Versalis Flexirene Ms 20 A Linear Low Density Polyethylene

Versalis Flexirene® MS 20 A Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® MS 20 A Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 341874
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Additive Antioxidant
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Density 0.920 g/cm3
    Melting Point 120 °C
    Vicat Softening Point A 50 94 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 700 %
    Flexural Modulus 250 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Resistance Md 100 g
    Elmendorf Tear Resistance Td 150 g
    Haze 10 %
    Gloss 45 60 %
    Processing Temperature 180-220 °C

    As an accredited Versalis Flexirene® MS 20 A Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® MS 20 A Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized for industrial use.
    Container Loading (20′ FCL) 20′ FCL: 25 kg bags of Versalis Flexirene® MS 20 A LLDPE, palletized or floor-loaded, shrink-wrapped; 18–20 MT per container.
    Shipping Versalis Flexirene® MS 20 A is shipped as non-hazardous LLDPE pellets in 25 kg bags, big bags, or bulk containers. It is not classified for transport. Keep packages closed, dry, and away from heat; avoid moisture and static buildup. No special DOT/ADR/IMDG labels required.
    Storage Store Versalis Flexirene® MS 20 A in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep bags sealed, palletized, and off the floor to protect from moisture, dust, and contamination. Avoid static discharge. Use first-in, first-out stock rotation and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life: approximately 24 months in original unopened packaging, stored dry, below 40°C, away from direct sunlight and ignition sources.
    Application of Versalis Flexirene® MS 20 A Linear Low Density Polyethylene

    On a high-speed cast stretch film line equipped with a 90 mm 30:1 L/D barrier screw and a coat-hanger slot die set at 0.8 mm, Versalis Flexirene® MS 20 A Linear Low Density Polyethylene is extruded with flat barrel temperatures from 220°C at the feed throat to 255°C at the die adapter. The nominal melt flow rate of the grade is 2.0 g/10 min when measured per ISO 1133-1:2022 at 190°C under 2.16 kg load, and the nominal density is 0.920 g/cm³ per ISO 1183-1:2019. The die-to-chill-roll air gap is held between 15 mm and 30 mm, with the primary chill roll maintained at 20°C to 25°C and secondary cooling rolls kept below 30°C. The resin is not normally pre-dried because linear low density polyethylene is non-hygroscopic, but when silo storage has exposed pellets to condensation at relative humidity above 80%, surface moisture is removed in a hopper dryer at 60°C for 1 h before extrusion. Additivation for cling performance is formulation-dependent: a polymeric or olefinic tackifier is introduced at 0.8 wt% to 2.5 wt% via a gravimetric side feeder, while the supplied slip package of MS 20 A is adjusted downward only after coefficient of friction values are checked per ISO 8295:2023. At tackifier loading above 3.0 wt%, roll blocking becomes a measurable failure mode on high-speed wrappers, and draw-down stability can degrade because the melt curtain oscillates at frequencies between 5 Hz and 15 Hz. Edge trim from the cast line is reintroduced at up to 15 wt% without severe optical penalty, though higher regrind fractions raise gel counts and reduce film clarity on lines running above 500 m/min. Film mechanical properties are checked per ASTM D882-18 at a test speed of 50 mm/min after conditioning at 23°C and 50% RH for 40 h. For direct food contact, finished pallet wrap based on this polyolefin is assessed under FDA 21 CFR 177.1520(c) and under Regulation (EU) No 10/2011 with overall migration limited to 10 mg/dm² when tested per EN 1186-1. Terminal finished products include machine pallet wrap at 17 µm to 23 µm gauge, hand pallet wrap, and bundling film for logistics consolidation.

    When Does Neck-In Become the Controlling Variable in Extrusion Coating?

    Extrusion lamination of Flexirene MS 20 A onto paper, aluminium foil, and metallised substrates differs from cast film production because the polymer curtain is unsupported between the die and the nip. A starting blend of 70 wt% MS 20 A and 30 wt% high-pressure LDPE is used to raise melt strength and reduce neck-in. The melt is delivered through a T-slot die with a gap of 0.6 mm to 0.8 mm at melt temperatures from 290°C to 310°C. The air gap is constrained to 100 mm to 180 mm; above 200 mm, draw resonance and edge weave produce coating weight variation exceeding ±5%. Coating weight is normally set between 15 g/m² and 25 g/m². At line speeds above 150 m/min, a 100% MS 20 A curtain is not recommended because neck-in per side can exceed 25 mm and melt curtain rupture becomes intermittent. Adhesion to the substrate is tested per ASTM F904-16 or ISO 11339:2022; the substrate surface tension is maintained at 38 mN/m to 42 mN/m by corona discharge immediately before lamination. For food-contact laminates, the sealant side is evaluated under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with specific migration testing for additives performed according to EN 1186-13 using simulant D1 for fatty foods. When the structure includes aluminium foil, pinholing is assessed after lamination by sodium chloride electrolyte penetration under ASTM B812-96. The operational boundary for this configuration is that the high melt temperatures required for substrate adhesion reduce the thermal stabiliser margin; residence time at 310°C should not exceed 10 min, otherwise oxidised gel formation becomes visible in the coated web. Terminal products include sachet laminates, soap wrappers, liquid carton barrier structures, and coated paper for dry food pouches.

    Blown Film Dilution Blends for High-Dart Sack Structures

    Heavy-duty sack production by blown film extrusion does not use the neat MS 20 A as the sole resin type. A starting blend of 70 wt% MS 20 A and 30 wt% high-pressure LDPE is processed on a 250 mm blown film die with a die gap of 1.8 mm, a blow-up ratio of 2.2:1 to 2.6:1, and frost line height maintained at 500 mm to 800 mm above the die. Extruder barrel temperatures are set from 190°C to 210°C, which limits oxidative gel formation while allowing stable bubble inflation. The LDPE fraction stabilises the bubble, and the linear low density fraction raises puncture resistance and low-speed dart impact. Dart drop is measured per ASTM D1709-22 Method A at 100 µm film thickness; puncture energy is measured per ISO 7765-1:2022; Elmendorf tear resistance is measured per ISO 6383-2:2022. Published data for MS 20 A in this exact 70:30 blend is limited, so converter-scale line trials are required to establish actual dart and tear values. Anti-block silica is added at 2,000 ppm to 5,000 ppm and additional slip erucamide at 500 ppm to 1,200 ppm, but the existing slip package in MS 20 A should be quantified first from the lot certificate to avoid excessive surface bloom and heat-seal reduction in subsequent converting steps. At film thickness below 50 µm, bubble instability in this blend can generate gauge variation of ±10%; in that case the die gap is reduced to 1.2 mm and the LDPE fraction is increased to 35 wt%. Compliance for industrial sacks that do not contact food is governed by REACH Article 33 obligations for substances of very high concern and by packaging waste directive 94/62/EC. When the sacks are intended for food ingredients, the base polymer must satisfy FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with migration testing depending on the packed food type. Terminal products include fertiliser sacks, free-flowing chemical sacks, bulk industrial liners, and woven bag lamination.

    Sealant Layer Heat Transfer and Hot-Tack Limits in Coextruded Barrier Film

    Coextruded barrier film lines running MS 20 A as the seal layer are configured with five-layer or seven-layer blown film dies, and the sealant layer thickness is typically set from 10 µm to 25 µm within a total film thickness of 50 µm to 120 µm. Heat seal initiation for a butene-based LLDPE of this density is commonly observed near 105°C, but the exact onset for MS 20 A must be confirmed on the converter’s seal curve generated per ASTM F2029-21 at 0.5 N/mm² jaw pressure and 1 s dwell. Hot-tack testing per ASTM F1921-20 is used to determine maximum vertical form-fill-seal packaging speed before the still-molten seal opens under product load. Sealant-layer formulations that blend more than 20 wt% LDPE into MS 20 A should be evaluated for hot-tack narrowing; the LDPE fraction can reduce the temperature window in which hot tack strength remains above 1 N/15 mm. For fast packaging lines at 80 to 120 pouches per minute, seal jaw temperatures are set 10°C to 15°C above the measured seal initiation temperature to accommodate heat loss through the substrate and jaw release dynamics. Compliance for food-contact sealant layers is assessed under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm² per EN 1186-1 and specific migration of slip additives controlled by EN 1186-14. The operational boundary is that sealant films containing erucamide slip can exhibit reduced seal strength after long-term storage at 40°C due to additive migration to the seal interface; seal strength should be rechecked after 30 days of accelerated ageing at 40°C before release to the packaging line. Terminal products include fresh produce bags, bakery overwrap, processed cheese film, and barrier lidding film for thermoformed trays.

    ApplicationRegulation or StandardTest ConditionLimit or Reporting Basis
    Direct food contact filmFDA 21 CFR 177.1520(c)Extraction per 21 CFR 176.170(c) end-use conditions A–HOlefin polymer specification
    EU food contact filmRegulation (EU) No 10/2011EN 1186-1 overall migration10 mg/dm²
    Tensile propertiesASTM D882-1850 mm/min, 23°C, 50% RHMPa and %
    Dart impactASTM D1709-22Method A or B at 23°Cg or g/µm
    Melt flow rateISO 1133-1:2022190°C, 2.16 kg2.0 g/10 min nominal

    At blast-freezer storage temperatures below -25°C, a 50 µm cast film based on MS 20 A retains sufficient dart impact resistance to resist edge puncture from frozen bread edges and irregular vegetable pieces. Conditioning for impact testing follows ASTM D1709-22, with specimens held at -20°C for 48 h before the striker is released. The glass transition of linear polyethylene is well below -100°C, so the film remains sealable at conventional sealing temperatures after exposure to -30°C, although frost on the film surface can delay seal initiation and requires seal jaw temperatures 10°C to 15°C above the dry-film onset. Vertical form-fill-seal packaging lines running frozen vegetable and seafood pouches operate at 80 to 120 cycles per minute; seal integrity is checked per ASTM F88/F88M-21 at 200 mm/min jaw separation speed. A high-slip erucamide system is maintained at 500 ppm to 1,000 ppm to keep the coefficient of friction below 0.25 on an inclined plane tester per ISO 8295:2023, because high-speed film transport over metal forming collars causes heat generation and surface scuffing. The slip additive migration rate is slower at freezer temperatures, so surface slip should be rechecked after 14 days of storage at -20°C before packing line start-up. Compliance for frozen food contact is evaluated under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration testing per EN 1186-1 and specific migration testing for slip additives under EN 1186-14. The operational boundary is that the base polymer is not an aroma barrier; strongly odorous contents such as cocoa or coffee require a coextruded barrier layer because flavour scalping through polyethylene is measurable. Terminal finished products include frozen vegetable pouches, frozen seafood bags, frozen dough overwrap, and frozen fruit packaging film.

    If Silage Film Requires Higher UV Stabiliser Loading, What Changes?

    Agricultural silage wrap produced with MS 20 A requires a UV stabiliser masterbatch at 0.5 wt% to 1.5 wt%, depending on the expected solar exposure and film thickness. The masterbatch carrier resin can shift the compounded melt flow rate by 0.1 g/10 min to 0.3 g/10 min, so extruder feed zone temperatures may be reduced by 5°C to 10°C to prevent pellet agglomeration at the feed throat. Blown film conditions use a blow-up ratio of 1.8:1 to 2.2:1, a die gap of 1.6 mm to 2.0 mm, and melt temperatures from 195°C to 215°C. The film is assessed for outdoor weathering by ISO 4892-2:2021 Method A exposure, with tensile elongation retained above 300% after 1,500 h of accelerated ageing. This requirement is not met by the base polymer alone; unmodified MS 20 A degrades under ultraviolet exposure and loses tensile elongation before one agricultural season is complete. For silage film exposed in southern latitudes above 1,200 kLy cumulative solar radiation, a higher stabiliser loading or a multilayer structure with a HALS-rich skin is required because the surface layer receives disproportionate UV degradation. Compliance for agricultural film that does not contact food is governed by REACH and by local packaging waste legislation; if the film is used as a temporary food-contact surface for ensiled feed, the converter must verify that the stabiliser masterbatch is listed in Regulation (EU) No 10/2011 for the intended contact conditions. The operational boundary is that the stabiliser package can interfere with surface tack in stretch applications; cling force should be measured on the final wrap per ASTM D5458-16 before bundling, because some UV stabilisers bloom in the first 72 h and lower cling peel force. Terminal products include silage bale wrap, agricultural stretch film, greenhouse repair film, and temporary cover film for chopped forage.

    Free Quote

    Competitive Versalis Flexirene® MS 20 A Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® MS 20 A is an injection-moulding grade linear low density polyethylene supplied in pellet form. The grade designation MS 20 A identifies a melt flow rate of 20 g/10 min measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. Density determined by ISO 1183-1:2019 is 0.924 g/cm³. This density places the product between very-low-density ethylene copolymers and high-density polyethylene; the result is a balance of low-temperature ductility, environmental stress crack resistance, and moderate short-term stiffness. The product is intended for thin-wall injection moulding of caps, closures, housewares, toys, and similar articles where high melt flow must fill long flow paths at reduced injection pressure. The current public technical datasheet does not disclose the α-olefin comonomer type or the short-chain branching distribution; therefore, comparisons with butene- or hexene-based LLDPE grades should be made using the complete certificate of analysis rather than density and melt flow rate alone.

    On injection moulding machines, the 20 g/10 min melt flow rate reduces filling pressure relative to film-grade LLDPE with MFR values below 4 g/10 min. A general-purpose three-zone screw with an L/D ratio of 20:1 to 24:1 and compression ratio of 2.5:1 is sufficient for homogeneous melt if back pressure is kept between 5 bar and 10 bar hydraulic. Barrel temperature profiles from 180 °C in the feed zone to 220 °C in the metering zone are typical. Nozzle settings above 240 °C are not recommended because LLDPE undergoes thermo-oxidative degradation under extended residence time, producing yellowing, gel particles, and a measurable loss in tensile elongation at break under ISO 527-2:2012. Mould temperature is normally maintained between 10 °C and 40 °C; higher mould temperatures may improve weld-line strength but increase cycle time and linear shrink. Published spiral-flow data for this specific configuration is limited; mould fillability should therefore be evaluated using instrumented short-shot trials on the production tool rather than by melt flow rate alone.

    Mechanical Behaviour in Thin-Wall Cross-Sections

    Representative values from the current Versalis technical datasheet are presented below. These are not specification limits and should be read together with the lot-specific certificate of analysis.

    PropertyMethodRepresentative value
    DensityISO 1183-1:20190.924 g/cm³
    Melt flow rateISO 1133-1:2022 (190 °C, 2.16 kg)20 g/10 min
    Tensile stress at yieldISO 527-2:201211 MPa
    Tensile elongation at breakISO 527-2:2012>500%
    Flexural modulusISO 178:2019240 MPa
    Vicat softening temperatureISO 306/A5089 °C

    Specimens for these measurements are generally prepared by injection moulding under ISO 294-1:2017 and conditioned at 23 °C and 50% relative humidity for at least 40 h according to ISO 291:2021. The tensile elongation at break above 500% indicates ductile behaviour in thin sections at room temperature. Notched impact resistance under ISO 180:2023 is not always reproduced in a public datasheet; when sub-ambient impact is critical, incoming inspection should include notched Izod or instrumented puncture testing on production-representative specimens. The flexural modulus of 240 MPa is lower than that of a 0.950 g/cm³ high-density polyethylene by approximately 40–60%, which reduces stress concentration at snap-fit features but also lowers long-term load-bearing stiffness. The Vicat softening temperature of 89 °C is a short-term thermal indicator and is not a design limit; creep resistance and heat deflection temperature under ISO 75-2:2013 should be evaluated for continuous service above 60 °C.

    When replacing LDPE or higher-density LLDPE in closure moulding

    Flexirene MS 20 A differs from a typical low density polyethylene of equivalent melt flow rate primarily in molecular architecture. LDPE contains long-chain branching, which produces strain hardening in extensional flow and lower melt viscosity at high shear, whereas LLDPE has a linear backbone with short-chain branches. Replacement of an LDPE injection grade by this material may require an increase in melt temperature of 5–10 °C or an increase in injection pressure because the high-shear viscosity of LLDPE can be higher in thin-wall gates. The resulting article, however, typically shows greater environmental stress crack resistance when tested under ASTM D1693-15, Condition B, and higher tensile yield stress under ISO 527-2:2012.

    Compared with a higher-density LLDPE of 0.935 g/cm³ to 0.940 g/cm³, the 0.924 g/cm³ density of MS 20 A produces lower flexural modulus and hardness but improved impact toughness at sub-ambient temperatures. This trade-off is relevant in caps and closures that must resist cracking at low temperature without excessive stiffening. The grade is not a direct substitute for HDPE in applications requiring continuous load-bearing at elevated temperature or high modulus. Linear thermal expansion of the lower-density grade is also greater; with a mould temperature of 20 °C and wall thickness between 1 mm and 2 mm, linear mould shrink for LLDPE in this density range is commonly reported between 1.5% and 2.5%, but part-specific values must be established on the production tool.

    Weld-line regions in closure moulding are particularly sensitive to molecular orientation. Because LLDPE of this type has a linear backbone without long-chain branching, weld lines may retain lower elongation at break than the bulk material; this can be assessed by cutting tensile specimens across the weld line according to ISO 527-2:2012. Higher mould temperature and optimised venting can measurably influence weld-line elongation at break; published data for this specific grade is limited, so validation on the target part is required.

    Food-contact and potable-water approvals are not automatic for any polyethylene grade. Converters must verify that the specific production lot carries the appropriate certificate of conformity and that the finished article meets the applicable migration limits of Regulation (EU) No 10/2011 as amended, or 21 CFR §177.1520 for olefin polymers in the United States. Colour concentrates, processing aids, or recycled material can alter the regulatory status and must be assessed separately.

    Verification areaReference standard or regulationRequired action
    Melt flow rateISO 1133-1:2022Compare with certificate of analysis
    DensityISO 1183-1:2019Incoming resin inspection
    EU food contactRegulation (EU) No 10/2011Finished-article migration testing
    US food contact21 CFR §177.1520End-use condition verification

    Melt viscosity is governed by short-chain branching distribution

    Although the datasheet does not disclose the comonomer type, the linear low density polyethylene structure of this grade means that melt viscosity is influenced by short-chain branching and molecular weight distribution. Under injection moulding shear rates above 100 s-1, the material exhibits shear thinning, which reduces viscosity in gates and runners. Because LLDPE has a narrower molecular weight distribution than many autoclave LDPE grades, the viscosity curve is flatter and the material can be more sensitive to gate freeze-off. The high melt flow rate of 20 g/10 min provides lower zero-shear viscosity than a 4 g/10 min LLDPE, but it also produces a less pronounced elongational plateau. In hot-runner systems, gate drool may occur when the nozzle temperature exceeds 230 °C and decompression is insufficient. Screw decompression of 2–3 mm and valve-gate hot runners are commonly used to control stringing and drool in high-speed closure production.

    Rheological data generated on a capillary rheometer under ISO 11443:2021 is preferred over MFR for gate design because MFR is a single-point low-shear measurement. Colour compounding for this grade should use polyethylene-compatible masterbatch carriers. Masterbatch addition rates above 4 wt% can shift viscosity and mould shrink, requiring re-validation of the moulding window. Flame-retardant or blowing-agent systems containing polar additives may not disperse uniformly in non-polar LLDPE and should be evaluated for plate-out and screw slippage. In-plant regrind addition above 20 wt% should trigger re-testing of melt flow rate and tensile elongation at break because repeated extrusion can reduce molecular weight and change screw recovery.

    Does the grade require pre-drying or special storage before processing?

    Pre-drying is not mandatory when the product is handled from sealed, undamaged packaging. LLDPE is non-hygroscopic; internal moisture uptake is negligible under ISO 62:2021 water absorption testing. Surface condensation is the main moisture source. If bags are opened in an environment with relative humidity above 60%, surface moisture may cause splay in moulded parts; in that case a dehumidified-air hopper dryer at 70–80 °C for 1–2 hours is sufficient. The material should be stored away from direct sunlight, strong oxidizers, and prolonged temperatures above 50 °C. Prolonged contact with chlorinated solvents, aromatic hydrocarbons, and strong oxidising acids can cause swelling, crazing, and loss of tensile properties under ISO 527-2:2012.

    In high-speed thin-wall injection moulding of caps and overcaps on machines with clamp forces between 1,500 kN and 3,000 kN, the combination of 20 g/10 min melt flow rate and 0.924 g/cm³ density supports short cycle times when the mould is cooled uniformly and gates are sized for shear rates above 1,000 s-1. Cavity pressure sensors help detect batch-to-batch variation; a shift in peak cavity pressure exceeding 5% without a corresponding machine parameter change indicates that melt flow rate or barrel temperature should be checked. The grade is not recommended for continuous service above 60 °C under mechanical load, or for applications requiring the stiffness of 0.950 g/cm³ HDPE. Incoming material acceptance should include density, melt flow rate, and tensile yield stress, using the standards cited in the certificate of analysis.

    Top