Versalis Hdpe 760

Versalis HDPE 760

    • Product Name: Versalis HDPE 760
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 568028
    Grade Versalis HDPE 760
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.960 g/cm³
    Melt Flow Rate 190c 2 16kg 0.25 g/10 min
    Melt Flow Rate 190c 5kg 1.3 g/10 min
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Break >600 %
    Flexural Modulus 1300 MPa
    Notched Izod Impact Strength 23c 20 kJ/m²
    Shore D Hardness 65
    Vicat Softening Temperature 127 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Cracking Resistance 10pct Igepal >1000 h
    Water Absorption <0.01 %
    Thermal Conductivity 0.40 W/m·K
    Mold Shrinkage 2.0-3.0 %

    As an accredited Versalis HDPE 760 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE 760 packaging: 25 kg polyethylene-lined bags, palletized and shrink-wrapped for secure industrial transport and storage.
    Container Loading (20′ FCL) Versalis HDPE 760: 20′ FCL container loading, palletized 25 kg bags, shrink-wrapped, securely stowed, approximately 18–20 MT net weight.
    Shipping Versalis HDPE 760 is typically shipped as non-hazardous polyethylene pellets in 25 kg PE bags, big bags, or bulk. Transport in clean, dry trucks/containers at ambient temperature. Protect from moisture, direct sunlight, and contamination. Store in a cool, dry, ventilated area and follow the SDS/local regulations.
    Storage Store Versalis HDPE 760 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Use pallets, avoid excessive stacking, and follow first-in, first-out rotation. Maintain ambient temperature; avoid prolonged UV exposure. Ensure good housekeeping and prevent static buildup during handling.
    Shelf Life Versalis HDPE 760 shelf life: typically 24 months in original, unopened packaging, cool, dry, away from direct sunlight.
    Application of Versalis HDPE 760

    Extrusion blow moulding of industrial jerrycans in the 5 L to 25 L range uses HDPE 760 as the base olefin polymer in a formulation comprising 100 parts by mass HDPE 760, a carbon black UV masterbatch at 2.0–3.0 wt%, an antistatic concentrate at 0.2–0.5 wt%, and a colour masterbatch at 1.0–2.0 wt%. Compliance for dangerous-goods packaging rests on the UN Model Regulations and ADR/RID 6.1 packaging provisions, with UN 3H1/Y1.5 jerrycans required for packing group II liquids; food-contact grades are further assessed under FDA 21 CFR 177.1520 and EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² for non-fatty simulants. Downstream production on an accumulator-head blow moulder with a 25:1 L/D extruder and 1.5–2.0 kg shot capacity maintains melt temperature between 190°C and 215°C, die temperature 5–10°C below melt temperature, blow pressure 0.6–0.9 MPa, mould cooling-water temperature 8–12°C, and blow-up ratio 2.0:1–2.5:1; parison programming is set to remove 25–35% of constant-thickness parison mass. Terminal finished products are 5 L, 10 L, and 20 L HDPE jerrycans for solvents, detergents, food oils, and UN-certified chemical transport. Published data for this specific configuration is limited where accumulator head volume and mould geometry are not fixed; cycle time and flash generation must be verified on the target line.

    When Injection-Moulded Crates Are Stacked at −20°C and Impact Resistance Governs the Specification

    Injection-moulded heavy-duty crates and logistics totes manufactured from HDPE 760 require a composition of 85–90 wt% HDPE 760 and 10–15 wt% of a C6-linear low-density polyethylene or equivalent impact modifier, with 1.5–3.0 wt% carbon black masterbatch and 0.5–1.5 wt% processing aid where cycle-time reduction is required. Compliance is anchored to ASTM D256-23 Izod notched impact, ASTM D638-14 tensile yield, ISO 178 flexural modulus, and ASTM D1693 environmental stress-cracking resistance under condition B, 10% Igepal; food-contact logistics containers are additionally assessed under FDA 21 CFR 177.1520 and EU 10/2011. Processing on a reciprocating-screw injection moulder with a 30:1 L/D screw and compression ratio 2.8:1–3.2:1 uses melt temperatures of 220–240°C, injection pressures of 70–100 MPa, hold pressures of 40–60 MPa, and mould temperatures of 10–15°C; at wall thicknesses of 3–5 mm, cooling time is 25–40 s and total cycle time 45–65 s. Terminal products include stackable beverage crates, agricultural totes, industrial pallet collars, and cold-chain distribution boxes. The operational boundary is low-temperature impact: below −20°C, sharp-corner geometries require impact-modifier loadings above 15 wt%, but loadings exceeding 20 wt% can reduce environmental stress-cracking resistance; lot-specific verification is mandatory before large-scale production.

    High-cavitation closure moulding uses HDPE 760 as the base polymer in a formulation of 100 parts by mass HDPE 760 with 500–1000 ppm erucamide slip, 0.08–0.12 wt% primary antioxidant, 0.5–1.5 wt% nucleating masterbatch, and 0.5–2.0 wt% colour concentrate. Regulatory assessment for food-contact closures follows FDA 21 CFR 177.1520 and EU Regulation 10/2011; carbonated soft drink closures are additionally tested for internal-pressure retention under the ISBT closure performance protocol, while tensile properties follow ISO 527-1:2019 and notched impact is measured under ASTM D256-23. The downstream process uses a 32- or 48-cavity hot-runner injection mould, melt temperature 210–230°C, injection speed 80–120 mm/s, hold pressure 30–50 MPa, and mould temperature 10–20°C; for a closure mass of 1.5–2.0 g, cooling time is 8–12 s. Terminal product types are 28 mm, 30/25 mm, and 38 mm screw closures with tamper-evident bands for still water, carbonated soft drinks, dairy, and pharmaceutical bottles. Mould temperatures below 10°C can induce thread ovality and intermittent band folding; above 20°C, orbit tear-off force can fall below customer specification unless hold time is extended.

    What Limits Contact-Heating Thermoforming of HDPE Sheet Above 165°C?

    HDPE 760-based sheet formulations for thermoformed cold-food packaging are compounded with 100 parts by mass HDPE 760, 0.5–2.0 wt% titanium dioxide white masterbatch, 0.5–1.5 wt% nucleating agent, 0.1–0.3 wt% slip additive, and, where anti-fog performance is required for chilled display, 1.0–2.0 wt% of a food-approved anti-fog concentrate. Regulatory assessments follow FDA 21 CFR 177.1520 and EU 10/2011; density is verified under ISO 1183-1:2019, flexural modulus under ASTM D790-17, and sheet thickness tolerance is held at ±5% of nominal. Sheet production on a single-screw extruder with 30:1–36:1 L/D barrier screw uses barrel temperatures of 180–215°C, a three-roll polishing stack at 60–80°C, and sheet thicknesses from 0.4 mm to 1.2 mm. Thermoforming uses contact heating at 140–160°C, plug-assisted positive moulding, and vacuum pressure 0.4–0.6 bar below atmospheric; for 0.5 mm sheet, forming cycle is 6–10 s. Terminal products include dairy lids, chilled food trays, cold cups, and deli container bases. The limiting boundary is sag: at 1.2 mm sheet thickness, heating above 165°C can cause non-uniform wall thickness and web sag before forming; no universally transferable forming window has been published for this exact sheet thickness and plug-assist geometry, so line-specific verification is required.

    Blown film extrusion for industrial sacks and drum liners uses HDPE 760 in a blend of 85–95 wt% HDPE 760 and 5–15 wt% of a C6 or C4 linear-low-density polyethylene to raise dart impact and tear resistance, with 0.5–1.5 wt% slip/antiblock masterbatch and 2.0–3.5 wt% carbon black or white masterbatch depending on end use. The compliance package includes ASTM D1709 dart drop impact, ASTM D882-18 tensile properties, ASTM D1922 Elmendorf tear, and, where liners contact dry food or non-fatty substances, FDA 21 CFR 177.1520 and EU 10/2011. Film production on a blown-film line with 25:1–30:1 L/D extruder, die gap 1.2–2.0 mm, and blow-up ratio 3:1–5:1 uses a melt temperature of 190–210°C and frost line height 6–10 die diameters. Film thickness ranges from 10 µm to 50 µm, with gauge variation controlled to ±8% after bubble stabilization. Terminal products are industrial drum liners, shipping sack overwrap, hardware packaging, and agricultural net-wrap separators. For film below 15 µm, melt strength limitations may require reducing blow-up ratio to 2.5:1 or blending with higher-melt-strength HDPE; published data for HDPE 760 in thin-gauge film is limited, so pilot-line verification is required.

    Rotational Moulding of Medium-Sized Agricultural Water and Chemical Storage Tanks

    Rotational moulding with HDPE 760 uses a powder fraction in which 100 parts by mass of HDPE 760 is blended with 0.3–0.8 wt% HALS UV stabilizer masterbatch, 1.0–3.0 wt% pigment masterbatch, and, where closed-loop recycled material is incorporated, 10–20 wt% of plant-reground HDPE with melt-flow characteristics confirmed against the virgin lot. Compliance for water-contact tanks is assessed under FDA 21 CFR 177.1520 and EU 10/2011, while chemical storage tanks are specified under ASTM D1998-21 for polyethylene upright storage tanks and ISO 527-1:2019 for tensile properties; weathering resistance may be evaluated under ISO 4892-2:2013. The process is biaxial rotational moulding with oven temperature 280–320°C, peak internal air temperature 190–200°C, rotomoulding ratio 4:1 to 8:1 depending on tool diameter, cooling through forced air and water mist, and demoulding at part surface temperature below 70°C. Wall thickness is typically 4–10 mm; cycle time for a 500 L tank is 25–45 min. Terminal products include 200–1000 L agricultural water tanks, chemical dosing tanks, pallet boxes, and septic chambers. The operational boundary is peak internal air temperature: below 190°C the inner surface may retain unmelted powder, while above 200°C oxidative degradation can increase yellowing and ESCR loss in thick sections; published data for this specific configuration is limited, so each tool must be thermally profiled before serial production.

    Free Quote

    Competitive Versalis HDPE 760 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE 760 is identified in manufacturer literature as a high-density polyethylene extrusion blow-moulding grade. The product is positioned for rigid packaging and industrial container applications in which parison hang strength, stiffness, and environmental stress-cracking resistance are required simultaneously. The grade is supplied as pellets; pellet size distribution and bulk density should be obtained from the supplier’s handling sheet before designing pneumatic conveying, hopper loaders, or feed-throat inserts.

    The current public grade summary lists nominal values of 0.7 g/10 min for melt flow rate measured at 190 °C with a 2.16 kg dead load according to ISO 1133-1:2022, and 0.959 g/cm³ for density according to ISO 1183-1. Tensile yield stress is quoted as 30 MPa under ISO 527-2; flexural modulus is quoted as 1250 MPa under ISO 178. These are nominal grade-selection figures, not lot-specific certificates of analysis. Lot-to-lot variation can occur with catalyst generation, comonomer feed, and production campaign; tool and process limits should therefore be set with a safety margin and confirmed during first-article approval.

    On a production extrusion blow-moulding line, the low melt flow index is not a direct throughput limit. The practical constraint is melt-temperature homogeneity and screw-drive load. The grade is processed on continuous shuttle or accumulator-head machines with screw length/diameter ratios of 24:1 to 30:1 and compression ratios of 2.5:1 to 3.5:1. Grooved-feed extruders can develop high pressure at low screw speed; however, screw speeds above 120 min⁻¹ in a 60 mm grooved-feed machine can generate local melt-temperature overshoot above 230 °C. At 230 °C and above, thermo-oxidative chain scission becomes measurable, reducing parison melt strength and increasing gel defects in the finished container.

    Does a Melt Flow Index below 1.0 g/10 min Restrict High-Shear Extrusion Throughput?

    Melt flow index is a low-shear datum and does not describe high-shear behaviour in the screw channel or die land. Capillary rheometry under ISO 11443 should be used to obtain apparent shear viscosity at the die-land shear rates encountered in production, typically 100 s⁻¹ to 1000 s⁻¹. For high-density polyethylene blow-moulding grades, apparent shear viscosity at 100 s⁻¹ and 190 °C generally falls between 600 Pa·s and 1200 Pa·s; published secondary data for Versalis HDPE 760 at all shear rates is limited, so a capillary flow curve from the specific lot is recommended before die design.

    Die-land shear stress controls surface quality. Sharkskin or melt fracture initiates when the critical shear stress of the melt is exceeded at the die exit. In high-density polyethylene, the critical shear stress is commonly in the range 0.10 MPa to 0.18 MPa; operation above this band produces periodic surface roughness, particularly at melt temperatures below 180 °C. The practical processing window for HDPE 760 is therefore bounded at the low end by surface defects and at the high end by thermal degradation. Barrel zones should be incremented by no more than 10 °C to 15 °C from feed to die, and the adapter and die head must be independently heated to compensate for shear heating.

    At melt temperatures below 180 °C, the melt does not wet the die land adequately, and weld-line integrity in the pinch-off zone deteriorates. At melt temperatures above 230 °C, parison sag increases, and the molecular weight distribution may shift due to chain scission. This narrow window requires tighter thermal control than grades with melt flow rates above 2 g/10 min. For a circular die land of radius R, wall shear rate can be estimated as 4Q/(πR³); for a rectangular slit of width w and gap h, the corresponding estimate is 6Q/(wh²). These calculations allow die-land shear stress to be estimated before production once the flow curve is known.

    Parison programming is the principal control variable on accumulator-head machines. Axial wall thickness is generated by moving the die mandrel relative to the die bushing during the extrusion shot. For containers of 0.5 L to 5 L, programmed wall thickness is generally maintained to ±0.05 mm of nominal; deviations beyond this concentrate thin spots at the pinch-off and reduce drop-impact performance. Die swell modifies parison diameter by approximately 15 % to 35 %, and the die gap must be set smaller than the target wall thickness by the observed swell ratio. The swell ratio is not constant; it varies with head pressure, die-land length, and melt temperature. On accumulator-head machines, head pressure variation between shots should be recorded and held within ±5 bar to avoid drifts in parison length.

    Parison sag is time-dependent. The 0.7 g/10 min melt flow index provides sufficient zero-shear viscosity for hang times up to approximately 8 s in unmodified HDPE containers. When hang times exceed 8 s, the operator must reduce die temperature or shorten the shot; otherwise bottom-wall thinning and unequal wall distribution occur. HDPE 760 should not be considered a direct substitute for a bimodal high-density polyethylene specifically engineered for sag-resistant long-hang-time applications unless plant-scale trials confirm wall-thickness uniformity.

    Cooling-Limited Cycle Architecture, Parison Sag, and Die Swell Correction

    Cooling is the rate-limiting step in rigid blow moulding. High-density polyethylene has low thermal diffusivity; for wall thicknesses of 1.0 mm to 2.0 mm, cycle time is governed by mould temperature, coolant flow, and contact pressure. Mould temperatures between 10 °C and 30 °C are typical. Lower mould temperatures increase crystallinity and improve top-load stiffness but reduce surface gloss and can raise frozen-in stress at the pinch-off. Blow pressure is commonly set between 6 bar and 10 bar; the parison must be held against the mould wall until the part surface has cooled below the recrystallization temperature. For a 1 L container with 1.5 mm nominal wall thickness, cooling time in industrial practice is typically 10 s to 15 s, but published data for Versalis HDPE 760 under this specific configuration is limited. Moulds should be designed with turbulent coolant flow; a Reynolds number above 4000 in the water channels is recommended to prevent scale fouling and maintain uniform heat transfer.

    Thermal conductivity of solid HDPE is approximately 0.40 W/(m·K), and specific heat capacity is approximately 1900 J/(kg·K). These values support finite-element cooling simulation; heat removal is limited primarily by the polymer thermal diffusivity, not by the mould material. For high-density polyethylene, the crystallization temperature on cooling is typically between 118 °C and 125 °C, although published data for HDPE 760 specifically is limited. Demoulding before the surface has stabilized below this range can produce post-mould shrinkage and dimensional variability.

    Top-load strength and drop impact are the relevant acceptance tests for rigid containers. Top-load strength is measured according to ASTM D2659 or ISO 12048; drop-impact resistance is evaluated by ISTA 1A or ISO 2248 procedures. A density of 0.959 g/cm³ produces higher modulus than medium-density polyethylene, but the higher crystallinity also reduces the intrinsic impact toughness of the polymer matrix. Therefore, container design must avoid sharp corners and abrupt wall-thickness changes; otherwise impact failure occurs at a lower drop height than would be predicted from tensile elongation alone.

    When a 0.959 g/cm³ High-Density Resin Replaces Injection-Moulding or Film-Extrusion Polyethylene Grades

    Substitution is not universal. Injection-moulding HDPE grades normally have melt flow rates of 4 g/10 min to 20 g/10 min; their lower molecular weight reduces melt viscosity to permit thin-wall filling at practical injection pressures. HDPE 760, with 0.7 g/10 min, is unsuitable for thin-wall injection moulding. At normal injection melt temperatures of 220 °C to 260 °C, the resin would require high injection pressure and would remain resistant to long fill paths, increasing the risk of short shots, weld-line weakness, and gate blush. Conversely, the injection-moulding grade has insufficient melt strength for parison hang and would collapse during blow moulding of containers above approximately 0.5 L.

    Compared with high-density polyethylene film grades, HDPE 760 has a higher density and a narrower molecular-weight distribution. The higher density increases stiffness and water-vapour barrier, but it can reduce environmental stress-cracking resistance in aggressive detergent and surfactant service. Environmental stress-cracking resistance is evaluated by ASTM D1693 or ISO 22088; the test liquid, conditioning time, and stress level must be specified before comparing grades. Published data for the specific ESCR of HDPE 760 under all conditions is limited; users should request a lot-specific testing report when the package is intended for concentrated surfactant or solvent-containing formulations.

    The difference from linear low-density polyethylene is starker. Linear low-density polyethylene has lower modulus and lower density but higher puncture resistance and toughness. HDPE 760 is selected when top-load stiffness, creep resistance, and moisture barrier dominate; linear low-density polyethylene is selected when puncture and slow-rack resistance dominate. Compared with high-load melt-index pipe grades of 0.2 g/10 min to 0.5 g/10 min, HDPE 760 provides a compromise between melt strength and extrusion output intended for bottle production rather than pipe extrusion.

    Regulatory and food-contact declarations are product-lot dependent, not grade-universal

    Regulatory status cannot be inferred from grade designation alone. A certificate of conformity from the resin manufacturer is required for the exact production lot. The following matrix lists the standard foundations commonly applied to high-density polyethylene used in rigid packaging, but each entry must be confirmed against the supplier’s declaration.

    Compliance matrix requiring manufacturer confirmation
    DomainStandard or regulationTypical condition
    Food-contact plasticsEU 10/2011Overall migration limit 10 mg/dm² unless specified otherwise
    US food-contactFDA 21 CFR 177.1520Olefin polymers; end-use temperature and food type control
    REACHRegulation (EC) 1907/2006SVHC concentration ≤ 0.1 % w/w per article
    RoHSDirective 2011/65/EUPb, Hg, Cd, CrVI, PBB, PBDE restricted
    Good manufacturing practiceRegulation (EC) 2023/2006Applies to food-contact materials

    The molecular architecture of HDPE 760 is not fully specified in public summaries. Users should not infer long-chain branching or bimodality from melt flow and density alone. The melt-flow ratio between 21.6 kg and 2.16 kg loads is a better indicator of shear thinning; when available, it should be compared with the supplier specification. Published data for this specific configuration is limited, and secondary trade summaries should not replace a controlled rheological fingerprint of the incoming lot.

    Storage before processing affects part quality. The resin is not strongly hygroscopic, but surface condensation at relative humidity above 60 % can introduce moisture into the feed throat and produce streak defects. In such conditions, predrying in a desiccant or hot-air hopper at 60 °C to 80 °C for 1 h to 2 h is recommended. Avoid unspecified antistatic or slip additives unless their compatibility with the resin system has been confirmed in low-shear rheological testing; amine-based additives can accelerate discolouration or destabilize the melt at elevated head temperatures.

    Regrind addition is common in blow moulding. Addition rates up to 20 wt% are typically tolerated without severe loss of processability, but higher loads can reduce impact toughness and environmental stress-cracking resistance. Published data for the effect of regrind level on HDPE 760 specifically is limited. A plant-scale trial with instrumented top-load and drop-impact testing is required before setting a maximum regrind ratio in the quality-control specification.