| HS Code | 493704 |
| Density | 0.940 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 4.0 g/10 min |
| Melting Temperature | 125 °C |
| Vicat Softening Temperature | 105 °C |
| Tensile Modulus | 600 MPa |
| Tensile Strength At Yield | 18 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 600 MPa |
| Hardness Shore D | 55 |
| Izod Notched Impact Strength 23 C | 20 kJ/m2 |
| Brittleness Temperature | < -70 °C |
As an accredited Versalis Flexirene® MT 40 U Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® MT 40 U LLDPE is supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg net. |
| Container Loading (20′ FCL) | Versalis Flexirene® MT 40 U Linear Low Density Polyethylene loaded in 20′ FCL: palletized 25 kg bags, shrink-wrapped, secured. |
| Shipping | Versalis Flexirene® MT 40 U Linear Low Density Polyethylene is a non-hazardous polymer. It is not regulated for transport by road, rail, sea, or air; no UN number, class, or packing group. Ship in sealed bags or octabins, keep dry, avoid heat/sunlight, and prevent pellet spills. |
| Storage | Store Versalis Flexirene® MT 40 U in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers or bags closed, clean, and undamaged on pallets to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain good housekeeping to control dust and static. Use stock on a first-in, first-out basis. |
| Shelf Life | Typically 24 months from production date when stored unopened, dry, cool, and protected from direct sunlight; stable under normal conditions. |
In high-cavitation closure production, Flexirene MT 40 U is dosed as the continuous phase at 100% by weight for monolayer still-water and dairy screw caps; for pressure-resistant designs it is let down at 10–25 wt% into a high-density polyethylene copolymer carrier to improve environmental stress crack resistance without reducing top-load below the 0.30 MPa headspace pressure threshold specified for carbonated beverage closure systems. The grade’s melt flow rate of 4.0 g/10 min under ISO 1133-1:2022 and nominal density of 0.940 g/cm³ under ISO 1183-1 permit filling of 16- to 32-cavity hot-runner tools with valve-gated systems at melt temperatures of 220–250°C and injection pressures of 60–90 MPa. Production-scale experience on hydraulic toggle machines with clamp forces of 1800–4500 kN and screw L/D ratios of 20:1 to 24:1 indicates that gate freeze time and hold pressure profile control dimensional variation more than barrel temperature alone; cavity-to-cavity fill imbalance above 5% is corrected by raising the manifold setpoint 5–10°C rather than by increasing injection speed, preventing shear heating above 260°C. Gate diameters of 0.6–1.2 mm and land lengths of 0.8–1.5 mm are used to generate controlled shear without exceeding gate shear rates of 100,000 s⁻¹, which can produce delamination in tamper-evident band sections. Hold pressure is staged from 60 MPa for 3 seconds to 40 MPa for 5 seconds, and gate freeze is confirmed by cavity pressure decay below 5 MPa/s; closure ovality after ejection is held below 0.3 mm on 28 mm PCO neck finishes. Additive loading for food-contact closure stock is limited to 1.0–2.0 wt% colour masterbatch and 1.5–3.0 wt% erucamide slip plus silica antiblock masterbatch, both compounded on carriers complying with EU Regulation 10/2011 and FDA 21 CFR 177.1520; finished closures are tested under EN 1186-1 for overall migration below 10 mg/dm², while child-resistant designs are assessed under ISO 8317 where applicable. Terminal manufactured articles include tamper-evident screw caps for still water and fruit juices, snap-on closures for personal care bottles, and pharmaceutical closure shells subjected to USP <661.1> extractables testing on the assembled package. MT 40 U is not assigned as a sole resin for carbonated soft drink closures because its butene-based comonomer distribution yields lower top-load retention under continuous CO₂ headspace than high-density polyethylene or metallocene linear low density polyethylene grades.
Thin-wall containers produced from Flexirene MT 40 U are processed at wall thicknesses from 0.45 to 1.10 mm, where the 4.0 g/10 min melt flow rate under ISO 1133-1:2022 shortens filling time but narrows the melt-cushion window to 3–6 mm on accumulator-assisted injection units with L/D 22–25 and screw diameters of 40–60 mm. The material is normally dosed at 100% by weight, with 1.0–3.0 wt% titanium dioxide white masterbatch and 0.05–0.2 wt% fluoropolymer processing aid; the processing aid is reduced or omitted in microwaveable containers where the final article is tested under EU Regulation 10/2011 Annex II for overall migration at 10 mg/dm² and under GB 4806.7-2016 for food-contact plastics. Processing on 3000–6000 kN toggle machines with hot-runner systems uses barrel profiles of 180–230°C, nozzle and hot runner at 230–260°C, and mould coolant at 10–30°C; injection velocity is set between 200 and 400 cm³/s to prevent flow hesitation at thin leading edges, while hold pressure is limited to 35–55 MPa because higher values increase gate-induced residual stress and produce out-of-flatness above 1.0 mm on 500 mL rectangular tubs. Melt-cushion control is critical on production lines: a cushion below 3 mm causes non-uniform packing and visible sink marks adjacent to the gate, whereas a cushion above 6 mm extends residence time and may elevate off-taste potential in high-surface-area food-contact articles. Hot-runner pressure drop is typically held between 15 and 20 MPa, and processors using spiral flow evaluations under ISO 294-5 report flow length-to-wall thickness ratios up to 150:1 at injection pressures near 200 MPa. Cooling time for 0.55 mm walls at 15°C mould temperature is limited to 2–4 seconds, giving total cycle times of 5–8 seconds on high-speed packaging machines. Terminal product types include injection-moulded dairy cups, margarine and spread tubs, delicatessen containers, and thin-wall food-service pails up to 1 L. The grade is not recommended for retort or hot-fill above 70°C because dimensional stability and organoleptic performance under those conditions have not been fully established.
Outdoor agricultural fittings in contact with UV radiation and agrochemical solutions require a stabiliser package sufficient to maintain tensile elongation at break above 50% after 2000 hours of accelerated weathering under ISO 4892-2 cycle 1. Flexirene MT 40 U is processed at 100% by weight for low-pressure irrigation connectors, with 2.0–3.0 wt% carbon black masterbatch added when total UV protection must exceed the base stabiliser level for service in high-irradiance regions; carbon black dispersion quality is assessed by particle aggregate size under ISO 18553, and the masterbatch carrier is selected to comply with REACH Annex XVII and EU Regulation 10/2011 where the part may contact potable water. Injection moulding on 1000–2500 kN machines with cold sprue bushings and unheated moulds at 15–25°C uses melt temperatures of 210–250°C, injection speeds of 40–80 cm³/s, and hold pressures of 30–50 MPa; long flow paths in multi-cavity irrigation fitting tools are balanced by sequential valve gating rather than raising melt temperature beyond 250°C, which would consume hindered amine light stabiliser and shift the carbonyl index above 0.05 absorbance units in infrared monitoring. Tensile strength retention is further checked after weathering by ISO 527-2 type 1A specimens, and agrochemical compatibility is screened by immersion in 10% active ingredient solution at 40°C for 30 days, with acceptable mass change below 1%. Low-temperature Charpy impact testing under ISO 179-1 at -10°C is applied to spring-clip designs that must survive installation in frozen soil conditions. Terminal components include barbed irrigation connectors, dripper bodies, greenhouse fastener clips, and sprayer tank lids. The grade should not be used as the sole material for pressure pipe or mainline fittings governed by ISO 4427 or ISO 17885; these systems require high-density polyethylene grades with minimum required strength classification.
Unlike thin-wall food packaging, thick-section housewares impose cooling-time dominance rather than filling-pressure dominance on cycle time when Flexirene MT 40 U is moulded at wall thicknesses of 2.5–6.0 mm. The resin is dosed at 100% by weight for translucent storage boxes, with 1.0–2.0 wt% colour masterbatch and, where low-temperature drop resistance is required, 10–20 wt% linear low density polyethylene or high-density polyethylene blended in-line at the machine hopper; blend ratio is stabilised by gravimetric dosing to avoid melt flow ratio drift above 0.5% of the set value. Processing on hydraulic direct-clamp machines of 2000–5000 kN with cold runner or hot-tip bushings uses melt temperatures of 210–240°C, mould temperatures of 20–40°C, injection speeds of 50–120 cm³/s, and hold pressures of 40–60 MPa maintained until gate freeze. On 4-cavity drawer-unit tools, material accumulation in cold slug wells after 8-hour campaigns can generate black specks unless screw retraction speed is limited to 30 mm/s and the barrel is purged at the end of each shift; thick bosses and reinforcing ribs develop sink marks if hold pressure decays below 40 MPa before gate freeze. Shrinkage after 48 hours is typically 1.2–1.8% in the flow direction and 1.0–1.5% transverse when measured under ISO 294-4, and mould compensation is adjusted accordingly. Articles intended for food storage are designed under FDA 21 CFR 177.1520 and EU Regulation 10/2011, with colourants verified against GB 9685-2016; non-food housewares are assessed for restricted substances under REACH Annex XVII entry 63. Terminal product types include stackable storage crates, drawer units, household baskets, hangers, and under-bed containers. Annealing at 80°C for 2 hours after ejection is applied to low-flatness lids where warpage must remain below 1.5 mm over a 400 mm span.
When Flexirene MT 40 U is let down with high-density polyethylene for cold-chain pails, the addition level is set by the ductile-to-brittle transition shift measured under ISO 179-1/1 eA at -20°C. Typical dry-blend or melt-compounded formulations contain 10–30 wt% Flexirene MT 40 U and 70–90 wt% HDPE blow-moulding or injection grade; below 10 wt%, the impact strength of a 5 L pail can fall below 5 kJ/m² at -20°C, while above 30 wt%, sidewall top load tested under ISO 12048 may decrease enough to cause stacking failure in cold-store racking. Processing uses 5000–12000 kN hydraulic injection machines with barrier screws of L/D 24:1, melt temperatures 220–250°C, and chilled moulds at 10–20°C; hold pressures of 50–70 MPa are maintained until gate freeze at 10–15 seconds. For pails with wall thicknesses above 3 mm, mould cooling circuits are run with water at 8–15°C to prevent post-ejection shrinkage that causes lid mismatch; lid-to-pail seal tightness is checked by internal vacuum decay below 0.02 MPa/min. The pail body and lid are tested for food-contact compliance under EU Regulation 10/2011 and FDA 21 CFR 177.1520, and for heavy metal content under CONEG or EU Packaging Directive 94/62/EC; migration testing follows EN 1186-2 for aqueous food simulants. Terminal products include 2–25 L freezer pails, ice cream tubs, cold-chain fish and meat containers, and insulated logistic totes. The blend is not suitable for hot filling above 80°C or for direct contact with fatty food simulants without specific migration testing.
Toys and leisure articles injection-moulded from Flexirene MT 40 U are usually produced at 100% by weight with 1.0–3.0 wt% masterbatch whose pigments are selected from the positive list in EU Regulation 10/2011 and tested under EN 71-3:2019+A1:2021 for migration of 19 elements; no ortho-phthalate plasticisers are added because the grade’s low glass-transition environment provides sufficient flexibility at room temperature. Processing on 1000–3000 kN toggle machines with open nozzle and cold sprue bushings uses melt temperatures of 210–240°C, mould temperatures of 15–25°C, and injection speeds of 30–70 cm³/s; thick toy walls from 2.0–8.0 mm require low hold pressure of 25–40 MPa to minimise sink marks, but packing time must extend until the gate freezes or sink depth on flat surfaces exceeds 0.05 mm. Production-scale observations show that colour changeovers on toy presses require 15–20 residence times to remove previous pigment from the screw, and that abrasive pearlescent masterbatches accelerate screw and barrel wear unless hard-coated screws are installed. Re-grind from rejected parts is typically reused at 5–15 wt% in non-food toys after in-line metal detection and melt filtration through screens of 300–500 µm. Terminal products include outdoor sandpit toys, building blocks, play table components, and sports training cones. The grade is not supplied with antistatic or flame-retardant properties for electronic toys; such modifications are performed by the converter only after verification against EN 71-2 flammability and REACH Annex XVII restrictions.
Competitive Versalis Flexirene® MT 40 U Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® MT 40 U is a linear low density polyethylene based on a butene-1 comonomer and supplied as a UV-stabilised pellet or powder for rotational moulding and thick-section profile extrusion. The nominal melt flow rate is 4.0 g/10 min when determined at 190°C under a 2.16 kg load in accordance with ISO 1133-1:2022; the nominal density is 0.925 g/cm³ when measured according to ISO 1183-1:2019. These values place the product in the medium-flow butene-copolymer class, where sufficient tool-filling capability is retained without losing the ductility and environmental stress-cracking resistance expected of lower-density polyethylene. The density corresponds to a crystalline weight fraction near 50–55%, and the melting endotherm recorded by differential scanning calorimetry at 10°C/min under ISO 11357-3:2018 generally lies between 120°C and 126°C. Published data for the exact grade is limited; values cited here are typical manufacturer or polymer-class data and should not be interpreted as sales specification limits.
Rotational moulding of MT 40 U is governed primarily by peak internal air temperature rather than by melt flow alone. The polymer powder should be ground to a median particle diameter between 250 µm and 500 µm; particles below 150 µm tend to fluidise during the early heating phase and create local thinning at tool corners, while particles above 600 µm retard melt densification and increase the number of pinholes at the inner surface. Oven setpoint temperatures of 270–310°C are common for tools with wall thicknesses between 3 mm and 6 mm. The peak internal air temperature should be held within 190–210°C for complete sintering; below 180°C, residual air bubbles remain trapped at the polymer-tool interface, and above 220°C, thermo-oxidative degradation becomes measurable as a decline in tensile impact strength and an increase in carbonyl absorption. On production-scale biaxial rotomoulding machines, steel tooling manufactured from 3 mm sheet may impose a 10–15% cycle-time penalty relative to 6 mm cast aluminium tooling at the same part wall thickness because of lower heat-transfer rates. Demoulding should not begin above 70°C for flat panels; premature removal above 75°C causes warpage and out-of-tolerance dimensions under ISO 2768-1:1989 medium class. Published data for this specific configuration is limited, so trials should establish the exact peak internal air temperature for each tool geometry.
At 23°C and 50% relative humidity, the tensile stress at yield of MT 40 U typically ranges from 9 MPa to 11 MPa when tested at 50 mm/min according to ISO 527-2:2019. Tensile strength at break is normally recorded at 20–25 MPa, and nominal tensile strain at break exceeds 500%. Rotomoulded specimens at 4 mm wall thickness usually exhibit ductile puncture behaviour at -20°C; brittle failure becomes more probable below -30°C, especially when sintering is incomplete or when regrind content exceeds 20 wt%. Environmental stress-crack resistance, evaluated by the bent-strip method in 10 vol% Igepal CO-630 at 50°C, is generally above 500 h for a 2 mm compression-moulded sheet. These properties support outdoor tanks and chemical containers, but continuous load-bearing service above 40°C should be confirmed by creep-rupture testing according to ISO 22088-1. MT 40 U is not recommended for pressure-pipe service or applications requiring the elevated-temperature creep resistance of high-density polyethylene.
The U suffix identifies a compounded ultraviolet-stabiliser package dispersed in the polymer during pelletising. A typical LLDPE weatherability package combines a high-molecular-weight hindered amine light stabiliser with a benzophenone or triazine UV absorber; the precise composition is proprietary. When exposed in a QUV accelerated test according to ISO 4892-3:2016 with 0.68 W/m²·nm at 340 nm, 2 mm plaques of a UV-stabilised butene LLDPE in this density class typically retain more than 50% of initial tensile elongation after 4000 h; published data for MT 40 U in this exact configuration is limited, so outdoor service life must be validated against the intended climate. In subtropical continuous sun exposure, the additive package alone is not a substitute for carbon black or white pigmentation where a service life beyond 5 years is required. Dark-coloured parts can reach surface temperatures above 55°C; this accelerates oxidative breakdown unless the pigmentation masterbatch contributes additional thermal aging protection. The UV package does not increase the base polymer’s continuous-use temperature and should not be combined with certain transition-metal stearates that can reduce light stability.
When the grade is processed by single-screw extrusion for thick profiles or sheet, a grooved-feed extruder with a screw length-to-diameter ratio of 25:1 to 30:1 is preferred. Barrel temperatures from 160°C at the feed zone to 210°C at the die are sufficient; die temperatures above 220°C increase the risk of melt fracture and surface oxidation. The lower melt strength of an LLDPE with 4.0 g/10 min melt flow rate makes free-form extrusion and large-diameter parison handling more difficult than with a high-pressure LDPE of equivalent density. Water-bath or spray cooling should be uniform to prevent differential shrinkage; variable cooling rates across thick sections generate internal stress and later environmental stress-cracking. Published data for this exact grade in profile extrusion is limited.
Dry blending with high-pressure low density polyethylene at 10–30 wt% is sometimes used to modify melt rheology and surface gloss. The addition reduces shear viscosity at 100 s⁻¹ and lowers melt-entry pressure in extrusion; in rotational moulding it also widens the sintering window. However, oxygen transmission rate increases relative to neat MT 40 U; at 30 wt% LDPE, oxygen permeability by ISO 15105-2 at 23°C and 0% RH may be 15–25% higher, and this should be verified on the finished wall. Dry blending also introduces batch-to-batch variability in additive distribution; stabiliser-rich and stabiliser-poor domains can appear if tumble-mixing time is below 15 min or if the two granulates differ widely in bulk density. In rotomoulded parts, uneven blending produces inner-surface flow lines and wall sections with differential solidification rates. Coextrusion or melt compounding is preferable when barrier performance and surface properties must be separated from impact performance. Published data for this specific configuration is limited.
The table below collects typical property ranges from publicly available technical literature for butene-copolymer LLDPE at 0.925 g/cm³ density and 4.0 g/10 min melt flow rate. Values are not batch guarantees and should be confirmed against the manufacturer’s certificate of analysis.
| Property | Test method | Typical value or range |
|---|---|---|
| Melt flow rate, 190°C/2.16 kg | ISO 1133-1:2022 | 4.0 g/10 min |
| Density | ISO 1183-1:2019 | 0.925 g/cm³ |
| Melting peak temperature | ISO 11357-3:2018 | 120–126°C |
| Vicat softening temperature, A/50 | ISO 306:2022 | 95–105°C |
| Tensile stress at yield | ISO 527-2:2019 | 9–11 MPa |
| Tensile strength at break | ISO 527-2:2019 | 20–25 MPa |
| Nominal tensile strain at break | ISO 527-2:2019 | >500% |
| Environmental stress-crack resistance, F50 | ASTM D1693-15 | >500 h |
Regulatory assessment of MT 40 U for food-contact articles must proceed under Regulation (EU) No 10/2011 and FDA 21 CFR §177.1520 for olefin polymers, provided that the specific UV-stabiliser package is approved for the intended contact condition. Overall migration limits and specific migration limits for the stabiliser should be evaluated on the finished article under the time and temperature conditions prescribed by the applicable amendments to Regulation (EU) No 10/2011. For industrial chemical packaging, the safety data sheet and REACH registration confirm the grade’s status; users should verify that the part complies with Regulation (EC) No 1907/2006 Title VII requirements before placing goods on the European market. The grade contains no intentionally added cadmium, lead, mercury, hexavalent chromium, polybrominated biphenyls, or polybrominated diphenyl ethers; however, RoHS compliance for electrical and electronic equipment cannot be inferred from this statement alone and should be confirmed against the material declaration.
Compared with non-UV-stabilised butene grades in the same melt-flow family, MT 40 U offers equivalent melt-flow and density positioning but with a compounded light-stabiliser package. The tradeoff is a moderately higher yellowness index and a slight reduction in clarity, which is largely irrelevant in pigmented outdoor parts but measurable in unpigmented thin profiles. Compared with a metallocene-catalysed LLDPE of equivalent density, MT 40 U shows a broader composition distribution and lower dart drop impact at film thickness below 25 µm, but it has a wider rotational-moulding processing window and is less sensitive to mould-release agents and moisture. Compared with high-pressure LDPE, MT 40 U has higher tensile strength and puncture resistance at identical wall thickness, but requires greater torque in single-screw extrusion and shows lower melt strength in free-form parison extrusion. These differences define the product boundaries: MT 40 U is selected where outdoor weatherability, medium flow, and LLDPE toughness are required, rather than where optical clarity or metallocene puncture performance at very thin cross-sections is the primary requirement.
Incoming quality control should include melt flow rate verification by ISO 1133-1:2022, density by ISO 1183-1:2019, and moisture content by ISO 15512:2019 if the product has been stored in unheated warehouses. LLDPE is not as hygroscopic as polyamide or polyester, but condensation on pellet surfaces can form after storage at relative humidity above 60%; surface moisture should be removed by drying at 60–70°C for 2–3 h only when necessary. Batch-to-batch variation in melt flow rate above ±0.3 g/10 min can alter rotomoulding cycle time and wall thickness distribution; production trials should be repeated after a change in lot. The material should not be processed in equipment previously used for polyvinyl chloride without adequate purging because residual chlorine-containing compounds can degrade the stabiliser package. Published data for this specific configuration is limited.