| HS Code | 563616 |
| Density | 0.926 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 250 MPa |
| Shore D Hardness | 54 |
| Dart Drop Impact Strength | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 14 % |
| Gloss 45 | 50 |
| Coefficient Of Friction | 0.2 |
| Water Absorption | <0.01 % |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >10^16 ohm·cm |
| Thermal Conductivity | 0.33 W/m·K |
| Specific Heat | 2.3 kJ/kg·K |
| Linear Thermal Expansion | 1.5E-4 /°C |
| Brittleness Temperature | < -70 °C |
As an accredited Versalis Flexirene® MS 26 A Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® MS 26 A Linear Low Density Polyethylene is packed in 25 kg polyethylene bags on pallets. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Versalis Flexirene® MS 26 A LLDPE, 25 kg bags, typically 22 MT per 20-foot FCL container. |
| Shipping | Versalis Flexirene® MS 26 A Linear Low Density Polyethylene is shipped as solid pellets in 25 kg PE bags or 1000 kg octabins, palletized and stretch-wrapped. It is typically non-hazardous, not UN-regulated, and should be kept dry, clean, and away from excessive heat in covered trucks or containers. |
| Storage | Store Versalis Flexirene® MS 26 A in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use clean handling equipment, follow first-in/first-out rotation, and comply with local regulations. Improper storage may affect product quality. |
| Shelf Life | Typically, 24 months from production when stored in original, unopened packaging under dry, cool conditions, away from direct sunlight. |
With a nominal melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load and a nominal density of 0.926 g/cm³ per ISO 1183-1:2019, the grade is used as a core resin in three-layer agricultural silage film. The line is equipped with a 30:1 L/D barrier screw and internal bubble cooling; EVA skins at 12–18 wt% vinyl acetate are metered at 15–30 wt% of total throughput, while the LLDPE core carries 70–85 wt% of the film structure. Die gap is held at 1.8–2.2 mm, blow-up ratio is set at 2.4:1–2.8:1, frost line height is maintained at 650–850 mm, and melt temperature is kept at 190–210 °C. Slip and anti-block performance is introduced through a 5–8 wt% masterbatch containing 800–1500 ppm erucamide and 2500–4000 ppm synthetic silica in the final film. Long-term ultraviolet stabilisation uses 0.20–0.50 wt% polymeric HALS and 0.05–0.12 wt% phenolic antioxidant in the core layer. The finished film is tested for dart impact by ASTM D1709, tear propagation by ISO 6383-2, and tensile properties by ISO 527-3. Agricultural silage covers and bale wraps fall under EN 13207:2001 mechanical durability requirements rather than the specific migration limits of EU Regulation 10/2011. Terminal articles produced on this line are round bale film, clamp cover sheets, and silage bags for forage preservation.
In cast pallet wrap conversion at 12–23 µm thickness, the grade is dry-blended with 5–20 wt% of a low-melt-index LDPE or a metallocene-catalysed plastomer to widen the draw resonance window. The main extruder uses a 75–120 mm single screw with 30:1 L/D, a feed zone at 170–190 °C, a transition zone at 190–210 °C, and a die temperature of 230–245 °C. The melt curtain is pinned to a matte or embossed chill roll at 18–25 °C with an air gap of 120–180 mm; edge bead trimming is maintained at 10–15 mm per side to avoid thick-edge tear. Cling is generated by 1.5–3.0 wt% polyisobutylene masterbatch, and unwind force is verified by ASTM D5458-18. Puncture resistance is measured by ASTM D5748, elongation at break by ISO 527-3, and tear propagation by ASTM D1922. The stable draw ratio is not a single number; it is governed by air-gap cooling rate, melt elongation viscosity, and plastomer addition. Edge tear begins at the outer deckle section before draw resonance occurs, so line operators adjust chill-roll speed and air-knife pressure simultaneously. When direct food contact is involved, the layer must comply with FDA 21 CFR 177.1520 olefin polymer limits and EU Regulation 10/2011 overall migration of 10 mg/dm². Terminal products are machine rolls, hand rolls, and pre-stretch rolls for pallet unitization at 180–250% elongation.
Extrusion coating of paperboard with this LLDPE grade is run at 300–320 °C melt temperature to reduce melt viscosity and promote wicking into the board surface. The extruder is a 90 mm single screw with 30:1 L/D, a screen pack of 60/80/100 mesh, and a coat-hanger die with a 0.5–0.8 mm lip gap. Coating weight is controlled at 12–25 g/m² by adjusting line speed from 150–400 m/min; the die-to-nip distance is kept between 150–250 mm to limit neck-in and oxidation. A chill roll with 0.8–2.0 µm Ra surface finish and 15–25 °C coolant temperature sets coating gloss and release. Adhesion to the paperboard is established by a coextruded EAA or EMA tie layer at 2–4 g/m²; peel strength is measured by ASTM D1876 T-peel testing. Heat seal strength of the converted structure is checked by ASTM F88, and pinholing is assessed by ASTM D3078 vacuum leak testing. In addition, 10–30 wt% LDPE is blended with the LLDPE to reduce neck-in and smoke generation during high-speed coating while maintaining low-temperature seal performance. Food-contact compliance for the finished carton includes FDA 21 CFR 176.170 for paper and paperboard in contact with aqueous and fatty food, FDA 21 CFR 177.1520 for the olefin polymer layer, and EU Regulation 10/2011 with overall migration limits of 10 mg/dm². Terminal products are gable-top cartons, paper cups, and coated board for frozen food packaging.
Compounding of halogen-free flame-retardant sheathing compound uses the grade as the polyolefin matrix at 35–45 wt% loading. Magnesium hydroxide is side-fed into a co-rotating twin-screw extruder with 40:1 L/D and 58 mm screw diameter at 55–65 wt% total filler. Barrel temperatures are held between 150 °C and 190 °C to avoid gel formation and premature consumption of the antioxidant package; vacuum venting at -0.06 MPa to -0.08 MPa removes moisture and low-molecular-weight volatiles. A vinyl silane coupling agent is metered at 0.5–1.5 wt% on the filler to improve tensile elongation and reduce water uptake. The compound is extruded through a two-strand die, water-bath cooled, and pelletised; final sheathing is applied on a 24:1 L/D single-screw cable line with a compression screw and gear pump before the crosshead. Fire performance of the final cable is tested by IEC 60332-1-2 for flame spread, IEC 61034-2 for smoke density, and ISO 4589-2 for limiting oxygen index. Oxidative induction time is monitored at 200 °C by ASTM D3895 to verify thermal stability of the sheathing compound. Regulatory compliance under RoHS Directive 2011/65/EU is confirmed by X-ray fluorescence screening for lead, mercury, cadmium, hexavalent chromium, and PBDE/PBB flame retardants. Construction product cables must meet CPR Regulation (EU) No 305/2011 and the associated hEN EN 50575:2014. Terminal products are conduit sheathing, tray cable jackets, and low-smoke control cable outer layers.
Three-layer heavy-duty sack film is produced with a 70 wt% LLDPE and 30 wt% high-molecular-weight HDPE core blend, while the skins are LDPE or EVA to preserve heat seal strength and surface gloss. The HDPE component has a density of 0.947–0.952 g/cm³ and a melt mass-flow rate of 0.05–0.10 g/10 min. The line uses a 90 mm single-screw extruder with 30:1 L/D, a 2.2–2.6 mm die gap, a blow-up ratio of 2.0:1–2.5:1, and a frost line height of 700–900 mm. Melt temperature is maintained at 195–215 °C. Adding the LLDPE grade to the core layer raises dart impact and machine-direction Elmendorf tear compared with an all-HDPE core; drop impact is validated by ASTM D1709, tear resistance by ISO 6383-2, and tensile yield by ISO 527-3. The film is printed with flexographic inks and converted into FIBC liners, construction rubble sacks, and chemical packaging for granular solids. When the sacks are used for dangerous goods, the empty packaging drop test is carried out according to UN 21.1 and ADR 6.1.5 conditions. Food-contact sacks additionally require EU Regulation 10/2011 or FDA 21 CFR 177.1520 depending on the export market.
Film-grade masterbatch producers use the grade as a pellet diluent in carbon black and TiO₂ masterbatches for subsequent letdown ratios of 5–10% in agricultural and packaging films. The 1.0 g/10 min melt flow rate creates higher shear stress in co-rotating twin-screw lines than a fractional-MI resin, so pigment loadings are limited to 40–60 wt% unless processing oil is added at 0.2–0.5 wt% to wet the pigment surface and reduce screw slippage. The screw configuration uses high-conveying elements and limited kneading blocks in the melt zone to avoid thermal degradation. Batch-to-batch variance in pellet colour is controlled by measuring filter pressure value and melt temperature at the die plate; melt temperature is kept below 210 °C for carbon black and below 180 °C for heat-sensitive organic pigments. Dispersion is assessed by a 20 µm pressure-rise test or a film-screen test using a 25 µm slot die. The masterbatch pellets are then used in LLDPE/LDPE blown film lines; the final film must comply with FDA 21 CFR 177.1520 when packaging food, and with EU Regulation 10/2011 for European food-contact use. Terminal articles are masterbatch pellets supplied to film converters, agricultural film producers, and extrusion coaters.
Competitive Versalis Flexirene® MS 26 A Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® MS 26 A Linear Low Density Polyethylene is an unfilled polyolefin supplied in pellet form for injection moulding. The grade is classified as a butene-copolymer LLDPE with a nominal melt mass-flow rate of 26 g/10 min measured at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022 and a density of 0.926 g/cm³ according to ISO 1183-1:2019. This flow index places the product among low-viscosity linear polyethylenes intended for multicavity injection moulding of thin-wall articles, caps, lids, closures, housewares, and packaging components where short cycle times and consistent mould filling are required. The comonomer distribution produces a lower melting peak and lower modulus than HDPE, while the linear backbone increases tensile yield stress and environmental stress-crack resistance relative to autoclave LDPE of similar density. The grade is supplied as natural translucent pellets; final colour is normally achieved with a polyolefin-compatible masterbatch added at the machine throat.
The product is not intended for long-term outdoor exposure unless a UV-stabiliser masterbatch is incorporated. The base resin contains antioxidant and processing stabiliser systems typical of polyolefin production. As with other low-density polyolefins, prolonged contact with aromatic or chlorinated solvents under stress can induce environmental stress cracking; immersion in such media should be avoided unless the finished part is tested under end-use conditions.
The standard melt flow test at 2.16 kg measures viscosity at low shear; it does not fully represent high-shear injection filling. At this flow index the material permits short filling times and reduced injection pressure relative to lower-MFR grades, but the processing window is constrained by the onset of surface defects such as jetting, gate blush, and flow marks when melt temperature or injection velocity is excessive. Published data for the spiral flow length of this specific formulation is limited; tooling trials are therefore the preferred basis for predicting fill in wall sections below 0.8 mm. In multicavity tools, packing pressures of 30–50 MPa are common for thin-wall LLDPE, while hold time is set by gate freeze-off as determined by part-weight stabilisation. Melt temperatures at the nozzle typically range from 210 °C to 250 °C, and mould surface temperatures from 20 °C to 50 °C are adequate. Mould shrinkage is anisotropic; typical allowances are 1.5–2.0 % in the flow direction and 1.0–1.5 % transverse, depending on wall thickness, packing pressure, and gate geometry.
Specimens for mechanical testing are normally prepared by injection moulding in accordance with ISO 294-1:2017. Rheological characterisation by capillary rheometry at 230 °C and apparent shear rates from 100 s⁻¹ to 10,000 s⁻¹ is recommended when transferring a tool from another polyolefin, because single-point MFR cannot predict shear viscosity under gate shear rates. Fitted Cross-WLF or Carreau-Yasuda parameters should be obtained from mouldflow laboratories rather than estimated from density and MFR. Published data for this specific configuration is limited, so process windows should be bracketed with design-of-experiment studies on the intended tool.
| Property | Method | Typical value |
|---|---|---|
| Melt mass-flow rate (190 °C, 2.16 kg) | ISO 1133-1:2022 | 26 g/10 min |
| Density | ISO 1183-1:2019 | 0.926 g/cm³ |
| Tensile modulus of elasticity | ISO 527-2:2021 | 250 MPa |
| Tensile stress at yield | ISO 527-2:2021 | 11 MPa |
| Nominal tensile strain at break | ISO 527-2:2021 | >700 % |
| Shore D hardness | ISO 868:2003 | 54 |
| Vicat softening temperature, A50 | ISO 306:2022 | 89 °C |
| Melting peak temperature | ISO 11357-3:2018 | 121 °C |
Values are typical for unfilled pellets and do not constitute minimum or maximum specification limits. They should be verified against the current manufacturer’s certificate of analysis for a given batch.
General-purpose polyolefin screws with length-to-diameter ratios of 20:1 to 24:1 and compression ratios of 2.5:1 to 3.5:1 are suitable. Because the linear molecular architecture has less shear thinning than long-chain branched LDPE, high screw rotation can generate shear heating and local temperature overshoot. Barrel settings from hopper to nozzle commonly follow a rising profile of 180 °C, 200 °C, 220 °C, and 230 °C, but the profile must be adjusted for shot mass, cycle time, and colourant carrier. Predrying is not normally required for this non-hygroscopic olefin; however, pellets stored below the dew point can carry surface condensation. At relative humidity above 60 %, surface moisture may cause splay and should be eliminated by closed silo storage or, if necessary, predrying at 60–70 °C for 2–4 h in a hot-air or desiccant dryer. Material changeover from HDPE or polypropylene should use a low-detergent polyolefin purge compound, because residual styrenic, acetal, or PVC materials can degrade in the required melt temperature range. Melt temperatures above 280 °C should be avoided; extended residence time above that threshold can initiate thermo-oxidative chain scission, yellowing, and loss of impact properties.
On actual production lines, screw recovery time rather than injection pressure may become the limiting factor for very short cycle times below 10 s. When the shot mass is large relative to screw diameter, plastication capacity must be checked against the required dry-cycle time. Lot-to-lot melt flow variation is normally controlled within the manufacturer’s specification, but moulders should verify MFR from the certificate of analysis and adjust holding time or temperature to compensate for minor shifts. Existing tooling with rough surfaces or insufficient vent depth can amplify flow marks; vent depth for LLDPE is generally maintained at 0.02–0.04 mm to permit air evacuation without flash.
Compared with autoclave LDPE of 0.918–0.930 g/cm³ density, Flexirene MS 26 A has a chemically linear backbone with short-chain branches from butene. This structure increases tensile yield stress and environmental stress-crack resistance while reducing melt elasticity and clarity. In closure and thin-wall packaging tooling, the material can fill long flow paths at high shear, but the lower melt strength may require more precise control of gas venting and packing to avoid warpage and sink marks. Compared with HDPE injection moulding grades, the product is lower in density, tensile modulus, and Vicat softening temperature; it is selected when low-temperature impact and flexibility are more important than stiffness and heat resistance. Compared with metallocene-catalysed LLDPE grades of equivalent density and flow, Ziegler-Natta butene-based products may exhibit a broader comonomer distribution, a broader melting range, and different optical and organoleptic properties; however, published data for this specific configuration is limited and direct comparisons should be made under the same test conditions.
| Property | Flexirene MS 26 A | LDPE injection grade typical range | HDPE injection grade typical range | Method |
|---|---|---|---|---|
| Density | 0.926 g/cm³ | 0.918–0.930 g/cm³ | 0.940–0.965 g/cm³ | ISO 1183-1 |
| Melt mass-flow rate | 26 g/10 min | 0.2–75 g/10 min | 0.04–40 g/10 min | ISO 1133-1 |
| Tensile modulus of elasticity | 250 MPa | 180–250 MPa | 700–1,200 MPa | ISO 527-2 |
| Tensile stress at yield | 11 MPa | 8–12 MPa | 20–30 MPa | ISO 527-2 |
| Vicat softening temperature, A50 | 89 °C | 80–95 °C | 115–130 °C | ISO 306/A50 |
Comparative values are representative literature ranges for unfilled moulding grades; they are not batch specifications and are shown only to distinguish the product class from adjacent polyolefin families.
Conversion of a cap, lid, or thin-wall container tool from autoclave LDPE to Flexirene MS 26 A requires recalculation of dimensional allowances and cooling times rather than direct substitution. The linear structure produces a different shrinkage tensor; packing pressure and gate seal time control flatness and roundness. Wall sections below 0.5 mm may require high injection speed and improved venting to compensate for lower melt elasticity. The material generally exhibits better environmental stress-cracking resistance than LDPE in the presence of surfactants and oils, as evaluated by ASTM D1693 or ISO 22088-1. Its higher flow index enables shorter cycle times in multicavity closures, but the grade cannot match the clarity of a high-clarity LDPE or metallocene LLDPE. Contact with aggressive aromatic or chlorinated media under stress can cause crazing; end-use compatibility tests are required when such chemicals are present. For food-contact caps, the finished article, including colour and additive masterbatches, must meet migration limits under Regulation (EU) No 10/2011 and, where applicable, FDA 21 CFR 177.1520. Dry blending with fatty acid amide slip agents at 0.05–0.15 wt% is used in some closure applications for torque reduction, but selection must be validated for migration and organoleptic effects. Processing trials on production-scale multicavity tooling are required to confirm the balance between filling pressure, gate size, and part weight; laboratory data alone do not establish a moulding window for this grade.
For closed-loop regrind operations, clean post-industrial scrap is commonly pelletised and blended with virgin material at levels that preserve the required MFR and impact properties; published data for this specific formulation is limited at higher regrind fractions. Waste generated during start-up and colour changes should be granulated only when free of contamination. Combustion of polyethylene releases carbon dioxide and water vapour; incomplete combustion can produce carbon monoxide, and severe thermal degradation produces acrolein and other oxygenated species. Industrial hygiene controls should therefore include local exhaust ventilation at melt-processing equipment and hot-runner maintenance stations. A melt filtration screen pack of 60/80/100 mesh may be used in compounding lines to reduce gel particulate from regrind or masterbatch; screen pack specification should be matched to extruder pressure capability.