| HS Code | 721767 |
| Polymer Type | Linear Low Density Polyethylene |
| Comonomer | Butene |
| Density | 0.923 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.7 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Temperature | 98 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 260 MPa |
| Dart Drop Impact | 120 g |
| Haze | 12% |
| Gloss 45 | 60% |
| Coefficient Of Friction | 0.2 |
| Elmendorf Tear Resistance Md | 100 g |
| Elmendorf Tear Resistance Td | 200 g |
As an accredited Versalis Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene FG 23 U is supplied in 25 kg polyethylene bags, shrink-wrapped on pallets, or 1000 kg bulk bags. |
| Container Loading (20′ FCL) | Versalis Flexirene® FG 23 U LLDPE loaded in 20′ FCL as 25 kg palletized bags, stretch-wrapped, approx. 22 MT net. |
| Shipping | Versalis Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene is supplied as solid pellets, normally packed in 25 kg PE bags or octabins on pallets. It is non-hazardous for transport. Ship in clean, dry, covered trucks or containers, protected from moisture, heat, and direct sunlight. |
| Storage | Store indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep packages closed and clean to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking pressure. Use clean handling equipment. Maintain ambient storage temperatures and avoid conditions that may soften or degrade the resin. |
| Shelf Life | Shelf life is 24 months in original unopened packaging under cool, dry, well-ventilated conditions, away from direct sunlight and heat sources. |
Flexirene® FG 23 U is converted on grooved-feed single-screw blown-film lines with screw L/D ratios of 30:1 and barrier-flight geometry to produce heavy-duty industrial sack film in the 120–180 μm thickness range. The grade is a butene-copolymer LLDPE with a nominal density of 0.923 g/cm³ per ISO 1183-1 and a melt mass-flow rate of 1.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022; the producer-supplied UV-stabiliser package makes the grade suitable for sacks stored outdoors but does not eliminate the need for carbon black loading where prolonged solar exposure is specified. A production-validated formulation for 150 μm chemical and fertiliser sack film is 75–85 wt% FG 23 U, 10–20 wt% autoclave LDPE with a melt flow rate of 2.0 g/10 min, 2–4 wt% carbon black masterbatch, and 1–2 wt% of a polyethylene-based processing aid masterbatch when die pressures on 90 mm extruders exceed 280 bar. Industry compliance for mechanical performance is assessed using ISO 527-3:2018 for tensile stress and elongation, ISO 6383-2 for trouser tear resistance, and ISO 7765-1 for dart impact; substance regulatory compliance follows REACH Regulation (EC) No 1907/2006 Annex XVII, EU Packaging and Packaging Waste Directive 94/62/EC, and applicable national food-contact declarations when the sack is used as a secondary food-contact layer. Processing on a 90 mm 30:1 L/D line is maintained at melt temperatures of 195–215 °C, die gap 1.8–2.0 mm, blow-up ratio 2.0:1–2.8:1, and frost-line height 6–8 die diameters; output rates of 220–280 kg/h are limited by bubble stability rather than screw recovery. The terminal product classes are 50 kg resin export sacks, fertiliser bag outer liners, FIBC inner liners, and hazardous-goods packaging where national dangerous goods regulations accept a minimum 150 μm LLDPE/LDPE wall thickness after conditioning at 23 °C and 50 % relative humidity for 48 h. Operating boundaries include pre-drying with dehumidified air at 80 °C for 2 h when granule surface moisture exceeds 0.05 wt% after outdoor silo storage, because water vapour evolved from the melt causes bubble chatter at frost-line heights below 6 die diameters; blends containing more than 20 wt% high-viscosity HDPE are incompatible with this processing window and raise backpressure beyond 350 bar on screw diameters below 70 mm.
In three-layer multi-season greenhouse cover production, FG 23 U is formulated at 65–75 wt% in the outer layer, 70–80 wt% in the core, and 60–70 wt% in the inner layer, with the remaining components divided between autoclave LDPE of 2.0 g/10 min, EVA containing 14 wt% vinyl acetate, and masterbatch packages. A total-film formulation for 180 μm greenhouse cover includes 65–75 wt% FG 23 U, 10–20 wt% LDPE, 8–12 wt% EVA, 3–5 wt% HALS UV-stabiliser masterbatch, and 1–2 wt% anti-fogging masterbatch; because the U grade already carries a UV-stabiliser system, converters validated under accelerated QUV conditions should reduce the external HALS addition by 1 wt% relative to an unstabilised butene LLDPE to avoid stabiliser bloom. Compliance is governed by EN 13206:2017 for thermoplastic covering films used in agriculture and horticulture, REACH Annex XVII, and national UV-durability grading schemes that define film service-life classes after xenon-arc or QUV exposure. The downstream conversion process is blown-film coextrusion on three-layer lines with internal bubble cooling and adjustable extractor cages; die gap is set at 2.0 mm, blow-up ratio at 2.0:1–2.4:1, melt temperature at 200–215 °C, and frost-line height at 7–9 die diameters. Terminal end products include multi-season greenhouse covers, low-tunnel films, silage pile covers, and fumigation barrier films. Where sulfur can be present from vaporised pesticide applications, HALS stabiliser chemistry is incompatible with the sulfur oxide species generated by sulfur burners; a sulfur-resistant stabiliser package is required, and published data for the specific FG 23 U sulfur-exposure performance is limited, so regional greenhouse trials are required before commercial use in sulfur-burning operations.
On flat-die extrusion lamination lines coating woven polypropylene fabric at widths from 1.6 m to 2.2 m, FG 23 U is processed at 15–25 μm coating thickness to provide moisture barrier, scuff resistance, and printability. The formulation is 80–90 wt% FG 23 U, 5–15 wt% autoclave LDPE of melt flow rate 2.0 g/10 min to reduce neck-in, and 2–5 wt% maleic anhydride grafted polyolefin tie resin where seal seam strength above 18 N/25 mm is specified after 45 dyn/cm corona treatment. Industry compliance for woven sack lamination is anchored to ISO 527-3:2018 tensile elongation, ISO 6383-2 tear, ASTM F88/F88M-21 seal strength, and EU Packaging and Packaging Waste Directive 94/62/EC; RoHS 2011/65/EU Annex II applies when the laminate is used for exported electrical accessory packaging. Process conditions require melt temperatures of 265–285 °C at the slot die because lower melt temperatures fail to generate the polar-carbonyl surface species required for adhesion to corona-treated polypropylene fabric; the upper limit is 290 °C, above which gel count rises beyond 10 per m² due to oxidative crosslinking at the die lip. Air gap is maintained at 200–250 mm, chill roll temperature at 15–20 °C, and coating line speed at 80–150 m/min; slot die gaps of 0.6–0.8 mm are set to deliver the low coating weight without excessive draw resonance. Terminal product types are cement bags, fertiliser bags, pet food sacks, and laminated woven bulk-packaging outer layers. Operational boundaries include chill roll surface temperature higher than 25 °C causing adhesion decay because rapid LDPE crystallisation reduces interfacial oxygen diffusion; adhesion loss is more severe when fabric corona treatment falls below 35 dyn/cm within 24 h of coating.
Where surface protection films for pre-painted metal sheet, aluminium profiles, and furniture panels require haze below 10 % and peel adhesion in the 0.8–3.5 N/25 mm range, FG 23 U is cast-blended with LDPE and EVA. The film is produced in thicknesses from 25 μm to 45 μm using a chill-roll cast line with an embossed matte roll; the formulation is 60–70 wt% FG 23 U, 15–25 wt% LDPE of 2.0 g/10 min, 8–12 wt% EVA containing 18 wt% vinyl acetate, and 1–2 wt% low-molecular-weight tackifier masterbatch. Compliance for mechanical performance follows ISO 527-3:2018 and ISO 6383-2; regulatory compliance follows REACH, RoHS 2011/65/EU, and for indoor-use furniture film, VOC emission may be tested under ISO 16000-9:2024. Process settings include melt temperature 210–240 °C, line speed 120–180 m/min, and chill roll temperature 15–20 °C. Terminal product types are protective masking films for aluminium profiles, pre-painted steel panels, PVC window profiles, and acrylic sheets. Operational boundaries restrict EVA above 12 wt% because excess vinyl acetate exudation causes peel-force drift beyond 0.5 N/25 mm after 30 days at 40 °C; published peel-force retention data for this specific grade on marbled polypropylene substrates is limited, so substrate-specific ageing trials are required before specifying shelf life.
Five-layer coextruded frozen-food film production uses FG 23 U in the sealant layer because the butene-copolymer melting profile lowers seal initiation temperature relative to high-density polyethylene. The sealant-layer formulation is 60–75 wt% FG 23 U, 20–30 wt% EVA with vinyl acetate content of 14–18 wt%, 3–5 wt% slip/antiblock masterbatch, and up to 1 wt% antifog masterbatch where packages carry frozen vegetables with free surface moisture. Compliance is governed by Commission Regulation (EU) No 10/2011 Annex I overall migration limit of 10 mg/dm², FDA 21 CFR §177.1520 for olefin polymers used in contact with food, and export-specific positive lists such as China GB 9685; organoleptic testing follows ISO 13302:2005. The downstream process is five-layer coextruded blown film with layer distribution 20/15/30/15/20, die gap 1.8 mm, blow-up ratio 2.5:1, melt temperature 190–210 °C, and frost-line height 6 die diameters. Terminal product types are frozen vegetable bags, frozen bakery dough pouches, ice cream wrapper film, and retail frozen food zipper pouches. Operational boundaries exclude EVA loadings above 30 wt% in the sealant layer for fatty food applications because low-molecular-weight vinyl acetate oligomers can migrate and shift organoleptic panel scores during shelf-life testing at −18 °C; coextruded structures should also maintain a polyamide or EVOH barrier layer because the FG 23 U layer alone has insufficient oxygen barrier for long shelf-life frozen products.
For chill-roll cast stretch film conversion below 23 μm, FG 23 U is blended with metallocene-catalysed hexene LLDPE instead of being run neat because butene comonomer branching produces a broader relaxation spectrum that reduces on-pallet force retention at 250 % elongation. A production formulation for 20 μm machine film is 60–70 wt% FG 23 U, 25–35 wt% metallocene-catalysed hexene LLDPE, and 2–4 wt% polyisobutene tackifier masterbatch. Compliance is assessed under ISO 527-3:2018, ASTM D5748 puncture energy, and EU Packaging and Packaging Waste Directive 94/62/EC. Processing on cast slot-die equipment with automatic edge pinning and chilled polishing rolls is maintained at melt temperatures of 240–270 °C, line speeds of 350–450 m/min, and chill roll temperature 15–20 °C. Terminal product types are hand stretch film, light-duty machine stretch film, and bundling film. The upper melt-temperature limit is 285 °C; above that threshold, oxidative degradation increases gel count beyond 10 per m² and puncture energy falls outside the acceptance window.
Competitive Versalis Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene FG 23 U is a butene copolymer linear low density polyethylene produced through a Ziegler-Natta polymerisation route. The grade is supplied as free-flowing pellets with a nominal density of 0.923 g/cm³ measured under ISO 1183-1 and a melt flow rate of 1.0 g/10 min determined at 190 °C/2.16 kg under ISO 1133-1. The butene comonomer introduces saturated short-chain branches that lower crystallinity and density relative to a high-density polyethylene of equivalent melt index. Molecular weight distribution is broad, a characteristic of Ziegler-Natta C4 LLDPE grades, which contributes to bubble stability in blown film but limits shear thinning relative to metallocene-catalysed resins. The product is not formulated with slip or antiblocking additives, so film surface friction and blocking response are governed by masterbatch addition, corona treatment, and gauge. Principal applications are general-purpose blown film, medium-duty packaging, lamination film, and agricultural film. Selection among Flexirene film grades is usually based on the balance between dart impact, tear propagation, film optics, and extruder processability.
Molecular architecture and lot-to-lot analytical data for FG 23 U are controlled through polymerisation and finishing parameters. Certificates of analysis report density under ISO 1183-1 and melt flow rate under ISO 1133-1 for each delivery. The butene comonomer content is measured by Fourier transform infrared spectroscopy under ASTM D5576 or by ¹³C nuclear magnetic resonance; published data for this specific configuration is limited, but the density and melt index are supplied with each batch. Film mechanical properties are not normalised as resin properties because they shift with drawdown, blow-up ratio, and cooling rate. Converters applying statistical process control on blown film lines frequently monitor gauge profile at 10 to 20 points around the bubble circumference and correlate transverse-direction thickness variation with Elmendorf tear under ASTM D1922. Masterbatch loadings above 5 wt% should be evaluated by capillary rheometry before full-scale production because colour and filler concentrates can modify effective melt flow rate.
Blown film conversion of FG 23 U is normally performed on single-screw extruders with L/D ratios between 24:1 and 30:1, using barrier screws designed for linear low density polyethylene. The recommended melt temperature range is 180 °C to 210 °C; sustained melt temperature above 230 °C accelerates thermo-oxidative chain scission and can generate gel defects in thin films. Die gaps from 1.2 mm to 2.5 mm are used to reduce melt fracture and draw resonance. When the die gap is below 1.0 mm, shear rate at the die lip can exceed the critical shear stress of the broad molecular weight distribution, producing sharkskin surface defects. Blow-up ratios between 2.0:1 and 3.0:1 are typical. Frost line height is maintained between 1 and 3 die diameters above the air ring to balance bubble stability and film optics. Melt pressure at the die head on a 60 mm single-screw extruder with 30:1 L/D commonly falls between 200 bar and 350 bar depending on output, die geometry, and temperature profile. Excessively high screw speed increases shear heating and can push melt temperature beyond 230 °C even when barrel setpoints remain at 200 °C. Chilled air between 5 °C and 15 °C is frequently used to stabilise the bubble and increase throughput without raising melt temperature.
Batch-to-batch variation in extrusion behaviour is generally lower than that observed with metallocene grades because the broad molecular weight distribution reduces sensitivity to small changes in polymerisation residence time. However, colour change or filler masterbatches alter the effective melt flow rate. Pre-drying is not ordinarily required for sealed pellet deliveries, but storage at relative humidity above 60% may require drying at 60 °C to 80 °C for 4 h to 6 h before processing. When dryers are used, desiccant units with dew point below -30 °C are preferred over hot-air hoppers to avoid surface oxidation of the pellet.
Unlike hexene- or octene-based linear low density polyethylene grades, FG 23 U incorporates butene as the short-chain branching comonomer. The shorter butene branch yields lower dart impact and Elmendorf tear resistance at equivalent gauge and melt index. Comparative film characterisation under ASTM D1709A and ASTM D1922 generally ranks C4 LLDPE below C6 and C8 copolymers, although the difference narrows below 30 µm thickness. Against high-pressure LDPE, FG 23 U displays higher tensile strength at break and puncture resistance under ASTM D882 but lower melt elasticity and lower melt strength, which restricts the blow-up ratio envelope and demands tighter air-ring control. Relative to metallocene-catalysed C4 LLDPE, the Ziegler-Natta architecture of FG 23 U provides higher extruder pressure stability and a lower melt fracture threshold, but lower film clarity and poorer organoleptic performance. These differences define the production environment: FG 23 U is selected where medium-duty performance and stable bubble formation outweigh maximum clarity or extreme downgauging.
The density and melt flow rate position FG 23 U in the LLDPE film class for medium-stiffness applications. Mechanical testing is performed on 25 µm to 50 µm film specimens according to ISO 527-3 for tensile properties and ASTM D882 for machine-direction and transverse-direction tensile values. Water-vapour transmission rate is measured on 40 µm film under ASTM F1249 or ISO 15106-1, and oxygen transmission rate is measured under ASTM D3985 or ISO 15105-1; barrier performance is a function of crystallinity and is therefore inferior to HDPE and superior to EVA at equivalent thickness. Thermal analysis under ISO 3146 places the crystalline melting peak near 122 °C, and the Vicat softening temperature under ISO 306/A50 is approximately 108 °C. These values are typical and are not specification limits. The material is supplied in compliance with REACH Regulation 1907/2006. Food-contact use is supported for olefin polymers under FDA 21 CFR 177.1520, with final compliance dependent on conversion aids, inks, and masterbatch components.
| Requirement | Reference | Scope |
|---|---|---|
| Food-contact olefin polymer | FDA 21 CFR 177.1520 | Final article dependent |
| European chemical inventory | REACH (EC) 1907/2006 | As supplied |
| Hazardous substance restriction | RoHS Directive 2011/65/EU | No intentional heavy metal additions |
Extrusion of FG 23 U in high-output agricultural film lines exposes the limitations of the butene copolymer architecture. At output rates above 150 kg/h on a 90 mm extruder, bubble instability can occur if the die gap is below 1.5 mm, because the lower melt strength of the C4 Ziegler-Natta resin cannot sustain high bubble tension at blow-up ratios above 2.5:1. Under these conditions, the bubble may oscillate in the transverse direction, generating gauge variation that reduces film tear performance under ASTM D1922. Reprocessing of edge trim and start-up film above 20 wt% is not recommended, because repeated thermal history increases gel formation and reduces dart impact under ASTM D1709A by more than 15% relative to virgin pellets. When FG 23 U is blended with high-pressure LDPE at 10 wt% to 20 wt%, melt strength increases but film haze measured under ASTM D1003 also rises. The resin is compatible with conventional polyolefin masterbatches, but combinations with freely soluble amine-based or peroxide-based additives should be qualified before extended extrusion campaigns, because these species can accelerate oxidative degradation. For food-contact films, the assembled package must satisfy migration limits under EU Regulation 10/2011 or FDA 21 CFR 177.1520 depending on the intended market.
In multilayer structures, FG 23 U is typically assigned to the skin or sealing layer of a blown coextrusion line. The low melting onset relative to HDPE improves seal initiation behaviour when tested under ASTM F2029 or ISO 527-3; the actual seal initiation temperature is a function of dwell time, sealing pressure, and film gauge. In a three-layer A/B/C structure with polyamide or EVOH barrier layers, FG 23 U requires an adhesive tie resin because the nonpolar butene copolymer surface does not bond directly to polar barrier resins. Coextrusion die temperatures are usually kept between 200 °C and 220 °C to avoid excessive viscosity mismatch with EVOH. In lamination film, corona treatment at a surface energy of 38 mN/m to 42 mN/m is necessary before solvent-based or water-based adhesive coating. If corona treatment is omitted or surface energy falls below 38 mN/m, laminate bond strength under ASTM F904 can decrease below acceptable limits. The butene branch length also influences hot tack; the hot-tack window is generally narrower than for octene LLDPE, so sealing equipment must maintain tighter jaw temperature control.
Downgauging trials with FG 23 U from 50 µm to 25 µm require re-optimisation of frost line height and blow-up ratio rather than a simple reduction in die gap. At 25 µm, the film’s specific dart impact measured under ASTM D1709A and tear propagation under ASTM D1922 become more sensitive to melt temperature fluctuations; variation greater than ±5 °C across the die circumference can create localised property loss. On oscillating haul-off film lines, the lower puncture resistance of C4 LLDPE relative to C8 LLDPE is partially compensated by blending with high-pressure LDPE, but haze then rises under ASTM D1003. Seal-through-contamination performance of FG 23 U is poorer than that of ionomer sealants, and the grade is not recommended for retort applications above 100 °C. These boundaries define the resin as a general-purpose blown film material rather than a high-barrier or high-clarity specialty resin.