| HS Code | 139770 |
| Productname | Versalis Flexirene® MT 40 A |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Additive | Antioxidant |
| Density | 0.940 g/cm³ |
| Meltflowrate | 4.0 g/10 min at 190 °C/2.16 kg |
| Meltingpoint | 125 °C |
| Vicatsofteningtemperature | 105 °C |
| Tensilestrengthatyield | 16 MPa |
| Tensilestrengthatbreak | 12 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 700 MPa |
| Hardnessshored | 55 |
| Thermalconductivity | 0.33 W/m·K |
| Specificheat | 2300 J/kg·K |
| Waterabsorption | <0.01% |
| Dielectricconstant | 2.3 |
| Volumeresistivity | >1.0 × 10^15 ohm·cm |
| Casnumber | 9002-88-4 |
| Chemicalformula | (C2H4)n |
| Appearance | Pellets |
| Color | Natural |
| Odor | Odorless |
| Solubilityinwater | Insoluble |
As an accredited Versalis Flexirene® MT 40 A Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® MT 40 A: supplied in 25 kg moisture-resistant polyethylene bags, palletized for convenient storage and handling. |
| Container Loading (20′ FCL) | Versalis Flexirene® MT 40 A Linear Low Density Polyethylene pellets, palletized in 25 kg bags, loaded into a 20′ FCL container. |
| Shipping | Versalis Flexirene® MT 40 A is shipped as non-hazardous, free-flowing LLDPE pellets in 25 kg PE bags or 500–1000 kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Keep away from moisture, heat, and direct sunlight. No special dangerous goods labeling required. |
| Storage | Store Versalis Flexirene® MT 40 A in a cool, dry, well-ventilated, clean indoor area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Palletize and stack securely to avoid deformation or falling. Maintain moderate temperatures, avoid prolonged UV exposure, follow first-in, first-out rotation, and protect from physical damage. |
| Shelf Life | Stable under normal storage; shelf life typically 24 months in unopened original packaging, dry, cool, away from direct sunlight. |
Versalis Flexirene MT 40 A is a butene-based linear low density polyethylene with a nominal density of 0.940 g/cm³ and a melt mass-flow rate of 4.0 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022. The grade is supplied as antioxidant-stabilised pellets and is applied in downstream industrial sectors requiring stress-crack resistance, low-temperature flexibility, and controlled melt rheology. The following application entries are limited to industrial configurations for which the melt viscosity and comonomer architecture of the grade are technically appropriate.
Flexirene MT 40 A is pulverized on commercial disc mills to a particle size distribution of 35 mesh (500 µm) with a median particle size of 250–300 µm before being charged into biaxial rotational moulding tools. For agricultural chemical storage and industrial water treatment tanks, the formulation is dry-blended with 2.5 wt% to 3.5 wt% carbon black masterbatch for ultraviolet stabilisation and with 0.5 wt% to 1.0 wt% hindered amine light stabiliser masterbatch for exposed service. The industry compliance framework for these vessels includes ASTM D1998-15 for upright polyethylene storage tanks and EN 12573-1:2000 for welded static thermoplastic tanks; where the tank enters food-contact service, the moulded wall must satisfy EU 10/2011 overall migration and specific migration limits after worst-case food simulant testing. The environmental stress-crack resistance of rotomoulded walls, tested under ASTM D1693-15 condition B in 10% Igepal CO-630 at 50 °C, is reported by industrial qualification programs to exceed 1,000 h for 2.5 mm wall thickness. On commercial shuttle or carousel machines, the mould is charged at a surface temperature of 60–70 °C, heated in an oven at 280–300 °C, rotated at a biaxial speed ratio of 4:1 until the peak internal air temperature reaches 180–200 °C, then cooled with forced air and water mist until demoulding at a mould surface temperature below 55 °C. Rapid cooling below 50 °C before part release is recorded on production lines as a cause of warpage in flat roof panels; therefore demoulding is staged to allow internal stress relaxation. Terminal parts produced from this grade include upright tanks up to 5,000 L, chemical dosing bins, seed hoppers, and agricultural spraying reservoirs.
On blown-film lines producing 200–400 µm heavy-duty construction and silage films, Flexirene MT 40 A is introduced as the core layer of three-layer coextruded structures at 60–70 wt% of the total film composition, with LDPE or HDPE skin layers at 15–20 wt% each to stabilise bubble geometry. In monolayer production, the formulation is 100 wt% Flexirene MT 40 A blended with 2–3 wt% carbon black masterbatch, and slip/antiblock additives are dosed at 500–1,500 ppm where roll blocking is observed during slit-film conversion. Compliance testing for industrial liners uses ASTM D882-18 for tensile yield and break, ASTM D1709-16a for dart drop impact, and ISO 4591:1992 for gravimetric thickness uniformity; silage films are tested under EN 13207:2018 for mechanical properties, oxygen permeability, and weathering resistance. Processing is carried out on grooved-feed extruders with a die gap of 2.0–2.4 mm, a blow-up ratio of 2.5:1 to 3.0:1, melt temperature 190–210 °C, and frost line height 8–10 die diameters. Bubble instability increases at blow-up ratios above 3.0:1 when 100% butene-based LLDPE is run; therefore 20–30 wt% LDPE is melt-blended to raise melt extension viscosity in high-neck configurations. Terminal products include construction vapour control layers, silage bags, agricultural grain storage envelopes, and industrial bin liners.
In injection moulding of 20 L industrial pails, drum lids, and chemical container closures, Flexirene MT 40 A is processed as 100% virgin pellets or blended with 1–2 wt% colour masterbatch and 0.5 wt% processing aid. For screw caps and hinged closures, the formulation frequently includes 10–15 wt% high-density polyethylene to raise top-load rigidity while the LLDPE continuous phase preserves hinge stress-crack resistance. Moulding equipment in the 300–500 t clamp force range is used with a barrel temperature profile of 180/200/210/220/230 °C, melt temperature 200–230 °C, injection pressure 80–100 MPa, holding pressure 60–80 MPa, and mould temperature 20–40 °C. The compliance matrix includes ASTM D1238-23 for melt mass-flow rate verification, ISO 1133-1:2022 for comparative MFR testing, ASTM D1693-15 condition A for environmental stress-crack resistance, and ASTM D256-23 for notched Izod impact. Where the finished pail or closure is used for dangerous goods packaging, design-type testing is required under applicable UN 1H2 or UN 3H1 performance codes. Melt residence time should not exceed 15 min above 230 °C because oxidative chain scission raises MFR and lowers ESCR despite the antioxidant package. Terminal products include open-top industrial pails, 50 L drum lids, and screw caps for chemical containers.
The addition of Flexirene MT 40 A to post-consumer polypropylene reclaim at 5 wt%, 10 wt%, and 15 wt% produces a measurable shift in notched Charpy impact and melt-flow stability without the need for pre-drying unless surface condensation is observed at relative humidity above 60% and temperature swings cause moisture on cold pellets. The recommended starting ratio for injection-moulded logistics crates from mixed-colour reclaim is 10 wt% Flexirene MT 40 A and 2 wt% compatibilizer masterbatch; for automotive interior carrier parts the loading is increased to 15 wt% but not beyond, because tensile modulus falls below the required 1,300 MPa benchmark and heat-deflection performance becomes marginal for painted assemblies. Compounding is performed on a co-rotating twin-screw extruder with L/D 44:1, barrel temperatures 190/200/210/220/225 °C, screw speed 300–350 rpm, and specific mechanical energy input 0.18–0.22 kWh/kg; the LLDPE phase is dispersed through high-shear mixing and screw-configuration-controlled domain size reduction. The compliance matrix uses ISO 527-2:2012 tensile modulus and yield stress, ISO 179-1:2010 Charpy unnotched impact at 23 °C, ISO 6603-2:2000 instrumented puncture impact, and ISO 1133-1:2022 melt flow rate at 230 °C/2.16 kg. Where recycled content enters electrical and electronic housings, REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU apply. Terminal products include stackable logistics crates, automotive trunk trim substrates, and garden furniture structural components.
Flexirene MT 40 A is employed as the polymer carrier in high-load carbon black and additive masterbatch where its 4.0 g/10 min melt mass-flow rate allows pigment loadings of 40–50 wt% without strand sagging during water-bath pelletising. In the masterbatch formulation, the carrier constitutes 50–60 wt% by mass for carbon black concentrates and 60–70 wt% for additive packages; at the finished-part level the letdown ratio is 2–4 wt% masterbatch into polyethylene or polypropylene compounds. Production lines use co-rotating twin-screw extruders with L/D 36:1 to 44:1, a barrel temperature profile of 180–210 °C, screw speed 250–350 rpm, and melt filtration through 100/125 mesh screen packs upstream of the strand die. Compliance is established under ISO 11469:2016 for polymer identification marking, REACH Regulation (EC) No 1907/2006 for substance registration, and Directive 2008/98/EC where post-industrial regrind is incorporated. Terminal products include carbon black masterbatch for agricultural films, processing-aid concentrates for blown-film extrusion, and custom colour masterbatch for injection moulding.
Three-layer polyethylene coating of steel pipelines introduces Flexirene MT 40 A as the outer topcoat in dry-blend with 2.5 wt% carbon black masterbatch, applied at a nominal thickness of 1.5–3.0 mm over an adhesive tie layer of 0.2–0.4 mm. In specifications where scratch hardness is critical, the topcoat is blended with 15–20 wt% HDPE; however, the butene-based LLDPE phase retains the low-temperature flexibility required for field bending at or below −20 °C. The coating process uses a crosshead extrusion die mounted on a travelling carriage; the steel pipe is preheated to 180–220 °C, grit-blasted to Sa 2½ under ISO 8501-1:2007, primed with an epoxy layer of 150–200 µm, then coated with adhesive and LLDPE topcoat in a single continuous pass. Compliance is governed by ISO 21809-1:2018 for external coatings for buried or submerged pipelines, DIN 30670:2012 for polyethylene coatings on steel pipes and fittings, and CSA Z245.21-18 for external polyethylene coating on steel pipe. Material tests include ASTM D792-20 density, ASTM D1603-20 carbon black content, and ISO 11357-6:2018 oxidation induction time; cathodic disbondment is evaluated under ISO 21809-1 at 23 °C for 28 days at −1.5 V polarisation. Continuous service above 60 °C is not recommended for the butene-based LLDPE topcoat because oxidative induction time depletes rapidly in contact with alkaline soil conditions. Terminal products include onshore gas transmission pipelines, water pipelines, and industrial effluent lines.
Competitive Versalis Flexirene® MT 40 A Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® MT 40 A is a linear low density polyethylene supplied in pellet form for injection moulding and compounding operations. The grade is positioned at a nominal density of 0.940 g/cm³ when evaluated under ISO 1183-1:2019 and a melt mass-flow rate of 4.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The density value places the polymer at the upper edge of the LLDPE range, producing a modulus and creep resistance above those of conventional film-grade LLDPE while retaining the low-temperature ductility associated with linear short-chain branching. Unlike high-pressure low density polyethylene, the molecular architecture contains limited long-chain branching. This characteristic raises low-shear viscosity and reduces draw resonance during extrusion, but it also restricts melt strength in blow moulding and tubular film processes. The product is differentiated from higher-flow Flexirene injection grades by its 4.0 melt flow rate, which limits thin-wall filling behaviour but improves environmental stress crack resistance and impact retention in thicker cross-sections.
The polymer is manufactured within the Flexirene linear polyethylene platform, historically associated with Ziegler-Natta catalysis and C4 comonomer incorporation. Public documentation identifies the product as a butene-based LLDPE; however, the exact comonomer content, molecular weight distribution, and catalyst formulation are controlled product parameters not fully disclosed in the technical data sheet. The short-chain branches introduced during polymerisation disrupt lamellar crystallisation, lowering crystallinity relative to HDPE while maintaining a higher tie-molecule concentration than high-pressure LDPE. This architecture explains the intermediate stiffness and the balance between tensile yield strength and impact toughness reported for the material.
At a density of 0.940 g/cm³, the crystalline fraction approaches the medium-density transition, so the product should not be treated as a low-modulus packaging film resin. The higher density reduces the permeability of moulded parts to oxygen and water vapour compared with lower-density LLDPE grades, but the effect is moderate and must be verified for barrier-critical closures using gas transmission test methods such as ASTM D3985 and ASTM F1249. Grade-specific barrier data are not fully disclosed in the public technical sheet; converters requiring defined oxygen or moisture transmission windows should request batch-specific data or evaluate the final part geometry under application conditions.
Thermal characterisation places the Vicat softening point near 118 °C under ISO 306 method A/10 N, and the crystallite melting range is typical of linear polyethylene with short-chain branching. The combination of softening point and density supports short-term service temperatures below 70 °C. Continuous exposure above this threshold is not advisable for load-bearing parts because the tensile modulus declines progressively with increasing temperature. The product is not inherently flame-retarded, and ignition behaviour should be assessed under the relevant end-product standard rather than inferred from polyethylene oxidative stability data.
Rheological behaviour is governed by the narrow molecular weight distribution common to Ziegler-Natta LLDPE injection grades. At a melt mass-flow rate of 4.0 g/10 min, the material exhibits shear-thinning behaviour under injection moulding shear rates, but the viscosity at low shear is higher than that of 20 g/10 min high-flow LLDPE grades. This limits thin-wall spiral flow and increases injection pressure demand. Mould filling studies for this specific grade are not fully published; processors should not extrapolate spiral flow data from general-purpose LDPE or high-flow LLDPE without confirmation.
Injection moulding of Flexirene® MT 40 A requires a screw geometry consistent with linear polyethylene processing: an L/D ratio between 20:1 and 25:1, a compression ratio of approximately 2.5:1 to 3.5:1, and a general-purpose or low-shear metering section. Melt temperatures between 220 °C and 250 °C are typical for injection moulding; the lower limit supports thick-wall parts requiring higher melt viscosity for holding pressure, while the upper limit increases flow length but accelerates oxidative chain scission if residence time is uncontrolled. Processing above 260 °C is not recommended because thermal degradation can generate aldehydes, ketones, and free-radical chain scission products that reduce notched impact strength and increase odour.
Screw speeds above 120 min−1 at elevated back pressure can produce shear heating sufficient to exceed the targeted melt temperature. This is particularly relevant on machines with shutoff nozzles or long hot-runner manifolds where the material experiences multiple shear cycles. When screw speed is increased, barrel temperature settings should be reduced incrementally, and the melt temperature should be verified with a needle pyrometer rather than inferred from barrel set points. Excessive shear heating manifests as surface splay, yellowing at hot-runner gates, and inconsistent shot weight. Maintaining screw recovery below 80 % of the cooling time is advised to avoid delayed plastication and thermal stratification in the shot.
Mould temperature influences crystallisation rate and part dimensional stability. For unfilled injection moulding grades with densities near 0.940 g/cm³, mould temperatures between 20 °C and 50 °C are commonly used. Higher mould temperatures increase crystallinity and shrinkage but improve weld-line strength and reduce moulded-in stress. Lower mould temperatures shorten cycle time but may reduce surface gloss and increase warpage in asymmetric parts. Processors should characterise mould shrinkage for the specific tool using ISO 294-4; a single shrinkage value cannot cover variations in wall thickness, gate geometry, and flow orientation.
Moisture absorption in polyethylene is low, and pre-drying is not normally required. However, condensation on cold pellets stored at relative humidity above 60 % can introduce surface moisture that produces voids and streaks during injection. If surface moisture is suspected, drying for 2 h at 70 °C in a desiccant dryer is sufficient. Long-term storage should avoid direct sunlight and temperatures above 40 °C to minimise oxidation of the stabiliser package.
Table 1 summarises representative property values from the technical data sheet and related polyethylene test practice. The table does not replace batch-specific certificates of analysis.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.940 | g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 | 4.0 | g/10 min |
| Tensile stress at yield | ISO 527-2 | 19 | MPa |
| Tensile strain at break | ISO 527-2 | >700 | % |
| Tensile modulus | ISO 527-2 | 650 | MPa |
| Flexural modulus | ISO 178 | 700 | MPa |
| Charpy notched impact at 23 °C | ISO 179-1/1eA | 45 | kJ/m² |
| Charpy notched impact at −20 °C | ISO 179-1/1eA | 15 | kJ/m² |
| Vicat softening point, A/10 N | ISO 306 | 118 | °C |
| Brittleness temperature | ASTM D746 | <−70 | °C |
| ESCR, 100 % Igepal, 50 °C | ASTM D1693/A | >1000 | h |
Reported tensile and impact values are thickness-dependent and may shift with moulding conditions, gate geometry, and post-mould ageing. The Charpy values above are based on notched specimens prepared under ISO 179 from injection-moulded plaques; they should not be applied directly to parts with weld lines, surface defects, or severe flow-induced orientation.
Flexirene® MT 40 A is distinguished from low density polyethylene primarily by its linear architecture and higher density. High-pressure LDPE typically exhibits a lower tensile modulus, lower yield stress, and higher melt strength because of its long-chain branching. In processes such as blow moulding, the long-chain branching of LDPE is advantageous for parison stability, but the resulting parts generally show lower environmental stress crack resistance and lower stiffness than an LLDPE of 0.940 g/cm³ density. Against HDPE, the product has a lower density and lower crystallinity, which reduces stiffness but improves impact and stress-crack behaviour in many injection-moulded profiles.
Within the Flexirene range, the product differs from higher-flow injection grades by its melt mass-flow rate. A grade such as Flexirene MS 20 A is intended for fast-cycle, thin-wall injection where spiral flow is more important than long-duration ESCR. Flexirene® MT 40 A provides a lower melt index and therefore a higher molecular weight; this increases notched impact retention and improves resistance to slow crack growth in applications such as caps, closures, and industrial containers. However, the lower flowability requires higher injection pressure and may extend cycle time when wall thickness is below 1.0 mm.
Compared with rotational moulding grades in the same density region, the product is not optimised for low-shear, long-cycle sintering. Rotational moulding resins are typically supplied at a higher melt flow rate or with a different stabiliser package to withstand prolonged oven residence times without oxidative surface degradation. Using Flexirene® MT 40 A in rotational moulding would require longer oven cycles and may produce incomplete sintering if the peak internal air temperature is not raised above the crystalline melting range. Published data for this specific configuration is limited, so the product should not be substituted for a designated rotational moulding grade without trial evaluation.
Table 2 provides a qualitative comparative framework for positioning the product among adjacent polyethylene families. The table is not a specification and cannot capture differences arising from molecular weight distribution, additive package, or catalyst type.
| Polymer family | Typical density range | Typical melt flow range | Relative stiffness | Relative ESCR | Primary processing boundary |
|---|---|---|---|---|---|
| High-pressure LDPE | 0.915–0.930 g/cm³ | 0.5–20 g/10 min | Lower | Lower | Strong melt strength for blow and film |
| Flexirene® MT 40 A | 0.940 g/cm³ | 4.0 g/10 min | Intermediate | High | Injection moulding; limited thin-wall flow |
| HDPE injection grade | 0.950–0.960 g/cm³ | 2–20 g/10 min | Higher | Variable | Higher temperature and modulus capability |
| Rotational moulding LLDPE | 0.930–0.940 g/cm³ | 4–8 g/10 min | Intermediate | High | Low-shear sintering; long oven cycles |
The qualitative differences above must be confirmed with side-by-side moulding trials. Differences in additive packages, solid-state structure, and orientation created during injection can reverse the expected ranking of ESCR or impact in specific part geometries.
Applications selected for Flexirene® MT 40 A generally involve thick-wall or semi-structural injection-moulded parts in which impact resistance and environmental stress crack resistance carry greater weight than ultimate flow length. Weld lines are the dominant failure mode in such parts because they interrupt molecular entanglement across the flow front. With a 4.0 g/10 min melt index, the material retains beneficial molecular weight, but weld-line strength is still controlled by melt temperature, mould temperature, and gas venting. Increasing melt temperature within the 220 °C to 250 °C range improves weld-line consolidation by delaying solidification at the flow front. Raising mould temperature above 30 °C may provide additional time for interdiffusion, but it also lengthens cycle time and increases post-mould shrinkage.
For closures and container components subjected to stress cracking from detergents, oils, or alcohol-based formulations, the slow crack growth resistance of a 0.940 g/cm³ LLDPE can outperform many LDPE and high-flow LLDPE alternatives. The ESCR value above 1000 h under ASTM D1693/A provides a comparative laboratory indicator, but it does not guarantee service life in concentrated stress-cracking fluids or under high constant strain. Parts with sharp corners, thick-to-thin transitions, or internal insert stress should be evaluated under the specific chemical environment and load condition expected in service.
The product is not optimised for high-speed thin-wall packaging where mould-fill ratio and part weight reduction are primary process economics goals. When wall thickness falls below 1.0 mm, the injection pressure required to fill the cavity may exceed the capability of smaller hydraulic clamp systems. For example, a projected-area clamp force requirement of 3.0 kN/cm² to 5.0 kN/cm² is common for semi-crystalline injection grades, but the exact value varies with flow length, wall thickness, and gate size. Thin-wall closure designs should be simulated using pressure-volume-temperature data for the grade and verified with short-shot studies.
The polymer is used in industrial containers, caps, closures, and general injection-moulded housings where the combination of moderate stiffness, high notched impact, and resistance to environmental stress cracking is required. Specific application test programmes should include drop impact testing under ASTM D2463 or equivalent, top-load testing for closures, and stress-crack evaluation under the intended chemical service condition. Published data for this specific configuration in a defined part geometry is limited; performance claims must be established on the final moulded article rather than extrapolated from raw material data.
Polyethylene grades in the Flexirene family may be certified for food-contact applications under FDA 21 CFR 177.1520 and European Union Regulation 10/2011, but compliance is grade-specific and dependent on the additive package and the final migration test of the finished article. The converter must verify the grade-specific regulatory certificate before using Flexirene® MT 40 A in direct food-contact packaging. Overall migration testing under EN 1186 or specific migration limits under the relevant simulant are end-product obligations, not raw material properties.
The product is supplied with a thermal processing stabiliser package. It is not UV-stabilised for long-term outdoor exposure. Applications requiring weathering resistance must incorporate carbon black, a hindered amine light stabiliser package, or another appropriate UV protection system. Without such protection, surface embrittlement and gloss loss can occur within months of outdoor exposure. The product is not intended for medical implant applications, and no claim of ISO 10993 biocompatibility is made without direct evaluation.
Chemical incompatibilities should be assessed for any service environment involving strong oxidising acids, chlorinated solvents, or high-aromatic hydrocarbon streams. Polyethylene can swell or stress-crack in some hydrocarbons and chlorinated organic compounds. The product should not be compounded with pro-oxidant additives intended for degradable packaging unless a controlled oxidative breakdown is required, since the additive would compromise the stabiliser package and reduce the long-term performance of injection-moulded parts.
For storage, the product should be kept in a dry, enclosed area away from direct sunlight and strong oxidising chemicals. Under prolonged storage above 40 °C, the effectiveness of the thermal stabiliser may decline over time. Batch-to-batch variability in melt flow rate and density should be expected within the supplier’s specification window, and incoming quality control should include ISO 1133-1 melt flow rate and ISO 1183-1 density measurement before release for critical production campaigns.