Versalis Flexirene Fg 30 Butene Copolymer Linear Low Density Polyethylene

Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 204591
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 121 °C
    Vicat Softening Temperature 94 °C
    Tensile Strength At Yield Md 11 MPa
    Tensile Strength At Yield Td 10 MPa
    Tensile Strength At Break Md 35 MPa
    Tensile Strength At Break Td 30 MPa
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Dart Drop Impact 110 g
    Elmendorf Tear Strength Md 120 g
    Elmendorf Tear Strength Td 200 g
    Haze 12 %
    Gloss 85 %

    As an accredited Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® FG 30 Butene Copolymer LLDPE is supplied in 25 kg polyethylene bags, palletized for transport.
    Container Loading (20′ FCL) Versalis Flexirene® FG 30 LLDPE: 20′ FCL loads 20 pallets double-stacked, 55 x 25 kg bags each, 27.5 MT net.
    Shipping Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene is shipped as non-hazardous solid pellets in moisture-proof 25 kg bags, palletized or in octabins/bulk containers. Transport in clean, dry vehicles at ambient temperature; avoid prolonged heat, sunlight, moisture, and contamination. No special dangerous goods labeling required.
    Storage Store in original packaging in a clean, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep containers sealed to prevent moisture and contamination. Maintain moderate temperatures and avoid prolonged UV exposure. Do not store near strong acids, bases, or incompatible materials. Use first-in, first-out stock rotation, ensure proper ventilation and spill containment, and follow local regulations.
    Shelf Life Typically 24 months when stored unopened in original packaging, cool, dry, away from direct sunlight and heat.
    Application of Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene

    Versalis Flexirene FG 30 is a butene copolymer linear low density polyethylene with nominal melt flow rate 3.0 g/10 min (ISO 1133-1:2022, 190 °C/2.16 kg) and nominal density 0.920 g/cm³ (ISO 1183-1:2019). The short-chain branching distribution of butene comonomer produces a practical balance between dart impact retention and drawdown, but it does not develop the long-chain branching behaviour characteristic of autoclave LDPE. The scenarios below are restricted to industrial film extrusion, cast film, extrusion coating, agricultural plasticulture, and masterbatch carrier applications where the grade is placed in direct contact with high-shear screw elements, chill rolls, and winders.

    In heavy-duty sack manufacturing on monolayer blown-film lines, a 65 mm single-screw extruder with a 30:1 L/D barrier screw and a 150–200 mm spiral mandrel die processes the grade at a melt temperature of 180–215 °C, a die gap of 1.6–2.2 mm, and a blow-up ratio of 2.0–2.5. When frost line height is held between 200 mm and 400 mm, gauge variation remains below 8 % as measured on a traversing beta thickness scanner; outside this band, bubble oscillation transfers into wound reel hard bands and seal thickness deviations in bag conversion. The formulation for 60–150 µm liners accepts FG 30 at 70–100 wt%, with LDPE film grades at 0–30 wt% to increase melt tension and dart impact as verified by ISO 7765-1 dart drop method A. Slip/antiblock masterbatch is metered at 0.3–1.0 wt% for roll-form packaging; carbon black masterbatch for UV-opaque sacks at 2.0–4.0 wt% requires a let-down ratio no higher than 50:1 to prevent visible pigment specking. Compliance for single-use food-contact liners is assessed under EU Regulation 10/2011/EC total migration limit of 10 mg/dm² and FDA 21 CFR 177.1520(c) for olefin polymers. Tensile acceptance on 100 µm film references ISO 527-3:2018 at 500 mm/min crosshead speed and ISO 6383-2 tear propagation. Terminal products include 60–120 µm heavy-duty sacks for granular resin and fertiliser, 80–150 µm industrial drum liners, construction debris bags, and UN performance-tested sacks. Wound rolls stored at temperatures above 40 °C exhibit increased blocking because the butene copolymer film surface softens; slit-edge nicks are only accepted if MD elongation at break by ISO 527-3 exceeds 400 %.

    What Restricts Pre-Stretch Ratio in Cast Stretch Film Made from Butene Copolymer Blends?

    Cast film production of machine and hand stretch wrap on a 75 mm extruder with a 30:1 L/D screw and a coathanger slot die of 0.8–1.0 mm die gap operates at a melt temperature of 220–240 °C and a die-to-chill-roll distance of 90–130 mm. The pre-stretch ceiling observed on lines running 20 wt% FG 30 in an octene-based mLLDPE matrix is 220–250 %; beyond this draw ratio, draw resonance and edge bead deviation increase gauge coefficient of variation above 5 % as measured by a non-contacting infrared thickness sensor. The limiting variable is the shorter side-branch length of butene comonomer, which provides lower elastic recovery than octene-based mLLDPE when the web is drawn on powered rollers. Published data for pre-stretch ceilings at die-to-chill-roll distances outside 90–130 mm are limited. Formulation addition ratios range from 10–30 wt% FG 30 in an mLLDPE/C8 base; antistatic masterbatch at 0.5–1.5 wt% is added only for pallet lines wrapping static-sensitive goods. Slip agents are excluded above 0.1 wt% because they suppress the cling measured by ASTM D5458-95(2012) and create unstable pallet stacks. Mechanical evaluation uses ASTM D882-18 for tensile and elongation, ISO 527-3:2018 for film tensile properties, and ASTM D5458-95(2012) for peel cling. Terminal products are 12–23 µm machine stretch film, 20–25 µm hand wrap, and 25–35 µm anti-static stretch cover for cold-chain distribution. Processing above 250 °C accelerates antioxidant depletion and increases die-lip gel deposits; chill-roll surface temperatures above 28 °C reduce quench rate and create cross-direction gauge bands that are visible as dark rings on the wound core.

    During extrusion coating of orientated polyester and aluminium foil laminates, a 90 mm extruder with a 33:1 L/D screw feeding a 0.8 mm slot die at 240–260 °C deposits a sealant web at 12–25 g/m² onto a primed substrate at line speeds of 80–180 m/min. Chill-roll temperature is held at 15–22 °C because lower quench temperatures preserve hot-tack performance; when chill-roll temperature exceeds 25 °C, seal initiation temperature shifts upward by 2–5 °C and hot-tack strength as measured by ASTM F1921-18 becomes insufficient for vertical form-fill-seal jaws. The sealant layer can be run as 100 wt% FG 30; for high-speed coating lines requiring reduced neck-in, 10–20 wt% LDPE is added. Antiblock concentrate at 0.05–0.20 wt% controls winding friction without reducing seal strength, but levels above 0.3 wt% create seal interruptions at gas-flush pouch corners. Food-contact compliance is tested under EU Regulation 10/2011/EC using simulants 3 % acetic acid, 10 % ethanol, and 50 % ethanol, depending on food type, and under FDA 21 CFR 177.1520(c). The grade is not recommended for retort pouches above 100 °C because sealant creep and bond reduction after pasteurisation are visible in seal strength testing according to ASTM F88/F88M-21. Published data for retort configurations above 100 °C with FG 30 as sole sealant are limited. Terminal finished products include frozen polypropylene/polyethylene pouches, dry mix sachets, wipes overwrap, aluminium blister lidding sealant webs, and laminated tube films for personal care.

    When Greenhouse Film Specifications Require Multi-Season UV Stabilisation

    Greenhouse and silage cover films manufactured on 80 mm grooved-feed extruders with a 30:1 L/D screw and a 200–250 mm spiral mandrel die operate at a melt temperature of 180–210 °C and a blow-up ratio between 2.5 and 3.2 to orientate the film equally in the machine and transverse directions. For a 150–200 µm greenhouse cladding film, FG 30 is used at 70–85 wt%, LDPE at 10–20 wt%, stabiliser masterbatch at 1.0–3.0 wt% producing active HALS at 0.1–0.5 wt%, anti-fog concentrate at 0.5–1.5 wt%, and diffusing white pigment concentrate at 1.0–3.0 wt%. The stabilisation package is checked by accelerated weathering according to ISO 4892-2:2013, with tensile retention measured by ISO 527-3:2018 after 3000 h and 6000 h exposure intervals; haze development is evaluated by ISO 14782:1999. European agricultural covering films are specified under EN 13206:2017, which sets requirements for light transmission, tensile properties, and resistance to weathering. Finished products include 80–200 µm silage bunker covers, 150–200 µm greenhouse cladding, 30–60 µm mulch films, and 150 µm bale wrap. When active HALS loading exceeds 0.8 wt%, die-lip plate-out appears after 8–10 h of continuous operation as clear specks in the film edge; presence of these specks requires a shutdown below 220 °C and a purge with polyethylene purge compound before restart.

    Carrier Resin Performance in Masterbatch and Recycled-Content Systems

    Masterbatch compounding with butene LLDPE carrier resin uses a co-rotating twin-screw extruder with a 40:1 to 44:1 L/D barrel, melt temperature of 185–210 °C at the die, and underwater pelletising at water temperature below 35 °C to prevent pellet agglomeration. Formulation addition ratios for pigment masterbatch are 40–60 wt% FG 30 carrier, 20–50 wt% pigment, 5–15 wt% dispersing wax, and 0.2–1.0 wt% processing stabiliser; in blown film, let-down ratios of 2–5 wt% keep Colour Index pigment loading within 1.0–2.0 wt% in the final article. Screen packs configured at 100/150/60 mesh retain gel particles and agglomerates; back pressure exceeding 180 bar indicates screen blinding and requires a screen change rather than a melt temperature increase greater than 10 °C. Compliance for recycled-content systems is verified under EN 15343:2007 for recycled plastics traceability and, where applicable, EuCertPlast audit criteria; for food-contact regrind, EU Regulation 10/2011/EC Article 17 requires that recycled material be used only behind a functional barrier unless specific authorisation is granted. Terminal products include colour masterbatch for blown and cast film, additive masterbatch for slip/antiblock systems, and recycled-content heavy-duty refuse sacks in which 20–50 wt% FG 30 acts as virgin let-down to restore dart impact measured by ISO 7765-1 and weld integrity measured by ISO 527-3. The upper limit of 50 wt% recycled content in heavy-duty refuse sacks is set by gel count and transverse tear propagation measured by ISO 6383-2; above this level, tear strength falls below the minimum acceptable for kerbside lifting.

    Free Quote

    Competitive Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene is a butene-1 copolymer film resin supplied in pellet form for blown-film extrusion. The nominal density is 0.918 g/cm³ when tested under ISO 1183-1:2019, and the melt mass-flow rate is 1.0 g/10 min at 190 °C with a 2.16 kg load under ISO 1133-1:2022. This density and flow combination places the grade in thin-gauge flexible packaging, including primary and secondary packaging, industrial liners, carrier films, freezer films, and lamination webs. The butene-1 comonomer creates a short-chain branching distribution that differs from hexene- and octene-based LLDPE; the branching controls crystallite thickness, tie-chain density, and the resulting balance of tensile yield, tear, and impact. Relative to high-pressure LDPE, the linear backbone of FG 30 provides higher tensile stress at yield and higher elongation at break under ISO 527-3:2018, but lower bubble stability and lower specular gloss in blown-film operation. The resin is intended for melt temperatures between 190 °C and 220 °C, with the final profile determined by die diameter, throughput, and layer configuration.

    What limits processing latitude in this butene-copolymer grade?

    Because the melt mass-flow rate is 1.0 g/10 min, the melt is more viscous than high-MFR film grades. On a 55 mm single-screw extruder with L/D 28:1, screw speed is normally adjusted to keep melt pressure below 35 MPa; higher pressures increase shear heating and may initiate thermomechanical degradation. Use of a barrier screw with a Maddock mixer is common to homogenize the melt and avoid localized gel formation. Barrel profiles are commonly set at 170 °C in the feed zone, 200 °C in the compression zone, and 210 °C in the metering zone; adapter and die zones are maintained at 210 °C to 220 °C. Melt temperatures above 240 °C are not recommended for extended residence times because the butene copolymer undergoes oxidative degradation, evidenced by gel formation, discoloration, and loss of dart impact under ASTM D1709-21. A die gap of 1.5 mm to 2.5 mm is used for film thicknesses from 20 µm to 120 µm; blow-up ratios from 2.0:1 to 3.0:1 provide balanced transverse and machine-direction properties. Frost-line height can be maintained between 6 and 10 die diameters to stabilize bubble geometry. Pre-drying is not normally required; however, when pellets are exposed to relative humidity above 60 %, surface moisture may produce film voids and drying for 2 h at 60 °C in a desiccant dryer is required. Start-up and grade-change procedures typically use higher-flow LDPE or MDPE purge material to reduce residence time; die lips should be cleaned after extended campaigns because oxidized gel accumulation can disturb gauge uniformity.

    Processing parameterRecommended rangeEquipment or standard reference
    Melt temperature190–220 °CMelt thermocouple
    Die gap1.5–2.5 mmSpiral die, single lip
    Blow-up ratio2.0:1–3.0:1Bubble geometry
    Frost-line height6–10 die diametersCooling air ring
    Pre-drying60 °C for 2 h when RH > 60 %Desiccant dryer

    The values in the table are starting points rather than absolute limits. Variations in extruder screw design, die condition, and ambient cooling-air temperature alter frost-line height and bubble symmetry. Because butene LLDPE has lower melt strength than high-pressure LDPE, sudden changes in air-ring velocity can produce bubble instability, especially at blow-up ratios above 2.5:1. Internal bubble cooling is beneficial for throughput, but published data for FG 30 with internal bubble cooling is limited.

    When a butene copolymer replaces hexene or octene LLDPE in film structures

    Substitution of a C4 butene LLDPE for a C6 hexene or C8 octene resin changes toughness and seal response at constant density. At 0.918 g/cm³ and 25 µm thickness, butene copolymers generally exhibit lower dart drop impact under ASTM D1709-21 and lower Elmendorf tear under ASTM D1922-23 than hexene or octene copolymers at equivalent melt mass-flow rate. The structural reason is that butene branches are shorter and less effective at increasing tie-chain density between lamellae. In industrial comparative studies, dart impact of C4 LLDPE is typically 20 % to 40 % lower than C6 LLDPE at equivalent density and melt index. Tensile yield strength under ISO 527-3:2018 is closer between C4 and C6 grades, often within ±5 %, so stiffness-driven applications are less affected. Seal initiation temperature measured under ASTM F88/F88M-23 is usually higher for C4 LLDPE than for C8 LLDPE, which creates a slower sealing response in high-speed vertical form-fill-seal operations. In coextruded film, FG 30 is therefore placed in core or skin layers, while C8 LLDPE is reserved for sealant layers when low seal initiation is critical. The optical clarity of FG 30 is generally lower than high-pressure LDPE and can be affected by die-lip oxidation; haze testing under ASTM D1003-21 should be monitored at melt temperatures above 220 °C. Blown film from FG 30 also shows lower bubble stability than LDPE, requiring tighter frost-line control. Mixing with reclaim streams containing C6 or C8 comonomer should be controlled because short-chain branching distribution is not additive in simple proportion, and the impact/tear response can be nonlinear.

    Film propertyTest methodFlexirene FG 30 butene LLDPEC6 hexene LLDPEC8 octene LLDPE
    Dart drop impactASTM D1709-21LowerHigherHighest
    Elmendorf tearASTM D1922-23Lower, especially MDHigherHighest
    Seal initiationASTM F88/F88M-23HigherIntermediateLower
    Tensile yieldISO 527-3:2018ComparableComparableComparable

    The ratings are relative comparisons at equivalent density and melt mass-flow rate; absolute values depend on film thickness, extrusion direction, and processing conditions.

    In terms of end-use conformity, flexible film produced from FG 30 may be evaluated for food-contact suitability under Regulation (EU) No 10/2011 and, for United States market clearance, under 21 CFR 177.1520 for olefin polymers. Compliance is not conferred by resin selection alone; the final film must be assessed for overall migration and specific migration limits in the intended food simulant. The grade is also subject to REACH registration obligations for monomer and polymer import in the European Union. Typical application thickness ranges are 20 µm to 120 µm; downgauging below 15 µm can be attempted only with a narrow die gap, elevated blow-up ratio, and bubble stabilization, but published data for FG 30 below 15 µm is limited. In stretch-film or freezer-film structures, the resin is coextruded with polyethylene layers; adhesion to ethylene-vinyl acetate or polyisobutylene tackifiers is process-dependent and should be confirmed by peel testing under ASTM F88/F88M-23. The grade is also used in agricultural and protective films where puncture resistance is measured under ASTM F1306-21.

    Mechanical property benchmarks for blown film quality control

    Quality control on FG 30 film involves tensile, tear, impact, and optical measurements. Tensile stress at yield and elongation at break are measured under ISO 527-3:2018 using 15 mm wide strips and a test speed of 500 mm/min; typical LLDPE film values at 50 µm thickness for this density class fall between 8 MPa and 14 MPa yield stress and above 500 % elongation at break, but specific FG 30 film values must be taken from the effective lot certificate. Elmendorf tear is measured under ASTM D1922-23 and dart drop impact under ASTM D1709-21; both are sensitive to film thickness and extrusion direction. Haze is measured under ASTM D1003-21 and gloss under ASTM D2457-21; butene LLDPE can show higher haze than LDPE under high melt temperatures, so optical checks should be performed on stabilized production lengths. Machine-direction and transverse-direction values should be recorded separately. At high blow-up ratios, transverse-direction Elmendorf tear increases while machine-direction tear decreases; tensile yield may exhibit the opposite anisotropy. This directional behavior is not product-specific but affects conversion and bag-opening performance. The film-grade specification for FG 30 may include density and melt mass-flow rate as release parameters, but mechanical film properties are usually treated as typical rather than guaranteed. Testing should include both machine-direction and transverse-direction specimens because anisotropy in tensile elongation and tear is a normal feature of blown polyethylene film and should not be interpreted as a defect unless it exceeds the supplier’s established control limits.

    Another operational boundary concerns additive tolerance and process compatibility. Avoid combination with amine-based additives or high concentrations of unsaturated slip agents unless pre-validated because thermal interactions can alter colour and odour during extrusion. The resin is not designed for injection moulding or high-shear compounding; use in such processes can degrade the polymer and produce inconsistent melt flow. For monolayer cast-film operation, cooling roll temperatures between 20 °C and 40 °C are typically used for this polymer class, but published data for FG 30 cast-film operation is limited. The same limitation applies to foam extrusion and oriented film processes where butene LLDPE is not the usual reference polymer. Because the product is a butene copolymer, it should not be blended with octene- or hexene-rich reclaim without adjusting the expected film impact and tear values, as mixed short-chain branching distributions can produce nonlinear property loss.