Versalis Flexirene Mr 50 A Linear Low Density Polyethylene

Versalis Flexirene® MR 50 A Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® MR 50 A Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 846691
    Product Name Versalis Flexirene® MR 50 A
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Additive Antioxidant
    Density 0.922 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.7 g/10 min
    Melting Point 122 °C
    Vicat Softening Temperature A 50 100 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 600%
    Tensile Modulus 250 MPa
    Flexural Modulus 250 MPa
    Shore D Hardness 50

    As an accredited Versalis Flexirene® MR 50 A Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® MR 50 A Linear Low Density Polyethylene is supplied in 25 kg bags, palletized and securely wrapped.
    Container Loading (20′ FCL) 20′ FCL container loading: Versalis Flexirene® MR 50 A LLDPE, 25 kg bags, palletized, stretch-wrapped, securely stowed for safe transport.
    Shipping Versalis Flexirene® MR 50 A Linear Low Density Polyethylene is shipped as non-hazardous pellets in 25 kg bags, big bags, or bulk. Transport in clean, dry, covered vehicles/containers, away from moisture, heat, and sunlight. No dangerous goods labeling; observe SDS and local rules.
    Storage Store Versalis Flexirene® MR 50 A Linear Low Density Polyethylene indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers or bags closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and static buildup. Follow local regulations and the manufacturer’s SDS.
    Shelf Life Shelf life is typically 24 months from production when stored unopened in original packaging, dry, away from direct sunlight.
    Application of Versalis Flexirene® MR 50 A Linear Low Density Polyethylene

    Which Rotational Moulding Variables Preserve Wall Thickness in Vertical Water Storage Tanks?

    Vertical water storage tanks are rotationally moulded from Flexirene MR 50 A powder at charge weights derived from target shell thicknesses of 6–10 mm for potable and utility water service; the published density of 0.935 g/cm³ (ISO 1183-1) and melt flow rate of 5.0 g/10 min (ISO 1133-1, 190 °C, 2.16 kg) determine the charge-volume relationship, and the powder is ground to a nominal top size of 35 mesh (500 µm) to prevent inconsistent melt-out on vertical walls. Wall-thickness preservation in this segment is controlled less by the resin than by the biaxial rotational ratio of 4:1 to 8:1 on a single-arm shuttle machine and by the peak internal air temperature, which is held between 200 °C and 210 °C for a 10 mm shell; exceeding 230 °C produces thermo-oxidative yellowing and a measurable decline in tensile elongation at break under ISO 527-2. A four-arm carousel architecture with independent spindle-speed control per station is preferred when oven and cooling stations must be tuned separately; production-scale plants frequently instrument the internal air profile with Rotolog infrared telemetry to confirm full powder coalescence before cooling initiates. Compliance is anchored to NSF/ANSI 61 for North American drinking-water contact, BS 6920-1 for UK water fittings, and AS/NZS 4020 for Australian potable service, each of which restricts the formulation space to unpigmented natural resin or a limited palette of approved pigment masterbatches; when colour is required, a water-grade masterbatch is loaded at 1.5–2.0 wt%, and when the tank will stand outdoors, a hindered amine light stabiliser masterbatch is added at 0.20–0.30 wt% to suppress ultraviolet embrittlement without violating extraction limits. The downstream production sequence for a 10 000 L cylindrical tank includes a 25–35 min hot-air oven residence at a set point of 270–290 °C, slow forced-air cooling to below 80 °C before demoulding, and on thick-walled vessels a post-mould annealing segment at 100–110 °C for 15–20 min to relax residual thermal stress; failure modes observed on production-scale equipment include under-melted corners from insufficient rotational ratio, concave sidewall deflection from premature demoulding, and environmental stress crack propagation at the lower knuckle when fast water-quench cooling is substituted for slow air cooling. Terminal products in this segment are vertical cylindrical water tanks from 500 L to 30 000 L, sectional panel tanks, and loft-mounted municipal storage units.

    When Fertiliser Concentrate Exceeds 1000 Hours of Environmental Stress Crack Resistance

    When agricultural sprayer and crop-protection product tanks enter service with liquid fertiliser formulations containing ammonium nitrate, urea, and surfactant packages, the plastic shell must demonstrate environmental stress crack resistance beyond 1000 h under ASTM D1693-21 testing in 100% Igepal CO-630 at 50 °C, a requirement that drives the selection of a 0.935 g/cm³ butene-copolymer LLDPE such as Flexirene MR 50 A rather than a homopolymer; the relatively lower crystal density compared with HDPE provides the tie-molecule population needed to arrest slow crack growth at sump radii and baffle attachment points. Agricultural tank formulators depart from water-tank practice in that a carbon black masterbatch is loaded at 1.5–2.5 wt% and a high-molecular-weight hindered amine light stabiliser package at 0.30–0.50 wt%, with a benzotriazole UV absorber at 0.10–0.20 wt% for field exposure in southern latitudes; these loadings are selected so that the tank wall retains at least 80% of its initial tensile yield strength after 2000 h of accelerated weathering under ASTM G154-23 UVA-340 lamps. The downstream production process for long horizontal tanks between 600 L and 1500 L favours a rock-and-roll machine, in which the mould rotates continuously through 360° on its long axis while rocking through ±30° on the transverse axis, and the peak internal air temperature is held between 210 °C and 220 °C for a 35–45 min oven cycle because the thicker sump sections must fuse without overheating the upper sidewalls; integrally moulded brass or stainless steel threaded inserts for drain fittings and level sensors are loaded into the tool prior to charging and require slow air cooling at 1–2 °C/min to prevent micro-void formation around the metal insert as the polymer crystallises. The crop-protection sector is regulated by ISO 16119-1:2013 and ISO 16119-2:2013 for environmental and performance requirements on sprayers, and chemical compatibility of the shell with active ingredients is screened by immersion testing under ASTM D543-21 for representative solvents and surfactant concentrates. Terminal products include tractor-mounted and trailed sprayer tanks, front-loading sump reservoirs, and pesticide induction hoppers.

    Sit-on-top kayak hulls with a nominal wall section of 7 mm are produced in a single-shot rotomoulding cycle during which the Flexirene MR 50 A powder is subjected to a peak internal air temperature of 205–215 °C inside a cast-aluminium mould mounted on a two-arm shuttle machine, and the hull is cooled in a forced-air chamber at 0.5–1.0 °C/min before demoulding at 80 °C to prevent dimensional deviation from the mould centreline. The marine leisure segment imposes a different additive schedule from land-based moulding: a hindered amine light stabiliser masterbatch is increased to 0.40–0.60 wt% and a benzotriazole UV absorber to 0.10–0.20 wt%, with a finely dispersed pigment masterbatch at 2.0–4.0 wt% for colour retention under saltwater immersion and high-latitude sunlight; these loadings are validated by xenon-arc exposure under ISO 4892-2:2013 with gloss retention specified at ≥ 80% after 1500 h and by tensile property retention tests under ISO 527-2. Compliance for recreational craft is framed by ISO 12217-1:2015 for stability and buoyancy of non-sailing craft of hull length below 6 m, while the material itself is assessed against ISO 1183-1, ISO 1133-1, and ASTM D1693-21 as a basis for design; European market acceptance additionally follows the Essential Requirements of Directive 2013/53/EU for recreational craft and personal watercraft, with conformity assessed by a notified body rather than by the resin supplier. The production process differs from industrial tank moulding in that the mould halves must provide vacuum venting of the melt path at the hull bow and stern, and the rotation ratio is often increased to 8:1 to maintain thickness at the sharp chine radii where melt-flow thinning occurs; specific failure modes known from production-scale marine moulding include pinhole leakage at skeg boxes and gas porosity at foam-filled seat inserts when moisture remains trapped in the mould cavity. Terminal product types in this segment are sit-on-top kayaks, rotomoulded dinghy hulls, stand-up paddleboard skins, marina fenders, and navigation buoy shells.

    Table 1 consolidates the compliance frameworks and specification criteria that distinguish the six application segments.

    Application segmentGoverning compliance frameworkCore test method designationTypical specification criterion
    Vertical water storageNSF/ANSI 61, BS 6920-1, AS/NZS 4020ISO 527-2 tensile elongationWall 6–10 mm, PIAT 200–210 °C
    Agricultural sprayer tanksISO 16119-1:2013, ISO 16119-2:2013ASTM D543-21 immersion, ASTM D1693-21ESCR > 1000 h, HALS 0.30–0.50 wt%
    Marine leisure craftDirective 2013/53/EU, ISO 12217-1:2015ISO 4892-2:2013 xenon arcGloss retention ≥ 80% after 1500 h
    Off-highway diesel cellsOEM-specific protocols; no unified product standardASTM D543-21, ASTM D1693-21Mass uptake < 3%, ESCR > 1000 h
    Returnable bulk containersEU 10/2011, FDA 21 CFR 177.1520Overall migration limitOML 10 mg/dm², regrind ≤ 30 wt%
    Playground and street furnitureEN 1176-1:2017ASTM G154-23Pigment/HALS MB 2.0–4.0 wt%

    Carbon Black Dispersion Governs Long-Term UV Retention in Diesel Cell Walls

    Off-highway and stationary-engine diesel day tanks are rotationally moulded from Flexirene MR 50 A in wall thicknesses of 8–10 mm because the tank shell must remain dimensionally stable under continuous exposure to diesel fuel at 40–60 °C and under exterior ultraviolet radiation on generator-set installations; published regulatory mapping for rotomoulded polyethylene diesel reservoirs is fragmented, so OEM specifications frequently substitute material qualification protocols based on ASTM D543-21 for chemical immersion and ASTM D1693-21 for stress crack resistance, with a minimum ESCR of 1000 h in 100% Igepal CO-630 at 50 °C. The formulation addition ratio in this segment is constrained by the requirement for long-term heat ageing rather than by food-contact limits: a carbon black masterbatch is loaded at 1.0–2.0 wt% to screen ultraviolet radiation, a phenolic/phosphite antioxidant blend at 0.10–0.20 wt% to extend oxidative induction time, and a hindered amine light stabiliser package at 0.20–0.30 wt%; published data for the specific oxidative induction time shift produced by these loadings in this resin configuration is limited, so batch-specific differential scanning calorimetry under ISO 11357-6:2018 is required before part release. The downstream production process uses a biaxial carousel or shuttle machine with a peak internal air temperature window of 205–210 °C, a 35–45 min oven cycle for the thicker shells, and slow air cooling at 0.5–1.0 °C/min rather than direct water spray because rapid crystallisation produces shrinkage voids around integrally moulded brass fuel fittings and sender flanges; on production-scale equipment, failure modes include under-cured weld seams at the baffle root, pinholing at the return-line boss when the mould rotation ratio falls below 4:1, and oil-canning on wide flat side panels when demoulding occurs above 80 °C. Terminal products in this segment are diesel day tanks of 50–500 L, hydraulic oil reservoirs of 20–200 L for compact construction equipment, and aqueous urea (AdBlue) tanks of 10–100 L.

    Table 2 records the formulation gradient across the six segments as the additive and regrind loadings are altered to meet the governing specification criterion.

    SegmentAdditive or regrind streamLoading rangePrimary process consequence
    Water storageHindered amine light stabiliser masterbatch0.20–0.30 wt%Ultraviolet retention without extraction-limit increase
    AgricultureCarbon black masterbatch1.5–2.5 wt%UV screening and long-term stress crack retention
    MarineHALS plus benzotriazole UV absorber0.40–0.60 wt% + 0.10–0.20 wt%Gloss retention under saltwater xenon exposure
    Diesel cellsPhenolic/phosphite antioxidant blend0.10–0.20 wt%Oxidative induction time extension
    Bulk containersClosed-loop regrind20–30 wt%Recycled content without low-temperature impact loss
    PlaygroundPre-dispersed pigment/HALS masterbatch2.0–4.0 wt%Weathering and colour retention on moulded surfaces

    Returnable Bulk Container Moulding with 30% Regrind Streams

    Returnable bulk containers and insulated fish bins are rotationally moulded from Flexirene MR 50 A at nominal wall thicknesses of 6–10 mm using a shuttle-machine process in which the peak internal air temperature is maintained at 200–210 °C and the oven set point at 260–280 °C for a 25–35 min cycle; food-contact configurations are governed by EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for aqueous and fatty simulants, and by FDA 21 CFR 177.1520 for olefin polymers in contact with food, where the resin must meet the density and melt flow specification of the clearance. The formulation addition ratio in this segment differs from tank and marine moulding because closed-loop regrind is routinely substituted for virgin powder at 20–30 wt% when the finished bin is not intended for direct food contact, and a food-grade pigment masterbatch at 1.0–2.0 wt% is used for colour identification of seafood species; antistatic additive masterbatches are occasionally incorporated at 0.5–1.0 wt% to reduce dust adhesion on dry-goods bins in packaging cleanrooms. The downstream production process for double-wall insulated fish boxes includes rotomoulding of the inner and outer shells as separate cycles followed by injection of polyurethane foam between the skins, and the shell must cool below 80 °C before demoulding to prevent foam-sidewall delamination; for single-wall bulk containers, the tool is a fabricated aluminium box into which a 4:1 biaxial rotation ratio is applied, and failure modes on production lines include warped base corners from excess charge weight and pinholing at drain plug bosses when the mould release agent is applied unevenly. Terminal products in this segment are insulated fish boxes of 20–100 L, returnable pallet boxes of 600–1000 L, and dry-bulk material bins.

    Where municipal park benches, picnic tables, and playground climbing panels are rotomoulded from a 0.935 g/cm³ butene-copolymer LLDPE, the governing standards are EN 1176-1:2017 for playground equipment safety and ASTM G154-23 for accelerated weathering of the pigmented shell; the formulation addition ratio for ultraviolet resistance comprises a pre-dispersed pigment masterbatch at 2.0–4.0 wt% combined with a hindered amine light stabiliser at 0.30–0.50 wt%, and the production sequence involves a carousel-machine rotomoulding cycle with a 5–8 mm wall, a peak internal air temperature of 200–210 °C, and demoulding after slow air cooling below 80 °C; terminal product types include rotomoulded slides, climbing panels, spring-rider bodies, bench slats, and bollard covers.

    Free Quote

    Competitive Versalis Flexirene® MR 50 A Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene MR 50 A Linear Low Density Polyethylene is a medium-flow rotational-moulding grade supplied in pulverized form with a nominal density of 0.935 g/cm³ and a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg measured in accordance with ISO 1133-1:2022. The polymer architecture is based on a linear ethylene backbone carrying short-chain branches introduced by alpha-olefin incorporation. That structural arrangement is distinct from high-pressure low density polyethylene, which contains long-chain branching and a more highly branched backbone. The grade is formulated with an antioxidant package; ultraviolet stabilization is not implied by the “A” suffix and must be confirmed separately if the part is intended for prolonged outdoor exposure. Typical rotational-moulding uses include storage tanks, containers, ducting, agricultural components, and outdoor parts with nominal wall thicknesses between 3 mm and 10 mm.

    Material property verification should be performed according to ISO 1183-1:2019 for density, ISO 527-2:2012 for tensile properties, ISO 178:2019 for flexural modulus, ISO 306:2013 for Vicat softening temperature, ISO 868:2003 for Shore hardness, ASTM D746 for brittleness temperature, and ASTM D1693 for environmental stress crack resistance. Because the product is delivered as a rotomoulding powder, particle size distribution and dry-flow behaviour are controlled by downstream pulverization rather than directly by the reactor granulation step.

    Material Identity and Specification Boundary

    The grade is classifiable as a linear low density polyethylene with a density inside the 0.930–0.940 g/cm³ band. The melt flow rate of 5.0 g/10 min places it in the medium-flow rotomoulding range, where low-shear coalescence and long oven cycles dominate. The supplier technical data sheet provides typical properties, not batch release limits. Processors should compare the certificate of analysis for each lot against the following typical value set and verify that density and melt flow rate tolerances do not alter part weight or demoulding behaviour.

    PropertyTest methodTypical value
    Melt flow rate at 190 °C / 2.16 kgISO 1133-1:20225.0 g/10 min
    DensityISO 1183-1:20190.935 g/cm³
    Tensile stress at yieldISO 527-2:201218.0 MPa
    Tensile elongation at breakISO 527-2:2012>400 %
    Flexural modulusISO 178:2019750 MPa
    Vicat softening temperature, A50ISO 306:2013118 °C
    Brittleness temperatureASTM D746-70 °C
    Shore D hardnessISO 868:200360
    Environmental stress crack resistance, F50ASTM D1693>1000 h

    Density variation of ±0.002 g/cm³ and melt flow rate variation of ±0.5 g/10 min between lots can shift flexural modulus, impact response, and cycle time. The tensile yield value of 18.0 MPa and elongation at break above 400 % indicate a ductile short-term response under standard tensile testing conditions. The brittleness temperature of -70 °C is relevant to demoulding and low-temperature service, but it does not replace full part testing under dynamic loading.

    In carousel rotational moulding lines, powder dry-flow consistency determines shot weight accuracy and uniform wall thickness. Bulk density and particle size distribution should be monitored after pulverization. A 35-mesh screen cut corresponds to a nominal opening of 500 µm; retention of oversize particles above this size can produce surface blemishes, while excessive fines below 200 mesh can reduce dry-flow reproducibility. Moisture on the powder surface can generate pinholes during sintering, so stored powder should be kept above the moulding bay dew point or dried if condensation is observed.

    What Distinguishes Flexirene MR 50 A from High-Pressure LDPE in Rotational Moulding?

    High-pressure LDPE carries long-chain branching, which lowers crystallinity, modulus, and melting peak temperature while improving melt extensibility. Flexirene MR 50 A is a linear low density polyethylene with short-chain branching, so at equivalent density it develops higher tensile yield strength, higher flexural modulus, and higher environmental stress crack resistance than a typical LDPE rotomoulding grade. Comparative tensile yield data for high-pressure LDPE rotomoulding resins frequently fall between 12 MPa and 14 MPa under ISO 527-2:2012, whereas MR 50 A exhibits a typical value of 18.0 MPa. The absence of long-chain branching also means lower shear-thinning and less melt extensional strain hardening; the LLDPE therefore requires a higher peak internal air temperature to complete bubble dissolution and densification.

    The higher melt flow rate of 5.0 g/10 min improves sintering and replication of fine mould texture compared with lower-flow rotomoulding grades, but it can increase warpage in asymmetric parts when cooling is non-uniform. Processors replacing an LDPE grade with MR 50 A should anticipate a higher oven setpoint or a longer heat cycle and should measure peak internal air temperature rather than relying on oven temperature alone. The increased stiffness and ESCR generally allow a nominal wall thickness reduction in tanks and containers, but only if the part design and loading conditions are revalidated.

    For structural design calculations, the flexural modulus of 750 MPa provides a basis for load-deflection estimates in flat panels and storage bins. Short-term tensile data are not sufficient for long-term creep prediction. Creep modulus, tensile creep rupture, and chemical-exposure data for the specific moulded part geometry are not provided in the grade data sheet; published data for this specific configuration is limited, so long-term load-bearing designs should be confirmed through prototype testing under service conditions.

    When Oven Temperature Exceeds 290 °C for More Than 25 Minutes

    The rotational moulding oven setpoint is not equivalent to the melt temperature. When a mould surface remains above 290 °C for more than 25 minutes, thermo-oxidative degradation risk increases in the inner surface layer. Degradation can appear as yellowing, pinhole formation, loss of environmental stress crack resistance, or a reduction in tensile elongation at break. For Flexirene MR 50 A, the maximum recommended peak internal air temperature is 220 °C. Exceeding this value accelerates consumption of the antioxidant package and can generate volatile carbonyl species. Processors should monitor both mould surface temperature by infrared pyrometry and internal cavity air temperature by thermocouple.

    A controlled heating cycle should maintain the peak internal air temperature for 8–12 minutes to complete sintering and densification. Extended holding beyond that window does not improve mechanical properties and increases the risk of thermo-oxidative failure. Cooling rate influences crystallinity, shrinkage, and warpage. Forced-air cooling followed by water mist reduces cycle time but can increase residual stress in thick sections. Air cooling to below 100 °C before demoulding is recommended to reduce post-demoulding deformation. In heated-tool moulding, mould release should be confirmed with the mould release agent supplier; silicone-based release agents can interfere with post-mould painting and adhesion.

    Compared with high-density polyethylene rotomoulding resins having densities above 0.940 g/cm³, Flexirene MR 50 A at 0.935 g/cm³ provides lower flexural modulus and higher elongation at break, reducing brittle failure at sharp corners but lowering top-load stiffness. Compared with lower-melt-flow LLDPE grades, the 5.0 g/10 min melt flow rate permits shorter oven residence time but may sacrifice some ESCR and impact strength. The grade is not intended for high-shear processes such as injection moulding or blown film extrusion; no processing data are supplied for those configurations.

    Regulatory status is lot-specific. The base olefin polymer falls within 21 CFR 177.1520(c) and may be used in food-contact articles subject to conditions of use and additive limitations specified in that section. Compliance with Commission Regulation (EU) No 10/2011 and REACH substance-of-very-high-concern reporting must be verified against the current supplier declaration. No statement in this introduction substitutes for a grade-specific food-contact certificate, migration test report, or lot-level declaration from the resin supplier.