| HS Code | 871470 |
| Product Name | Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.930 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 350 MPa |
| Shore D Hardness | 55 |
| Film Haze | 12% |
| Film Gloss 45 | 50% |
| Dart Impact Strength | 120 g |
As an accredited Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® FG 30 U Butene Copolymer LLDPE is supplied in 25 kg bags, palletized and shrink-wrapped for transport. |
| Container Loading (20′ FCL) | Versalis Flexirene® FG 30 U butene copolymer LLDPE in 20′ FCL: 25 kg bags, palletized, approximately 20–22 MT, subject to weight limits. |
| Shipping | Versalis Flexirene® FG 30 U is a non-hazardous, solid LLDPE copolymer. It is not regulated for transport, with no UN number, hazard class, or packing group. Ship in moisture-resistant bags, octabins, or bulk containers. Keep cool, dry, and protected from UV, heat, and contamination. Use normal industrial hygiene. |
| Storage | Store in original, closed packaging in a cool, dry, well-ventilated warehouse below 50°C, away from direct sunlight, heat, flames, and strong oxidizers. Keep pallets off the floor to prevent moisture and contamination. Maintain good housekeeping to avoid dust accumulation, and use first-in, first-out stock rotation. Ensure bags remain sealed; avoid UV exposure and ignition sources. |
| Shelf Life | Shelf life is typically 24 months from production when stored unopened in a dry, cool place, away from direct sunlight. |
In heavy-duty sack production for filled goods in the 15–60 kg range, Versalis Flexirene® FG 30 U is converted on grooved-feed blown-film extruders with screw L/D ratios of 25:1–30:1, die gaps of 2.0–2.6 mm, and blow-up ratios between 2.8:1 and 3.5:1. With a nominal density of 0.918 g/cm³ and a melt flow rate of 0.30 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022, the grade produces a bubble with sufficient melt strength for low-neck-height, high-output film lines. Melt temperature at the die lip is held at 190–215 °C; at die lip temperatures below 190 °C, production lines exhibit melt pressure variation greater than ±8 bar across the die circumference, while residence times above 20 min at temperatures exceeding 220 °C accelerate antioxidant consumption and generate oxidised gel formation, visible as fisheye defects in the finished web. The formulation for a 120–200 μm sack film is 80–100 wt% FG 30 U, 0–20 wt% recompounded butene LLDPE post-industrial recyclate, 400–800 ppm erucamide slip, 1000–2500 ppm synthetic silica antiblock, and 300–800 ppm of a phenolic/phosphite process stabiliser blend. Pre-drying is not normally required for pellet stored below 60% relative humidity, but condensation on cold pellet surfaces is removed by drying at 70 °C for 2 h. Tensile properties are verified according to ISO 527-3, tear propagation by ISO 6383-2, and dart impact by ASTM D1709 Method A. Packaging waste matrix compliance is assessed under EU Directive 94/62/EC, Article 11 concentration limits for lead, cadmium, mercury, and hexavalent chromium with a combined limit of 100 mg/kg, while polymer registration obligations are covered under REACH Regulation (EC) No 1907/2006. Finished goods from this conversion route are heavy-duty sacks for polymer pellets, mineral fillers, granular fertilizers, and construction debris.
Agricultural film production using FG 30 U is structured as a three-layer A/B/A coextrusion on IBC blown-film lines with die diameters of 250–400 mm, die gap 1.8–2.4 mm, and blow-up ratio 2.0:1–3.0:1. The core layer comprises 80–90 wt% FG 30 U and 10–20 wt% high-pressure LDPE to stabilise the bubble at lower melt strength; the two skin layers contain 0.3–0.8 phr of a polymeric hindered amine light stabiliser and 0.1–0.3 phr of a benzotriazole UV absorber, dispersed via a 30–40% carrier masterbatch metered at the throat. Direct dry blending of HALS powder into the hopper without a masterbatch produces additive agglomeration and uneven UV protection, which appears under solar exposure as localised cracking after approximately 18 months in southern European irradiation regimes; accelerated weathering is monitored under ISO 4892-2 with UVA-340 lamps. The film is extruded at melt temperatures of 185–205 °C, with frost line height held at 6–8 die diameters and a thickness of 150–250 μm. Agricultural-use conformity is assessed under EN 13206:2017 for thermoplastic agricultural and horticultural films, including mechanical resistance and weathering classes; food contact is not relevant for silage covers. Finished product types include silage covers, round bale underfilm, and greenhouse side-sheet film.
For frozen food packaging lines operating at sealing bar temperatures of 115–135 °C and dwell times below 0.8 s, FG 30 U is processed as the sealant layer in a three-layer coextruded blown film with total thickness 45–80 μm. The sealant layer formulation is 70–90 wt% FG 30 U, 10–20 wt% high-pressure LDPE, 500–1000 ppm erucamide slip, and 1200–2500 ppm zeolite or silica antiblock; the inclusion of LDPE lowers the hot-tack initiation temperature by 5–10 °C and widens the seal plateau, which is required for vertical form-fill-seal operation at line speeds above 25 m/min. The film is blown with a die gap of 1.4–1.8 mm, blow-up ratio 2.2:1–3.0:1, and melt temperature 190–220 °C; the frost line is set higher than for heavy-duty film to suppress excessive crystalline orientation, because orientation-driven free shrink during deep-freeze storage at −30 °C causes bag curl and seal area distortion. Direct food contact compliance is established under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011, with the overall migration limit of 10 mg/dm² verified under food simulant conditions specified in the regulation. Seal strength is measured by ASTM F88/F88M and film tear by ISO 6383-2. Finished product types include IQF vegetable bags, frozen potato pouches, seafood bags, and ice cube packaging.
| Application | Primary regulation or standard | Mechanical or migration test method |
|---|---|---|
| Heavy-duty industrial sacks | EU Directive 94/62/EC; REACH Regulation (EC) No 1907/2006 | ISO 527-3, ISO 6383-2, ASTM D1709 |
| Agricultural silage covers | EN 13206:2017 | ISO 4892-2, ISO 6383-2 |
| Frozen food packaging | FDA 21 CFR 177.1520; EU Regulation (EU) No 10/2011 | ASTM F88/F88M, ISO 6383-2 |
| Laminated stand-up pouch sealant layer | FDA 21 CFR 177.1520; EU Regulation (EU) No 10/2011 | ASTM F88/F88M, ISO 527-3 |
| Non-food can liners with PCR | REACH Regulation (EC) No 1907/2006; EU Directive 94/62/EC | ISO 6383-2, ISO 527-3 |
| Under-slab vapour barrier membranes | EN 13984:2013 | ASTM E96/E96M, ASTM D6241, ISO 527-3 |
Heat-seal integrity in laminated stand-up pouches produced at seal bar pressures of 2.5–4.0 bar and temperatures of 125–145 °C depends on the short-chain branch distribution and molecular weight of the butene copolymer. FG 30 U is coextruded as an inner sealant layer at 20–35% of total film thickness, with the total film between 70 μm and 120 μm; the outer web is typically metallised polyethylene terephthalate, biaxially oriented polyamide, or a paper-based laminate. The sealant layer formulation is 60–85 wt% FG 30 U and 15–40 wt% LDPE, with 400–900 ppm synthetic silica antiblock; slip agent is deliberately omitted from the formulation because migration of the slip additive to the seal surface after corona treatment can depress wetting tension below 38 mN/m and create lamination peel failures. Production is carried out on five-layer IBC blown-film lines with die gap 1.2–1.6 mm, blow-up ratio 1.8:1–2.5:1, and melt temperature 200–225 °C; the air ring is chilled to 15–20 °C to control surface cooling rate and heat-seal layer clarity. If the melt is held above 230 °C for longer than 20 min, oxygenated gel formation and die-lip drool increase, requiring an 8 h purge interval on continuous lines. Packaging compliance for dry and pet food contact is covered under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011; seal initiation, peel resistance, and tensile properties are tested under ASTM F88/F88M and ISO 527-3. Finished products include stand-up pouches for dry foods, resealable pet food pouches, bag-in-box inner films, and laminated film for confectionery wrapping.
Post-consumer PE recyclate incorporation at 20–40 wt% with FG 30 U is confined to non-food contact refuse sacks and industrial can liners because the recyclate stream cannot guarantee compliance with food contact migration limits. The formulation is 60–80 wt% FG 30 U, 20–40 wt% washed PE PCR, 0.1–0.2 wt% process stabiliser replenishment, 500–1000 ppm slip, and 1500–3000 ppm antiblock; batch-to-batch variance in the recyclate is controlled by limiting residual polypropylene contamination to less than 2 wt%, because PP inclusions above 60 μm form gel-like defects at the collapsing frame and increase film splits. The material is extruded on a grooved-feed single-screw extruder with L/D 25:1–30:1, a screen pack of 100/150/250 mesh, die gap 2.0–2.5 mm, barrel temperatures 180–210 °C, and head pressure maintained below 320 bar to restrain shear heating and odour generation from recycled fractions. Blown film is produced at a blow-up ratio of 2.5:1–3.5:1 and thickness of 25–60 μm; on high-output lines above 200 kg/h, an automatic screen changer is required because pressure build-up from melt filtration shortens filter life to 4–6 h when post-consumer contamination is high. Non-food packaging compliance is assessed under REACH Regulation (EC) No 1907/2006, EU Directive 94/62/EC heavy metal limits of 100 mg/kg combined, and US state toxics in packaging regulations. Mechanical performance is monitored by ISO 6383-2 tear resistance and ISO 527-3 tensile strength. Finished product types are refuse sacks, industrial can liners, construction debris bags, and retail carry-out bags.
Under-slab vapour barrier extrusion with FG 30 U requires cross-web thickness variation below ±10% over widths of 3–6 m, because local thinning reduces water vapour resistance and raises puncture risk during aggregate placement. The film is produced on a three-layer blown-film line with die gap 2.2–2.6 mm, blow-up ratio 2.0:1–2.8:1, melt temperature 190–215 °C, and thickness 200–400 μm; the formulation is 90–100 wt% FG 30 U, 0–10 wt% LDPE, and 2–4 wt% carbon black masterbatch for UV protection and opacity. Bubble stability is controlled with internal bubble cooling and a stabilisation cage; die lip temperature uniformity must be held within ±3 °C, as thermal scans from operating lines show that deviations above 5 °C at the edge zones produce edge bead thickness variation up to 18%. Water vapour transmission is evaluated according to ASTM E96/E96M, puncture resistance by ASTM D6241, and tensile properties by ISO 527-3; published data for this specific configuration is limited above 300 μm thickness. Compliance for construction vapour control layers is established under EN 13984:2013 for flexible sheets for waterproofing and vapour control layers, and the product is CE marked under this harmonised standard. Finished product types are under-slab vapour barriers, crawl space membranes, wall vapour retarders, and temporary weather protection sheeting.
Competitive Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® FG 30 U is a butene copolymer linear low density polyethylene supplied by Versalis S.p.A. for blown film extrusion. The grade is defined by two nominal physical properties: a melt mass-flow rate of 0.30 g/10 min determined at 190 °C and 2.16 kg in accordance with ISO 1133-1, and a density of 0.918 g/cm³ determined in accordance with ISO 1183-1. Those values place the material in the high-melt-strength segment of the LLDPE film range, where the resin is used to produce monolayer and multi-layer blown films requiring a combination of bubble stability, puncture resistance, and controlled heat-seal performance.
The product is manufactured by gas-phase polymerisation of ethylene with 1-butene comonomer. The butene comonomer introduces ethyl short-chain branches along an otherwise linear backbone. Those branches reduce crystallite thickness and disrupt lamellar packing, lowering density to the 0.918 g/cm³ band without the long-chain branching characteristic of high-pressure low-density polyethylene. The grade is supplied as cylindrical pellets containing antioxidant and processing stabiliser additives for thermal protection during extrusion.
The “U” suffix identifies a film-grade formulation within the Flexirene family; the “30” indicates the nominal melt flow rate class. Because the base polymer is non-hygroscopic, pre-drying is not normally required. Surface condensation on pellets moved from cold storage into a humid plant can be corrected by a 80 °C desiccant-air hopper dryer for 2 h before the feed throat. Regrind from edge trim and start-up film may be dry-blended into the feed stream, but the proportion should remain constant to limit variability in bubble pressure and film gauge.
Typical end-use applications include heavy-duty sacks, industrial liners, carrier bags, agricultural greenhouse and tunnel films, frozen-food packaging, mulch films, and coextruded sealant webs. In those applications, the grade is selected for its low melt index, which contributes to puncture and tear resistance at thin gauge, and for its density, which retains flexibility at low outdoor temperatures without requiring plasticiser addition.
On a single-screw extruder with an L/D ratio of 24:1 to 30:1, FG 30 U develops higher die pressure at a given throughput than a 1.0 g/10 min LLDPE of similar density. The pressure differential is magnified in narrow spiral mandrel dies with die gaps of 0.8 mm to 1.2 mm. Barrel set-points are typically set between 190 °C and 230 °C at the adapter and die, with the first barrel zone maintained below 180 °C to support solids conveying. Screw configurations with a barrier flight and a Maddock mixing section are preferred because they provide the shear required to homogenise the broad molecular weight distribution without generating excessive melt temperature. Operators should monitor melt temperature directly at the die; increasing barrel temperature to compensate for high pre-die pressure can accelerate oxidation of the stabiliser package if melt temperature exceeds 240 °C for extended residence time.
The flow behaviour of FG 30 U is shear-thinning but less so than high-pressure LDPE at equivalent melt index. The resin does not exhibit a Newtonian plateau in the shear-rate range encountered in film extrusion. This has consequences for die design: a spiral mandrel die with a shallow spiral angle and long lands maintains layer uniformity at higher throughput. The low melt index also increases the residence-time distribution in the die as a function of local flow-channel depth, which can lead to stagnation in certain die geometries if the purge procedure is inadequate.
The use of 1-butene rather than 1-hexene or 1-octene has a measurable effect on solid-state mechanical properties. At equivalent density, the ethyl branches of FG 30 U are shorter than the butyl and hexyl branches of C6 and C8 copolymers. Shorter branches reduce the probability of effective tie-molecule formation between adjacent lamellae, which lowers dart drop impact and Elmendorf tear strength relative to hexene or octene LLDPE of the same 0.918 g/cm³ density and 0.30 g/10 min melt flow rate. The same structural feature lowers the seal initiation temperature and broadens the sealing window when compared with higher alpha-olefin grades. Published data for this specific grade’s hot-tack curve is limited; converters should verify seal strength on the target film structure using ASTM F88 and hot-tack using ASTM F1921, because seal-bar design, dwell time, and coextruded skin thickness modify the result more than the base resin alone.
Compared with metallocene C4 LLDPE of the same density, FG 30 U has a broader molecular weight distribution and broader comonomer distribution. This reduces extrusion amperage and improves melt-fracture tolerance, but it can increase haze and lower dart drop impact. The broad composition distribution means that a small fraction of chains with low comonomer incorporation melt at higher temperature; these may form visible gel particles in thin films if the melt temperature is not high enough or if the screw fails to disperse the high-molecular-weight fraction adequately.
Compared with high-pressure LDPE of the same density, FG 30 U has a predominantly linear backbone and therefore lower extensional melt strength and less strain-hardening response. On a high-stalk blown film line, the frost-line height and internal bubble pressure must be rebalanced to avoid a narrow processing window. LDPE is often coextruded or dry-blended with FG 30 U to improve bubble stability; the addition level is commonly between 5 wt% and 20 wt% depending on die diameter and film gauge, because higher levels reduce tear strength and increase haze. This blending practice is one of the most common process modifications when a C4 LLDPE replaces a C6 or C8 LLDPE in an existing film formulation.
In a three-layer coextruded film where the sealant layer is changed from a hexene or octene LLDPE to FG 30 U, the heat-seal initiation temperature generally decreases because the shorter branch length reduces lamellar thickness. The DSC melting peak measured under ISO 11357-3 is commonly close to 122 °C for a 0.918 g/cm³ C4 LLDPE. The seal plateau may narrow, and hot-tack strength at 0.5 s dwell may be lower because tie-molecule formation is less effective. The shift can be offset by increasing the sealant layer thickness by 10% to 15%, reducing packaging line speed, or blending with 10 wt% to 20 wt% of a higher-alpha-olefin LLDPE. Final seal performance must be verified on the packaging machine because package cooling time and contamination at the heat-seal jaw affect hot-tack more than the DSC melting point alone.
Typical blown film extrusion trials on this grade use a die diameter of 100 mm to 300 mm, a die gap of 0.8 mm to 2.0 mm, and a blow-up ratio of 2.0:1 to 3.0:1. The frost-line height is set to maintain a bubble neck height of 5 to 8 die diameters in high-stalk lines; shorter necks reduce orientation and increase impact strength, while longer necks improve tear resistance. These settings are not universal acceptance criteria but are starting conditions that account for the resin’s melt strength and density. Film samples are conditioned at 23 °C and 50% relative humidity for 48 h according to ASTM D618 before measuring dart drop impact in accordance with ASTM D1709, Elmendorf tear in accordance with ISO 6383-2, and tensile elongation at break in accordance with ISO 527-3. The producer’s certificate of analysis normally reports only melt flow rate and density as release criteria; mechanical values are typical data and should not be used as lot-acceptance limits.
The low melt index and 0.918 g/cm³ density produce a film that is less stiff than a 0.926 g/cm³ or 0.930 g/cm³ LLDPE, but more resistant to creep and tear than a 0.912 g/cm³ grade. Those differences are useful where a converter must maintain packaging integrity under low-temperature abuse conditions, such as frozen-food distribution at −30 °C or heavy-duty sack filling with sharp-edged granular solids.
For food-contact packaging, the converter must verify that the finished film meets the applicable regulatory framework. The following standards and directives are commonly used for documentation when FG 30 U is evaluated for direct food contact or for use in electrical and electronic equipment housings.
| Regulatory reference | Scope relevant to FG 30 U film | Verification threshold or test condition |
|---|---|---|
| EU Regulation 10/2011 | Plastic materials and articles intended for food contact | Overall migration limit 10 mg/dm² of food contact surface |
| FDA 21 CFR 177.1520 | Olefin polymers for direct food contact | Compliance with extraction limits for fatty and aqueous foods, as applicable |
| REACH Regulation (EC) 1907/2006 | Registration, SVHC communication and restriction | SVHC content 0.1% w/w per article |
| RoHS Directive 2011/65/EU | Restriction of heavy metals and brominated flame retardants in EEE | Pb, Hg, Cr(VI), PBB, PBDE each below 0.1% w/w; Cd below 0.01% w/w |
Under EU Regulation 10/2011, it is the finished film, not the raw pellet, that must be tested with the appropriate food simulant: 10% ethanol for aqueous foods, 3% acetic acid for acidic foods, and isooctane or 95% ethanol for fatty foods. Because C4 LLDPE is nonpolar, total migration is dominated by the antioxidant and slip additives rather than the base polymer. For FDA compliance, 21 CFR 177.1520 covers olefin polymers used as articles or components of articles for direct food contact; the additive package must also be covered by a specific Food Contact Substance Notification or threshold-of-regulation exemption before use in food-contact applications.
On production-scale blown film lines, the most frequent failure modes when converting FG 30 U are bubble instability above a frost-line ratio of 6:1, pinhole formation when the die gap is 0.8 mm or less and melt temperature exceeds 230 °C, and die-lip plate-out when the stabiliser package is depleted by repeated regrind exposure. Those failures are caused by the interaction between the resin’s low melt flow rate and the specific line design. Managing them requires controlling the frost-line height, using a wider die gap during start-up, and maintaining a constant regrind fraction below 20 wt% to avoid additive depletion. The resin is not inherently incompatible with commercial polyethylene processing aids or colour masterbatches, but each masterbatch should be evaluated for melt index mismatch and thermal stability under the final melt-temperature profile.