Versalis Flexirene Ms 40 U Linear Low Density Polyethylene

Versalis Flexirene® MS 40 U Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® MS 40 U Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 288061
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.940 g/cm³
    Meltflowrate 190c 2 16kg 4.0 g/10 min
    Meltingpoint 125 °C
    Vicatsofteningtemperature 105 °C
    Shoredhardness 55
    Tensilestressatyield 15 MPa
    Tensilestressatbreak 20 MPa
    Elongationatbreak >800 %
    Flexuralmodulus 550 MPa
    Charpynotchedimpactstrength 23c 8 kJ/m²
    Thermalconductivity 0.33 W/m·K
    Waterabsorption <0.01 %
    Dielectricconstant 2.3
    Uvstabilization Yes

    As an accredited Versalis Flexirene® MS 40 U Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® MS 40 U Linear Low Density Polyethylene comes in 25 kg polyethylene bags, palletized for convenient transport and storage.
    Container Loading (20′ FCL) 20′ FCL: approx. 25 MT Versalis Flexirene® MS 40 U LLDPE in 25 kg bags, floor loaded.
    Shipping Versalis Flexirene® MS 40 U Linear Low Density Polyethylene is shipped as non-hazardous pellets, normally in 25 kg polyethylene bags or bulk octabins, palletized and stretch-wrapped. It requires clean, dry trucks or containers at ambient temperature, protected from moisture, sunlight, and contamination. No special dangerous-goods labeling is typically required.
    Storage Store Versalis Flexirene® MS 40 U LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and ignition sources. Keep bags or containers closed to prevent moisture and contamination. Avoid contact with strong oxidizing agents. Stack securely on pallets, use first-in, first-out rotation, and follow local regulations. Maintain good housekeeping and inspect for spills or damaged packaging.
    Shelf Life Store in a cool, dry, ventilated area away from direct sunlight; shelf life typically 12–24 months in unopened original packaging.
    Application of Versalis Flexirene® MS 40 U Linear Low Density Polyethylene

    Pulverised to a 35-mesh particle size distribution with a bulk density of 0.32–0.38 g/cm³, Versalis Flexirene® MS 40 U is charged into a three-arm carousel rotational moulding line at wall thicknesses of 5.0–12.0 mm for potable water tanks. The grade carries a density of 0.940 g/cm³ and a melt flow rate of 4.0 g/10 min under ISO 1133-1:2022, and its tensile modulus by ISO 527-2:2012 is 650 MPa, sufficient for vertical tank sidewalls without the high melt strength of 0.2–0.5 g/10 min rotomoulding grades. Compliance at the finished-article level relies on FDA 21 CFR 177.1520(c)3.1, NSF/ANSI/CAN 61 for potable water contact, AS/NZS 4766:2006 for polyethylene storage tanks, and EN 13575:2012 for rotationally moulded static thermoplastic tanks. The formulation is run at 100 wt% MS 40 U for first-generation tanks or at 70–85 wt% virgin resin blended with 15–30 wt% clean in-house regrind pulverised to the same 35-mesh profile; regrind above 30 wt% raises melt flow rate and lowers notched low-temperature impact because multiple heat cycles introduce chain scission. Carbon black masterbatch is added at 2.0–2.5 wt% with a 40% carbon black loading in LDPE carrier only when black colour is specified; pigment loading above 3.5 wt% is not recommended because agglomerates reduce impact at wall-thickness transitions. During production the oven set point is maintained at 280–300 °C, the biaxial rotation ratio is held at 4:1, and the peak internal air temperature reaches 200–210 °C before cooling begins. Forced-air cooling for 10–15 min followed by water mist at 2–4 K/min suppresses warpage at fitting bosses; cooling rates faster than 6 K/min introduce sink marks around threaded fittings. Terminal product types include 500 L to 20,000 L vertical water storage tanks, underground cisterns, septic tanks, and rainwater harvesting vessels. Environmental stress cracking resistance by ASTM D1693-15 condition B exceeds 1000 h; published data for ESCR under chlorinated potable water at 60 °C is limited.

    PropertyTest methodAcceptance range
    DensityISO 1183-1:20190.939–0.941 g/cm³
    Melt flow rateISO 1133-1:20223.8–4.2 g/10 min
    Tensile modulusISO 527-2:2012630–670 MPa
    ESCR, condition BASTM D1693-15>1000 h
    Notched Charpy impact at -20 °CISO 179-1/1eA≥20 kJ/m²

    What Limits Regrind Inclusion Rates in Agrochemical Rotomoulded Vessels?

    The critical constraint is oxidative resistance of the rotomoulded wall, not melt-flow parity. For aqueous crop protection formulations with pH between 4.0 and 9.0, the vessel wall is moulded from 70–80 wt% MS 40 U and 20–30 wt% in-house regrind of the same grade, pulverised to 35-mesh; for oxidising active ingredients such as hydrogen peroxide above 10 wt% or solvent-borne formulations, the addition ratio is locked at 100 wt% virgin resin because regrind brings peroxide-degraded chain segments and increases pinhole risk. The process uses a drop-arm shuttle rotational moulding machine with steel or cast-aluminium moulds; the oven set point is 285–305 °C and the peak internal air temperature is 195–205 °C. An internal air purge of 0.2–0.5 bar during cooling is introduced through the vent tube to limit sink marks around tank neck threads and outlet bosses. Compliance is governed by the UN Model Regulations when the rotomoulded vessel is certified as UN 1H1 or UN 3H1 transport packaging, and by AS/NZS 4766:2006 for static water tanks that are not UN-rated; chemical resistance testing is performed under ASTM D543-21 with the target liquid at 40 °C for 30 days, and the wall is rejected if mass gain exceeds 1.5% or visible cracking appears. Terminal finished products include crop sprayer reservoirs of 100 L to 1500 L, fertigation nurse tanks, chemical dosing tanks, and seed treatment mixing vessels. Operation above 40 °C continuous service for solvent-borne chemicals is outside the recommended boundary; published data for high-concentration bromine-based oxidising mixtures in MS 40 U is limited.

    When a double-wall rotomoulded slide panel is produced for outdoor playground equipment, the processing problem shifts from impact resistance to viscosity control during moulding of hollow sections with wall thickness variation from 4.0 mm to 10.0 mm. The formulation for this sector is 96–98 wt% MS 40 U and 2.0–4.0 wt% inorganic pigment masterbatch based on an LLDPE carrier with no cadmium, lead, or hexavalent chromium; additional hindered amine light stabiliser is normally unnecessary because the U grade carries UV stabilisation, but tropical installations above 1500 h QUV testing may use 0.1–0.3 wt% HALS masterbatch. The finished part must meet EN 1176-1:2017 for playground equipment, EN 71-3:2019 migration limits for accessible coloured surfaces, and RoHS Directive 2011/65/EU for restricted heavy metals. Production takes place on a carousel rotational moulding machine using CNC-machined aluminium moulds; the heating chamber is set at 280–310 °C, cycle time for an 8.0 mm average wall is 22–35 min, and cooling uses forced air at 8 m/s for the first 5 min followed by water mist at 0.5–1.0 L/min to set double-wall ribs without thermal shock. Low-temperature notched Charpy impact by ISO 179-1/1eA at -20 °C is the key incoming-resin release criterion, with a minimum value of 20 kJ/m² required for outdoor play structures. Terminal product types include slide segments, climbing panels, tunnel sections, benches, litter bins, and outdoor planters.

    Marine Buoy Foam-Filled Structures and Saltwater Crack Resistance

    Closed-cell polyurethane foam filling imposes a low exotherm boundary on MS 40 U shells because the polyethylene wall must remain dimensionally stable during foaming. The outer shell is rotomoulded at 100 wt% MS 40 U, with 0–2.0 wt% UV masterbatch permitted only if the buoy colour is not naturally supplied by the base resin; no regrind is added where floatation certification requires consistent shell density. The shell wall is moulded to 6.0–10.0 mm using a shuttle rotational moulding machine with biaxial rotation at a 3.5:1 ratio, oven set point 285–305 °C, and peak internal air temperature 200–210 °C. After cooling, a two-component rigid polyurethane foam with in-place density of 20–40 kg/m³ is injected through a 25 mm port; the exotherm must be kept below 120 °C to prevent localised shell softening. Saltwater crack resistance is assessed by ASTM D543-21 immersion in 3.5 wt% NaCl solution at 50 °C for 30 days, with no visible cracking permitted; UV weathering is validated under ISO 4892-3:2016 for 2000 h with a Delta E target below 3.0. Load points require through-bolted backing plates rather than moulded-in threaded inserts because point stress above 2 MPa accelerates environmental stress cracking in warm marine service. Terminal product types include navigational marker buoys, mussel floats, floating dock segments, and pontoon floats. Published data for the effect of strong barnacle-cleaning chemicals on MS 40 U is limited, so oxidative cleaning agents are not recommended.

    Thin-wall injection moulding of dunnage trays draws on the 4.0 g/10 min melt flow

    For thin-wall dunnage trays, a melt temperature window of 220–250 °C is established because the 4.0 g/10 min melt flow rate under ISO 1133-1:2022 reduces injection pressure compared with film-grade LLDPE of 0.8–1.0 g/10 min. The formulation is 80–90 wt% MS 40 U blended with 10–20 wt% LDPE having melt flow rate of 20 g/10 min to improve melt strength for large dunnage trays with wall sections below 2.0 mm; 1.0–2.0 wt% silicone-based mould release masterbatch is added to reduce cycle time and prevent gate sticking. Processing is carried out on an injection moulding machine with a three-zone screw of 18:1 L/D, shot capacity 1.5–3.0 kg, clamp force 150–250 t, injection speed 80–120 mm/s, holding pressure 40–60 MPa, and mould temperature 15–40 °C. Compliance for industrial logistics articles references FDA 21 CFR 177.1520 for olefin polymers where incidental food contact is possible, and ISO 8611-1:2021 for pallet and tray mechanical testing where load ratings are specified. Terminals include dunnage trays, collapsible bulk containers, tote bins, separation sheets, and conveyor-compatible pallet boxes. Warpage in flat trays is controlled by balanced gates and cooling time of 20–35 s; hot runners maintained above 250 °C can create local degradation, so temperature-limited hot runner systems are required.

    When Carbon Black Masterbatch Loading Reaches 3.0 wt%, Outdoor Crack Resistance Changes

    Dispersion of carbon black in the rotomoulded wall of water-filled traffic barriers becomes the primary quality variable because agglomerates above 50 µm act as crack initiation sites under repeated vehicle impact and freeze-thaw cycling. The barrier shell is moulded from 97–98 wt% MS 40 U with 2.0–3.0 wt% carbon black masterbatch at 45–50% carbon black in LDPE carrier; below 2.0 wt% the UV protection is insufficient for 5-year outdoor exposure in desert or high-altitude service, while above 3.0 wt% low-temperature impact decreases and surface pinholes increase. Traffic orange parts replace carbon black with 2.0 wt% inorganic/organic pigment masterbatch that must meet REACH and RoHS Directive 2011/65/EU heavy-metal restrictions. The production process uses a carousel rotational moulding machine with steel moulds for double-wall barriers, oven temperature 290–310 °C, peak internal air temperature 200–215 °C, and slow air cooling at 1–2 K/min to reduce fill-port thread shrinkage. Weathering is validated under ISO 4892-2:2013 cycle 1 for 1500 h, with tensile strength retention above 80% required. Terminal product types include water-filled road barriers, channeliser drums, speed humps, parking stops, and construction site barricades. Impact resistance after weathering is measured by ISO 179-1/1eU at -30 °C; published data for long-term fatigue under heavy-vehicle wheel load is limited, so barriers are positioned as static control devices rather than crash-rated systems.

    Free Quote

    Competitive Versalis Flexirene® MS 40 U Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® MS 40 U Linear Low Density Polyethylene is a UV-stabilised ethylene copolymer supplied in pellet form. The grade is positioned for rotationally moulded parts that require higher stiffness than conventional lower-density LLDPE of 0.918 g/cm³ nominal density while retaining ductile failure under multiaxial impact. The following data are typical manufacturer-reported values, not specification limits, and lot-to-lot variation should be verified against the current technical bulletin.

    Product Identification and Material Designation

    The base resin is classified as a linear low density polyethylene with a nominal density of 0.940 g/cm³ determined in accordance with ISO 1183-1. The melt mass-flow rate is 4.0 g/10 min when measured at 190 °C under 2.16 kg in accordance with ISO 1133-1. The designator MS 40 U identifies the density class, melt-flow range, and ultraviolet stabiliser package; exact additive loading is lot-specific and should be confirmed for prolonged outdoor service. The grade is typically supplied in natural or black variants depending on regional availability.

    PropertyTest methodTypical value
    Melt mass-flow rateISO 1133-1:2022, 190 °C, 2.16 kg4.0 g/10 min
    DensityISO 1183-1:20190.940 g/cm³
    Tensile stress at yieldISO 527-2:2012, type 1A, 50 mm/min18 MPa
    Tensile strain at breakISO 527-2:2012, type 1A>700%
    Flexural modulusISO 178:2019780 MPa
    Charpy notched impact strength, 23 °CISO 179-1:2010/1eANo break reported
    Vicat softening temperature, A50ISO 306:2022121 °C
    Shore hardness, DISO 868:200362
    Brittleness temperatureISO 974:2000−70 °C

    What Limits the Processing Window in Rotational Moulding?

    The practical oven temperature window is constrained by the need to sinter all powder particles into a void-free melt while avoiding thermal oxidative degradation. On single-carousel machines with 3.0 m offset arms, oven set temperatures between 280 °C and 300 °C are typical for this density class. Peak internal air temperature should reach 180–200 °C; below 170 °C, incomplete densification can leave pinholes and weld-line porosity. Above 220 °C, the antioxidant package may be consumed and yellowness index can increase.

    Mould rotation ratio is commonly maintained at 4:1, with primary-axis speed in the range 4–6 min⁻¹ and secondary-axis speed at 12–18 min⁻¹. Cooling rate affects wall-thickness uniformity and post-mould shrinkage. Forced-air cooling to 80 °C before demoulding reduces differential shrinkage; water fog or full water quench may reduce cycle time but can increase warpage in thick-walled parts. Equilibrium moisture absorption of the resin is below 0.01% by weight under ISO 62, so desiccant drying is not normally required. Surface condensation at relative humidity above 60% should be removed by warm-air circulation at 40 °C before processing.

    For injection moulding trials on machines with clamp force between 800 kN and 2500 kN, melt temperature is typically set between 200 °C and 240 °C, with mould temperature held at 20–40 °C. Screw back-pressure should be kept low because the 4.0 g/10 min melt flow rate permits rapid filling without excessive shear heating.

    Stiffness–Impact Balance Under Multi-Axial Loading

    The density of 0.940 g/cm³ places this product between conventional lower-density LLDPE film resins and high-density polyethylene. The flexural modulus of 780 MPa under ISO 178 is higher than that of a typical 0.918 g/cm³ LLDPE, which commonly falls below 350 MPa. This stiffness increase reduces wall deflection in upright tanks and improves dimensional stability in flat-panel structures. The trade-off is a reduction in environmental stress-crack resistance relative to lower-density rotomoulding grades under aggressive detergent or fatty-acid exposure.

    Multiaxial impact resistance in rotationally moulded parts depends less on the resin alone than on moulded-in stress, wall-thickness variation, cooling history, and internal air temperature at the end of the heating phase. Charpy notched impact testing at 23 °C reports no break, indicating ductile behaviour. For low-temperature service, notched Charpy data at −30 °C should be obtained from the supplier because published data for this specific configuration is limited. Polyethylene tanks can be assessed for long-term service fitness under ASTM D1998.

    When Narrow Molecular Weight Distribution Replaces Conventional LLDPE

    If narrow molecular weight distribution is present from metallocene catalysis, the melt rheology shifts relative to conventional Ziegler-Natta LLDPE of equivalent density and melt flow rate. The shear viscosity at high shear may be lower, mould filling may be more uniform, and the solidification transition may be sharper. This can reduce warpage in thin-wall regions but can also narrow the processing window because the plateau between complete sintering and degradation is less forgiving.

    Compared with conventional LLDPE film grades, the higher density of this material lowers permeation coefficients because increased crystallinity reduces the amorphous fraction available for gas transport. Oxygen transmission rate should be confirmed by ASTM D3985 or ISO 15105-2 on the actual moulded wall thickness. Direct substitution of this product into a Ziegler-Natta tooling design should be supported by capillary rheometry under ISO 11443; published data for this specific comparative configuration is limited.

    Batch-to-batch variation in the UV stabiliser system can affect colour retention and surface chalking. For outdoor articles with multi-year service life, lot-specific additive certificates should be retained. The table below summarises the principal regulatory areas that require confirmation before commercial use.

    Regulatory areaRequirementStatus
    EU Regulation (EU) No 10/2011Food-contact plastics, specific migration limits, overall migration ≤ 10 mg/dm²Confirm with manufacturer for target food simulant and time–temperature condition
    FDA 21 CFR 177.1520Olefin polymer requirements for food-contact articlesFinal article compliance must be assessed because processing aids and mould release agents can alter status
    REACH (EU) 1907/2006SVHC content < 0.1% w/wSupplier statement valid at date of release
    RoHS Directive 2011/65/EULead, cadmium, mercury, chromium VI, PBB, PBDE thresholdsRaw pellet not expected above limits

    Chemical Resistance Data Are Required Before Contact with Oxidizing Fertilizers

    For agricultural storage tanks, liquid fertilizers containing surfactant adjuvants or fatty acids can accelerate environmental stress cracking. The grade should be tested under the specific chemical concentration and service temperature using ISO 22088-3 or ASTM D1693. Continuous exposure to strong oxidizing acids, aromatic hydrocarbons, or ketones at elevated temperature should be avoided because these media can swell the amorphous phase and shorten service life.

    Outdoor weathering performance depends on UV irradiance, ambient temperature, wall thickness, and surface pigmentation. The ultraviolet stabiliser package is intended for general outdoor exposure, but no single stabiliser system is effective in all climates. Accelerated weathering in accordance with ISO 4892-2 should be correlated with natural weathering under ISO 877 before extended service life is predicted. Food-contact compliance must be confirmed on the finished article because mould release agents, regrind content, and processing temperature can change the regulatory outcome.

    Top