    Specifications
    HS Code 994050
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.925 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 122 °C
    Vicat Softening Temperature 96 °C
    Tensile Strength At Break 28 MPa
    Elongation At Break 800 %
    Flexural Modulus 260 MPa
    Dart Drop Impact 140 g
    Elmendorf Tear Resistance Md 110 g
    Elmendorf Tear Resistance Td 240 g
    Haze 11 %
    Gloss 45 80
    Blocking 40 g
    Coefficient Of Friction 0.20

    As an accredited Versalis Flexirene® FF 25 U Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene FF 25 U LLDPE film grade is supplied in 25 kg polyethylene bags, typically 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL loaded with Versalis Flexirene® FF 25 U Film Grade LLDPE, palletized 25 kg bags, shrink-wrapped, max payload.
    Shipping Versalis Flexirene® FF 25 U Film Grade LLDPE is shipped as non-hazardous, free-flowing pellets in 25 kg moisture-barrier bags or 1,000 kg big bags, palletized and stretch-wrapped. Transport in clean, dry trucks, containers, or railcars at ambient temperature; protect from moisture, heat, sunlight, and contamination. No special dangerous-goods documentation required.
    Storage Store Versalis Flexirene® FF 25 U in a clean, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, ignition sources, and strong odors. Keep bags sealed, on pallets, off the floor, and avoid excessive stacking. Protect from moisture, dust, and contamination. Maintain moderate ambient temperatures and use first-in, first-out stock rotation.
    Shelf Life Typically 24 months from production when stored unopened in original packaging, dry, below 40°C, away from direct sunlight and heat.
    Application of Versalis Flexirene® FF 25 U Film Grade LLDPE

    On high-output three-layer blown film lines producing 80 μm to 120 μm heavy-duty sacks, Flexirene FF 25 U is normally fed as the core layer without pre-drying unless ambient relative humidity exceeds 60% for more than 12 h prior to processing. The nominal melt flow rate of the resin is 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022, and the density is 0.918 g/cm³ under ISO 1183-1:2019. Extruder configuration comprises grooved feed bushings, 30:1 L/D barrier screws, and a die gap of 1.2 mm to 1.5 mm. Melt temperatures are held between 180 °C and 205 °C, with die pressure below 280 bar to avoid screw-speed-induced pulsation. The bubble is operated at a blow-up ratio of 2.2:1 to 2.6:1 and a frost line height between 600 mm and 800 mm.

    Blending with LDPE at 20 wt% to 40 wt% stabilizes bubble geometry and increases melt strength. The direction of the effect on dart impact and machine-direction tear is evaluated by ASTM D1709-16a, ISO 7765-1:2015, and ASTM D1922-15. Published data for this specific blend configuration is limited; converters qualifying heavy-duty sacks therefore run a three-point LDPE ladder at 20 wt%, 30 wt%, and 40 wt% to capture the inflection in tear-propagation resistance. Valve sacks and FIBC liners that require high tear-propagation resistance are generally processed at the lower LDPE addition, while paper-sack film and loose-fill sacks use the higher LDPE content to maintain low backpressure and stable bubble geometry.

    Sealing on high-speed form-fill-seal lines is performed with impulse sealers set to 135 °C to 150 °C and dwell times of 0.5 s to 0.8 s. Seal strength is measured under ASTM F88/F88M-21, and hot tack is measured under ASTM F1921/F1921M-18. Inadequate backpressure or poor mixing produces unmelted gels that act as seal defects and may reduce hermetic package integrity under ASTM F2096-11. Gels also create localized thickness reduction at the seal interface, increasing the risk of channel leakers during drop tests performed according to ASTM D5276-19.

    Where Does High-Stalk Extrusion Introduce Machine-Direction Tear Anisotropy?

    In high-stalk blown film processing, the stalk height is maintained at 8 to 12 times the die diameter before the frost line, compared with the low-stalk 600 mm to 800 mm setting used for heavy-duty sacks. The elongational stress imposed on the molten tube increases as the stalk height advances. Tensile elongation at break measured under ISO 527-3:2018 on 25 μm mono-layer film can fall below 600% in the machine direction while remaining above 700% in the transverse direction, although published data for this exact grade in high-stalk geometry is limited. This anisotropy is selected for perforation resistance but can reduce bag drop resistance if the film is sealed parallel to the machine direction.

    Bubble instability in high-stalk geometry is observed as a sinusoidal oscillation with a frequency of 1 Hz to 2 Hz when melt temperature at the die falls below 170 °C. The correction is a reduction in screw speed to 90 min⁻¹ or an increase in the lower die zone setpoint by 10 K. Die pressure below 240 bar is preferred because higher pressure amplifies die-lip pressure oscillation and generates gauge bands. Qualification trials should include repeated runs over 4 h to detect drift in bubble diameter and frost line height.

    Agricultural Silage Film Oxygen Ingress Barriers and Residual Acidity

    For silage film produced from Flexirene FF 25 U, the typical construction is a three-layer coextrusion with a white outer layer, a carbon-black or white middle layer, and a tackified inner layer. Target oxygen transmission at 25 μm is below 8,000 cm³/(m²·day·bar) under ASTM D3985-17 at 23 °C and 0% RH. The ethylene-based LLDPE chemistry provides cold-temperature flexibility for bale wrapping, but the resin is supplied without UV stabilization and must be compounded with a hindered amine light stabilizer masterbatch for outdoor storage exceeding 6 months.

    Farm-scale exposure to silage acids requires the film to retain at least 50% of initial elongation at break after 18 months contact with acetic and lactic acid solutions. Accelerated screening under ISO 4892-2:2013 xenon-arc weathering and ISO 175:2010 chemical resistance provides comparative data; published data for this exact grade in silage liquor is limited, and producer datasheets do not replace farm-scale trials. The film should not be stored in contact with aromatic hydrocarbon solvents or strong oxidizing agents, because environmental stress cracking may initiate at printing or folding creases.

    A five-layer barrier film for processed meat packaging can use Flexirene FF 25 U in the skin and tie layers around an EVOH core. The structure matches maleated LLDPE tie layers and a low-melt-index LDPE seal layer. At a total gauge of 70 μm, the EVOH content is held to 8 μm to 10 μm, with LLDPE skins contributing 45 μm to 50 μm of the structure. Interlayer adhesion is checked after ethylene oxide sterilization or pasteurization; peel strength between EVOH and tie layer measured by ASTM F904-16 should exceed 4 N/15 mm before retort. Die design must avoid extended residence time above 220 °C, because EVOH degradation produces acetic acid and can lower the pH of the adjacent LLDPE melt, reducing adhesion and creating gels.

    Regulation (EU) No 10/2011 requires overall migration below 10 mg/dm² for this compliant polyolefin food-contact layer. For shipments into the United States, FDA 21 CFR 177.1520 provides the olefin polymer specification and extraction test framework. The resin must be verified against the certificate of analysis for heavy metals and residual catalyst; packaging converters must file a declaration of compliance under EU 10/2011 Article 15.

    When Frozen-Food Packaging Demands Puncture Resistance at -30 °C

    Frozen-food bags manufactured from Flexirene FF 25 U are exposed to repeated flexing at low temperature. Films for IQF vegetables and seafood are produced at 50 μm to 70 μm gauge where the cold-temperature brittleness of conventional LDPE produces leakers. The key test is puncture resistance under ASTM D5748-19 at -25 °C and the impulse seal integrity after conditioning at -18 °C. Blown film produced at a blow-up ratio of 3.0:1 develops higher transverse direction tear resistance but lower machine direction tear resistance. The orientation balance must be adjusted for bag opening and print registration, particularly when the film is surface-printed with nitrocellulose-based inks.

    Cold-room sealing lines run at 130 °C to 145 °C. If the film is overdrawn, the heat-seal initiation temperature increases and the seal window narrows. Operators measure seal strength with ASTM F88/F88M-21 after conditioning at 4 °C for 24 h. Failure at the seal-to-film interface rather than film tearing indicates insufficient wetting, corrected by raising seal bar temperature 5 K or increasing dwell by 0.2 s. Wetting is also impaired by excessive slip additive blooming at the sealing surface; slip levels above 800 ppm erucamide are not recommended for the seal layer.

    Melt Fracture, Die-Lip Shear Stress, and Gauge Band Formation in Liner Applications

    Because can liners and waste sacks require high throughput on narrow die gaps of 0.8 mm to 1.0 mm, Flexirene FF 25 U may exhibit sharkskin melt fracture at screw speeds above 120 min⁻¹ on a 70 mm extruder. The critical wall shear stress for liner-grade LLDPE at the die lip ranges from 0.1 MPa to 0.3 MPa depending on melt temperature and molecular weight distribution, and sharkskin appears as regularly spaced transverse ridges with a wavelength of 0.5 mm to 2.0 mm. Gauge bands arise from melt flow instability in the die, not from die gap irregularities. Reducing die lip temperature by 5 K or decreasing screw speed by 10% suppresses sharkskin without the use of processing aids.

    When line speed cannot be reduced, a fluoropolymer processing aid masterbatch is used at 200 ppm to 400 ppm active content to condition the die metal surface. The additive is not part of the standard grade and must be incorporated without exceeding 0.1 wt% total, because higher levels can reduce heat-seal strength. The compounded film should be checked for optical defects using ASTM D2457-13 gloss and ASTM D1003-13 haze measurements, because processing aid accumulation is visible as surface haze if the die is not purged after each production run.

    Free Quote

    Competitive Versalis Flexirene® FF 25 U Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® FF 25 U is a butene-copolymer linear low-density polyethylene film resin supplied as pellets for blown-film conversion. Public technical data position the grade with a nominal density of 0.919 g/cm³ and a melt flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load when tested according to ISO 1133-1:2022. The resin is intended for general-purpose packaging films, heavy-duty sacks, liners, carrier bags, lamination substrates, and collation-shrink or stretch-hood structures. The FF 25 U designation identifies a film-grade package; the U suffix and the exact slip/antiblock loading must be confirmed against the current Versalis technical data sheet because additive levels can vary by production location. Compared with high-pressure LDPE film grades, FF 25 U provides higher tensile yield and puncture resistance at equivalent thickness, but its linear molecular architecture reduces melt strength and narrows the bubble-stability window unless the line uses blending or specific die-gap adjustments.

    Table 1. Indicative property envelope for Versalis Flexirene® FF 25 U; values should be verified against the current technical data sheet and lot certificate.
    PropertyTest methodTypical range
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20220.9–1.0 g/10 min
    DensityISO 1183-1:20190.918–0.920 g/cm³
    Tensile stress at yield, MD/TDISO 527-3:201810–12 MPa
    Tensile elongation at break, MD/TDISO 527-3:2018>600%
    Dart drop impact, F50, 25 µmISO 7765-1:200590–130 g
    Elmendorf tear, MDISO 6383-2:19833–6 N
    Elmendorf tear, TDISO 6383-2:19836–10 N
    Haze, 25 µmISO 14782:19998–15%
    Vicat softening temperature, A50ISO 306:202295–100 °C

    How does FF 25 U compare with high-pressure LDPE and higher-alpha-olefin LLDPE?

    Relative to high-pressure LDPE, FF 25 U has a higher concentration of tie molecules at the same film density because the short-chain branches from butene are placed along a linear backbone without the extensive long-chain branching of autoclave or tubular LDPE. The result is higher dart drop impact at 25 µm, often in the range 90–130 g for FF 25 U instead of 40–80 g for a comparable film-grade LDPE, measured by ISO 7765-1:2005. Tensile yield strength is also higher, typically 10–12 MPa versus 7–10 MPa for LDPE. However, strain-hardening character and melt strength are lower in FF 25 U, so the bubble is less tolerant of variable air drafts, high blow-up ratios, and sudden changes in internal bubble pressure. Compared with hexene-based LLDPE, FF 25 U has lower dart impact and tear propagation at similar density because the butene branch is shorter and less effective in disrupting crystallinity. Compared with octene-based metallocene LLDPE, the differences are larger in hot-tack, sealing onset, and puncture resistance. In blown film, octene-based metallocene LLDPE may show Elmendorf tear values in the machine direction that are 20–40% higher when compared under ISO 6383-2:1983, although this difference narrows at higher film gauges and depends on orientation balance. Published data for a direct FF 25 U head-to-head comparison with a specific metallocene grade is limited.

    In single-layer blown-film lines with extruder screw diameters from 45 mm to 90 mm and length-to-diameter ratios of 25:1 to 30:1, the barrel temperature profile is commonly set between 180 °C and 220 °C, with adapter and die zones at 210 °C to 230 °C. Die gap selection is a primary control factor: a 1.5 mm die gap intensifies shear and improves mixing but raises backpressure; a 2.5 mm gap reduces melt pressure and can increase output at the expense of orientation. A blow-up ratio of 2.0:1 to 2.5:1 and frost line height of 4 to 8 die diameters maintain gauge uniformity for films from 20 µm to 150 µm. When melt temperature exceeds 250 °C, oxidative degradation can generate crosslinked gel particles that appear as fish eyes; residence time in the die and adapter should therefore be kept below 5 min at these temperatures. If backpressure on a 45 mm extruder exceeds 250 bar, the addition of 5–10 wt% high-pressure LDPE reduces shear heating and stabilizes the bubble, but lowers dart impact proportionally.

    Extruder feed behavior also differentiates FF 25 U from high-pressure LDPE. The pellets are harder and can bridge in the feed throat if the hopper temperature is too high; grooved-feed barrels improve solids conveying but increase barrel wear. Barrier screw designs with a melt channel length of 10–12D are applied at output rates up to 1.0 kg/h per mm of screw diameter. Beyond that output, unmelted material can persist and appear as pinholes in thin film. Maintaining rear barrel temperatures below 200 °C in the feed zone avoids premature pellet agglomeration while the compression section completes melting before the die.

    Melt fracture and gel formation become the controlling limits above 250 °C

    Processing of FF 25 U at the upper end of the film extrusion envelope is governed by the interaction of shear rate, melt temperature, and additive stabilization. On dies with narrow gaps and high output, melt fracture appears as sharkskin or cyclic gloss bands on the film surface. The onset of melt fracture for butene LLDPE is generally at shear rates above 1000 s⁻¹ in the die land; in practice this corresponds to high-output lines where specific output exceeds 1.5 kg/h per mm of die circumference. Because FF 25 U has a relatively narrow molecular weight distribution compared with blown-film LDPE, the shear-thinning response is less pronounced, so die pressures can remain high at low melt temperatures. Adding processing aids or using a wider die gap reduces fracture severity. Gel formation becomes a separate limit when melt temperature exceeds 250 °C in the presence of oxygen; the induction time under oxidative conditions shortens rapidly above this temperature. Field observations on single-layer lines show that frequent screen-pack changes and die lip cleaning are necessary when the same resin lot is kept in the extruder during line stoppages longer than 30 min at temperatures above 220 °C.

    When seal dwell time drops below 250 ms on vertical form-fill-seal lines

    Seal performance of FF 25 U in high-speed vertical form-fill-seal service depends on sealing pressure, dwell time, and jaw geometry. The seal initiation temperature is typically observed from 95 °C to 110 °C on films in the 30–60 µm thickness range when tested with flat heated jaw sealers at 0.3–0.5 N/mm². Compared with metallocene-catalyzed octene LLDPE, FF 25 U has a narrower hot-tack plateau and a higher minimum seal temperature, which can reduce sealing throughput when dwell times fall below 250 ms. Films requiring high hot-tack strength should be evaluated by ASTM F1921 on the actual packaging line because published hot-tack curves for this specific resin configuration are limited. The butene-based melting endotherm peak is near 122 °C to 124 °C by ISO 11357-3:2018; this supports a stable seal plateau but also means that sealing at excessive jaw temperature can create edge thinning and stringing. For heavy-duty sacks, the seal temperature is set above 115 °C to achieve full bond strength, but the film must be supported by correct jaw release timing to prevent distortion.

    For lamination substrates and heavy-duty sacks, FF 25 U is specified when the converter prioritizes tear resistance in the transverse direction and puncture resistance over high melt strength. On solventless lamination lines, the film is corona treated to surface energies above 38 mN/m before adhesive coating; treatment levels decay with time and storage temperature, so in-line treatment is preferred. On flexographic and rotogravure presses, the surface must be re-verified because slip additives can migrate to the corona-treated surface and reduce adhesion. In stretch-hood and silage film applications, the butene LLDPE base is commonly blended with metallocene LLDPE or LDPE to adjust cling, puncture, and elongation; a pure FF 25 U structure may be insufficient for high-performance agricultural films because dart impact and tear propagation limits become visible at thicknesses below 25 µm.

    Dart impact, tear propagation, and optical haze as downgauging thresholds

    Downgauging trials with FF 25 U are constrained by three measurable property thresholds. Dart drop impact at 25 µm is typically 90–130 g, but values fall as film thickness is reduced toward 12–15 µm; in load-stability applications, a minimum dart drop of 60 g is often used as a practical acceptance limit, depending on pack geometry and cold-chain handling. Elmendorf tear in the machine direction is the more restrictive property for thin film because the orientation balance created by the blow-up ratio and frost line can shift failure from a ductile to a brittle mode. Haze is typically 8–15% at 25 µm under ISO 14782:1999, and gloss is influenced by die gap and frost line; a high frost line combined with low melt temperature can increase haze beyond 15% by promoting surface roughness. For high-clarity lamination, a metallocene-catalyzed octene LLDPE is usually preferred unless the lower cost structure of FF 25 U can be compensated by a thicker gauge or by blending with LDPE.

    Compliance for food-contact applications must be established from the lot-specific declaration. Olefin polymers of this composition are generally covered by FDA 21 CFR 177.1520 for food-contact uses subject to end-use limitations and migration testing, and by EU Regulation 10/2011 when the converter validates the overall migration limit against the intended food simulant. The product is not a direct food additive and should not be used in contact with strong oxidizing agents or solvents at temperatures above the stated use condition. For non-food packaging, compliance with REACH and the EU Packaging Directive 94/62/EC requires confirmation of the additives and heavy metals in the finished packaging article. Storage of pellets should be in dry conditions; if relative humidity exceeds 60%, surface condensation during transfer from cold storage can introduce moisture defects in the film. Pellets stored below 10 °C should be conditioned to ambient temperature before entering the hopper to avoid condensation on the pellet surface.