| HS Code | 554652 |
| Product Name | Versalis Flexirene® MS 40 A Linear Low Density Polyethylene |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer Type | Butene-1 |
| Density | 0.925 g/cm³ (typical) |
| Melt Flow Rate 190c 2 16kg | 40 g/10 min |
| Melting Temperature | 123 °C |
| Vicat Softening Temperature | 94 °C |
| Crystallinity | 45–50 % |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 12 MPa |
| Elongation At Break | >800 % |
| Flexural Modulus | 260 MPa |
| Shore D Hardness | 50 |
| Notched Izod Impact Strength 23c | 60 kJ/m² |
| Brittleness Temperature | < -70 °C |
| Water Absorption | < 0.01 % |
| Mold Shrinkage | 1.5–2.5 % |
| Thermal Conductivity | 0.33 W/m·K |
| Volume Resistivity | >10^15 Ω·cm |
| Dielectric Constant 1khz | 2.3 |
As an accredited Versalis Flexirene® MS 40 A Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® MS 40 A Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags on 1,000 kg pallets. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags on pallets, 50 bags/pallet, 20 pallets, 25 MT net for Versalis Flexirene MS 40 A LLDPE. |
| Shipping | Versalis Flexirene® MS 40 A is typically shipped as non-hazardous LLDPE pellets in 25 kg bags, jumbo bags, octabins, or bulk containers. Transport in clean, dry vehicles at ambient temperature, protecting from moisture, heat, and UV. No ADR/IMDG/IATA dangerous goods classification is required. Keep away from ignition sources and contamination. |
| Storage | Store Versalis Flexirene® MS 40 A LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, and ignition sources. Keep original bags or containers sealed, palletized, and off the floor. Protect from moisture, dust, and contamination. Separate from oxidizers, acids, and strong chemicals. Avoid prolonged high temperatures. Maintain good housekeeping, use first-in, first-out stock rotation, and follow the SDS. |
| Shelf Life | Store in original packaging, cool, dry, ventilated conditions, away from direct sunlight; shelf life approximately 24 months from production date. |
Rotational moulding of medium-wall agricultural and industrial tanks constitutes a processing route in which the 4.0 g/10 min MFR at 190 °C/2.16 kg per ISO 1133-1 and the 0.940 g/cm³ density per ISO 1183-1 define the sintering curve, air-pocket elimination, and final environmental stress-cracking resistance. The polymer is dry-blended rather than melt-compounded before charging, and the powder particle size distribution is the first process variable that separates acceptable tanks from rejected batches: a typical specification requires ≥95 wt% passing through a 35 mesh screen, with less than 5 wt% retained on a 50 mesh screen and a fines content below 10 wt% passing through a 70 mesh screen. An outdoor-grade formulation for a 5–10 mm wall tank contains 100 parts by weight of Flexirene MS 40 A, 0.25–0.50 wt% of a hindered amine light stabilizer, 0.15–0.40 wt% of a benzotriazole UV absorber, and 0.05–0.15 wt% of a processing antioxidant; pigment concentrates are limited to 0.5–2.0 wt% and must use an LLDPE carrier with a melt flow rate within ±1.0 g/10 min of the base resin to avoid localized gel formation. In food-contact potable-water tanks, the additive inventory is restricted to substances authorized in Commission Regulation (EU) No 10/2011 Annex I and the polymer itself must meet FDA 21 CFR 177.1520, with overall migration tested to EN 1186-1:2002 at a limit of 10 mg/dm² in 10% ethanol and 3% acetic acid simulants.
Industrial rotomoulders using this grade run biaxial machines with arm ratios of 4:1 or 5:1 and a heating programme that is controlled primarily by internal air temperature. The mould enters a forced-air oven at 280–310 °C; the oven setpoint alone is not a reliable control parameter, because batch mass, wall thickness, and mould thermal conductivity shift the time-to-peak internal air temperature. The critical densification window is 195–210 °C internal air temperature: below 190 °C the powder remains incompletely fused and the inner wall exhibits a brittle, granular skin detectable by cross-polarized microscopy, while above 215 °C oxidative yellowing appears and notched impact strength measured to ISO 179-1/1eA drops. Cooling must be staged from forced air to water mist at 85 °C, then to water spray at 50 °C; demoulding below 45 °C prevents post-mould distortion in flat sidewalls. Terminal articles include agricultural sprayer tanks, seed-hopper liners, potable-water storage tanks, playground panels, and industrial pallet boxes.
| Rotational moulding control parameter | Industrial range | Out-of-range failure mode | Verification method |
|---|---|---|---|
| Powder fraction passing 35 mesh | ≥95 wt% | Inner-wall pinholes and unmelted particles | Mechanical sieve stack per ISO 2591-1 |
| Peak internal air temperature | 195–210 °C | Below: brittle inner skin; above: oxidative yellowing | IAT probe and ISO 179-1/1eA |
| Cool-down air-to-water transition | 85 °C to 50 °C | Warpage and irregular wall shrinkage | Dimension audit and surface flatness gauge |
| Demoulding temperature | ≤45 °C | Post-mould distortion and stress whitening | Infrared surface thermometry |
At wall thicknesses between 1.2 mm and 3.0 mm, the resin is injection moulded on hydraulic or toggle presses with clamp force ratings of 800–3000 kN and general-purpose polyolefin screws with L/D ratios of 20:1–24:1. The cylinder profile is set from 190 °C at the feed throat to 230 °C at the nozzle; the melt temperature measured by a needle pyrometer should remain between 205 °C and 225 °C, because lower temperatures increase melt viscosity and create flow hesitation at the hinge area of a storage lid, while higher temperatures accelerate odour formation in food-contact articles. A standard formula uses 100 parts by weight of Flexirene MS 40 A, 1.5–3.0 wt% of a polyolefin-based colour masterbatch, and if frozen-layer build-up is observed on the screw, 0.05–0.10 wt% of a fluoropolymer processing aid; regrind from the same production line is allowed at 20 wt% maximum only when the regrind is dry and free of mixed resin contamination.
The holding-pressure profile is critical because LLDPE solidifies gradually and the gate seal time must be verified by weight-stability trials; a typical holding pressure of 35–55 MPa hydraulic is applied for 4–8 s, with back pressure at 0.5–1.0 MPa. Mould temperature is maintained at 15–40 °C with turbulent water channels, and cooling is continued until the part reaches ≤55 °C at ejection. Multiple ejection strokes may be required because the flexible part can adhere to polished cores; air blow with 0.4–0.6 MPa is used to release large flat surfaces. Compliance includes Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520; overall migration is tested by EN 1186-1:2002 with a limit of 10 mg/dm², and sensory migration is assessed by EN 1622. Terminal articles include reusable storage boxes, food containers, thin-wall lids, clips, and toy components.
| Regulation/standard | Relevant clause | Requirement or limit |
|---|---|---|
| Commission Regulation (EU) No 10/2011 | Annex I, Article 12 | Only listed monomers and additives; overall migration limit 10 mg/dm² |
| FDA 21 CFR | 177.1520 | Olefin polymers may contact food subject to extractables limits in paragraph (c) |
| REACH Regulation (EC) No 1907/2006 | Article 33, Annex XVII | SVHC communication; restrictions on listed substances |
| RoHS 2011/65/EU | Annex II | Pb, Hg, Cd, Cr(VI), PBB, PBDE restrictions |
The use of Flexirene MS 40 A as an impact modifier in injection-moulded PP compounds is governed by the modulus loss in the final part rather than by the melt flow of the LLDPE. In heterophasic PP formulations, the resin is compounded at 10–30 wt% into a 12 g/10 min PP homopolymer to raise Charpy notched impact strength measured to ISO 179-1/1eA; the actual improvement depends on the base PP, but the LLDPE contributes through its 0.940 g/cm³ density and comonomer content, which lower the brittle-to-ductile transition and reduce the sharp notch sensitivity of the PP. The blend is produced on a co-rotating twin-screw extruder with an L/D of 40:1, barrel profile 190–230 °C, screw speed 300–450 rpm, and a die-face pelletizer; the LLDPE is fed at the main throat to maximize dispersion, while the PP is also fed at the main throat.
The addition ratio is limited by the flexural modulus loss and surface streaking. At loadings above 30 wt%, the flexural modulus measured to ISO 178:2019 commonly falls below 800 MPa for appliance housings, and the compound begins to show weld-line weakness and scratch whitening. If the compound contains recycled PP with a melt flow below 5 g/10 min, the LLDPE fraction must be kept in the 10–15 wt% range to maintain the final MFR above 8 g/10 min for thin-wall injection. Automotive interior components are subject to REACH Regulation (EC) No 1907/2006 Article 33 and VOC limits by VDA 277; appliance components follow RoHS 2011/65/EU and EN 60335-1. Terminal articles are automotive interior pillar trim, appliance housings, and distribution crates.
Colour and additive masterbatch production uses the resin as a carrier phase at 20–60 wt% of the masterbatch formulation, with pigments at 20–50 wt% and a wax dispersant at 5–15 wt%. The ingredients are compounded on a co-rotating twin-screw extruder with segmented screws and L/D 36:1–44:1, using a melt temperature of 190–220 °C and a die-face pelletizer; the carrier fraction must be matched to the target moulding resin, so that a letdown ratio of 25:1 to 50:1 does not introduce a separate melt phase. When the masterbatch is intended for food-contact packaging, the pigment and carrier components must comply with Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520; for technical articles, REACH Regulation (EC) No 1907/2006 and RoHS 2011/65/EU apply. Terminal forms are pelletized colour concentrates and additive masterbatches for injection moulded and rotationally moulded articles.
Small-volume extrusion blow moulding of collapsible dispensing bottles and laboratory wash-bottle liners uses the resin in a monolayer structure with wall thickness 0.8–1.5 mm. The formulation is 100 parts by weight Flexirene MS 40 A plus 1.0–2.0 wt% of a silicone-containing slip masterbatch to allow the bottle to recover without stress whitening at the crease. The blow moulding extruder uses a 20:1–24:1 L/D screw and a temperature profile from 180 °C at the feed zone to 215 °C at the die; the die gap is set at 0.8–1.2 mm and the parison is inflated at 0.3–0.6 MPa. The pinch-off weld is the primary failure site, and its integrity is verified by drop testing to ASTM D2463-15. For food-contact dispensers, migration testing follows Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520; for general technical bottles, REACH and RoHS 2011/65/EU apply. Terminal products include collapsible dispensing bottles, bellows containers, and low-pressure air ducts.
Flexible snap-fit closures and dispensing spouts are injection moulded with the resin at 100 parts by weight, with colorant at 1.0–2.5 wt%, under melt temperatures 200–225 °C and mould temperatures 10–25 °C to achieve a tight plug seal without cracking. The closure wall at the tamper-evident band is 0.8–1.2 mm; stress-crack resistance is measured to ASTM D1693-15 condition B, and finished closures undergo torque retention tests per ASTM D2063-12. Compliance includes Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 for food-contact closures; technical closures require REACH Regulation (EC) No 1907/2006 and RoHS 2011/65/EU. Terminal products are snap-fit lids, dispensing spouts, and tamper-evident caps for detergent, agrochemical, and food containers.
Competitive Versalis Flexirene® MS 40 A Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene MS 40 A is a linear low-density polyethylene injection-moulding grade supplied in pellet form. The producer’s published technical data list a melt mass-flow rate of 4.0 g/10 min when tested at 190 °C under 2.16 kg load according to ISO 1133-1:2022, and a density of 0.940 g/cm³ according to ISO 1183-1. Although the density places the material at the upper boundary of the conventional LLDPE range, the producer’s product-family designation remains linear low-density polyethylene. The grade is additivated with an antioxidant package and is positioned for short-cycle injection-moulded articles in which processability, rigidity, and surface hardness are combined.
| Property | Test method | Typical value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 4.0 g/10 min |
| Density | ISO 1183-1 | 0.940 g/cm³ |
| Tensile modulus, secant 1 mm/min | ISO 527-2 | 850 MPa |
| Tensile stress at yield | ISO 527-2 | 19 MPa |
| Tensile strain at break | ISO 527-2 | >700% |
| Shore D hardness | ISO 868 | 62 |
| Vicat softening temperature, A10 | ISO 306/A10 | 121 °C |
| Brittleness temperature | ASTM D746 | −70 °C |
| Melting temperature | ISO 3146 | 126 °C |
These values are typical values and not release limits; the certificate of analysis for each production lot carries the normative values against the applicable specifications. The density of 0.940 g/cm³ is higher than that of typical film-grade LLDPE, which commonly lies between 0.918 g/cm³ and 0.925 g/cm³. The density difference, rather than the melt-flow difference alone, determines the stiffness, hardness, and permeability characteristics in moulded parts.
Surface moisture from condensate on cold pellets is a frequent source of splay, silver streaks, and dimensional variability on production-scale reciprocating-screw injection moulding machines. The producer’s technical guidance for LLDPE injection-moulding grades in the 4.0 g/10 min melt-flow class does not impose mandatory drying as a release condition; however, plants receiving bulk containers in winter or in coastal warehouses with relative humidity above 60% should not transfer cold pellets directly into a heated hopper. If condensation is visible, pre-drying at 80 °C for 1–2 h in a desiccant or hot-air dryer with a dew point below −20 °C is sufficient to remove surface water. Feed-throat venting must remain unobstructed to prevent moisture vapour from returning into the melt stream.
On a machine with screw L/D ratio between 20:1 and 25:1 and compression ratio near 2.5:1, a melt cushion of 3–6 mm is normally maintained to prevent nozzle starvation and short-shot variation. Barrel temperature profiles are set between 190 °C and 230 °C, with the nozzle between 210 °C and 220 °C. Melt temperatures above 250 °C or residence times over 15 min can promote oxidative chain scission, yellowing, and loss of impact resistance. Mould temperatures from 15 °C to 60 °C control crystallisation rate and shrinkage; lower mould temperatures shorten cycle time but raise orientation and post-mould shrinkage.
In thin-wall articles with nominal wall thickness below 1.2 mm, the melt-flow rate of 4.0 g/10 min reduces injection pressure and permits filling of multi-cavity cold-runner tools at short screw-forward times. Shear-thinning becomes significant at channel shear rates above 1000 s⁻¹, allowing practical melt temperatures in the 190–230 °C range without resorting to excessive barrel temperatures. However, low melt cushion and high injection speed can generate jetting in edge-gated cavities. A valve-gated hot runner or a tab gate with land length below 1 mm is preferred to reduce free-jet turbulence and surface flow marks.
Mechanical performance in service is governed by density-driven stiffness and the linear polyethylene backbone. Tensile yield stress of 19 MPa and tensile modulus near 850 MPa support rigid containers, closures, and general-purpose injection-moulded articles. Shore D hardness of 62 contributes to resistance to dry-surface handling damage. The −70 °C brittleness temperature under ASTM D746 indicates that the material retains low-temperature ductility under moderate strain-rate conditions, but continuous load-bearing applications at sub-zero temperatures require verification by ISO 8256 or ISO 6603-2 impact testing. Environmental stress cracking resistance is lower than that of lower-density, fractional-melt LLDPE; any application exposed to surfactants, mineral oil, or aggressive cleaning formulations must be qualified using ASTM D1693 or a full-scale container test. Published data for this specific ESCR configuration is limited, so lot-to-lot validation is required.
Bulk silo storage and handling should maintain pellet temperature above the dew point of ambient air to avoid surface condensation that later appears as splay or screw slip. Material transferred from outdoor silos at locations with day-night temperature swings above 10 °C should be allowed to equalise for 12–24 h before process hopper loading. If the pellet surface is warmer than the surrounding air, condensation may not occur on the pellet but can occur on metal hopper surfaces and transport lines; stainless-steel hopper liners and feed-throat magnets are common interventions against rust and metallic contamination.
Regulatory data for unreinforced polyolefin pellets in this class typically indicate non-classification under Regulation (EC) No 1272/2008, provided the material is not reduced to respirable dust. In food-contact applications, the finished article must satisfy EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 olefin polymer requirements; migration testing must reflect the actual food simulants and worst-case temperature. Because the grade is supplied as a pellet raw material, the final article manufacturer holds the obligation to verify global migration and specific migration of any non-polymeric components. Electrical and electronic applications under Directive 2011/65/EU should not rely only on the polymer grade name; supplier declarations for the exact batch and any masterbatch added are required.
| Regulatory area | Reference | Verification requirement |
|---|---|---|
| EU REACH | Regulation (EC) No 1907/2006 | Confirm monomer and additive registration; SVHC content in article below 0.1% w/w per batch declaration |
| EU CLP | Regulation (EC) No 1272/2008 | Supplier safety data sheet confirmation; typical unreinforced polyolefin pellets are not CLP-classified |
| RoHS | Directive 2011/65/EU | Not applicable to non-electrical raw material; batch declarations for Pb, Cd, Hg, Cr(VI), PBB, PBDE required for EEE |
| EU food contact | Regulation (EU) No 10/2011 | Migration testing on final article with intended food simulants |
| US food contact | FDA 21 CFR 177.1520 | Verification against olefin polymer conditions of use |
| Workplace safety | Site exposure assessment | Avoid dust accumulation; thermal processing above 250 °C generates degradation vapours |
At the converter, the main operational boundary is not chemical incompatibility with other polyolefins but contamination by PVC, PET, or acetal residues in hot-runner systems. These resins degrade at different temperature setpoints and can generate carbonised deposits that block hot-runner nozzles. If a material change is performed from a higher-temperature resin, purging with a low-MFR polyolefin at 180–200 °C before introducing this grade is recommended. Re-pelletised scrap from the same production lot can be blended up to 20 wt% in closed-loop operations, but only if the granulate is dust-free and generated from unpigmented, non-crosslinked feedstock. Higher recycled content requires mechanical property reassessment according to ISO 527-2 and ISO 1133-1.
A direct substitution of this grade for a film-extrusion LLDPE is not appropriate despite the shared LLDPE backbone. Film grades in the 0.918–0.925 g/cm³ density range and 1.0 g/10 min MFR class are designed for bubble stability, high tear resistance, and controlled seal initiation, whereas this product is optimised for short-cycle injection moulding. In a cold-runner mould, the 4.0 g/10 min melt-flow rate reduces flow-length versus pressure requirements and permits the use of lower clamping force; the same property weakens melt extensibility and makes the product unsuitable for blown-film bubble processing.
Compared with high-pressure LDPE at similar melt-flow index, the higher density and linear backbone of Flexirene MS 40 A produce higher tensile modulus and hardness, but lower clarity and a different shear-thinning envelope. This shifts application selection toward moulded items where stiffness and cycle time are dominant, and away from applications requiring glass-like clarity or high elongational viscosity. The producer’s product line also includes lower-flow Flexirene grades with different density values. The relevant difference is not only the 4.0 g/10 min MFR but also the 0.940 g/cm³ density, which creates a stiffer, less flexible part than a 0.918 g/cm³ LLDPE at equivalent wall thickness.
Operational boundaries and incompatibilities include melt temperatures above 250 °C, extended residence times beyond 15 min, and contamination with high-melting resins that impose incompatible heating profiles. Where this material is processed on machines with long barrels above 25:1 L/D, barrel residence time must be monitored because the combination of a relatively high melt-flow rate and long screw flights can promote early melt formation and screw slip. Feed-throat temperature should be held at 30–50 °C to maintain pellet hardness and prevent premature melting in the feed zone. For ultraviolet-exposed parts, carbon black loading or a suitable UV stabilizer masterbatch should be selected according to ISO 4892-2 testing; unpigmented resin is not a long-term outdoor material without additional stabilisation.