| HS Code | 896981 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.934 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 5.0 g/10 min |
| Melting Temperature | 125 °C |
| Vicat Softening Temperature 10 N | 110 °C |
| Tensile Modulus | 700 MPa |
| Tensile Stress At Yield | 15 MPa |
| Tensile Strain At Break | 800% |
| Flexural Modulus | 650 MPa |
| Shore D Hardness | 55 |
| Escr 10 Igepal F50 | >1000 h |
| Uv Stabilization | Yes |
| Brittleness Temperature | < -60 °C |
| Thermal Stability | >200 °C |
As an accredited Versalis Flexirene® MR 50 U Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® MR 50 U LLDPE is supplied in 25 kg polyethylene bags, stacked on pallets for industrial handling. |
| Container Loading (20′ FCL) | Versalis Flexirene® MR 50 U in 20′ FCL: approximately 18 MT net, 720 x 25 kg bags, floor-loaded. |
| Shipping | Versalis Flexirene® MR 50 U is typically supplied as non-hazardous LLDPE pellets in 25 kg bags, big bags, or bulk trucks/railcars. Ship in clean, dry, covered vehicles/containers, protecting from moisture, sunlight, and contamination. No ADR/RID/IMDG/IATA hazard class; store cool, dry, ventilated, away from ignition sources. Consult SDS for exact classification. |
| Storage | Store Versalis Flexirene® MR 50 U in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers or bags closed to prevent moisture and contamination. Use pallets or racks, maintain first-in/first-out stock rotation, and avoid prolonged UV exposure. Protect from dust and static buildup; ground equipment during handling. |
| Shelf Life | The shelf life is 2 years when stored in its original packaging under dry, cool conditions, away from direct sunlight. |
In rotational moulding of stationary chemical storage vessels, Versalis Flexirene® MR 50 U is specified as the sole matrix resin because the combination of a 0.934 g/cm³ density (ISO 1183-1:2019) and a 5.0 g/10 min melt flow rate (ISO 1133-1:2022, Method A, 190 °C/2.16 kg) places the melt within the viscosity window required for uniform wall formation on carousel or shuttle machines with biaxial rotation ratios between 4:1 and 6:1. The resin is pulverized to a 35-mesh powder fraction with less than 10% retained on 500 µm screens and dry-blended with 0.5–2.0 wt% of a compatibilized UV/HALS or carbon black masterbatch before charging; loadings above 3.0 wt% have been associated with reduced low-temperature impact and environmental stress crack resistance in 6 mm sections because additive-rich domains act as stress concentrators during post-mould cooling. The processing window is narrow: oven air temperature is maintained at 280–310 °C, peak internal air temperature is held at 190–210 °C for 4–8 min, and the mould surface is cooled at 6–12 °C/min under forced air followed by water mist after the solidification plateau. Cooling rates above 15 °C/min produce differential shrinkage across the tank sidewall and induce warpage at the threaded neck region, while rates below 4 °C/min extend cycle time without improving impact properties. Compliance verification for the finished tank follows ASTM D1998-21 for polyethylene upright storage tanks and UN 31A/Y requirements where the vessel is used as an intermediate bulk container shell; chemical resistance data are generated according to ISO 175:2020 immersion testing. Published data for MR 50 U in direct potable-water contact structures is limited; therefore, NSF/ANSI/CAN 61 certification must be confirmed on the finished vessel rather than assumed from resin datasheet values. Terminal parts produced in this scenario include 100–1,000 L vertical cylindrical dosing tanks, acid and alkali storage vessels for metal finishing lines, and rotationally moulded outer shells for composite intermediate bulk containers.
Stackable pallet tools with 1,200 mm × 1,000 mm projected dimensions process MR 50 U either at 100 wt% or as a 70–90 wt% matrix fraction diluted with closed-loop post-industrial LLDPE regrind; coarser dilution beyond 30 wt% regrind has been observed on production tools to destabilize the filling pattern and create visible knit lines at the fork entries. The melt temperature at the nozzle is set within 210–240 °C; exceeding 260 °C for more than 20 min of residence time causes chain scission and a drop in notched impact strength below the minimum required by ASTM D256-23e1, while temperatures below 200 °C produce unmelted core defects and inconsistent tensile elongation under ASTM D638-14. A three-zone screw with L/D ratio 22:1 and back pressure of 0.3–0.8 MPa is used to control the spread of a 5.0 g/10 min melt across the flow path; the mould is held at 15–40 °C and clamp force is selected to maintain cavity pressure at 35–50 MPa in the gate region. Hold pressure is set at 60–80% of injection pressure for 8–12 s, and cooling time is 20–35 s for a 4–6 kg shot. If powder moisture exceeds 0.05 wt% after storage above 60% RH, drying at 70 °C for 2 h is applied before hopper feed. Compliance for load-bearing use is verified under ISO 8611-1:2021 and ASTM D642-20; tensile and impact data are generated according to ASTM D638-14 and ASTM D256-23e1. Terminal products include stackable pallets, industrial crates, and tote boxes used in distribution centres and automotive parts handling.
For agricultural chemical storage and spray rig reservoirs, the specification typically requires minimum F50 environmental stress crack resistance above 1,000 h under ASTM D1693-15, Method B, 10% Igepal CO-630, because the moulded part is exposed to surfactants, crop-protection formulations, and liquid fertilizer mixtures. MR 50 U is charged at 100 wt% or with 0.5–1.5 wt% carbon black masterbatch for black or dark green tanks; light-coloured reservoirs are produced with 1.0–2.0 wt% hindered amine light stabilizer masterbatch, and loadings above 2.5 wt% are not recommended on thin-walled sprayer tanks because weld-line ductility and low-temperature drop performance decline. The rotational moulding process uses a shuttle machine with a swing diameter up to 2.5 m, oven air temperature of 270–290 °C, peak internal air temperature of 185–200 °C held for 8–12 min, and cooling controlled at 5–10 °C/min until the part surface temperature falls below 80 °C before demoulding. Premature demoulding on slow-cooled thin walls creates internal voids at the baffle bosses and outlet inserts; excessive oven temperature above 300 °C causes surface pitting and gel particles that later act as crack initiation sites. Compliance is verified through ASTM D1693-15 ESCR, ISO 175:2020 chemical resistance, ISO 4892-3:2016 cycle 1 weather exposure, and applicable REACH and RoHS directives for finished articles. Terminal products include 200–1,500 L boom sprayer tanks, induction hoppers, fertigation reservoirs, and pre-mix chemical transfer vessels.
| Application class | Critical standard set | Process boundary | Formulation limit |
|---|---|---|---|
| Rotational moulded chemical storage | ASTM D1998-21; UN 31A/Y; ISO 175:2020 | PIAT 190–210 °C; cooling 6–12 °C/min | masterbatch ≤ 3.0 wt% |
| Injection moulded pallets | ISO 8611-1:2021; ASTM D642-20; ASTM D256-23e1 | melt 210–240 °C; residence ≤ 20 min | regrind ≤ 30 wt% |
| Agricultural sprayer tanks | ASTM D1693-15; ISO 4892-3:2016; ISO 175:2020 | oven 270–290 °C; demould ≤ 80 °C | additive masterbatch ≤ 2.5 wt% |
| Masterbatch carrier | FDA 21 CFR 177.1520; EU 10/2011 | barrel 160–200 °C; specific energy 0.18–0.25 kWh/kg | additive loading 25–40 wt% |
| Playground panels and outdoor furniture | EN 1176-1:2017; EN 71-3:2019+A1:2021; ISO 4892-3:2016 | cooling 4–8 °C/min; PIAT 185–200 °C | surface regrind ≤ 10 wt% |
A 75 mm co-rotating twin-screw compounding line can load MR 50 U as the carrier phase for color, additive, and UV masterbatches intended for polyolefin films, pipes, and rotational mouldings. The 5.0 g/10 min melt flow rate allows pigment and additive loadings between 25 wt% and 40 wt% to be dispersed through a co-rotating twin-screw extruder with L/D ratio 40:1 and specific energy input of 0.18–0.25 kWh/kg while maintaining strand pelletizing line speeds above 800 kg/h. At loadings above 40 wt%, torque excursions on the kneading block section and frequent screen-pack pressure spikes above 5.5 MPa are observed; these conditions generate melt fracture at the die, strand breakage, and uneven pellet geometry. Barrel temperatures are set between 160–200 °C, with the die head held at 180–200 °C and the water bath at 20–40 °C. The carrier resin is not dried unless stored above 60% RH; if moisture exceeds 0.05 wt%, drying at 70 °C for 2 h is required to prevent hydrolysis of moisture-sensitive pigments. For masterbatches intended for food-contact applications, the finished pellet must comply with FDA 21 CFR 177.1520 and EU Regulation 10/2011 migration limits; MR 50 U carries no implicit food-contact approval across all pigment types, so migration testing is performed on the final compound. Terminal products include 40–50 mesh masterbatch pellets supplied to PE film converters, pipe compounders, and rotational moulders.
Where public playground panels, modular seating shells, and outdoor planters are specified for multi-year exterior exposure, MR 50 U is rotationally moulded because the pre-stabilized base resin retains mechanical properties under accelerated weathering regimes described by ISO 4892-3:2016 cycle 1; however, published data for this specific configuration is limited, so finished-article exposure tests should be conducted when warranty terms exceed 5 years. The formulation uses 100 wt% MR 50 U for internally pigmented wall sections or 1.0–2.0 wt% formulated pigment masterbatch for through-coloured parts; post-industrial regrind above 10 wt% is avoided on visible surfaces because it creates flow lines and dull matte patches on textured mould surfaces. Oven air temperature is controlled at 275–295 °C and peak internal air temperature at 185–200 °C for 5–9 min; cooling is ramped at 4–8 °C/min with forced air followed by water mist to balance impact retention and shrinkage. Cooling rates above 12 °C/min create internal shrinkage voids around metal inserts and thick bosses, while cooling below 3 °C/min prolongs demould time without measurable property improvement. Structural panels used in playground equipment are assessed under EN 1176-1:2017, and where the panel is accessible to young children and resembles a toy component, EN 71-3:2019+A1:2021 migration of elements is applied. Terminal parts include rotationally moulded playground roof panels, modular seating shells, planter boxes, and outdoor storage cabinets.
Competitive Versalis Flexirene® MR 50 U Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® MR 50 U is a linear low density polyethylene powder formulated for rotational moulding. The U suffix in the Versalis nomenclature is associated with a UV-stabilised additive package intended for outdoor service, although the exact package should be confirmed from the lot certificate and technical datasheet. Manufacturer-published typical values list a nominal density of 0.940 g/cm³ under ISO 1183-1 and a melt mass-flow rate of 5.0 g/10 min under ISO 1133-1 at 190 °C/2.16 kg. These two base specifications place the grade between general-purpose linear low density polyethylene rotomoulding materials near 0.930 g/cm³ and high-density polyethylene rotomoulding grades near 0.945–0.950 g/cm³. The density is selected to raise flexural modulus and environmental stress crack resistance while retaining sufficient low-temperature ductility for rotationally moulded tanks, agricultural water containers, outdoor furniture, playground components, chemical dosing tanks, and industrial packaging. The grade is supplied as a ground powder because rotational moulding requires fine particle size distribution and dry flow rather than pellet feed.
| Property | Test Method | Unit | Manufacturer-Published Typical Value |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 0.940 |
| Melt mass-flow rate | ISO 1133-1 | g/10 min | 5.0 (190 °C/2.16 kg) |
| Tensile stress at yield | ISO 527-2 | MPa | 18 |
| Tensile elongation at break | ISO 527-2 | % | >400 |
| Flexural modulus | ISO 178 | MPa | 760 |
| Shore D hardness | ISO 868 | — | 61 |
| Vicat softening point | ISO 306 A50 | °C | 116 |
| Brittleness temperature | ASTM D746 | °C | <-70 |
| Environmental stress crack resistance | ASTM D1693 condition B | h | >1,000 |
Process data from multi-arm carousel rotational moulding lines indicate that a melt mass-flow rate of 5.0 g/10 min is high enough to permit sintered powder coalescence and bubble removal at peak internal air temperatures of 190–200 °C, yet low enough to resist sagging and wall thinning on large vertical flat surfaces. The grade is typically processed on biaxial equipment with a rotation ratio near 4:1, where the major-axis speed is held at 8–12 min⁻¹ and the minor-axis speed at 2–3 min⁻¹. Oven air temperature is commonly set between 280 °C and 300 °C, but the controlling variable is not oven temperature alone; peak internal air temperature is the decisive fusion parameter. When peak internal air temperature remains below 180 °C, residual sintered particle boundaries and microvoids persist, producing pinholes at corners and weld line leakage. When peak internal air temperature exceeds 210 °C, the thermo-oxidative stabiliser system is consumed more rapidly, and the accompanying yellowing, inner-surface roughness, and loss of low-temperature impact become observable defects. The practical processing window is therefore narrow, and production lots with higher volatile content or poor powder bulk density can shift the effective fusion point.
Pulverising is performed on counter-rotating disc mills operating below 90 °C to limit agglomeration and oxidative consumption of the stabiliser package. The resulting powder is screened to a nominal top size of 500 µm; commercial rotational moulding powders typically have a median particle size of 200–250 µm. Coarse particles above 600 µm melt slowly and can form surface defects in thin-walled sections, while excessive fines below 100 µm may reduce dry flow and increase dusting during charging. Apparent density is monitored under ISO 60, and dry flow behaviour is assessed under ISO 6186. Moisture absorption by linear polyethylene is below 0.01 % at 23 °C and 50 % relative humidity, so pre-drying is not normally required. Condensation on cold powder during storage or transfer, however, can introduce surface water that produces steam pinholes in the sintered layer. Storage and processing contact with copper or copper-bearing alloys should be avoided because transition metals catalyse hydroperoxide decomposition and accelerate thermo-oxidative degradation.
For structural design of rotationally moulded tanks, the flexural modulus of 760 MPa under ISO 178 provides a measurable increase over conventional 0.930 g/cm³ linear low density polyethylene rotomoulding grades, which typically exhibit flexural modulus values in the 600–650 MPa range. The tensile stress at yield of 18 MPa under ISO 527-2 permits thin-wall sections to withstand hydrostatic loading without gross yielding, while tensile elongation at break above 400 % retains ductility at corners and compounded curvatures. The brittleness temperature below -70 °C under ASTM D746 indicates that the material remains ductile under freeze conditions, but published instrumented impact data for rotationally moulded notched parts manufactured from this specific grade is limited. Acceptance testing of finished tanks should therefore be based on part-level drop-impact and leak testing protocols, such as those required for thermoplastic static tanks under EN 13575 or equivalent producer specifications.
Long-term mechanical design should account for creep and stress relaxation. At 20 °C, linear polyethylene under a constant tensile stress of 6 MPa can exhibit creep strain above 2 % over 1,000 h; the exact creep modulus for MR 50 U should be obtained from manufacturer creep curves rather than inferred from short-term flexural modulus. Environmental stress crack resistance is specified by ASTM D1693 condition B using 100 % Igepal CO-630 at 50 °C, with a typical failure time above 1,000 h. This parameter is critical for tanks holding surfactants, detergents, and agricultural chemicals, where moulded-in stress and chemical contact act simultaneously. The grade should be evaluated with the actual packaged chemical because environmental stress cracking is formulation-specific and cannot be predicted solely from the resin datasheet value.
When MR 50 U is benchmarked against high-density polyethylene rotomoulding grades with density of 0.945–0.950 g/cm³, the HDPE grades often provide higher flexural moduli, commonly in the 900–1,100 MPa range, but their environmental stress crack resistance and low-temperature impact behaviour can be lower. Many HDPE rotomoulding grades show reported environmental stress crack resistance values between 100 h and 500 h under the same ASTM D1693 condition B. The 0.940 g/cm³ density of MR 50 U is therefore a compromise that preserves environmental stress crack resistance above 1,000 h while retaining a flexural modulus of 760 MPa. Compared with a general-purpose 0.930 g/cm³ linear low density polyethylene rotomoulding grade, MR 50 U raises flexural modulus by approximately 150–200 MPa and increases Vicat softening point by roughly 5–8 °C. The trade-off is a modest density increase and a somewhat narrower processing window because the higher crystallinity can increase shrinkage and warpage in thick sections. Published side-by-side moulded part data for this specific comparison is limited, so direct substitution should be qualified on production tooling before changing grades.
The UV-stabiliser package indicated by the U suffix is intended for outdoor exposure. Accelerated weathering under ISO 4892-2 with xenon-arc irradiation is commonly used to screen colour change and embrittlement, but comparative rankings require identical specimen thickness, lamp filters, and exposure protocols. Dark pigmentation increases surface temperature and may shorten service life of the stabiliser system; long-term outdoor applications in high-solar-radiation environments should be validated at the specific wall thickness and pigment loading. Published data for all possible pigment combinations is not available, and lot-specific stabiliser concentration should be verified from the certificate of analysis when outdoor service is critical.
Immersion data for linear polyethylene in aqueous media indicate that MR 50 U is suitable for dilute acids, alkalis, brine, and many polar organic compounds at temperatures up to 40 °C. It is not recommended for continuous exposure to strong oxidising acids, aromatic hydrocarbons, chlorinated solvents, or hydrocarbon fuels without specific barrier or crosslinking modifications. For chemical storage tanks, design wall thickness is governed by hoop stress calculations based on the flexural modulus and by the chemical resistance factor established under EN 13575 or the producer’s engineering manual. No single resin datasheet value replaces part-level chemical immersion testing. Rotational moulding of MR 50 U components should be conducted with adequate ventilation to control volatile degradation products when processing temperatures exceed 230 °C.