| HS Code | 985231 |
| Chemical Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 260 MPa |
| Dart Impact Strength | 100 g |
| Elmendorf Tear Strength Md | 100 g |
| Elmendorf Tear Strength Td | 200 g |
| Haze | 12% |
| Gloss 45 | 60% |
| Coefficient Of Friction | 0.2 |
| Physical Form | Pellets |
As an accredited Versalis Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® CL 10 U is supplied in 25 kg polyethylene bags, palletized for safe handling and transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Flexirene CL 10 U butene copolymer LLDPE, palletized 25 kg bags, dry container, ambient, secured cargo. |
| Shipping | Versalis Flexirene® CL 10 U is supplied as non-hazardous LLDPE pellets, typically in 25 kg polyethylene bags on pallets, stretch-wrapped, or in bulk octabins/trucks. It is not regulated for transport. Keep dry and store away from heat, sunlight, and ignition sources during shipping. |
| Storage | Store in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, ignition sources, and incompatible materials. Keep original bags or containers closed, clean, and palletized. Protect from moisture, dust, and contamination. Avoid prolonged UV exposure. Use first-in, first-out stock rotation. Handle carefully to prevent static buildup; avoid excessive stacking. Do not expose to open flames or strong oxidizers. |
| Shelf Life | Shelf life: typically 12 months when stored in original, unopened packaging, dry, cool, and protected from direct sunlight. |
Versalis Flexirene® CL 10 U enters heavy-duty industrial liner conversion as a butene-copolymer linear low density polyethylene with a published density of 0.918 g/cm³ and melt flow rate of 1.0 g/10 min at 190 °C under a 2.16 kg load per ISO 1133-1. The pellet is not hygroscopic under normal sealed storage. Drying is required only after exposure above 60% RH, using a hot-air hopper dryer at 70 °C for 2 h. For vapour barrier membranes and waste containment liners, the material is blended with 20-30 wt% high-pressure LDPE to increase bubble stability and improve gauge control on large annular dies. Additive loadings follow final-use requirements: 1500-2500 ppm synthetic silica antiblock, 400-800 ppm erucamide slip, and 2-4 wt% carbon black masterbatch for UV-opaque construction films. Extrusion is performed on a single-screw extruder with 30:1 L/D barrier screw and Maddock mixing section, equipped with a 250-400 mm annular die having a 1.8-2.2 mm die gap. Blow-up ratio is held between 2.5:1 and 3.0:1. Melt temperature is controlled at 204-218 °C, and frost line height is fixed at 6-8 die diameters to balance transverse direction orientation and tear resistance. Surface melt fracture appears as sharkskin on the bubble when die exit shear stress exceeds the critical level for this MFR. Addition of 200-400 ppm fluoropolymer processing aid conditions the die metal surface and typically permits a 5-10% output increase before melt rupture reappears. The converted film is fabricated into 100-200 µm heavy-duty sacks, pallet covers, and construction vapour barriers. Compliance is verified under REACH Article 33 and EU Directive 94/62/EC Article 11, with total heavy-metal concentration below 100 ppm in the packaging article.
In frozen food packaging, thin-gauge film must retain seal strength and puncture resistance after exposure to -25 °C. CL 10 U provides butene-comonomer short-chain branching but lower low-temperature impact than octene-copolymer LLDPE. Converters are therefore required to validate dart drop impact according to ASTM D1709, Elmendorf tear according to ASTM D1922, and tensile energy to break according to ASTM D882 on each gauge and frost line setting. The process uses a high-stalk bubble with internal bubble cooling, die gap 2.0-2.3 mm, blow-up ratio 2.2:1-2.8:1, and frost line height 6-8 die diameters. Melt temperature is maintained at 210-225 °C. Slip and antiblock loadings are reduced compared with industrial liners to protect seal integrity: 1000-1500 ppm silica antiblock and 300-600 ppm erucamide slip. The film is converted into 35-60 µm bags for frozen vegetables, ice cream liners, and bakery pre-portioning films. Food-contact compliance is assessed under EU Regulation No 10/2011 overall migration limit of < 10 mg/dm² and under FDA 21 CFR 177.1520 for olefin polymers. The specific condition of use must be selected from the regulation according to the intended food type and heating profile. If microwave reheating is intended, the additive package must be re-evaluated against the time-temperature conditions listed in 21 CFR 176.170(c) or equivalent national rules.
| Control point | Standard or regulation | Measured parameter |
|---|---|---|
| Food-contact formulation | EU Regulation No 10/2011 | Overall migration < 10 mg/dm² |
| Resin composition | FDA 21 CFR 177.1520 | Olefin polymer specification |
| Low-temperature impact | ASTM D1709 | Dart drop impact at -25 °C |
| Tear resistance | ASTM D1922 | Elmendorf tear in MD/TD |
| Seal strength | ASTM F88 | Peak seal force |
Agricultural mulch and silage clamp liners impose gauge uniformity standards that are tighter than industrial liner production. CL 10 U is converted on wide annular dies of 1200-1800 mm diameter with die gap 1.9-2.1 mm, blow-up ratio 2.5:1-3.0:1, and melt temperature 205-220 °C. The target film thickness ranges from 25-60 µm for mulch and 150-250 µm for silage clamp liners. UV stabilisation is achieved by dry-blending 3-6 wt% of a UV masterbatch containing 18-22% hindered amine light stabiliser and 8-12% ultraviolet absorber. The final film carries 0.20-0.40 wt% HALS and 0.10-0.20 wt% UV absorber. Carbon black is added at 2-5 wt% for mulch films to increase opacity and reduce UV transmission. High filler and masterbatch loadings raise screen pressure. Filter screens of 60/80/100 mesh are inserted and pressure drop is recorded at each shift. A pressure increase of 15-20% from the clean condition signals replacement. The terminal articles are black mulch film and silage clamp liners. REACH applies to the supplied resin. CL 10 U is not biodegradable and does not meet EN 17033 for biodegradable mulch films unless compounded with certified biodegradable additives. Published data for that specific configuration is limited.
In multiwall paper sack production, solvent-based adhesive lamination is replaced by a coextruded sealant web or pre-formed blown film to reduce retained solvent and improve moisture resistance. CL 10 U is used as the sealant layer at 60-80 wt% blended with 20-40 wt% LDPE or EVA. The LDPE or EVA fraction lowers the viscosity for interface wetting and reduces neck-in during any coextrusion step. Direct high-line-speed extrusion coating with this resin is limited by its 1.0 g/10 min melt flow rate. Die temperatures above 280 °C and high draw-down speeds may exceed the thermal stabilisation window. Pre-formed blown film lamination is therefore the preferred route. Film is produced on a standard blown line with die gap 1.8-2.2 mm, blow-up ratio 2.2:1-2.8:1, and melt temperature 205-220 °C. The film is bonded to kraft paper on a solventless laminator with polyurethane adhesive applied at 1.2-2.0 g/m². Nip temperature is 60-80 °C and web tension is 100-150 N/m. Seal strength is verified according to ASTM F88 and hot tack according to ASTM F1921. Terminal products are moisture barrier plies in multiwall sacks for pet food, cement, and mineral fillers. For indirect food-contact use, the adhesive must comply with FDA 21 CFR 175.105 and the PE layer with 21 CFR 177.1520. EU compliance is assessed under Regulation (EU) No 10/2011 when the packaging is placed on the EU market.
Carbon black masterbatch compounding uses CL 10 U as a carrier resin when the final masterbatch is intended for LLDPE blown film. The resin is loaded at 50-60 wt% of the formulation, with carbon black at 35-45 wt% and a hydrocarbon wax dispersant at 3-8 wt%. Compounding is carried out on a co-rotating twin-screw extruder with 40:1 L/D, side feed at 48-52% of screw length, melt temperature 190-210 °C, and vacuum venting at -0.08 MPa. Dispersion quality is measured by extruding the compounded masterbatch through a 14 µm or 25 µm screen pack. A pressure rise below 2.0 MPa after 100 kg passage is considered acceptable for film-grade black masterbatch. The masterbatch is let down at 2-6 wt% in final film to give a carbon black concentration of 1-2.5 wt% for opacity and UV resistance. Terminal products include agricultural film, refuse sacks, and industrial liners. REACH applies to the supplied resin and the carbon black masterbatch. If the masterbatch is used in food-contact packaging, migration testing under EU Regulation No 10/2011 is required because carbon black quality and PAH content vary by producer.
In pallet unitisation, stretch hood films must combine machine direction tensile strength with sufficient elastic recovery to maintain clamp force during transit. CL 10 U alone has limited elastic recovery because butene-copolymer branches are shorter than octene-copolymer branches. The material is therefore used in blends at 30-50 wt% with metallocene LLDPE or octene-based LLDPE to reduce cost while preserving elastic retention. Conversion is performed on a high-stalk blown film line with internal bubble cooling, die gap 2.0-2.4 mm, blow-up ratio 3.0:1, melt temperature 210-230 °C, and film thickness 50-80 µm. Mechanical targets are verified according to ASTM D882 for tensile stress at break, ASTM D5748 for puncture resistance, and a 50% extension elastic recovery test with 10 min relaxation. Terminal products are pallet hoods, transit wraps, and bundling films. Blends containing more than 50 wt% CL 10 U typically reduce load retention and should be qualified through simulated transport vibration testing. REACH applies. If pallet wrap is used in contact with packaged food, it must meet the applicable food-contact requirements under EU Regulation No 10/2011 or FDA 21 CFR 177.1520 depending on the market.
Competitive Versalis Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® CL 10 U is a 1-butene–copolymer linear low-density polyethylene supplied for extrusion blown-film conversion. The product designation identifies a film-oriented resin supported by specifications on melt mass-flow rate and density: the melt mass-flow rate is 1.0 g/10 min at 190 °C/2.16 kg measured under ISO 1133-1:2022, and the solid-state density is 0.918 g/cm³ determined by ISO 1183-1:2019. These two values position the grade in the general-purpose butene LLDPE film class: density governs stiffness and crystallinity, while melt flow governs head pressure and output behaviour in single-screw extrusion. The comonomer is 1-butene, which introduces short-chain ethyl branches along the linear backbone rather than the long-chain branching characteristic of high-pressure LDPE.
Public technical documentation lists the product as a pelletised, stabilised compound for blown-film applications; the quantitative additive package is not fully disclosed in typical commercial datasheets. The “U” suffix in the Flexirene® CL series is treated in the field as the product modifier identifying a blown-film formulation with processing and stabilisation additives, not as a change in the base resin architecture. Because additive type and loading can affect slip, blocking, organoleptic performance, and food-contact status, absence of published lot-specific additive composition means the converter should verify these properties against current Versalis documentation or by approved extraction and surface-analysis methods.
Butene-copolymer LLDPE differs from high-pressure LDPE by having a linear polyethylene backbone with controlled short-chain branching instead of a highly branched long-chain architecture. This structural difference reduces shear sensitivity and melt elasticity under extensional deformation. In tubular film processing, the lower melt elasticity is observed as reduced bubble stability at high stalk heights or high draw ratios, especially when the frost-line height is increased to increase orientation. The effect can be quantified indirectly by extensional rheology or by the magnitude of draw-resonance onset on a cast-film line; published data for this exact CL 10 U grade is limited, but the class behaviour is well documented in polyolefin reactor-copolymer literature.
Compared with octene-copolymer LLDPE at equivalent melt index and density, a butene-based grade generally produces lower dart impact and lower machine-direction tear because the shorter 1-butene branch is less efficient at increasing the population of tie molecules in the amorphous phase. The comparative measurement is normally performed under ASTM D1709-16a for impact and ASTM D1922-15 for tear. Converters should not use a single thickness or blow-up ratio as a universal comparator; film property magnitude changes with gauge, frost-line height, and orientation. Where direct cross-polymer data are required, substitution trials on the intended blown-film line are the only technically reliable method.
Molecular-weight distribution and comonomer distribution also control process behaviour. A Ziegler-Natta butene LLDPE such as the CL 10 U type generally has a broader composition distribution than most metallocene LLDPE grades, which may lower ultimate optical performance and increase film-blocking variability. Melt-flow and density are therefore insufficient for lot acceptance; they must be supplemented by film-based tests, gel-count inspection, and coefficient-of-friction determination when the use involves high-speed packaging equipment.
On a production-scale monolayer blown-film line equipped with a 45 mm grooved-feed extruder, 30:1 L/D barrier screw, and 1.8 mm die gap, the material is processed with barrel temperatures from 170 °C to 190 °C and adapter/die temperatures from 190 °C to 210 °C. Blow-up ratios between 2.0:1 and 3.0:1 support bubble stability in monolayer films from approximately 20 µm to 150 µm. These values are common industrial starting points for 0.918 g/cm³ butene LLDPE; specific frost-line height, air-ring settings, and haul-off speed influence final gauge variation and orientation.
Melt temperature should not exceed 230 °C during normal extrusion. Prolonged residence time at upper temperatures can initiate oxidative degradation and generate cross-linked gel particles that appear as discontinuities in film and accumulate on screen packs. Screen packs of 250–400 µm are typically installed ahead of the die to trap these gels; a pressure rise above 50 bar across the screen pack indicates accumulation and requires replacement. Purge with low-melt-index LDPE between product transitions minimises hang-up in spiral mandrel grooves and colour-change carryover.
Thin-gauge converters evaluating CL 10 U against octene LLDPE or high-strength LDPE should compare tensile elongation and tear resistance using ASTM D882-18 and ASTM D1922-15 on films of identical thickness, blow-up ratio, and frost-line geometry. Butene-copolymer LLDPE typically displays lower dart-drop energy than octene LLDPE at the same gauge because of lower tie-molecule density. This difference is evaluated under ASTM D1709-16a; the exact percentage shift depends on orientation and additive package, and published data for this specific commercial configuration is limited. Converters should establish their own comparative data on their actual line rather than relying on single-point literature values.
When the application requires resistance to localised puncture, stretch wrapping, or heavy-duty industrial liners, the specification may be shifted toward C8 or C6 copolymers or toward blends with LDPE to increase melt strength and impact toughness. For general-purpose packaging film, however, the butene-copolymer route provides an adequate balance between output and strength. Fogging, gel formation, and odour can be more pronounced when regrind ratio is elevated; the maximum acceptable regrind level should be validated on-line against the final film property specification using the same test standards.
Optical properties are affected by die-end stress, frost-line cooling rate, and additives. Haze and clarity are measured under ASTM D1003-21; gloss is assessed under ASTM D2457-13 or similar procedures. The additive package of CL 10 U is intended to reduce blocking and stabilise slip behaviour, but coefficient of friction must be verified on the final film because it changes with time, gauge, corona treatment, and storage temperature. Static and kinetic coefficients of friction are measured according to ISO 8295:1995/ASTM D1894-14. Film-to-metal slip on form-fill-seal machines can shift after additive bloom; measurements taken immediately after extrusion may not represent performance after 24 h or longer aging.
For printing and lamination, surface tension is raised by corona discharge. The treatment level for solvent-based inks is commonly maintained at 38–42 mN/m; for water-based inks, 44–48 mN/m is used. Additive migration to the film surface can reduce surface energy over time, requiring re-verification after storage under controlled conditions. The selection of CL 10 U for printed or laminated structures therefore requires evaluation of dyne retention, ink adhesion after tape pull, and lamination bond strength rather than assumption of permanence.
Film properties and process stability are influenced by additive dispersion and resin homogeneity. A uniform melt stream reduces thickness variation, gel streaking, and variability in additive bloom. The following measurement matrix is applied for incoming resin lot qualification and film-based verification. Film specimens require conditioning under ISO 291:2008 or ASTM D618-13 prior to mechanical and optical testing.
| Measured property | Test method | Function in lot acceptance | Published CL 10 U specification value |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Extrusion consistency and migration potential | 1.0 g/10 min at 190 °C/2.16 kg |
| Density | ISO 1183-1:2019 | Film stiffness, optical and barrier balance | 0.918 g/cm³ |
| Tensile elongation at break | ASTM D882-18 | Ductility in machine and transverse directions | Thickness- and orientation-dependent; not published as a single lot limit |
| Dart-drop impact | ASTM D1709-16a | Impact toughness of blown film | Thickness- and blow-up-ratio-dependent; not published as a single lot limit |
| Elmendorf tear | ASTM D1922-15 | Tear propagation resistance | Orientation-dependent; not published as a single lot limit |
| Haze | ASTM D1003-21 | Optical clarity of final film | Cooling-rate-dependent; not published as a single lot limit |
| Coefficient of friction | ISO 8295:1995 / ASTM D1894-14 | Film-to-film and film-to-metal slip | Time- and surface-treatment-dependent; verify on final film |
Extensional viscosity of the butene-copolymer melt is lower than that of high-pressure LDPE under typical blown-film deformation. In the Hencky strain-rate range of 0.5 s⁻¹ to 5 s⁻¹, branched LDPE exhibits strain hardening, whereas the butene LLDPE exhibits limited strain hardening. On high-stalk lines requiring large draw-up ratios, this can appear as bubble sag, transverse gauge variation, and fluctuations at the collapsing frame. Processing measures include reducing frost-line height, increasing die gap to 2.0 mm, or blending 10–20 wt% high-pressure LDPE to increase melt tension. The exact blend ratio should be established by capillary rheometry under ISO 11443:2021 and verified by bubble stability observation on the production line.
Thermal oxidative stability is assessed by differential scanning calorimetry using oxidation-onset procedures; for polyethylene, isothermal or dynamic OIT protocols are described in ISO 11357-6:2018. Published OIT data for the exact CL 10 U additive package is limited. The polyethylene processing guides nevertheless bound normal operation below 240 °C to avoid initiating peroxide-assisted degradation. Residence time at full production output is commonly kept below 10 min; longer residence times increase the probability of gel formation and melt discoloration, particularly in spiral mandrel channels with stagnant flow zones.
| Material class | Molecular architecture | Process consequence |
|---|---|---|
| Butene-copolymer LLDPE, 0.918 g/cm³ | Linear backbone with ethyl short-chain branching | Moderate melt strength; balanced output and cost; lower dart than C8 at equal density/MFR |
| High-pressure LDPE | Branched long-chain architecture | Higher melt tension; wider bubble stability; lower drawn-film strength at equal gauge |
| Octene-copolymer LLDPE | Linear backbone with hexyl short-chain branching | Higher dart and tear at equivalent density/MFR; generally higher cost |
| Metallocene LLDPE | Narrow composition and molecular-weight distribution | Improved optics and toughness; lower melt elasticity; may require modified extruder screws |
Among Versalis Flexirene® film grades, the CL series is differentiated by comonomer type, melt-flow placement, and additive package. CL 10 U is positioned near the lower melt-flow side of the CL film series. Grades with higher melt flow reduce head pressure but may show lower impact toughness. Comparative material substitutions should be based on current Versalis product datasheets and on converter-run evaluations at constant gauge, blow-up ratio, and frost-line setting.
In the European Union, food-contact suitability is assessed under Regulation (EU) No 10/2011 and its amendments. Overall migration must not exceed 10 mg/dm², and specific migration limits for individual additives must be confirmed against the positive list. In the United States, olefin polymers may fall within FDA 21 CFR 177.1520, but the converter must verify that the exact additive package and conditions of use are covered by the intended food-type and temperature category. The presence of slip and antiblock additives can affect migration behaviour; therefore a finished-article migration study is required when the film contacts fatty foods or is subjected to hot filling.
Workers handling pellets should follow the safety data sheet. Melt spillage, thermal decomposition fumes, and dust from regrinding require local exhaust ventilation. The material is not intended for prolonged outdoor exposure unless coextruded or blended into a UV-stabilised structure; prolonged weathering of unpigmented film can cause embrittlement measurable as a loss of elongation under ISO 527-3:2018 after accelerated weathering or outdoor exposure.
Cast-film processing of CL 10 U may be carried out with chill-roll temperatures from 20 °C to 30 °C and melt temperatures near the lower end of the recommended range to limit oxidative by-products. Neck-in and draw resonance are more pronounced than with high-pressure LDPE because of the linear backbone and lower melt elasticity. Edge trim and die-lip adjustments are therefore required to maintain web width and thickness uniformity. Published data for this specific configuration is limited, so cast-process substitution should be validated on the intended equipment before commercial production.