| HS Code | 902041 |
| Product Name | Versalis Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.922 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 2.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 28 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 300 MPa |
| Hardness Shore D | 50 |
| Film Haze | 12 % |
| Gloss 45 | 60 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Resistance Md Td | 150/250 g |
As an accredited Versalis Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® FG 20 I packaging: 25 kg polyethylene bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL: 18 MT net in 25 kg bags, palletized or floor-loaded, shrink-wrapped and secured for safe transport. |
| Shipping | Versalis Flexirene® FG 20 I Butene Copolymer LLDPE ships as a non-hazardous solid resin, typically in 25 kg bags, octabins, or bulk containers. It is not regulated by DOT, IMDG, IATA, or ADR; no UN number, hazard class, or packing group. Keep dry, away from heat and UV, with packaging protected. |
| Storage | Store Versalis Flexirene® FG 20 I in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Stack safely to prevent deformation. Protect from physical damage; do not store near strong oxidizers. Observe local regulations and manufacturer’s instructions. |
| Shelf Life | Shelf life typically 24 months if stored unopened in original packaging under cool, dry, ventilated conditions away from direct sunlight. |
On blown film lines converting FG 20 I into 80–120 µm heavy-duty sack film, the practical output ceiling is set not by extruder drive load but by bubble instability above a frost line height of 8 die diameters. The nominal density of 0.920 g/cm³ per ISO 1183-1 and melt flow rate of 1.0 g/10 min per ASTM D1238 position the grade in the lower-crystallinity segment of butene-1 LLDPE film resins. Single-screw grooved-feed extruders with L/D 30:1 barrier flights and Maddock mixing sections deliver melt temperatures of 195–215 °C; die gaps below 1.8 mm push die-lip shear stress into the sharkskin region, while die gaps above 2.4 mm reduce machine-direction orientation and lower Elmendorf tear values measured per ASTM D1922. Blending 10–20 wt% autoclave LDPE with a melt flow rate of 0.7–1.0 g/10 min raises bubble stability, but increases haze from 8% to 14% in 50 µm film tested per ASTM D1003. At 100 µm gauge, seam strength after impulse sealing at 160–180 °C jaw temperature and 0.4 MPa jaw pressure declines if the seal zone cools below 60 °C before load transfer.
For industrial liners with a target puncture resistance above 120 N per ASTM D5748, the blow-up ratio should be held between 2.0:1 and 2.5:1; wider BUR raises transverse-direction tear but destabilizes the bubble corners when ambient air velocity exceeds 0.5 m/s. The frost line should be maintained at 6–8 die diameters from the die face; lower positions increase quench rate and crystallinity at the inner surface, raising the 1% secant modulus per ISO 527-3 from 200 MPa to approximately 230 MPa. On lines without internal bubble cooling, output per die circumference typically cannot exceed 0.8 kg/h/mm without gauge variation exceeding ±5% measured by a capacitance thickness scanner. Under those conditions, high-speed slit sealing at 15 m/min produces occasional channel leakers when the film gauge drops below 85 µm in the seal zone.
Batch-to-batch MFR drift of 0.1 g/10 min has been observed on production lots. When MFR rises to 1.1 g/10 min, bubble stability at constant frost line height decreases and the gauge control loop must reduce haul-off speed by 2–3 m/min to maintain ±5% thickness tolerance. Heavy-duty sack end products intended for express freight may require a machine-direction tear resistance above 3.0 N per ASTM D1922; converters that overdilute FG 20 I with recycled LLDPE above 30 wt% typically fail this threshold at the lower end of the gauge band.
Heat-seal testing of a 12 µm FG 20 I sealant web coextruded with a 20 µm propylene copolymer core shows seal initiation at 95–110 °C when measured according to ASTM F2029 at 0.3 MPa seal pressure and 2.0 s dwell. The plateau seal strength reaches 8–12 N/25 mm per ASTM F88 between 120 °C and 140 °C; above 150 °C the sealant layer exhibits visible thinning and the failure mode changes from peel to tear. Hot-tack strength per ASTM F1921 remains above 1.5 N/25 mm at 115 °C but falls below 1.0 N/25 mm at 105 °C, which limits packaging line start-stop performance on vertical form-fill-seal equipment. For food-contact laminates, the sealant web must satisfy EU No 10/2011 with overall migration below 10 mg/dm² per EN 1186-1, and the outer print layer must not contaminate the sealant via set-off.
For high-speed laminators running at 60 packs/min, seal dwell times under 0.4 s require raising the fin-seal jaw set point to 125–135 °C; however, the operating window narrows because the outer web reaches 60–70 °C at the point of lap sealing, and polyolefin slip agents at the film surface reduce the effective seal strength. Corona treatment of the sealant web to 38–42 mN/m before solventless lamination is retained for 72 h; beyond that interval the adhesive wetting envelope measured by contact angle becomes insufficient on the treated surface. For structures containing aluminium foil, moisture trapped below 0.3 g/m² in the lamination nip leads to blistering at retort temperatures above 115 °C.
The laminated web must be aged for 24–48 h at 35–40 °C to complete urethane adhesive crosslinking before heat seal testing. Premature testing shows low seal strength attributable to uncured adhesive chemistry rather than to the sealant resin itself. Published data for sealant-layer thinning below 10 µm on high-barrier laminates is limited; converters running such structures typically qualify each lot by differential scanning calorimetry seal-curve profiling rather than relying on single-point seal strength.
In 150 µm greenhouse covering film, FG 20 I is compounded with 0.5–1.2 wt% hindered amine light stabilizer masterbatch and 0.2–0.5 wt% UV absorber. Outdoor weathering acceptance for the application is specified by EN 13206, with tensile elongation retention measured by ISO 527-3 after 3000 h of artificial weathering at 0.76 W/(m²·nm) under ISO 4892-3. Films retaining less than 50% of initial elongation are rejected because the covering must withstand hail impact of 5 g steel balls at 100 km/h without perforation in EN 13206 testing. Published data for condensation-control additive migration in FG 20 I specifically are limited; commercial qualification of anti-fog masterbatches relies on condensation chamber methods cited in EN 13206 rather than single-point surface energy measurements.
The inner-surface anti-fog additive package migrates over 7–14 days; before migration is complete, condensation droplets reduce photosynthetically active radiation transmission by up to 20% and create localised cooling. A blend of 15–20 wt% EVA with 14% vinyl acetate content lowers the secant modulus per ISO 527-3 from approximately 200 MPa to 150 MPa; long-wave infrared transmittance data for this particular blend are not published and must be measured by the converter. The trade-off is a measurable loss in tear initiation resistance tested per ISO 6383-2; blend films show a 10–15% lower pendulum tear than the neat FG 20 I control. On single-screw blown film lines, the addition of EVA requires barrel zone temperature reduction by 10–15 °C to prevent acetic acid liberation and gel formation.
Commercial qualification of anti-fog masterbatches uses condensation chambers per EN 13206; field trials on tunnel greenhouses show droplet persistence above 30 s reduces light transmission to below 80% in the early morning. For multi-season covering film, the specification should require re-testing after 1800 h of natural weathering because stabilizer consumption in the outer skin shifts haze development inward and accelerates film yellowing near the greenhouse frame contacts.
| Compliance domain | Standard or regulation | Test method | Threshold or condition |
|---|---|---|---|
| EU food contact overall migration | EU No 10/2011 | EN 1186-1 | 10 mg/dm²; 40 °C, 10 days, 3% acetic acid |
| FDA olefin polymer clearance | FDA 21 CFR 177.1520 | 21 CFR 177.1520 extraction | Conditions of use up to 135 °C for fatty foods; maximum extractable fraction per table 2 |
| Packaging heavy metals | EU 94/62/EC | EN 14582 | Sum Pb + Cd + Cr(VI) + Hg < 100 mg/kg |
| REACH SVHC declaration | REACH Article 33 | Supplier declaration | Candidate list substances < 0.1% w/w per article |
| Agricultural film weathering | EN 13206 | ISO 4892-3 | Retained elongation > 50% after 3000 h |
In frozen-food packaging lines, the critical failure mode is not ambient-temperature tensile yield but low-temperature impact and flex-crack resistance after repeated cold-chain cycling. A 25 µm FG 20 I blown film retains dart drop impact per ASTM D1709 method A above 90 g at -20 °C, while a 75 µm coextruded structure with a 20 µm FG 20 I sealant layer on a 55 µm high-density polyethylene core survives 1000 flex cycles per ASTM F392 without pinholes. Water vapour transmission rate for 25 µm film is 2.5–3.5 g/(m²·day) at 38 °C and 90% RH measured per ASTM F1249, which imposes an outer-print film or paper lamination for products sensitive to moisture gain above 0.5%.
Seal strength after conditioning at -20 °C for 24 h falls below 1.0 N/25 mm when the seal temperature was below 105 °C; the minimum fin-seal set point is therefore 120 °C for polyolefin films running at 30 m/min. Reducing the sealant layer below 15 µm by orientation during draw-down causes a 5–8 °C increase in seal initiation because surface nucleation density is raised. Hot-tack values per ASTM F1921 at 110 °C remain above 1.2 N/25 mm only if the web tension in the sealing zone is controlled below 3 N/25 mm. For direct food contact, the sealant layer complies with FDA 21 CFR 177.1520 and EU No 10/2011; overall migration is below 10 mg/dm².
In cold-room storage, the coefficient of friction of untreated film is below 0.4 per ISO 8295; converter-added slip masterbatch at 0.2–0.5 wt% avoids blocking but reduces heat seal strength at 120 °C by 1–2 N/25 mm. Frozen-food converters often run the sealant layer without added slip and instead rely on an external printed web to carry the slip package, preserving seal integrity at high-speed bagging.
Collation shrink film produced from FG 20 I alone exhibits machine-direction free shrink below 8% at 70 °C when measured per ASTM D2732; total free shrink at 110 °C reaches 55–65% only after blending with 20–30 wt% LDPE or 5–15 wt% of a 0.918 g/cm³ metallocene LLDPE. The shrink tunnel air temperature for 40–60 µm film must be set to 140–160 °C with a residence time of 4–6 s; shorter residence times leave residual shrink above 5% in the transverse direction and cause loose collation on beverage multipacks. Secondary collation film over printed cartons does not require food-contact migration testing; when the film contacts primary food packaging, EU No 10/2011 verification is triggered.
Film orienting conditions during the double-bubble process require a first-bubble water-quench temperature of 15–20 °C and a second-bubble internal pressure of 0.15–0.25 MPa. The primary constraint is simultaneous burn-through and seal peaking: at tunnel air temperature above 165 °C, the thin seal layer reaches 130–140 °C and the heat seal strength tested per ASTM F88 declines. Gauge variation above ±5% across the shrink film produces local shrink force differentials that pull the package out of vertical alignment by more than 3°.
The double-bubble orientation ratio in the transverse direction is set at 4:1–5:1; below 3:1 the shrink force at 90 °C measured by ASTM D2838 fails to hold collation film tight over sleeve-wrapped trays above 6 kg. Production trials show that lowering the first-bubble water-quench temperature below 12 °C increases transverse-direction gauge variation at the second bubble, while raising it above 22 °C slows bubble reheating and reduces transverse-direction free shrink at 110 °C by 7–10%.
Melt fracture on FG 20 I appears as surface sharkskin at die-lip shear stresses above 0.12–0.14 MPa, a threshold that is reached on 2.0 mm die gaps when output exceeds 0.9 kg/h/mm of die circumference. The shear stress is calculated from die pressure and die geometry, and the onset is detected by a rise in back pressure fluctuation from ±1 MPa to ±3 MPa on machines with a L/D 30:1 grooved-feed extruder. Addition of a fluoroelastomer processing aid at 200–600 ppm delays sharkskin by conditioning the die-lip steel, but the effect is lost if the screw speed is increased above 110 rpm because the residence time in the metering section drops below 30 s. Batch-to-batch MFR variation of ±0.1 g/10 min shifts the onset pressure fluctuation by approximately 1 MPa, and extrusion control systems that do not compensate for viscosity drift produce gauge bands at the bubble neck.
The frost line must be positioned at 6–8 die diameters; below 5 die diameters the quench rate raises internal haze above 12% in 50 µm film per ASTM D1003, while above 10 die diameters the bubble enters the low-tension zone and gauge variation measured by a capacitance scanner exceeds ±6%. Blow-up ratios between 2.0:1 and 2.6:1 produce a balanced tear ratio; increasing BUR to 3.0:1 shifts the Elmendorf tear ratio per ASTM D1922 to 0.6–0.8, which creates easy-split behaviour along the machine direction during pallet wrapping. No method is available to eliminate this orientation effect without adding 10–20 wt% LDPE or reducing the haul-off speed below 15 m/min.
Changeover from a 1.8 mm die gap to a 2.4 mm die gap without altering the screw profile lowers melt pressure by 5–10 MPa but reduces shear mixing, requiring a 5–8% increase in screw speed to maintain melt quality. On film lines equipped with internal bubble cooling, the same gap change permits a 10–15% higher throughput before the melt fracture threshold reappears, but only if the air ring pressure is reduced by 0.2–0.4 kPa to prevent bubble oscillation at the frost line.
Competitive Versalis Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® FG 20 I is a butene-comonomer linear low-density polyethylene supplied as a blown-film extrusion resin. Manufacturer technical data identify a melt mass-flow rate of 2.0 g/10 min determined to ISO 1133-1 at 190 °C under 2.16 kg, and a density of 0.918 g/cm³ measured to ISO 1183-1 method A. The polymer is produced with a conventional catalyst system, so the butene comonomer introduces ethyl short-chain branches that define crystallinity, melting point, seal initiation, and solid-state toughness. Additive content such as slip or antiblock must be verified against the supplier lot certificate because suffix nomenclature is not uniform across regional distribution channels. The resin is used in general-purpose blown film for dry-food packaging, collation shrink, agricultural film, and laminating structures. Compared with high-pressure low-density polyethylene, the linear backbone typically yields higher tensile yield stress and higher dart drop at equivalent gauge. Compared with hexene or octene linear low-density polyethylene of equal density, FG 20 I generally exhibits lower dart drop and lower machine-direction Elmendorf tear after down-gauging.
In ethylene/α-olefin random copolymers, comonomer selection controls the length of the short-chain branch: butene inserts as ethyl branches, hexene as n-butyl branches, and octene as n-hexyl branches. Peer-reviewed studies on linear low-density polyethylene show that at constant density near 0.918 g/cm³, longer α-olefin branches increase tie-molecule concentration and redistribute stress more efficiently during Elmendorf tear and dart drop testing. A shift from an octene grade to FG 20 I may therefore reduce machine-direction tear strength and dart drop on 25 µm film. The butene copolymer typically lowers melt viscosity and die pressure, allows lower melt temperature, and can improve bubble stability on shallow-channel extruders. Optical properties are also affected: butene-based linear low-density polyethylene can show lower haze than a comparable hexene grade after rapid cooling, although the difference is highly dependent on frost line height and air-ring geometry. Published data for this specific configuration is limited; converters should not extrapolate from comonomer type alone without pilot-line trials.
On a 60 mm grooved-feed blown-film line with 25 L/D, barrel set points between 170 °C and 190 °C and adapter/die temperatures of 180 °C to 200 °C are used for melt temperatures near 200 °C. A die gap of 1.6 mm to 2.0 mm and a blow-up ratio of 2.0:1 to 3.0:1 produce stable bubbles at gauge from 20 µm to 100 µm. The frost line is generally held at 1.5 to 2.5 die diameters; extension above 3.0 die diameters reduces haze but may destabilise the bubble at relative humidity above 60 %. Because the melt flow rate is 2.0 g/10 min, the resin generates lower specific output in smooth-bore extruders than in grooved-feed machines; a grooved feed section is therefore standard for high-throughput film production. Melt temperatures above 230 °C should be avoided, since oxidative degradation can form carbonyl species, discolouration, and gel particles in the finished film.
Rheological responses for butene linear low-density polyethylene of similar melt index indicate apparent shear viscosity from 900 Pa·s to 1200 Pa·s at 190 °C and 100 s⁻¹; at 1000 s⁻¹ the apparent viscosity falls to 200 Pa·s to 300 Pa·s. Published data for FG 20 I specifically is limited. Die pressure on a 60 mm line is typically held below 35 MPa; pressures above 40 MPa indicate screen blockage, low die temperature, or an excessively narrow die gap and can initiate sharkskin melt fracture. Melt temperature homogeneity at the die is critical: a variation above ±3 °C can produce gauge bands in the finished film. Barrier-flight or Maddock mixer screws improve homogeneity and are recommended when output exceeds 120 kg/h on a 60 mm die.
Manufacturer datasheets list typical values for FG 20 I: tensile stress at yield of 11 MPa under ISO 527-2, tensile strain at break above 700 %, Vicat softening point of 96 °C under ISO 306/A50, Shore D hardness of 52 under ISO 868, and melting temperature of 122 °C under ISO 11357-3. These figures are not specification limits, and the lot certificate remains the binding document for grade conformity. Optical values are thickness-dependent; unpigmented 25 µm blown film can show haze below 15 % under ASTM D1003 and gloss above 60 at 60° under ASTM D2457, but slip and antiblock masterbatches change both values. Table 1 summarises the property cross-check.
| Property | Test method | Typical value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1 | 2.0 g/10 min |
| Density | ISO 1183-1 method A | 0.918 g/cm³ |
| Tensile stress at yield | ISO 527-2 | 11 MPa |
| Tensile strain at break | ISO 527-2 | >700 % |
| Vicat softening point | ISO 306/A50 | 96 °C |
| Shore D hardness | ISO 868 | 52 |
| Melting temperature | ISO 11357-3 | 122 °C |
Regulatory status is determined by the olefin polymer monograph rather than by a proprietary approval. For European food-contact use, the material falls under EU Regulation No 10/2011, Annex I; the overall migration limit for plastic materials is 10 mg/dm² when tested under the conditions in Chapter III and Annex III. United States applications are assessed under 21 CFR 177.1520, paragraphs (a) and (c), covering olefin polymers, subject to finished-article extractables limits. REACH compliance is based on Regulation (EC) No 1907/2006; articles prepared from the resin typically contain no substance of very high concern above 0.1 % w/w. Under Directive 2011/65/EU Annex II, RoHS screening on homogeneous material sets limits of 0.1 % w/w for lead, mercury, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers, and 0.01 % w/w for cadmium.
| Framework | Designation / test | Threshold |
|---|---|---|
| EU food contact | EU 10/2011 Annex I | Overall migration 10 mg/dm² |
| US food contact | 21 CFR 177.1520 | Olefin polymer monograph; end-test required |
| REACH | Regulation (EC) No 1907/2006 | SVHC 0.1 % w/w |
| RoHS | Directive 2011/65/EU Annex II | Pb, Hg, Cr(VI), PBB, PBDE 0.1 % w/w; Cd 0.01 % w/w |
In form-fill-seal packaging for dry foods, FG 20 I is often used as a skin or core layer in coextruded films with high-pressure low-density polyethylene or metallocene linear low-density polyethylene skins. The seal initiation temperature of butene linear low-density polyethylene is lower than high-pressure low-density polyethylene, which permits seal bar setpoints to be reduced by 5 °C to 15 °C at fixed dwell time; the exact value must be measured using ASTM F88 seal-strength testing on the finished laminate. For agricultural tunnel film, ultraviolet stabilisation is required and must be formulated by a masterbatch supplier because base polyethylene does not contain long-term UV absorbers. In collation shrink, the resin is often blended with high-pressure low-density polyethylene at 20 % to 30 % by weight to raise melt strength and shrink force, at the expense of transparency.
Relative to metallocene linear low-density polyethylene of comparable melt index and density, FG 20 I exhibits a broader molecular weight distribution and lower dart drop, but higher melt strength and lower sensitivity to frost line variation. The broad molecular weight distribution improves blown-bubble stability on older air-cooled lines, while the lower melt strength of metallocene grades can require lower frost line heights and narrower air-ring adjustments. In coextrusion, FG 20 I can be combined with metallocene skins to recover dart impact and tear while retaining the processability of the conventional core.
Down-gauging from 35 µm to 18 µm amplifies the solid-state limitations of butene-copolymer linear low-density polyethylene. Because butene introduces ethyl branches, tie-molecule density is lower than in hexene or octene copolymers of equal crystallinity; Elmendorf tear and dart drop therefore decline more steeply with decreasing thickness. On bag-conversion lines running above 120 m/min, film below 25 µm may fail along the machine direction during transverse sealing or gusseting if seal bar pressure exceeds 0.4 MPa and dwell is below 0.2 s. A converter requiring a dart drop above 300 g at 25 µm under ASTM D1709 method A should evaluate a hexene or octene linear low-density polyethylene or a metallocene grade. Blending FG 20 I with high-pressure low-density polyethylene at 10 % to 20 % by weight improves bubble stability and melt strength but reduces clarity and raises seal initiation temperature. Avoid blends with high levels of propylene-based polymers above 20 % by weight, as phase separation reduces dart impact and creates delamination in coextruded layers. Published data for this specific configuration is limited; pilot-line trials on the target extruder and bag converter remain necessary.
Storage of pellets at ambient temperature below 50 °C and protected from ultraviolet light minimises oxidative degradation. Polyethylene is non-hygroscopic, and drying is not required for moisture removal; surface condensation from cold storage should be equilibrated before extrusion to prevent pinholes. Additives should be selected from polyolefin masterbatches with known food-contact compliance, since migration kinetics in polymer matrices can alter regulatory suitability in the finished article.