Versalis Flexirene Ms 20 U Linear Low Density Polyethylene

Versalis Flexirene® MS 20 U Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® MS 20 U Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 590266
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Melting Temperature 125 °C
    Vicat Softening Temperature 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 250 MPa
    Shore D Hardness 50
    Film Haze 12%
    Film Gloss 45 50%
    Dart Drop Impact 100 g
    Tear Strength Md Td 200/400 g
    Processing Method Blown Film Extrusion
    Form Pellets
    Color Natural

    As an accredited Versalis Flexirene® MS 20 U Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® MS 20 U is packaged in 25 kg polyethylene-lined bags, palletized for transport and storage.
    Container Loading (20′ FCL) Versalis Flexirene® MS 20 U LLDPE in 25 kg bags, palletized and stretch-wrapped; 20′ FCL holds about 20–22 metric tons.
    Shipping Versalis Flexirene® MS 20 U ships as non-hazardous linear low-density polyethylene pellets, typically in 25 kg bags, big bags, or bulk trucks/containers. Transport in clean, dry, covered vehicles at ambient temperature. Protect from moisture, sunlight, heat, and contamination. Keep packaging sealed. Not classified as dangerous goods for transport.
    Storage Store Versalis Flexirene® MS 20 U in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags or containers closed and palletized off the floor. Protect from moisture, acids, UV exposure, and prolonged high temperatures. Use grounded equipment to control static. Follow local regulations and the safety data sheet. Avoid dust generation.
    Shelf Life Two years from production when stored in original unopened packaging, cool, dry, well-ventilated area, protected from sunlight and ignition sources.
    Application of Versalis Flexirene® MS 20 U Linear Low Density Polyethylene

    On blown-film lines producing heavy-duty industrial liners from Versalis Flexirene MS 20 U, the conversion window is bounded by melt fracture at high screw speeds and bubble instability at low stalk heights. The resin, a linear low density polyethylene with a nominal density of 0.920 g/cm³ and melt flow rate of 2.0 g/10 min at 190 °C/2.16 kg, is generally processed as the major phase in blends with a high-pressure LDPE at 10–30 wt% to increase bubble stability; however, large-diameter dies above 300 mm, internal bubble cooling, and die gaps narrower than 1.4 mm shift the onset of melt fracture to higher output rates. In this segment, formulation addition ratios are driven by blocking tendency at film thicknesses of 25–150 µm and by coefficient of friction requirements on converter filling lines: an antiblock masterbatch based on synthetic silica or diatomaceous earth is added at 2–5 wt%, and erucamide slip concentrate is introduced only when the finished liner must maintain a kinetic coefficient of friction below 0.30 under ISO 8295. Compliance for non-food industrial liners is evaluated against REACH (EC) No 1907/2006, while liners used inside flexible intermediate bulk containers for dangerous goods require compatibility with UN Model Regulations Chapter 6.5 and the associated testing under ISO 21898. If the same film is converted for contact with bulk food ingredients, FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 apply, but the resin supplier’s conformity statement must be supplemented by migration testing because end-use thickness, temperature, and contact time determine the result. Processing on a 90 mm single-screw extruder with a 30:1 L/D ratio and a barrel profile from 170 °C in the feed zone to 210 °C at the die is typical; the die temperature is held at 195–210 °C, the die gap at 1.6–2.2 mm, the blow-up ratio at 2.2:1–3.0:1, and the frost line height at 400–650 mm. Terminal product types include 25–150 µm liners for FIBCs, chemical drum liners, pallet covers, and heavy-duty sacks for granular polymers and mineral fillers.

    When UV Stabilization Becomes the Limiting Factor in Silage and Greenhouse Film

    Agricultural film production with Versalis Flexirene MS 20 U requires a different additive package than industrial liners because ultraviolet exposure, pesticide contact, and condensation stress dominate service life. The base resin is coextruded in three layers with a UV-stabilized outer layer containing 5–8 wt% HALS/UV absorber masterbatch, 2–3 wt% titanium dioxide white masterbatch where thermic performance is specified, and a middle layer with 20–30 wt% post-industrial regrind where EN 13207:2018 permits closed-loop recyclate in silage film so long as final mechanical values meet the standard’s minimum tensile and tear thresholds. Compliance for agricultural films is assessed under EN 13207:2018 for silage bags and stretch film, EN 13206:2017 for greenhouse covers, and EN 13655:2018 for recoverable mulch films; where food-producing crops are covered, REACH and national pesticide-contact rules may require additional screening. The addition ratio for anti-fogging additives is 0.5–1.5 wt% in the inner layer to maintain film transparency after condensation; excessive anti-fog addition above 2 wt% can produce surface tack that increases dust retention and reduces light transmission in greenhouse production. The downstream production process uses a three-layer blown film die, typically 250–350 mm in diameter, with a die gap of 1.6–2.0 mm, blow-up ratio of 2.5:1–3.5:1, and frost line height of 500–800 mm. Extruder temperatures are lower than those used for LDPE-rich film, with die zones at 190–205 °C, to avoid degrading the HALS package. Terminal product types include 150–250 µm silage bale wrap, 25–75 µm greenhouse covering film, silage clamp sheets, and black/white mulch films.

    Does Melt Temperature Affect Seal Initiation in Frozen-Food Packaging Film?

    Frozen-food packaging based on Versalis Flexirene MS 20 U is processed in thin-gauge blown film between 20 µm and 60 µm, where seal initiation temperature and hot-tack strength determine packaging line speed. Melt temperature at the die is held at 185–200 °C; above 210 °C the slip additive migration rate accelerates and can reduce seal strength after storage, while below 175 °C the melt is too viscous to stabilize a 2.5:1 blow-up ratio bubble on single-screw lines. The formulation addition ratio in this segment is typically 0.5–1.5 wt% of a masterbatch containing erucamide or oleamide as slip agent, and 1–2 wt% of a silica antiblock masterbatch, with total additive letdown not exceeding 5 wt% because film haze measured under ASTM D1003 can exceed 12% in thin gauge if antiblock concentration is not matched to particle size and film thickness. Compliance for food-contact use is controlled by FDA 21 CFR 177.1520(c) for the olefin polymer and by EU Regulation 10/2011 with food simulants A, B, and D2 depending on the packaged food category; good manufacturing practice is established under Commission Regulation (EC) No 2023/2006, and the converter is responsible for migration testing of the finished printed laminate. The downstream production process uses a three-layer coextrusion line with a layer ratio of 20/60/20, die gap of 1.4–1.8 mm, blow-up ratio of 2.2:1–3.0:1, and a chilled air ring with internal bubble cooling to lower the frost line to 300–500 mm. Terminal product types include frozen vegetable bags, ice cream over-wrapping film, fish block bags, and bakery pre-formed liners.

    Application segmentStandard or regulatory referenceScopePass criterion relevant to MS 20 U conversion
    Heavy-duty industrial linersREACH (EC) No 1907/2006, UN Model Regulations Chapter 6.5, ISO 21898Chemical safety and FIBC inner liner performanceSVHC screening and converter burst/stacking data
    Agricultural silage and greenhouse filmEN 13207:2018, EN 13206:2017, EN 13655:2018Tensile, tear, UV durability, and recoverabilityGrade-specific tensile and tear retention after weathering
    Frozen food packaging filmFDA 21 CFR 177.1520(c), EU Regulation 10/2011, EC No 2023/2006Food-contact olefin polymer and migrationOverall migration below 60 mg/kg or simulant-specific limit
    Cast pallet stretch filmASTM D4649, ASTM D5458, EUMOS 40509Film selection, cling, and load retentionDocumented elongation, cling force, and load shift
    Microporous breathable filmISO 10993-5, ISO 10993-10, EN 13859-1:2014Cytotoxicity and roofing underlayment resistanceBiocompatibility scoring and water penetration limits

    In cast film conversion for hand pallet wrap, Versalis Flexirene MS 20 U is used as a butene-LLDPE component rather than the sole resin because its 2.0 g/10 min melt flow rate is below the 2.8–4.0 g/10 min range preferred for high-output slot-die extrusion. In a typical formulation, MS 20 U is added at 20–40 wt% to an octene-LLDPE, and 0.5–1.5 wt% polyisobutylene or hydrogenated hydrocarbon tackifier masterbatch is introduced to control unwind cling. Compliance in this segment is governed by ASTM D4649 for stretch film selection, ASTM D5458 for cling measurement, and EUMOS 40509 for load stability; machine-grade film is not generally food-contact unless overwrapped. The conversion process uses a cast film line with a 150 mm single-screw extruder, 30:1 L/D, barrel temperatures of 220–260 °C, die temperature of 260–270 °C, and chill roll temperature of 18–25 °C, with a 25 µm film running at 250–400 m/min. Published data for this specific grade in high-speed cast stretch lines is limited; converter trial data should confirm output and cling stability. Terminal product types include 17–23 µm machine pallet wrap, 25–35 µm hand pallet wrap, and pre-stretched film sold at 100% or 200% elongation.

    Microporous Breathable Films from Calcium Carbonate-Filled Compounds

    Where Versalis Flexirene MS 20 U is diluted with 45–55 wt% surface-treated calcium carbonate masterbatch and extruded into a cast or blown precursor film, uniaxial stretching opens microvoids at the filler-polymer interface; this is the basis for breathable backsheet films used in hygiene and pitched roofing underlayments. The addition ratio is determined by the drawing ratio: at 2.0:1–3.0:1 stretch ratios, 50 wt% CaCO₃ having a median particle size of 1.5–2.0 µm gives water vapour transmission rates above 2000 g/m²·24 h under ISO 15106-1, but filler above 60 wt% reduces transverse tensile strength below 8 MPa and creates film ruptures during MDO stretching. Compliance for hygiene applications may require biocompatibility evaluation under ISO 10993-5 and ISO 10993-10 when the film is classified as a medical device component; roofing underlayments are tested under EN 13859-1:2014 for tensile properties and resistance to water penetration. The production process uses a compounding twin-screw extruder with L/D 44:1 at barrel temperatures of 170–210 °C, and the compounded pellets are cast-extruded on a slot die with 0.8–1.2 mm gap, quenched at 25–35 °C, and stretched in the machine direction on a roll-stretch unit at 50–90 °C. Terminal product types include 18–35 g/m² breathable backsheets, housewrap and roof underlay films, and disposable hygiene cover stock.

    Free Quote

    Competitive Versalis Flexirene® MS 20 U Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® MS 20 U Linear Low Density Polyethylene is a butene-1 based LLDPE supplied in pellet form for blown and cast film conversion. The nominal melt flow rate is 2.0 g/10 min when determined at 190 °C under 2.16 kg load according to ISO 1133-1, and the nominal density is 0.920 g/cm³ according to ISO 1183-1. The linear backbone contains short-chain branching from the C4 comonomer and lacks the long-chain branching characteristic of high-pressure LDPE. That difference lowers melt elasticity, modifies extensional viscosity, and changes bubble stability, seal initiation, and tear behaviour relative to both LDPE and high-density polyethylene grades.

    The grade is positioned as a general-purpose film resin rather than a precision packaging specialty. It is suitable for applications where a balance of processability at moderate melt temperature, seal flexibility, and controlled gauge is required. It is not intended as a direct substitute for C6 or C8 LLDPE grades in puncture-critical, high-abuse packaging without additional verification. It also differs from HDPE in that the lower density reduces stiffness and improves stress crack resistance in flexible structures, while reducing maximum tensile strength and barrier character.

    Specification Matrix and Film-Specific Release Parameters

    The two primary values used for incoming lot release and extruder setup are melt flow rate and density. The melt flow rate is measured by extruding the material through a standard die under a deadweight of 2.16 kg at 190 °C, and the density is determined after a standard annealing history by graduated column or equivalent method. The table below lists the release parameters most frequently referenced on film lines.

    Nominal specification matrix for Versalis Flexirene® MS 20 U
    ParameterNominal valueTest method
    Melt flow rate2.0 g/10 minISO 1133-1
    Density0.920 g/cm³ISO 1183-1
    ComonomerC4 butene-1Internal FTIR/CRYSTAF where data is available
    Physical formPelletsVisual and sieve inspection

    Lot-to-lot variation within release limits is sufficient to shift extrusion pressure and film gauge distribution. Processors should obtain the current technical data sheet for full tensile, impact, and optical values because published grade-specific data for the complete mechanical profile is limited outside the supplier-controlled documentation set.

    On blown film lines with air-ring-only cooling, the low melt strength of the C4 LLDPE requires a conservative frost-line height and stable venturi control. Typical industrial settings use melt temperatures between 190 °C and 230 °C, an annular die gap of 1.8 mm to 2.5 mm, and blow-up ratios below 3.0 unless internal bubble cooling and high-flow air rings are present. At higher blow-up ratios, bubble flutter and edge folds are the dominant failure modes reported on single-lip air-ring equipment. The melt is more shear-thinning than long-chain-branched LDPE, but it can still exhibit lower melt strength; the bubble must therefore be supported by reduced frost-line height and balanced exhaust volume.

    Grooved-feed extruders with 30:1 to 35:1 L/D typically deliver adequate melt quality if barrel zones are profiled to avoid excessive viscous shear. Screen packs should be sized for the relatively low viscosity; back pressure may be lower than fractional-melt grades at equivalent output, which can improve motor load but may reduce mixing uniformity. Film gauge defects attributable to helical melt flow instability are possible when screw temperature gradients exceed 15 °C between adjacent zones, particularly on older extruders without barrier-flight mixing sections.

    What Limits Bubble Stability When Butene-Based LLDPE Is Run on Unmodified LDPE Lines?

    A butene-based LLDPE has a different extensional hardening response than high-pressure LDPE. The absence of long-chain branching reduces melt tension at high draw rates, and the C4 branch length contributes fewer effective tie chains than hexene or octene copolymers at the same density. This molecular architecture limits the maximum stable take-up speed on extruders calibrated for LDPE. Bubble instability appears as periodic diameter oscillation and frost-line wavering, which translates into film thickness bands and downstream printing defects.

    Operational correction involves reducing die gap strain rate, lowering frost-line height, and stabilising the air ring exit velocity. When the bubble is not stable at the target output, processors may blend the grade with LDPE or adjust die temperature to reduce melt viscosity. The use of an internal bubble cooling system can extend the stable output window, but published data for this specific grade under internal bubble cooling is limited. Film tensile properties should be verified according to ISO 527-3 or ASTM D882 after any process change because stability improvements can alter molecular orientation and tear anisotropy.

    When This Grade Is Let Down into LDPE at Ratios Above 20 wt% for Shrink Film

    Addition of 15 wt% to 30 wt% MS 20 U into high-pressure LDPE is a common route to improve seal initiation and hot-tack in heavy-duty shrink film. The blend lowers the crystalline melting range relative to LDPE-rich formulations and can increase elongation at break, but it also reduces optical clarity and changes shrink tension. On a three-layer blown line, placing the linear component in the core layer preserves surface gloss while maintaining seal advantages when the skin layers are LDPE or metallocene LLDPE.

    In blending operations, melt pressure at the die is typically lower than for a fractional-melt LDPE at the same screw speed because of the higher melt flow rate. However, the blend is more sensitive to gel formation if hold-up time is excessive. Purging with a medium-viscosity linear polyethylene is recommended before short shutdowns. Pre-drying is normally unnecessary unless pellets have been stored in cold conditions and condensation is visible; in such cases, a pellet dryer at 65 °C for 1–2 h is sufficient to remove surface moisture.

    For cast stretch film, the melt-flow rate permits lower head pressure and reduced motor load on high-output cast lines compared with fractional-melt LLDPE grades. Cast film dies with narrow lip gaps of 0.8 mm to 1.5 mm are used, and melt temperature is usually held between 220 °C and 245 °C to optimise web edge stability. Chill roll temperatures of 20 °C to 40 °C are typical. The absence of long-chain branching reduces neck-in but also reduces melt curtain tautness; edge pinning must be maintained at high line speeds.

    In stretch film compositions, the grade can be used as a core or skin-layer component. When used in a cling layer, the base resin requires a cling additive such as polyisobutylene or a glycerol-based tackifier, because the base LLDPE itself has low cling. The force-time response of the final film should be evaluated under ASTM D5458 or a stretch-frame test, depending on the packaging line. Stretch wrap producers should not extrapolate laboratory results from one film structure to another without gauging, pre-stretch, and wrap-speed fixed.

    The Grade Is Not a Direct Substitute for C8 LLDPE in Puncture-Critical Structures

    Compared with octene-based LLDPE grades of the same 0.920 g/cm³ density and 2.0 g/10 min flow rate, the butene-based polymer generally exhibits lower puncture resistance, lower Elmendorf tear propagation resistance in machine direction, and lower dart drop impact. This difference emerges because the shorter C4 branch produces less effective interlamellar tie chains per unit mass than the C8 branch. The result is a resin that is lower in cost and easier to dilute with LDPE, but less robust for high-abuse applications such as sharp-edged frozen products, heavy pouches, or agricultural films requiring extended outdoor durability.

    When film performance is specified under ISO 7765-1 for dart impact or ISO 6383-2 for tear resistance, direct substitution of an octene grade with MS 20 U at constant gauge may fail lot acceptance unless the structure is redesigned. Published data for this specific grade under those standards should be obtained for comparison rather than relying on typical C4 class averages. The grade can still meet many general-purpose applications if the specification does not include high puncture energy or extreme low-temperature abuse.

    Thermal degradation of the grade begins to accelerate when melt temperature exceeds 250 °C, particularly in high-shear coextrusion with long residence times. Films processed above this boundary may show gel formation, yellowing, and changes in melt viscosity from chain scission. The stabiliser package protects against standard processing conditions but is not formulated for prolonged high-temperature hold-up. Extruder profile settings should avoid idle periods longer than 20–30 min at temperature without purging, especially in the presence of oxygen. If outdoor weathering is required, the grade must be modified with carbon black or a hindered amine light stabiliser package; the unmodified resin is not intended for long-term UV exposure without additional stabilisation.

    In food-contact applications, the grade may fall under the base polyolefin provisions of FDA 21 CFR 177.1520 and European Regulation EU No 10/2011 for plastic materials and articles intended to come into contact with food. Compliance is not automatic by resin type; it depends on the additives, colourants, processing aids, and final film structure. Processors should obtain a current Declaration of Compliance from Versalis for the specific grade and lot, and should verify overall and specific migration limits for the final article. The table below summarises the relevant reference standards used in food-contact and mechanical property qualification.

    Typical compliance and qualification references for film applications
    Application or propertyReference standardUse
    US food-contact polyolefin resinFDA 21 CFR 177.1520Base resin compliance conditions
    EU plastic food-contact materialRegulation (EU) No 10/2011Overall and specific migration
    Film tensile propertiesISO 527-3 / ASTM D882Quality control and structure comparison
    Dart drop impactISO 7765-1 / ASTM D1709Film impact resistance
    Elmendorf tear resistanceISO 6383-2 / ASTM D1922Film tear propagation
    Hot-tack and seal strengthASTM F1921 / ASTM F88Packaging line sealing verification

    REACH Article 33 communication obligations apply only when a listed substance above 0.1% w/w is present in the supplied article, and processors should request a grade-specific statement for current SVHC status. RoHS restrictions are generally outside the base polymer scope but may apply to finished electrical and electronic equipment in which the film is incorporated.

    Top