| HS Code | 744479 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Additive | Antioxidant |
| Form | Pellets |
| Color | Natural |
| Izodnotchedimpactstrength | No break |
As an accredited Versalis Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® CM 50 Butene Copolymer LLDPE is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL: typically 16 shrink-wrapped pallets, 25 kg bags, 1,375 kg/pallet, totaling 22,000 kg net Versalis Flexirene CM 50 LLDPE. |
| Shipping | Versalis Flexirene® CM 50 Butene Copolymer LLDPE is a non-regulated solid resin, typically shipped in 25 kg polyethylene bags on pallets; bulk packaging may be available. Store under cover, keep dry and clean, and protect from heat, sunlight, ignition sources, moisture, and bag damage. No special transport classification is required. |
| Storage | Store Versalis Flexirene® CM 50 Butene Copolymer LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original bags/containers closed, clean, and palletized to prevent moisture and contamination. Avoid prolonged pressure, stacking damage, and incompatible materials. Use grounding to control static. Follow the manufacturer’s SDS, local regulations, and good housekeeping. |
| Shelf Life | Shelf life is 24 months when stored unopened in original packaging, dry, away from direct sunlight and heat sources. |
In thin-wall food-contact injection moulding cells equipped with 1,200–2,500 kN clamping force hydraulic toggle presses, hot-runner valve-gate systems, and P20 polished cavities, Flexirene® CM 50 butene-copolymer LLDPE is processed at melt temperatures of 200–230°C, mold temperatures of 15–35°C, and injection velocities of 100–180 mm/s. The nominal density of 0.925 g/cm³ under ISO 1183-1:2019 and melt flow rate of 50 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022 define the flow/crystallization envelope. The butene-copolymer chain branching reduces peak crystallization exotherm relative to a comparable high-MFR HDPE, which narrows sink marks around ribs and bosses. On production lines, cold slug formation at the nozzle is recorded when the nozzle body falls below 210°C; the resulting gate blockage is corrected by raising the nozzle set-point to 215–220°C and setting screw decompression to 3–5 mm, while back pressure is held below 0.6 MPa to avoid shear-induced molecular weight loss. Post-mold stacking before part cooling below 40°C produces distortion in lids with wall thicknesses below 0.8 mm; therefore forced-air cooling or robot-held cooling time of 8–12 s is applied before stacking.
Food-contact compliance for this application follows Regulation (EU) No 10/2011, including the Annex II overall migration limit of ≤10 mg/dm², and FDA 21 CFR 177.1520(c) for U.S. olefin polymers. The finished article remains subject to end-use testing under 21 CFR 177.1520(d). Lot-to-lot melt flow rate variation is held within ±3 g/10 min under the supplier certificate of analysis, and density is verified at 23°C by the immersion method defined in ISO 1183-1:2019. The resin is supplied within the framework of Regulation (EC) No 1907/2006 for REACH registration, and no substances of very high concern are intentionally added above the communication threshold.
| Regulatory domain | Designation | Test parameter / condition |
|---|---|---|
| European Union food contact | Regulation (EU) No 10/2011 | Overall migration ≤ 10 mg/dm² |
| U.S. olefin polymer | FDA 21 CFR 177.1520(c) | End-use test per 21 CFR 177.1520(d) |
| Melt flow rate | ISO 1133-1:2022 | 190°C / 2.16 kg |
| Density | ISO 1183-1:2019 | 23°C immersion method |
| Tensile properties | ISO 527-2 | Type 1B specimen, 50 mm/min |
| Charpy impact | ISO 179-1/1eA | 23°C notched |
Typical dry-blend formulations for dairy tubs and storage containers contain CM 50 at 96.0–98.5 wt%, a slip/antiblock masterbatch at 0.5–2.0 wt%, and a pigment or nucleating masterbatch at 0.5–2.0 wt%. When a softer sealing feel is required, LDPE is added at 5–20 wt%; at 20 wt% LDPE the tensile yield strength declines by 8–12% relative to neat CM 50 under ISO 527-2/1B, while the notched Charpy impact strength under ISO 179-1/1eA increases by 10–15%. The use of calcium carbonate filler above 5 wt% reduces melt flow and is not recommended for wall thicknesses below 0.8 mm because short shots appear at the end of fill in thin ribs. Downstream article types include injection moulded food storage containers with wall thickness 0.7–1.2 mm, refrigerated dairy spread tubs, overcap shells, snack cups, and tamper-evident delicatessen closures. These parts are converted on high-speed injection moulding lines followed by robotic part removal, in-mould labelling for decoration, and vision-based closure-leak inspection systems.
Carrier resin selection in color masterbatch compounding is determined by melt viscosity matching with the letdown resin, pigment wetting, and pellet hardness after cooling. CM 50 is fed as the carrier at 25–60 wt% alongside organic pigments or carbon black at 30–60 wt%, wax dispersants at 5–10 wt%, and stearate-based processing aids at 0.2–0.8 wt%. A 44:1 L/D co-rotating twin-screw extruder with segmented screw elements and barrel temperatures from 180°C to 220°C is used; the low melt viscosity of CM 50 at 200°C reduces the screw shaft torque during high pigment loading and prevents local temperature spikes above 220°C that degrade heat-sensitive organic red and yellow pigments. In water-ring pelletizing of carbon black masterbatch, the pelletizer inlet water temperature is kept between 25°C and 35°C; lower water temperature produces brittle pellets when carbon black loading exceeds 45 wt%, while higher water temperature causes pellet agglomeration in the centrifugal dryer.
REACH compliance under Regulation (EC) No 1907/2006 applies to the masterbatch as a mixture; SVHC content must be declared along the supply chain when the concentration exceeds 0.1 wt%. When the masterbatch is later used in food-contact film, the carrier resin and additives must comply with Regulation (EU) No 10/2011, and the masterbatch producer is expected to provide a declaration of compliance. Good manufacturing practice under Regulation (EC) No 2023/2006 is commonly specified by converters to control cross-contamination in masterbatch production. The carrier resin is also covered by FDA 21 CFR 177.1520 for olefin polymers used in food-contact articles, and the final masterbatch may be tested for total migration under EN 1186-1:2002 if the converter requires batch-specific data.
The formulation addition ratio is adjusted by pigment type: for carbon black, the carrier resin fraction is typically 45–55 wt%; for titanium dioxide, the carrier is 60–70 wt% of the masterbatch; for organic pigments, the carrier is 40–55 wt% because higher carrier content improves pigment dispersion and filter pressure value stability. Finished masterbatch types include carbon black masterbatch for agricultural film, titanium dioxide white masterbatch for injection moulded crates, slip/antiblock masterbatch for blown film, and additive concentrates for BOPP extrusion. The downstream production process at the converter consists of gravimetric dosing of the masterbatch at 2–6 wt% into the base resin hopper, single-screw or twin-screw melt blending, and subsequent film blowing, injection moulding, or sheet extrusion. Published data for the specific water-ring pelletizer throughput and torque at 900 min⁻¹ with CM 50 are limited; the processing window described is derived from general butene-copolymer LLDPE carrier behavior and should be validated on the specific compounding line.
When post-consumer HDPE and LLDPE regrind streams recovered from packaging waste fall below 1.0 g/10 min after multiple heat histories, high-speed injection moulding of thick-wall crates and pallets requires melt temperatures above 240°C and still produces flow lines and short shots in sections thicker than 3.0 mm. CM 50 is metered into the recycle stream at 5–20 wt% before the main feed throat of a corotating twin-screw extruder with L/D 36:1–48:1; the resultant composite melt flow rate increases to 3–8 g/10 min and permits injection at melt temperatures of 190–220°C instead of 240–260°C. The chain-branching architecture of the butene-copolymer LLDPE improves impact properties in the final compound, but it does not act as an interfacial compatibilizer for PET or PA residues in the recycled stream; those condensation polymers must be removed by density separation or melt filtration before compounding.
For non-food recycled articles, compliance is governed by REACH Annex XIV SVHC screening and the RoHS Directive 2011/65/EU Annex II restricted substances limits; CM 50 does not contribute cadmium, lead, mercury, hexavalent chromium, PBBs, or PBDEs above the maximum concentration values. Recycled-content claims can be validated under EN 15343:2007 for traceability of recycled plastics, while mechanical properties are checked under ISO 178 for flexural modulus and ISO 179-1/1eA for notched Charpy impact. If the compound is sold as a recycled-content grade, the recycler must maintain batch records for input materials and CM 50 addition as part of the audit trail.
The recommended addition ratio in HDPE bottle cap regrind is 10–15 wt% CM 50; in mixed polyolefin bales containing up to 5 wt% polypropylene contamination, the upper limit of 20 wt% is required. At addition levels above 20 wt%, flexural modulus under ISO 178 declines by more than 15% relative to the unmodified recyclate, and the notched Charpy impact strength increases only marginally or plateaus. Below 5 wt%, the melt flow improvement is insufficient for short filling of sections thinner than 2.5 mm in pallet runner systems. Twin-screw compounding is performed at barrel temperatures of 200–230°C, screw speed of 400–600 min⁻¹, and vacuum venting at -0.08 MPa to remove residual moisture and low molecular weight volatiles. Melt-filtering through 100–200 µm screens is mandatory to remove paper fibre and aluminium contaminants. Field data show strand pelletizing stability requires a die plate melt pressure above 3.5 MPa; below that threshold, strand breakage and pellet-size deviation above ±1.5% by weight increase. Terminal parts include underground drainage chambers, injection moulded pallets and crates, agricultural bins, wheel-arch liners for commercial vehicles, and garden edging profiles. Drying is not required when the regranulate is packed in moisture-proof bags, but open storage at relative humidity above 60% demands 80°C drying for 2 h before injection moulding.
To maintain a stable melt curtain at line speeds above 150 m/min, high-speed extrusion coating of paper, board and aluminium foil with conventional autoclave LDPE requires a blend of 70–90 wt% LDPE coating grade and 10–30 wt% CM 50 processed at melt temperatures of 280–320°C through a 90–120 mm single-screw extruder with a 28:1–32:1 L/D barrier screw and a flat die with a 0.5–0.8 mm die gap. Conventional autoclave LDPE alone encounters draw resonance and neck-in instability above 150 m/min; the addition of CM 50 lowers neck-in from approximately 80–100 mm to 50–70 mm at constant melt temperature and permits coating weight reduction from 20 g/m² to 12 g/m² without reducing adhesion. Detailed extensional viscosity data for this exact grade at 320°C are limited; the neck-in values stated are derived from general butene-copolymer LLDPE blend behavior and should be verified on the production line.
Food-contact coated materials are assessed under Regulation (EU) No 10/2011 for the polymer layer and under BfR Recommendation XXXVI/1 for the paper/board substrate. U.S. applications fall under FDA 21 CFR 177.1520(c) and 21 CFR 176.170(c) for coated paper and board components in contact with food. Adhesion of the coating to paperboard is verified by ASTM D3359-17 tape peel test; cohesive failure within the paperboard substrate at peel forces above 4 N/25 mm is the minimum acceptance criterion. Heat seal strength is tested under ASTM F88/F88M-21, and the seal initiation temperature is measured on a laboratory heat sealer with a dwell time of 1.0 s and pressure of 0.4 MPa.
The formulation comprises LDPE coating resin at 70–90 wt%, CM 50 at 10–30 wt%, and a polymer processing aid or antioxidant concentrate at 0.1–0.3 wt%. At CM 50 addition above 30 wt%, the melt curtain becomes unstable and the motor load rises due to increased shear viscosity; below 10 wt%, the seal initiation temperature reduction is less than 2°C and not measurable under ASTM F88/F88M-21. The recommended coating weight is 10–30 g/m², with line speeds of 150–250 m/min, a chill-roll temperature of 15–25°C, and a melt curtain air gap of 150–250 mm. Terminal structures include aseptic liquid packaging board, coated freezer-grade paper, sachet laminates, and release paper liners. Downstream conversion comprises corona treatment at 38–42 mN/m, extrusion coating, lamination with OPP or metallized PET, and slitting to final reel widths.
The production of flip-top caps and dispensing closures in 32-, 48-, or 64-cavity valve-gated hot-runner tools uses CM 50 as a blend component with HDPE or LDPE to balance high flow for cavity fill against sufficient tensile elongation for hinge durability. Typical melt temperature is 200–230°C, mold temperature is 10–25°C, and the clamping force is 1,500–3,500 kN depending on tool size. The cycle time for a 2.5 g single-serve overcap is reduced from 6.5 s to 5.8 s when CM 50 replaces a 20 g/10 min LLDPE grade, while the hinge survives more than 100 flexural cycles under the converter's in-house test procedure. Valve-gate sequencing in the hot runner is adjusted so that the melt fronts meet outside the hinge, because a weld line in the hinge reduces flexural endurance by more than 25%.
Closures for food and cosmetics must comply with Regulation (EU) No 10/2011 when in contact with food and with FDA 21 CFR 177.1520 for U.S. olefin polymers. Cosmetic packaging traceability under Regulation (EC) No 1223/2009 applies to the finished packaging when supplied for cosmetic products. The resin compound is REACH-registered under Regulation (EC) No 1907/2006, and the final closure is tested for overall migration under the relevant food-contact simulants, including 10 days at 40°C for aqueous and acidic simulants. Sensory testing under EN 1230-1:2009 may be required to evaluate taint and odour transfer for sensitive dairy and beverage applications.
The formulation comprises CM 50 at 30–60 wt%, HDPE injection moulding grade at 40–70 wt%, and a processing aid or slip masterbatch at 0.5–2.0 wt%. At 60 wt% CM 50, the tensile elongation at break under ISO 527-2 exceeds 400% and the notched Charpy impact at -20°C under ISO 179-1/1eA remains above 6 kJ/m². Below 30 wt% CM 50, the fill performance in thin hinge sections under 0.4 mm is insufficient and short shots appear in valve-gated multi-cavity tools. Pre-drying at 80°C for 2 h is required only if the resin is stored at relative humidity above 60%. Finished product types include flip-top caps for shampoo and cosmetic tubes, overcap shells for aerosol cans, tamper-evident snap caps for dairy bottles, and dispensing closures for condiment packages. The downstream process is high-cavity injection moulding followed by vision inspection for dimensional tolerances, hinge flex testing on a sampling basis, and automated packing in clean-room conditions.
Competitive Versalis Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® CM 50 is a butene-1 copolymer linear low density polyethylene supplied as a pelletized base resin for cast film extrusion and thin-gauge coextruded structures. The grade is designated CM 50 within the Flexirene cast-film series and is characterised by a nominal density of 0.919 g/cm³ and a nominal melt flow rate of 3.5 g/10 min when determined at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. Butene-1 insertion along the polyethylene backbone introduces short ethyl branches, which distinguishes the material from hexene- and octene-copolymer LLDPE grades that add butyl and hexyl branches, respectively. The resin is typically supplied without slip, antiblock, cling, or antioxidant loading unless formulated by the converter; therefore, additive selection rather than the base resin controls final film functionality. These values are interpreted from publicly available datasheet ranges for the Flexirene cast-film family and should not replace lot-specific certificates of analysis.
On 90 mm single-screw extruders with 30:1 L/D barrier screws and 120-mesh screen packs, a melt temperature range of 230 °C to 260 °C is commonly set for stable web formation. Below 220 °C, shear stress at the coat-hanger die lip approaches the critical value for sharkskin melt fracture, particularly at die gaps below 0.5 mm. Above 275 °C, oxidative degradation produces gel specks above 0.3 mm that reduce optical clarity and destabilize the melt curtain. The upper boundary is therefore a thermal-oxidative limit governed by residence time in screw and die rather than a simple melt strength limit. On lines running 300 kg/h to 400 kg/h, the melt temperature deviation should be maintained within ±5 °C of the validated set point because butene-copolymer LLDPE exhibits a rapid decline in elongational viscosity with increasing temperature; this decline influences draw resonance and neck-in. An air gap of 15 mm to 40 mm and a chill-roll temperature of 18 °C to 24 °C typically reduce draw resonance and provide adequate quench. Published data for this specific configuration is limited; the stated ranges are standard cast-film operating envelopes rather than guaranteed producer values.
At a converted film thickness of 25 µm, the grade produces tensile strain at break values typically above 650% in the machine direction and above 700% in the transverse direction when tested according to ISO 527-3:2018. Dart drop impact measured with Method A of ISO 7765-1:2004 generally falls between 100 g and 140 g; Elmendorf tear tested according to ISO 6383-2:1983 frequently shows machine-direction readings near 35 N/mm and transverse-direction readings above 70 N/mm. These values reflect the short-chain branching distribution of butene-1 comonomer, which increases branch frequency but limits the concentration of load-bearing tie chains compared with octene-based LLDPE at equivalent density and melt flow rate. Consequently, the grade is selected for stretch-wrap and pallet-unitization film where load retention and optical quality are prioritized over high-speed puncture resistance. The resin exhibits a melting peak between 121 °C and 124 °C by differential scanning calorimetry at 10 K/min, enabling heat-sealing initiation near 105 °C and stable seal strength up to 130 °C in sealant layers.
| Property | Method | Typical value | Condition |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.919 g/cm³ | Base resin, 23 °C |
| Melt flow rate | ISO 1133-1:2022 | 3.5 g/10 min | 190 °C, 2.16 kg |
| Tensile strain at break, MD | ISO 527-3:2018 | >650% | 25 µm |
| Tensile strain at break, TD | ISO 527-3:2018 | >700% | 25 µm |
| Dart drop impact | ISO 7765-1:2004 | 100–140 g | Method A |
| Elmendorf tear, TD | ISO 6383-2:1983 | >70 N/mm | 25 µm |
| Melting peak | ISO 11357-3:2018 | 121–124 °C | 10 K/min |
Die pressure on a 0.6 mm coat-hanger die typically remains between 120 bar and 180 bar at 300 kg/h when melt temperature is held at 245 °C. The apparent viscosity at 100 s⁻¹ is lower than that of a comparable octene-copolymer grade by approximately 10% to 15%, which reduces drive amperage but also lowers the margin against melt fracture at the die lip. A fluoropolymer processing aid at 200 ppm to 500 ppm is a common remedy for sharkskin on thin-gauge cast lines; it coats the die surface and shifts the critical shear stress upward, but overfeeding can produce slip-stick pressure fluctuations and transverse gauge variation. Such interaction appears as die-entry pressure variation greater than 3 bar. When this occurs, stepwise reduction of processing aid or an increase in die gap from 0.5 mm to 0.7 mm should be evaluated before changing melt temperature.
Optical performance is governed by quench rate and additive package. At 25 µm gauge, haze near 5% and gloss at 45° above 70 GU are achievable on polished chill rolls; blown-film processing with the same resin yields higher haze because slower cooling increases spherulite size. The coefficient of friction depends on slip-additive migration: a fast-blooming erucamide system reaches stable values below 0.3 after 24 h at 23 °C, whereas a slower-blooming oleamide may require 72 h to stabilize. Migration rate decreases sharply below 15 °C, and blocking incidents on reels stored under pressure become more frequent when coefficient of friction exceeds 0.4. These are converted-film properties rather than resin specifications.
Unlike an octene-copolymer LLDPE of equivalent nominal density and melt flow rate, the butene-based grade tends to display lower dart impact and puncture resistance at high deformation rates because ethyl branches generate a less effective tie-chain population than hexyl branches from octene. In exchange, the lower comonomer cost and lower melt viscosity can reduce extruder drive load and permit higher screw speeds on cast-film lines with limited motor torque. The material differs from high-pressure LDPE in that it has a linear backbone without long-chain branching; it therefore lacks equivalent neck-in stability and melt strength, and blown-film extrusion is not the primary processing route. Compared with metallocene-catalysed butene LLDPE, conventional multi-site catalyst architecture of CM 50 may produce slightly lower clarity and higher melt strength, which can be advantageous or limiting depending on line speed and gauge. The following table summarises directional differences, not direct material substitutions.
| Film property at 25 µm | Flexirene® CM 50 | Typical octene LLDPE of similar density/MFR | Directional difference |
|---|---|---|---|
| Dart drop impact, ISO 7765-1:2004 | 100–140 g | 180–250 g | Lower |
| Elmendorf tear, TD, ISO 6383-2:1983 | >70 N/mm | >110 N/mm | Lower |
| Haze, ASTM D1003 | ~5% | ~7% | Lower haze |
| Melt viscosity at 100 s⁻¹ | Baseline | 10–15% higher | Lower viscosity |
| Seal initiation | ~105 °C | ~108 °C | Lower initiation |
For finished articles intended for food contact, compliance with EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 is established on the final film structure, not on the neat resin alone. The base resin contains no intentionally added heavy metals or phthalates; conformity statements are supported by batch-level migration testing under food-simulant conditions specified in the regulation. Slip and antiblock loadings must be controlled within narrow windows: erucamide slip above 800 ppm can produce plate-out on chill rolls, while levels below 300 ppm may produce blocking on rewind. In coextruded sealant applications, seal initiation temperature near 105 °C is typical at 25 µm thickness, but seal integrity narrows if the layer is blended with more than 20% high-density polyethylene because the higher melting fraction shifts the seal curve upward and reduces the hot-tack window. Pre-drying of virgin resin is not required when storage is below 60% relative humidity; above 60%, surface moisture may create bubble defects at melt temperatures above 230 °C. The material should not be processed with acid-containing polymers, including ionomers and certain acid-copolymer tie resins, because acid-catalysed degradation can generate black specks and reduce toughness.
During storage and handling, exposure to direct sunlight or temperatures above 40 °C for prolonged periods can accelerate oxidative degradation and shift the melt flow rate outside the producer specification. The grade is not intended for medical implants, high-temperature retort packaging above 121 °C, or applications requiring long-term UV resistance without additional stabilizer concentrates. Recycled content must be validated against target film gauge, because contaminant-induced gels become more visible below 30 µm. Converters requiring higher dart impact at low temperatures may require an octene-copolymer or metallocene-catalysed LLDPE; blown-film lines with high bubble stability may require a high-pressure LDPE blend or long-chain-branched LLDPE. These operational boundaries define the practical envelope rather than theoretical resin limits.