarily as the outer UV-stabilised layer and as the regrind-bearing core layer. The reason is its high low-shear viscosity and parison stiffness, which reduce layer-thickness variation across large tank geometries under long parison hang times. The outer layer is commonly blended with 2.0–2.5 wt% carbon black masterbatch to meet exterior weathering and opacity requirements, while the regrind layer may constitute 40–50 wt% of the total tank wall when supported by a barrier layer. Barrier structures typically combine an EVOH inner layer at 1.5–3.0% of total wall thickness with maleic-anhydride-grafted polyethylene tie layers on both sides; BB 76 is not used as the direct EVOH bonding layer because tie resins with higher polar compatibility are required. For designs that omit EVOH, surface fluorination after moulding is applied at 0.5–2.0 vol% fluorine in nitrogen, with contact times of 20–60 s at 20 °C to 50 °C, reducing permeation by crosslinking the exposed HDPE surface. The downstream process requires accumulator-head machines with parison programming across the tank length, as the polymer’s swell and sag behaviour must be compensated at the filler neck, flange bosses, and pinch-off regions. Published data for this specific configuration is limited, but processing practice for HMW-HDPE fuel-tank grades indicates a melt-temperature window of 200 °C to 230 °C, with head tooling designed for high swell and melt-pressure stability. The tank wall is typically designed at 2.5–4.5 mm nominal thickness, with ultrasonic wall-thickness scanning used to reject parts showing local thinning beyond 0.3 mm from the CAD target. Compliance anchors include UN ECE Regulation No. 34 for fuel-tank fire resistance and mechanical integrity, FMVSS 301 for rear-impact fuel-system integrity, SAE J1737 for permeation measurement, and evaporative emission limits enforced through EPA 40 CFR 86.1813-17. Operational limitations apply when EVOH is combined with HDPE BB 76: the EVOH layer must be dried to below 0.1% moisture before extrusion, and melt-temperature differentials between the HDPE outer layers and the EVOH core must be controlled to avoid viscosity mismatch that causes interfacial distortion. Terminal products include diesel fuel tanks, auxiliary fuel containers, and fuel filler necks for off-road and on-road vehicle platforms.
Because emulsifiable concentrate formulations and solvent-based pesticide premixes exert strong oxidative and permeation stress on monolayer packaging, BB 76 is used in co-extrusion blow-moulded containers for crop-protection chemicals where a polyamide barrier layer or post-mould fluorination provides the required resistance to solvent penetration. The compliance framework is set by the FAO/WHO Guidelines for Packaging and Storage of Pesticides, together with UN transport requirements for dangerous goods when the active substance is classified under ADR/IMDG. In these containers, the five-layer structure may consist of an outer regrind layer at 55–60%, tie resin at 2%, polyamide barrier at 3–5%, tie resin at 2%, and an inner virgin HDPE food-package-compatible layer at 30–35% of total bottle mass. The inner virgin layer prevents direct contact between regrind and the pesticide formulation, while the polyamide barrier reduces permeation of aromatic solvents such as xylene and cyclohexanone. However, the use of polyamide requires regeneration of the barrier layer from production scrap, and viscosity differences between HDPE BB 76 and polyamide during extrusion can produce melt-flow instabilities if the die-head design does not isolate the layers at the mandrel and spiral distributor. ISO 180 Charpy impact testing is used to evaluate low-temperature drop resistance at −18 °C, with formulations adjusted through regrind ratio reduction and impact-modifier-free virgin HDPE content if failures occur. Addition ratios during dry-side blending include 2.0–3.0 wt% colour/UV masterbatch and 0.05–0.2 wt% antioxidant concentrate, with regrind restricted to 20–25% to protect ESCR and to reduce the presence of degraded polymer from previous thermal cycles. The downstream blow-moulding process uses reciprocating-screw or accumulator-head machines with separate parison programming for handle zones and closure bosses, along with post-mould leak testing at 20–30 kPa internal pressure to detect pinholes. Terminal product types include 1 L, 5 L, 10 L, and 20 L narrow-neck bottles, as well as wide-mouth jars for granular herbicide formulations, all intended for agricultural chemical distribution channels.
The production of 1000 L composite IBC inner bottles from BB 76 relies on the grade’s high-molecular-weight distribution, which provides the hot parison rigidity needed to hold wall thickness tolerances during shot masses of 7–12 kg. Large accumulator-head blow-moulding machines with clamp forces above 2500 kN are used, and the parison is released from a diverging die head with axial and radial parison programming to compensate for thinning at the bottom discharge outlet and the top filling neck. The polymer’s melt temperature is maintained between 190 °C and 215 °C, while the mould is chilled to 10 °C to 20 °C to accelerate cooling and reduce cycle time. Blow air pressure in the range of 0.5–0.7 MPa is applied after mould closing, followed by post-blow cooling to allow dimensional stabilisation before demoulding. Because these inner bottles are inserted into steel or wire cages and may be stacked under load at elevated warehouse temperatures, the creep modulus is evaluated by compression tests at 40 °C and 60 °C, with deformation limits referenced against ISO 9969 or equivalent bearing-load test methods. Addition of external lubricant or release agent is normally avoided because it can reduce cage-fit friction and create mismatch between bottle and frame. The compliance matrix for the IBC inner bottle includes the UN Model Regulations Chapter 6.5 requirements for composite IBCs, designated by the code 31H1, and the hydrostatic pressure and leakproofness test provisions of ADR 6.5.2.5. Terminal products are closed-top inner bottles for 1000 L composite IBCs used in non-food chemical distribution, including lubricating oil additives, water-treatment chemicals, and non-oxidising industrial liquids.
Extrusion blow-moulded washer fluid reservoirs and coolant expansion tanks made from BB 76 require controlled wall thickness at deeply recessed mounting bosses and at the integral filler neck. The downstream process uses multi-cavity blow-moulding cells with needle-blow or robot-inserted fitting placement after demoulding, followed by hot-plate welding of spigots, sensor bosses, and mounting brackets. Melt temperature is kept between 190 °C and 210 °C, and the parison is programmed with a thicker lower section to prevent thinning at the deepest draw point. In service, the reservoir undergoes thermal-pressure cycling from −40 °C to 80 °C, and leak testing is performed at 0.03–0.05 MPa internal pressure to detect weld-line failures. The formulation for this application is simpler than for fuel tanks: the base resin is combined with 2.0–2.5 wt% carbon black masterbatch for UV protection and 0.05–0.1 wt% antioxidant concentrate, with regrind content held below 20% because OEM appearance and weld strength requirements penalise higher recycle fractions. Compliance is defined by OEM engineering specifications invoking ISO 188 for accelerated ageing and ISO 4892-2 for xenon-arc exposure, while material certification includes density and high-load MFR data per ISO 1183-1:2019 and ISO 1133-1:2022. Terminal product types include 3–8 L windshield washer reservoirs, coolant overflow reservoirs, and auxiliary fluid tanks for passenger cars and light commercial vehicles.
Competitive Versalis HDPE BB 76 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE BB 76 is a high-density polyethylene resin designated for extrusion blow moulding of rigid packaging and technical hollow parts. The material is supplied as pelletised homopolymer with a European material identification of PE-HD under ISO 11469:2021. Manufacturer technical literature lists a typical density of 0.956 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 0.40 g/10 min at 190 °C with a 2.16 kg load under ISO 1133-1:2022. The corresponding high-load melt index is 23 g/10 min at 21.6 kg, indicating a shear-thinning response suitable for parison stability in shuttle and accumulator blow moulding machines. Typical mechanical values include a tensile stress at yield of 25 MPa under ISO 527-2, a flexural modulus of 950 MPa under ISO 178, a notched Charpy impact strength of 9 kJ/m² at 23 °C under ISO 179-1/1eA, a Vicat softening temperature of 127 °C under ISO 306/A50, and an environmental stress-cracking resistance greater than 200 h under ASTM D1693B in 100% Igepal CO-630 at 50 °C. The reported values are typical values, not batch-release specification limits; the current manufacturer certificate of analysis and technical data sheet govern lot-level compliance.
Principal applications include detergent, agricultural-chemical, sanitary-product, and industrial-fluid containers in the 5–30 L range. The grade may be evaluated for food-contact packaging only when the final formulation, processing aids, and colourants are confirmed against EU No 10/2011 and FDA 21 CFR 177.1520 through the appropriate supply-chain documentation. BB 76 is not intended for blown film, monofilament, thin-wall injection moulding, or pressure pipe service.
The low-load melt flow rate of 0.40 g/10 min places BB 76 in the high-viscosity region that is generally unsuitable for thin-wall injection moulding. General-purpose injection moulding HDPE grades often operate from 8 g/10 min to 40 g/10 min to fill high-flow-length closure moulds. Processing BB 76 in a standard injection moulding machine with screw L/D below 20:1 typically increases screw recovery time and can require melt temperatures above 230 °C, where oxidative gel formation becomes a practical risk. Compared with HDPE film grades, BB 76 has higher density and higher flexural modulus, which improves top-load stiffness but reduces dart impact and tear propagation; it is not formulated for blown film extrusion.
Against bimodal PE100 pipe grades, BB 76 does not carry a PE100 minimum required strength classification under ISO 9080. Pipe resins are characterised by strain-hardening modulus under ISO 18488 and by notched pipe test data under ISO 13479. BB 76 is instead specified around bottle ESCR, parison sag resistance, and consistent wall-thickness distribution in extrusion blow moulded parts. For pressure-bearing applications, the long-term creep and crack-propagation resistance of BB 76 are not covered by a pipe-grade hydrostatic design basis.
The following table consolidates manufacturer-published typical values for BB 76. They are not specification limits and may vary by production campaign, sampling protocol, and conversion method.
| Property | Typical value | Test standard |
|---|---|---|
| Density | 0.956 g/cm³ | ISO 1183-1:2019 |
| Melt flow rate at 190 °C/2.16 kg | 0.40 g/10 min | ISO 1133-1:2022 |
| Melt flow rate at 190 °C/21.6 kg | 23 g/10 min | ISO 1133-1:2022 |
| Tensile stress at yield | 25 MPa | ISO 527-2 |
| Tensile modulus | 1000 MPa | ISO 527-2 |
| Flexural modulus | 950 MPa | ISO 178 |
| Charpy notched impact strength at 23 °C | 9 kJ/m² | ISO 179-1/1eA |
| Vicat softening temperature, 10 N load | 127 °C | ISO 306/A50 |
| Environmental stress-cracking resistance, 100% Igepal CO-630 at 50 °C | >200 h | ASTM D1693B |
| Shore D hardness | 62 | ISO 868 |
Extrusion blow moulding of BB 76 is typically conducted on single-station shuttle or accumulator-head machines equipped with parison programming. On a 100 mm grooved-feed extruder with screw L/D of 28:1, a barrel profile from 160 °C to 210 °C and a die temperature of 200–210 °C are used in many production campaigns for 20 L containers. Melt temperature at the die exit should not exceed 220 °C during prolonged runs. Sustained operation above 220 °C is associated with dark die-lip deposits and a gradual loss of parison stretch uniformity. Head tooling with a diverging mandrel is preferred because BB 76 exhibits pronounced die swell at production shear rates. Die swell values specific to BB 76 are not ordinarily published; the 25–40% range reported for HDPE blow moulding grades of this melt-index class is based on shear rates from 100 s⁻¹ to 1000 s⁻¹. The exact swell depends on die land length, die gap, melt temperature, and extruder head pressure.
Parison sag is controlled by maintaining the high-load melt index near 23 g/10 min and adjusting the die gap to 0.8–1.5 mm for sidewall thicknesses from 0.6 mm to 1.2 mm. Mould cooling is normally maintained at 10–25 °C. Higher mould temperatures reduce gloss and increase cooling time, while mould temperatures below 5 °C can create surface condensation and uneven shrinkage. Blow air pressure of 0.5–0.8 MPa is adequate for most containers in the 5–30 L range, provided the exhaust path does not create excessive back-pressure. For a shuttle line producing 20 L containers on a 18 s cycle, regrind fractions above 30 wt% should be revalidated for ESCR, because published data for this specific configuration are limited.
Post-industrial HDPE regrind from the same production line may be introduced at loadings up to 20 wt% without additional densification testing, provided the regrind is screened through a 2 mm mesh and stored below 60% relative humidity. Higher loadings require revalidation of melt flow shift, density drift, and environmental stress-cracking resistance. Post-consumer recycled HDPE should not be assumed compatible without quantifying polypropylene contamination. Polypropylene concentrations above 5 wt% tend to form separate domains in the polyethylene matrix and reduce weld-line strength in the pinch-off area of blow moulded parts. When wet storage is suspected at RH > 60%, regrind should be dried at 80 °C for 2–3 h before blending to reduce microvoid formation.
Food-contact use is limited to formulations that meet the relevant overall migration limit and specific migration limits under EU No 10/2011. For aqueous or dairy products with pH <4.5 or fat content above 5%, the container producer must verify migration of additives and oligomers under the test conditions selected from Annex III and Annex V of EU No 10/2011. In the United States, FDA 21 CFR 177.1520 permits olefin polymers for food contact provided the prescribed density, extractables, and end-group limits are met. BB 76 is not suitable for hot-fill above 80 °C or retort sterilisation. The HDPE matrix begins to soften near its Vicat temperature of 127 °C, and sustained top-load creep above 60 °C can exceed dimensional tolerances in thin-walled panels.
In narrow-neck container production with a multi-cavity shuttle machine, the practical melt-temperature window for BB 76 is approximately 190–215 °C when regrind levels exceed 15 wt%. Below 190 °C, the melt exhibits excessive die pressure and poor parison surface finish. Above 215 °C, the residence-time limit for gel control shortens and the parison becomes prone to sag-related wall thinning. On long accumulator runs, the melt residence time should not exceed 10 min at 220 °C. These conditions are equipment-dependent and should be confirmed through pressure-rise measurements and visual inspection of die-lip deposits.
Containers for agricultural emulsifiable concentrates benefit from the base ESCR rating above 200 h under ASTM D1693B; however, compatibility testing must be performed with the actual formulation. Solvent blends containing xylene, cyclohexanone, or n-methyl-2-pyrrolidone can reduce ESCR below the base value by plasticising the amorphous fraction of the semicrystalline matrix. Drop-impact testing after conditioning at -20 °C is required for outdoor or cold-chain distribution, because the notched Charpy value of 9 kJ/m² at 23 °C does not guarantee low-temperature ductility. The material may be used for pharmaceutical intermediate packaging only when the finished container is validated for extractables and leachables under the relevant pharmacopoeia protocol, and when the blow moulding line maintains a defined purge procedure to prevent cross-contamination.
Electrical and electronic packaging made from BB 76 may be assessed for heavy-metal restrictions under RoHS Directive 2011/65/EU. Unfilled high-density polyethylene is not usually constrained by the 0.1 wt% lead, 0.1 wt% mercury, 0.1 wt% hexavalent chromium, or 0.01 wt% cadmium limits, but energy-dispersive X-ray fluorescence screening is still recommended when recyclate content is used. REACH Regulation EC No 1907/2006 obligations must be confirmed through the supplier’s current safety data sheet and substance-of-very-high-concern declarations. Batch traceability of BB 76 should include retention of the lot number, production date, and certified melt flow rate, density, and ash content.