Versalis Flexirene Ff 25 Butene Copolymer Linear Low Density Polyethylene

Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 270852
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.925 g/cm³
    Meltflowrate 190c 2 16kg 0.8 g/10 min
    Meltingpoint 120 °C
    Vicatsofteningtemperature 95 °C
    Tensilemodulus 250 MPa
    Tensilestressatyield 10 MPa
    Tensilestrainatbreak 700 %
    Dartdropimpact 120 g
    Haze 10 %
    Gloss 45deg 80 %
    Coefficientoffriction 0.2
    Molecularweightdistribution Broad
    Thermaloxidativestability Good

    As an accredited Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® FF 25 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading: Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene in 25 kg bags, approximately 20 metric tons.
    Shipping Versalis Flexirene® FF 25 Butene Copolymer LLDPE is a non-hazardous solid resin. It is typically shipped in sealed 25 kg bags, bulk bags, or octabins, palletized and shrink-wrapped. Use standard land or sea freight. Store dry, away from heat, sunlight, and moisture; no dangerous-goods classification applies. Ensure labels remain intact.
    Storage Store Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and ignition sources. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged temperatures above 50°C and UV exposure. Use first-in, first-out rotation, and handle with appropriate grounding to control static.
    Shelf Life Shelf life is 24 months from production date when stored in original packaging, dry, cool, ventilated, away from direct sunlight.
    Application of Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene

    Heavy-duty industrial sack film failures concentrate at sewn seams, not at the centre of the panel; torn stitch holes are the primary field return in sacks carrying granular polymer and mineral products. A monolayer or three-layer blown film structure formulated with 70–85 wt% FF25, 10–20 wt% LDPE, and 0–5 wt% HDPE as modulus correction is processed on grooved-feed blown film lines with L/D 30:1, die diameter 250–350 mm, die gap 2.0–2.5 mm, blow-up ratio 2.5:1 to 3.5:1, and melt temperature 190–215 °C. Frost line height is kept between 6× and 10× die diameter; when a 300 mm die is operated above its stable output band, bubble flutter at the nip increases thickness variation beyond ±6%, requiring either a 5 °C reduction in melt temperature or a lower BUR setpoint. Regulatory compliance for these structures is anchored to ISO 21898:2004 for FIBC construction, UN 13H3/UN 13H4 for dangerous goods liner qualification where applicable, ASTM D1709 for dart drop impact, and ISO 527-3 for film tensile properties. Terminal product types include sewn heavy-duty shipping sacks for polymer granules, FIBC inner liners for fine chemicals, and protective overpacks for granular fertilizer.

    Why Do Silage Cover Films Favor Butene Copolymer Fractions Over Hexene-Toughened Grades in UV-Stabilised Blends?

    For silage clamp covers, the critical film requirement shifts from high-speed puncture to low-temperature flexure and long-wave UV resistance over storage periods of 9–14 months. A formulation of 95–100 wt% FF25 plus 1–3 wt% UV-stabiliser masterbatch containing HALS and carbon black or titanium dioxide is blown in thicknesses from 80–150 µm; the butene comonomer distribution in FF25 maintains fold-over flexibility when silage shoulders are covered at ambient temperatures below 5 °C. Mono-layer blown film processing on a 200 mm die with a 1.8–2.4 mm die gap and blow-up ratio 2.2:1 requires grooved feed sections to remain below 240 °C to prevent crosslinked gel particles from reprocessed edge trim. Weathering stability is validated under ISO 4892-2, thickness uniformity under ISO 4593, and agricultural film classification under EN 13206:2017. Published data for the specific FF25 UV formulation under ISO 4892-2 cycles is limited; outdoor lifetime claims should be supported by converter-run weathering trials rather than extrapolation from accelerated tests alone. Terminal products include silage clamp covers, bunker silo side sheets, greenhouse side curtains, and temporary compost windrow covers.

    Cast film lamination for flexible packaging processes a sealant web formulated at 70–100 wt% FF25, extruded at 220–250 °C through a coextrusion feedblock and nipped onto PET or BOPP primary substrates; direct food-contact compliance is governed by EU (EU) No 10/2011 and FDA 21 CFR 177.1520, seal strength is measured under ASTM F88, and hot tack under ASTM F1921. Terminal products include dry snack pouches and single-serve sachets.

    When Pallet Load Stability Depends on Transverse Direction Tear Resistance Rather Than Machine Direction Stretch

    During pallet unitization, film failures occur at the pallet corners where transverse direction tear and dart impact are both limiting; a three-layer A/B/C blown film structure is therefore formulated with 70–90 wt% FF25 in the core layer, 10–20 wt% LDPE in the skins, and 1–3 wt% cling masterbatch in the inner skin, with 5–10 wt% HDPE optionally replacing an equivalent LDPE fraction for higher load rigidity. The structure is processed on a coextrusion blown film line equipped with internal bubble cooling, a die gap of 2.0–2.5 mm, blow-up ratio 4.0:1 to 5.0:1, and melt temperature 190–210 °C. Transverse stretch ratios are typically limited to 110–130%; above this range stress whitening and pallet-corner tear initiation increase. Compliance is evaluated by ISO 527-3:2018 for tensile properties, ISO 6383-2:1983 for Elmendorf tear, ASTM D1709 for dart drop, and ASTM D5458 for cling behaviour. Terminal products include stretch hood covers for palletized building materials, chemical bags, beverage kegs, and domestic appliance packaging.

    Frozen Food Films Shift Ductile-to-Brittle Threshold Downward in High-Speed Vertical Form-Fill-Seal Lines

    High-speed vertical form-fill-seal packaging of IQF products imposes a narrow seal window because the film must achieve seal bar adhesion without melting through the outer surface at short dwell times. A three-layer blown film structure containing 85–100 wt% FF25 in the core and 0–15 wt% LDPE dilution in the skins, with anti-fog masterbatch at 0.5–2.0 wt% in the sealant skin, is processed on a coextrusion line with die gap 1.8–2.0 mm, blow-up ratio 2.5:1 to 3.0:1, and melt temperature 185–210 °C to minimize thermal oxidative gel formation. Seal strength is validated under ASTM F88, hot tack under ASTM F1921, and low-temperature impact resistance under ASTM D1709 or ISO 7765-1. Direct food-contact compliance is governed by FDA 21 CFR 177.1520, EU (EU) No 10/2011, and Regulation (EC) 1935/2004. Terminal products include frozen vegetable bags, IQF poultry film, and frozen seafood pillow packs.

    For temporary surface protection of stainless steel coil and aluminium composite sheet, a three-layer cast coextruded structure is used in which the core layer is formulated with 70–90 wt% FF25 and 10–30 wt% LDPE, while the adhesive skin layer contains a polyolefin elastomer or EVA plus tackifier at 5–15 wt%; the film is extruded at 200–230 °C through a 0.7–1.0 mm die gap and nipped to a polished chill roll maintained at 15–25 °C to set low-haze surfaces. Peel adhesion is measured under ASTM D3330 Test Method A; EU compliance is covered by REACH 1907/2006, RoHS 2011/65/EU, and CLP Regulation 1272/2008 for adhesive components. Using FF25 in the core limits adhesive migration into the film after 30-day contact with textured stainless steel, though published data for specific peel adhesion retention after outdoor ageing of FF25-based protective films is limited. Terminal product types include protective films for stainless steel coil, aluminium composite panels, glass sheets, and furniture edge-banding laminates.

    ScenarioLayer positionFF25 addition rangeCompliance / boundary standard
    Heavy-duty sacks / FIBC linersMonolayer core70–85 wt%ISO 21898:2004, UN 13H3/UN 13H4, ASTM D1709, ISO 527-3
    Silage coversMono-layer95–100 wt%EN 13206:2017, ISO 4892-2, ISO 4593
    Lamination sealant webCast sealant layer70–100 wt%EU (EU) No 10/2011, 21 CFR 177.1520, ASTM F88, ASTM F1921
    Stretch hood3-layer core70–90 wt%ISO 527-3:2018, ISO 6383-2:1983, ASTM D5458
    Frozen food packaging3-layer core85–100 wt%FDA 21 CFR 177.1520, EU (EU) No 10/2011, ASTM F88, ASTM D1709
    Surface protection filmCast core70–90 wt%ASTM D3330, REACH 1907/2006, RoHS 2011/65/EU
    Free Quote

    Competitive Versalis Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® FF 25 is a butene-1 copolymer linear low density polyethylene supplied by Versalis S.p.A. The grade is intended for blown film extrusion and is characterized by a nominal density of 0.918 g/cm³ determined in accordance with ISO 1183-1:2019 and a nominal melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load, determined in accordance with ISO 1133-1:2022. The polymer architecture consists of a linear ethylene backbone with short-chain branches introduced by butene-1 incorporation, reducing crystalline density relative to high density polyethylene while retaining film stiffness. The resin is supplied in pellet form and is typically formulated with antioxidant, slip, and antiblocking additives; exact lot-specific additive concentrations and food-contact statements must be confirmed against the current manufacturer technical data sheet.

    What Distinguishes a Butene-1 Copolymer from Long-Chain Alternatives?

    Short-chain branch length controls crystallization kinetics, solid-state stiffness, and tie-chain formation in linear low density polyethylene. Butene-1 comonomers produce a less efficient density reduction per mole than octene-1 or hexene-1; consequently, at equal density, a butene-based LLDPE tends to retain higher crystalline fraction and exhibits higher modulus but lower dart impact and Elmendorf tear resistance than an octene-based resin of equivalent melt index. The conventional polymerization chemistry used for many butene LLDPE grades also yields a broader molecular weight distribution than metallocene-catalysed long-chain comonomer grades, which typically reduces die pressure at equal throughput but does not provide the same low-seal-initiation clarity profile.

    In comparison with high-pressure low density polyethylene, the linear butene copolymer has lower melt strength and a narrower bubble stability window on air-cooled lines. In comparison with metallocene C6 or C8 LLDPE, the butene grade generally occupies a more rigid, less impact-resistant position but offers better processing on simple extruders without high-pressure LDPE blending. At the melt flow rate of 1.0 g/10 min, the molecular weight is relatively high, favoring impact strength and bubble load-bearing capacity while limiting drawdown to gauges below approximately 20 µm on conventional monolayer lines unless optimized internal bubble cooling is available.

    On 40 mm to 60 mm grooved-feed extruders with L/D 24:1 to 30:1, stable extrusion of this grade is maintained with a flat or slightly reversed temperature profile: feed zones at 170–180 °C, compression and metering zones at 190–200 °C, and die zones at 200–210 °C. Melt temperature should not exceed 230 °C for extended periods because thermo-oxidative chain scission increases gel formation and reduces transverse-direction tear strength. The die gap is set between 1.0 mm and 2.0 mm; larger gaps reduce die shear stress but may produce lower draw stability, while smaller gaps increase wall shear stress and narrow the shark-skin-free processing window. A blow-up ratio of 2:1 to 3:1 balances machine-direction and transverse-direction orientation. Blow-up ratios below 1.8:1 create high machine-direction tear anisotropy, and ratios above 3.5:1 on conventional external air rings are associated with bubble whip and gauge variation.

    Frost line height is typically positioned between 5 and 8 die diameters. A frost line below 4 die diameters chills the bubble too rapidly and may reduce transverse-direction tear strength; a frost line above 9 die diameters permits slow crystallisation and can elevate spherulitic haze. On production-scale lines, operators adjust air-ring lip geometry and internal bubble cooling pressure rather than making abrupt screw-speed changes when gauge bands appear, because sudden screw-speed changes alter viscous dissipation, back pressure, and melt temperature at the die, which then shifts bubble diameter and film thickness profile.

    Moisture sensitivity is low, but opened bags stored at relative humidity above 60% can develop pellet surface moisture that appears as bubbles or splay during film extrusion. Pre-drying at 60 °C for 2–4 h in a desiccant dryer is applied when surface moisture is visible or when start-up porosity defects occur.

    Film property benchmarks are reported under standardized test conditions.

    Mechanical, optical, and seal performance data for Flexirene® FF 25 are meaningful only when specimen thickness, conditioning, and testing speed are fixed. Blown film produced at 50 µm nominal gauge is commonly characterized by ISO 527-3 for tensile properties, ISO 7765-1 for dart impact, ISO 6383-2 for Elmendorf tear, ASTM D1003-21 for haze, and ASTM D2457-21 for gloss. Butene LLDPE films in this density and melt-flow class typically show tensile strength at break above 20 MPa and elongation at break above 500%; exact lot-average values for this specific grade may vary because catalyst residues, additive dispersion, and melt homogenization influence the failure mechanics.

    Differential scanning calorimetry in accordance with ISO 11357-3 places the melting peak of this density class in the range 120–124 °C, with a broad crystallization exotherm that depends on cooling rate. At a reference cooling rate of 10 K/min, the non-isothermal crystallization shifts to lower temperature and reduces crystalline perfection, lowering density slightly and improving impact strength while reducing modulus. Capillary rheometry at 190 °C indicates shear-thinning behavior with a power-law index of approximately 0.3–0.4 in the 100–1000 s⁻¹ shear-rate range typical of film dies. The activation energy for viscous flow is low compared with polar polymers; a 10 °C melt-temperature change alters apparent viscosity by roughly 5–7%, which explains why bubble stability responds more strongly to air-ring and frost-line settings than to small temperature adjustments.

    When Seal Initiation and Hot Tack Demand Tight Control

    In high-speed vertical form-fill-seal and pouch packaging, seal initiation temperature and hot tack determine whether seal-bar dwell time can be reduced below 0.5 s. Butene-1 LLDPE of this density class typically exhibits a seal initiation temperature approximately 5–10 °C lower than high-pressure LDPE of equivalent density, because the lower melting peak permits interfacial chain interdiffusion at lower jaw temperatures. However, the hot-tack plateau is narrower than for metallocene-catalysed very low seal resins; a drop of 3–5 °C in jaw temperature near the seal initiation boundary can produce intermittent leaks and higher reject rates. Blending 10–20 wt% high-pressure LDPE broadens the sealing range and improves bubble stability but raises haze and reduces film stiffness.

    Corona treatment for lamination or printing is typically conducted to reach surface energies of 38–42 mN/m. Decay of surface energy after treatment is faster on nonpolar butene-based LLDPE than on polar substrates or long-chain comonomer LLDPE with different surface restructuring kinetics. Rewound film stored for more than 24 h may require retreatment if surface energy falls below 38 mN/m. This constraint is relevant in structures using polyurethane adhesives or solvent-based inks that require persistent wettability.

    Melt fracture, shark skin, and bubble oscillation are the principal extrusion defects on high-output blown film lines running butene LLDPE. Shark skin initiates near the die exit when wall shear stress exceeds approximately 0.14 MPa. On small production lines with 50 mm extruder and 1.2 mm die gap, the onset can appear at throughputs reported between 50 kg/h and 90 kg/h, depending on melt temperature and die geometry. Addition of 2–5 wt% high-pressure LDPE or a fluoropolymer processing aid shifts the defect to higher output, but fluoropolymer dosage must remain below the level causing die-lip plate-out and visible die lines.

    Regrind from edge trim and start-up film may be incorporated at 10–15 wt% without major mechanical loss when the material is dry and free of degraded gels. Above this level, repeated thermal history and contamination from labels or floor sweepings raise gel counts and reduce dart impact. Screen-pack condition also influences melt quality: as screens blind, back pressure rises; if the extruder reaches its maximum pressure limit before scheduled screen change, melt residence time lengthens and the risk of crosslinked gel formation in stagnant adapter zones increases.

    Food-contact compliance and regulatory boundary conditions

    Olefin polymers used in food packaging are assessed under 21 CFR 177.1520, which imposes specification limits on density, extractable fraction, and end-use temperature. In the European Union, plastic food-contact materials must satisfy EU Regulation 10/2011, with overall migration below 10 mg/dm². A compliance declaration for Flexirene® FF 25 must be obtained from Versalis for the specific production site and lot, because food-contact status depends on monomer residues, additive composition, and national positive-list entries. Users should not infer compliance solely from the resin grade designation.

    Under REACH, communication obligations apply if a substance of very high concern is present above 0.1% w/w; the current safety data sheet is the authoritative source for classification and exposure control. The grade is not designed for medical implant or pharmaceutical primary packaging unless separately validated under the applicable pharmacopoeia requirements.

    The resin is used in general-purpose monolayer blown film where balanced puncture resistance, tear strength, and sealability are required: carrier bags, frozen food packaging, light agricultural film, and collation shrink film. In coextruded structures, it functions as a sealing layer or core layer adjacent to high-pressure LDPE skins; the LDPE skin improves bubble stability and melt strength, while the butene LLDPE core contributes tear and puncture resistance. Published data for this specific configuration is limited for high-barrier coextrusions with EVOH or polyamide, so pilot-line trials are recommended to confirm interlayer adhesion, seal integrity, and gauge uniformity before scaling to production.