| HS Code | 159224 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Butene |
| Form | Pellets |
| Color | Natural |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Temperature | 95 °C |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Shore D Hardness | 50 |
| Film Haze | 13% |
| Film Gloss 45 | 60 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Resistance Md | 150 g |
| Elmendorf Tear Resistance Td | 300 g |
| Coefficient Of Friction | 0.2 |
| Blocking | 20 g |
As an accredited Versalis Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene FG 20 F is supplied in 25 kg polyethylene bags, 55 bags per pallet, stretch-wrapped; each pallet holds 1,375 kg. |
| Container Loading (20′ FCL) | 20′ FCL loading: Versalis Flexirene® FG 20 F butene copolymer LLDPE, 25 kg bags, palletized, moisture-protected, secured inside container. |
| Shipping | Versalis Flexirene® FG 20 F is shipped as non-hazardous solid polyethylene pellets, typically in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Store cool, dry, away from sunlight, heat, and moisture; no special dangerous goods classification required. |
| Storage | Versalis Flexirene® FG 20 F Butene Copolymer LLDPE should be stored in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Keep original bags closed and clean, protected from moisture, dust, and contamination. Avoid prolonged storage above 50°C. Stack safely to prevent deformation and rotate stock first-in, first-out. |
| Shelf Life | Typically 24 months when stored in original unopened packaging, cool and dry, away from direct sunlight and heat sources. |
Tubular blown-film conversion of Versalis Flexirene FG 20 F, a butene copolymer linear low-density polyethylene with nominal density 0.920 g/cm³ measured under ISO 1183-1:2019 and nominal melt flow rate 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022, is executed on high-output monolayer and coextruded heavy-duty sack lines. For form-fill-seal shipping sacks and industrial liners, a representative formulation is 70–100 wt% FG 20 F with a fractional-MFI LDPE at 0–30 wt%; internally generated edge trim and start-up film are re-incorporated at 10–20 wt% provided they are dry and free from paper fibre, metal fines, or pallet debris. The melt is processed through a grooved-feed extruder with L/D 30:1, a reverse-taper barrier screw, and a screen pack of 100–250 µm to trap gel particles that would otherwise appear as optical defects or thin spots in the web. Melt temperature at the die head is held between 190 °C and 230 °C; operation above 240 °C is not recommended because surface autoxidation can generate low-molecular-weight odorous species during extrusion and downstream hot-bar sealing. Internal bubble cooling and a dual-lip air ring are required to maintain gauge tolerance at ±8–15%, and a collapsing frame with bowed rollers should be adjusted to prevent centre-to-edge orientation differential. Blow-up ratio is set at 2.5:1–3.2:1 to balance dart impact and machine-direction tear; a lower blow-up ratio increases machine-direction tensile yield but weakens transverse tear resistance. Industry compliance is anchored to REACH Regulation EC 1907/2006, RoHS Directive 2011/65/EU, and, where dry-food contact is specified, FDA 21 CFR 177.1520 and EU Regulation 10/2011. Seal strength is validated by ASTM F88/F88M, dart impact by ASTM D1709, and tensile properties by ISO 527-3:2018. Terminal product types are FFS sacks for mineral fertilizers, petrochemical granular resins, plastic pellet masterbatch, dry construction chemicals, and heavy-duty liners for box and drum containment.
Wide-web agricultural film conversion requires a film that maintains puncture resistance after slit-width reduction, field installation at low temperature, and prolonged UV exposure. In this scenario, FG 20 F is typically formulated at 80–85 wt% with a fractional-MFI LDPE at 15–20 wt%; a carbon black or hindered-amine light stabilizer masterbatch is added at 3–6 phr according to masterbatch supplier let-down guidance. Published data for the specific tensile retention of FG 20 F in multi-season outdoor configurations is limited, so converter trials should measure retained tensile strength under ISO 527-3:2018 and retained dart impact under ASTM D1709 after weathering exposure. Extrusion is performed on blown-film lines with die diameters above 250 mm, die gap 2.2–2.8 mm, and blow-up ratio 2.8:1–3.5:1; higher cross-direction orientation increases Elmendorf tear resistance measured by ASTM D1922. Melt temperature is held between 200 °C and 230 °C. The bubble is stabilised with a high-arch collapsing frame and lateral bubble guides to permit layflat widths greater than 10 m. Wide-web rollstock is wound on steel mandrels and converted into sheets or inlet-mounted rolls. Compliance is driven by EN 13206:2017 for thermoplastic covering films, REACH Regulation EC 1907/2006, and field-use restrictions under national agrochemical contact rules; direct food-contact claims are not standard unless the finished structure is explicitly validated under EU Regulation 10/2011. Terminal product classes are silage clamp cover sheets, bunker silo barrier films, low tunnel film, and soil fumigation sheeting where gauge is 150–250 µm and puncture resistance is the primary mechanical requirement. The main process conflict occurs when the blow-up ratio is too low; moving from 2.0:1 to 3.0:1 improves transverse-bias tear orientation but can increase gauge scatter unless air-ring control is recalibrated.
| Downstream scenario | FG 20 F addition ratio | Primary compliance/test designations | Terminal product types |
|---|---|---|---|
| Heavy-duty FFS sacks | 70–100 wt% | REACH EC 1907/2006; RoHS 2011/65/EU; ASTM D1709 | Fertilizer sacks, resin packaging, dry bulk liners |
| Agricultural covering film | 80–85 wt% | EN 13206:2017; ISO 527-3:2018 | Silage clamp covers, low tunnel film |
| Collation shrink film | 20–40 wt% | ASTM D2732; FDA 21 CFR 177.1520 | Bottle, can, glass jar shrink bundling |
| Laminated pouch sealant web | 100 wt% sealant web | ASTM F88; EU 10/2011 | Snack pouches, sachets, ancillary pharma packs |
| Stretch hood logistics film | 100 wt% | REACH EC 1907/2006; ISO 527-3:2018 | Pallet hoods, tile and beverage tray covers |
Across cast and blown collation shrink extrusion, addition of FG 20 F at 20–40 wt% into a fractional-MFI LDPE matrix provides high-melt-strength base resin for oriented shrink film. The melt blend is processed on high-output blown-film equipment with die gap 2.0–2.3 mm, blow-up ratio 3.0:1–4.0:1, and melt temperature 190–220 °C. After primary bubble collapse, the web is slit and wound with controlled tension because shrink energy is locked in during fast quenching and later released in the hot tunnel. Free shrink is characterised by ASTM D2732; operators adjust frost-line height and take-off speed to shift shrinkage symmetry between machine and transverse directions. Collation packaging is sealed by hot-wire or hot-knife stations that sever and seal in a single step, requiring clean thermal cut formation without char accumulation at 150–180 °C. Compliance designations include FDA 21 CFR 177.1520 and EU Regulation 10/2011 for incidental food-contact overwrap, REACH Regulation EC 1907/2006, and RoHS Directive 2011/65/EU. Terminal products are shrink bundling films for beverage bottles, food cans, glass jars, and paper tissue bundles; thicknesses are normally 40–80 µm, with lower gauge limited by shrink-tunnel burn-through and upper gauge limited by rising shrink force that can distort lightweight containers. The primary process risk is transverse-direction shrink inconsistency caused by uneven air-ring cooling; this is controlled by measuring web width before and after a heated relaxation stage and by keeping the chill-room air temperature below 25 °C.
For flexible packaging laminates, a cast or blown sealant web produced from FG 20 F at 100 wt% is combined with PET, BOPP, or aluminium foil to form the heat-sealable inner layer. The sealant layer is extruded at 20–60 µm on cast-film lines with chill-roll temperatures between 15 °C and 25 °C, then surface-treated by corona discharge to a wetting tension of 38–42 mN/m measured under ASTM D2578 before adhesive lamination. In the overall laminate, the addition ratio is the sealant web thickness fraction, typically 20–35% of total laminate thickness; no intermediate dilution with other polyolefins is required unless a lower seal-initiation temperature is specified. Seal strength is evaluated with ASTM F88/F88M, hot tack with ASTM F1921, and kinetic coefficient of friction with ISO 8295 after slip and anti-block additive dispersion has stabilised for at least 24 h. Regulatory compliance for food contact rests on FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 with overall migration and specific migration verification conducted on the finished laminate, not on the pellet. Terminal product types include dry-food snack pouches, portion sachets, cosmetic wipe outer laminate, and pharmaceutical ancillary packaging when the structure is validated against the applicable pharmacopoeia test for extractables. The process constraint in lamination is the onset of puckering when web tension is too high relative to the low bending stiffness of 20 µm film; this is controlled by reducing roll pressure and maintaining unwind tension under 20 N per linear metre.
When pallet securing is achieved by stretch-hood equipment rather than heat shrink, FG 20 F is extruded at 100 wt% on high-output blown-film lines with die gap 2.0–2.5 mm, blow-up ratio 2.5:1–3.0:1, and melt temperature 190–230 °C. Film gauge is held between 80 µm and 120 µm, and the extruder screw is configured for moderate shear to preserve molecular weight distribution; excessive melt temperature above 240 °C is avoided because it reduces film elongation at break measured by ISO 527-3:2018. The blown film is converted into tubular hoods that are drawn horizontally over a pallet and vertically downward, requiring coefficient of friction below 0.50 on the outside surface and high cling-free slip on the inside surface. Compliance is general chemical registration under REACH Regulation EC 1907/2006 and RoHS Directive 2011/65/EU; direct food-contact use is not standard and requires explicit validation under EU Regulation 10/2011. Terminal product types are stretch hoods for palletised beverage trays, ceramic tile stacks, paperboard sheet bundles, and construction-material loads.
Competitive Versalis Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Among butene-copolymer linear low-density polyethylene grades specified for blown-film conversion, Versalis Flexirene® FG 20 F occupies a defined position in the 0.920 g/cm³ density band. The product is a 1-butene/ethylene copolymer supplied in pellet form and designated for film extrusion. Manufacturer-published typical properties list a density of 0.920 g/cm³ determined to ISO 1183-1:2019 and a melt flow rate of 0.9 g/10 min at 190 °C/2.16 kg determined to ISO 1133-1:2022. The grade is specified for general packaging film, overwrap, carrier film, laminating film, and sealant webs; exact suitability is governed by line trials because film properties are affected by gauge, blow-up ratio, die gap, frost-line height, and downstream treatment. In comparison with high-pressure low-density polyethylene, the polymer architecture lacks long-chain branching and exhibits lower melt strength but higher tensile properties at equivalent density. In comparison with hexene- and octene-copolymer LLDPE grades, the shorter butene branches generally reduce dart impact and Elmendorf tear at equivalent density and MFR, while maintaining a measurable melt-flow/density balance. The nominal data are not release limits; converter specifications must be confirmed through the producer’s certificate of analysis.
The resin’s density of 0.920 g/cm³ lies between lower-density film grades that provide softer sealing and higher-density grades that provide higher modulus. The melt flow rate of 0.9 g/10 min is relatively low for blown-film extrusion, favouring melt strength but requiring sufficient shear heating and screw torque. Screw designs without mixing sections may show lower output and higher melt-temperature variation; therefore the material is commonly run on equipment with barrier screws and stable barrel cooling.
Processing of a 0.920 g/cm³ butene LLDPE in a single-screw blown-film line is controlled by melt temperature, die gap, and cooling-air distribution. Typical extruders used for this grade class have L/D 25:1–30:1, barrier or mixing screw elements, and spiral mandrel or radial-spider blown-film dies. Die gaps for LLDPE are conventionally wider than those used for LDPE; 1.6–2.4 mm gaps are common, with blow-up ratios of 2.0:1–2.8:1. At melt temperatures below 180–190 °C, die shear stress rises and sharkskin may appear at high output, particularly with die gaps below 1.2 mm. At melt temperatures above 230–240 °C, the bubble may lose stalk stability because the elongational viscosity is insufficient to resist internal pressure fluctuations. On production lines with internal bubble cooling and dual-lip air rings, the frost line is typically maintained between 300 mm and 900 mm above the die, depending on film gauge and line speed. Production-scale records often attribute gauge scatter to insufficient air-ring uniformity and frost-line movement; operators commonly observe bubble oscillation if the air-ring pressure is increased without a corresponding rise in melt temperature or die throughput. Published melt-pressure curves specific to FG 20 F are limited; therefore, grade-specific rheology measurements by capillary rheometry at 190 °C and 210 °C across shear rates of 50–1000 s−1 are advised before transferring between equipment with different die diameters. The high-load melt flow rate at 190 °C/21.6 kg according to ISO 1133-1:2022 can be used with the standard MFR to estimate the melt-flow ratio and shear-thinning character, but it does not replace a full viscosity curve.
On a 90 mm single-screw blown-film line with a 300 mm spiral mandrel die running 25 µm film, screw speed and output are limited by torque and cooling capacity. LLDPE with 0.9 g/10 min MFR generally produces higher die pressure than LDPE of similar MFR; die gaps are therefore widened to keep die pressure below common mechanical limits. Production-scale failures observed on this grade class include bubble instability caused by incorrect air-ring settings, wound-roll blocking from inadequate cooling, and gauge scatter caused by melt temperature oscillation. These failures are typically remedied by adjusting internal bubble cooling, reducing suction or exhaust imbalance, and stabilising extruder barrel temperatures within ±3 °C.
Film fabricated from Flexirene® FG 20 F is commonly tested for tensile properties according to ISO 527-3 or ASTM D882, Elmendorf tear according to ISO 6383-2 or ASTM D1922, dart drop impact according to ASTM D1709 Method A, and haze according to ISO 14782. Conditioning is performed for at least 48 h at 23 °C and 50% relative humidity before mechanical testing. Because exact film values are gauge- and process-dependent, the supplier’s nominal resin data cannot replace line-trial results. The butene comonomer gives lower puncture and tear performance than hexene or octene copolymers at the same density; the difference is measurable under 25–50 µm film thickness but may be less pronounced in thicker sheet. In applications where sealing temperature is less critical than abuse resistance, a C6 or C8 grade is usually selected after comparative testing. The FG 20 F grade is therefore used for general packaging where film optics, processability, and consistent gauge control dominate the specification. Published data for this specific configuration is limited, and processors validate substitution through full-film testing.
Water vapour transmission of blown film in this density class is typically measured according to ISO 15106-2 or ASTM F1249; at 0.920 g/cm³ the moisture barrier is higher than high-pressure LDPE of lower density but lower than MDPE/HDPE. Oxygen permeability measured by ISO 15105-2 is not a primary selection criterion for this polyolefin. Optical haze measured by ISO 14782 and gloss measured by ASTM D2457 depend on frost-line height and cooling rate; slow cooling produces larger spherulites and higher haze.
In coextruded structures, the placement of Flexirene® FG 20 F in the sealant skin changes the heat-seal plateau. Butene-copolymer LLDPE typically exhibits a higher seal initiation temperature than an octene-copolymer grade of similar density; the measured difference depends on film gauge, sealing pressure, and dwell time. Seal strength is determined to ASTM F88, and hot tack to ASTM F1921. In multilayer film containing EVOH or polyamide, this polyolefin layer must be bonded with a functional tie resin; direct adhesion to polar barrier polymers is not expected. The butene comonomer distribution influences the crystallization rate of the surface layer, and corona treatment to 38–42 mN/m (ISO 8296) is typical before printing or lamination. The processor should monitor film blocking when this grade is used as the inside skin of a collapsed bubble; winder tension and contact-roller pressure are adjusted to maintain coefficient of friction below target values measured by ISO 8295. Differences from other LLDPE products become pronounced in this layer: conventional C4 grades tend to provide wider processing windows on older lines, whereas metallocene grades may offer lower extractables and better optical performance but often require more precise temperature control.
Blending FG 20 F with LDPE at 5–20 wt% is practiced on lines where bubble stability is insufficient. At higher LDPE addition, haze increases and seal initiation shifts upward; at lower addition, the improvement in bubble support may be negligible. The blend ratio is therefore set by trial, with film properties measured for dart impact and tear. In comparison with high-pressure LDPE, the LLDPE component contributes improved tensile strength and permits reduced gauge for equivalent tensile performance but reduces machine-direction tear in some formulations. Published data for the exact FG 20 F/LDPE blend family is limited; the processor should generate blend curves on the target line.
Compared with Flexirene® C4 grades of different density, FG 20 F is selected when the film must balance stiffness and sealability; lower-density C4 grades provide softer sealing and higher dart impact, while higher-density grades increase modulus and moisture barrier. The difference is density-driven and is confirmed by ISO 1183-1:2019 and film tear measurements rather than by melt flow rate alone.
Storage of polyethylene pellets is not as moisture-sensitive as polyamide or polyester, but condensation control remains important. Sacks should be stored in closed indoor conditions at 5–40 °C and kept away from direct sunlight. If material has been cold-stored, sealed bags should be allowed to equilibrate to 20–25 °C before opening; condensation on pellet surfaces at relative humidity above 80% can produce surface moisture that may require drying at 60–70 °C for 2–4 h only if moisture is observed. Flexirene® FG 20 F is not supplied as a UV-stabilised agricultural film grade; outdoor service requires addition of a UV stabiliser masterbatch at the processor’s site, with accelerated weathering validated by ISO 4892-2 or equivalent. The product is not intended for medical implant applications. Food-contact status should be confirmed through the supplier’s declaration; polyethylene of this composition is typically assessed under FDA 21 CFR §177.1520 and EU Regulation (EU) No 10/2011 as amended. Compliance of the finished article with overall migration limits requires testing according to EN 1186-2 and specific migration methods relevant to the food simulant. Migration of lipophilic additives into fatty simulants is time- and temperature-dependent; the converter must verify organoleptic properties and printing-ink offset through end-use testing.
| Standard or regulation | Scope |
|---|---|
| ISO 1183-1:2019 | Determination of resin density |
| ISO 1133-1:2022 | Melt flow rate at 190 °C/2.16 kg |
| FDA 21 CFR §177.1520 | Olefin polymer suitability for food-contact surfaces |
| EU Regulation (EU) No 10/2011 | Plastics intended for food contact |
| EN 1186-2 | Overall migration testing in food simulants |
| REACH (EC) No 1907/2006 | Registration, evaluation, authorisation and restriction of chemicals |
Edge trim and rejected film from FG 20 F are compatible with mechanical recycling streams within polyolefin recycling facilities. Regrind addition is normally controlled at 10–20 wt% of the total feed to avoid gel accumulation; higher levels can be used only where the reclaim is clean and homogeneous. The material does not contain halogenated flame retardants or PVC. Disposal by incineration with energy recovery follows local regulatory requirements; the combustion products are those typical of polyethylene hydrocarbons.