| HS Code | 713624 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Catalyst | Ziegler-Natta |
| Density | 0.920 g/cm³ |
| Meltflowrate 190c 2 16kg | 1.0 g/10 min |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 95 °C |
| Tensilestrengthatyield | 11 MPa |
| Tensilestrengthatbreak | 25 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 250 MPa |
| Dartdropimpact | 110 g |
| Elmendorftearstrength Md | 180 g |
| Elmendorftearstrength Td | 380 g |
| Haze | 12% |
| Gloss 45deg | 55 |
| Coefficientoffriction | 0.2 |
| Processingtemperature | 160-220 °C |
As an accredited Versalis Flexirene® CL 10 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Flexirene® CL 10 Film Grade LLDPE is supplied in 25 kg polyethylene bags, palletized in 1,000 kg lots. |
| Container Loading (20′ FCL) | Versalis Flexirene® CL 10 Film Grade LLDPE: 20′ FCL loading in 25 kg bags, approximately 22 MT net. |
| Shipping | Versalis Flexirene® CL 10 Film Grade LLDPE is supplied in 25 kg bags or octabins, palletized and stretch-wrapped. Transport in dry, covered vehicles; avoid moisture, heat, and UV. Non-hazardous; follow SDS and local regulations. Store in original packaging in a cool, ventilated area. Keep away from direct sunlight and contamination. |
| Storage | Store Versalis Flexirene® CL 10 Film Grade LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Keep in tightly closed original packaging on pallets, protected from moisture, dust, and contamination. Avoid excessive stacking; rotate stock, use first-in, first-out, and follow local regulations and the supplier’s SDS. |
| Shelf Life | Typical shelf life is 24 months when stored in unopened original packaging, dry, away from direct sunlight, below 50°C. |
On 90 mm single-screw extruders with 30:1 L/D and barrier screws, Versalis Flexirene® CL 10 Film Grade LLDPE is dry-blended with a high-molecular-weight LDPE at 10–20 wt% to stabilize bubble geometry in FIBC inner liners and heavy-duty transport sacks on mono-layer blown-film lines with die diameters above 250 mm. The LDPE fraction raises melt extensibility and reduces die-lip buildup, but it sacrifices dart impact strength; an increase from 15 wt% to 18 wt% LDPE typically lowers ISO 7765-1 dart energy by more than 15% at 60 µm final thickness. Compliance for the film is assessed under ISO 21898:2016 for FIBC assemblies, ISO 527-1:2019 and ISO 527-3 for tensile properties, ISO 6383-2 for tear propagation, and ASTM D1709 Method A/B for dart impact. The formulation is held at 80–90 wt% CL 10, 10–20 wt% LDPE, 1–2 wt% slip/antiblock masterbatch, and 1.5–2.5 wt% carbon black masterbatch where outdoor UV exposure is required. Extrusion parameters are set at a die gap of 1.6–2.4 mm, blow-up ratio 2.5–3.0, melt temperature 190–220 °C at the die, and frost-line height 7–9 die diameters. At CL 10 fractions above 90 wt%, field data from converting trials show melt pressure at the breaker plate can rise 12–18% relative to an LDPE-rich reference, and the risk of sharkskin melt fracture increases if the die gap is reduced below 1.4 mm. Terminal products include FIBC inner liners at 60–120 µm, heavy-duty sack liners, construction debris bags, and temporary containment films for industrial bulk handling.
Three-layer greenhouse film operations running CL 10 at 75–85 wt% in the core layer must control EVA addition at 5–15 wt% because EVA raises low-temperature toughness but its lower melt viscosity creates interfacial instability in coextrusion when the EVA-rich outer or inner layer exceeds 15 wt%. Compliance for agricultural covering film is evaluated under EN 13206:2017 for mechanical and weathering requirements, ISO 4892-2 for accelerated weathering, and ISO 527-3 for tensile properties. The additive formulation consists of 0.2–0.6 wt% final hindered amine light stabilizer, 1–2 wt% anti-fog masterbatch, 0.1–0.3 wt% silica antiblock, and 2–5 wt% infrared thermic masterbatch; the HALS loading is not increased above 0.6 wt% because field reports show die-lip plate-out and surface bloom increase with no proportional gain in weathering retention. On three-layer blown-film lines with die gap 1.8–2.4 mm, blow-up ratio 2.0–2.5, and melt temperature 200–230 °C, total film thickness is held at 150–200 µm to balance light transmission and mechanical stability. Process limitations include a melt-temperature ceiling of 230 °C for formulations containing high halogen-free thermic additives, because thermal degradation of the mineral-based thermic additive can shift visible light transmission and raise haze beyond 20%. Terminal product types include multi-season greenhouse covers, low-tunnel film, and horticultural row covers, where the CL 10-rich core provides tear resistance while EVA-rich skins carry anti-fog and thermic additives.
When cast stretch-film line speed exceeds 450 m/min, CL 10 is used at 70–90 wt% with metallocene LLDPE at 10–20 wt% to postpone draw resonance at 15 µm; below 10 wt% mLLDPE, edge thickening and periodic thickness bands become measurable, consistent with draw resonance under high melt draw. Compliance for pallet wrap mechanical and cling performance is tested under ASTM D5458 for cling, ISO 527-3 for film tensile, and ISO 6383-2 for tear. The formulation includes 1–3 wt% polyisobutylene tackifier and 0.5–1.5 wt% antiblock masterbatch; PIB loading above 3 wt% increases cling at the cost of unwind force and can deposit residues on metal tension rollers. The cast process uses a flat die gap of 0.4–0.8 mm, melt temperature 240–260 °C, and chill-roll temperature 18–25 °C, with line speeds between 350 m/min and 600 m/min. Thickness is held between 10 µm and 25 µm for machine and hand grades; at 10 µm, the gauge coefficient of variation must be below 3% to avoid transverse-direction tear propagation in automated pallet wrapping. Terminal products include machine stretch film for rotary-arm or turntable wrappers, hand pallet wrap, and manual bundling film for distribution centers.
In dry-food lamination lines running corona-treated sealant webs at 300 m/min, CL 10 is blended at 70–85 wt% with LDPE at 10–20 wt% and a slip/antiblock masterbatch at 1–3 wt% to create the heat-seal layer in three-layer blown-film coextrusion. Food-contact compliance is demonstrated under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation No 10/2011, with overall migration below 10 mg/dm² when tested under the intended food-simulant conditions; the converter must verify that the slip additive masterbatch and processing aid do not introduce non-conforming substances. The blown-film process uses a die gap of 1.8–2.5 mm, blow-up ratio 2.0–2.5, and melt temperature 190–220 °C, after which the sealant web is corona-treated to 38–42 mN/m and laminated to BOPP or PET with solventless adhesive cured for 24–48 h at 35–45 °C. If corona treatment exceeds 46 mN/m, heat-seal strength measured by ASTM F88 can decline because of surface oxidation of the polyethylene sealant. Terminal products include frozen food pouches, dry mix sachets, snack packaging, and non-fatty dry-food lamination structures; for high-acid or high-fat foods, specific migration testing under EU 10/2011 is required rather than total migration alone.
Refuse sack conversion on high-output mono-layer blown-film lines uses a different additive loading logic because recycled LLDPE is commonly introduced at 15–35 wt% alongside 60–85 wt% CL 10 to meet post-consumer recycled content targets without collapsing bubble stability. The relevant product standard is EN 13592:2017 for household waste sacks, with film tensile measured under ISO 527-3 and tear resistance under ISO 6383-2. Carbon black masterbatch is added at 2–4 wt% and a processing aid at 0.5–1.0 wt%; carbon black above 4 wt% reduces dart impact and increases die-lip deposit formation. The blown-film line operates with a die gap of 1.6–2.0 mm, blow-up ratio 2.0–3.0, and melt temperature 180–210 °C, producing thicknesses of 18–35 µm. Terminal products include household refuse sacks, wheelie-bin liners, and lightweight carrier bags; published data for this specific configuration with high recycled LLDPE fractions is limited, so converters run a pilot batch to set the recycled content ceiling rather than relying on a fixed universal addition ratio.
Competitive Versalis Flexirene® CL 10 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Flexirene® CL 10 Film Grade LLDPE is a butene-1 comonomer linear low-density polyethylene produced for blown film conversion. The grade-identification parameters are a nominal density of 0.918 g/cm³ and a nominal melt flow rate of 1.0 g/10 min when measured under 190°C and 2.16 kg load according to ISO 1133-1:2022 or ASTM D1238-20. Density is determined by ISO 1183-1 or ASTM D792. The melt flow rate places the product in a medium-viscosity extrusion range; it is normally processed on grooved-feed or smooth-bore single-screw extruders with barrier screws and is not intended for injection molding or rotational molding. Applications include general-purpose blown film, heavy-duty packaging sacks, industrial liners, agricultural mulch film, and carrier bags where the film is exposed to puncture, tear, and low-temperature stress. The product is supplied in pellet form and is classified as a film-grade linear low-density polyethylene rather than a high-pressure low-density polyethylene or a metallocene-catalyzed polyethylene.
The product data sheet identifies Flexirene® CL 10 by the following controlled parameters. The nominal density of 0.918 g/cm³ corresponds to the crystalline-amorphous balance typical of a butene-based linear low-density polyethylene intended for blown film. The melt flow rate of 1.0 g/10 min indicates a higher viscosity than common 2.0 g/10 min film grades and therefore supports greater bubble stability at higher frost line heights, but it also requires sufficient screw torque and head pressure to maintain output. Melt flow rate is not a direct measure of molecular weight but an index of melt viscosity; grades with identical melt flow rate can differ in molecular weight distribution and shear thinning. For CL 10, the shear-thinning behavior is associated with a Ziegler-Natta molecular architecture and a broader molecular weight distribution than metallocene-catalyzed linear low-density polyethylene.
| Parameter | Test Method | Unit | Published Grade Value |
|---|---|---|---|
| Nominal density | ISO 1183-1 / ASTM D792 | g/cm³ | 0.918 |
| Melt flow rate | ISO 1133-1:2022 / ASTM D1238-20 | g/10 min | 1.0 |
| Comonomer type | — | — | Butene-1 |
| Polymer class | — | — | Linear low-density polyethylene |
The nominal density and melt flow rate should be used for incoming resin inspection only; film mechanical properties are not inherent and must be evaluated on finished film because they depend on gauge, blow-up ratio, die gap, frost line height, and cooling air temperature. Comparative claims between products should therefore be made only on films produced under identical extrusion conditions.
Short-chain branching in Flexirene® CL 10 arises from butene-1 incorporation and yields ethyl side groups along the polyethylene backbone. At a given density, ethyl branches are generally less effective at increasing tie-chain concentration than the butyl branches from hexene-1 or the hexyl branches from octene-1. Consequently, a butene-based LLDPE at 0.918 g/cm³ typically shows lower dart drop impact and lower Elmendorf tear resistance than an octene-based LLDPE at the same density and melt flow rate. The practical result is that CL 10 is positioned for applications where moderate impact, adequate tear resistance, and reliable blown film processability are required, rather than maximum puncture resistance in frozen-food or high-abuse packaging.
Film properties are commonly measured by ISO 527-3 for tensile stress and elongation, ISO 6383-2 or ASTM D1922 for Elmendorf tear resistance, ISO 7765-1 or ASTM D1709 for dart drop impact, and ASTM D1003 for optical haze. On blown film lines, tensile properties are anisotropic; machine-direction strength is influenced by draw down ratio and frost line height, while transverse-direction strength is influenced by blow-up ratio. A typical evaluation film for a grade of this melt flow rate is produced at 25 µm to 40 µm thickness with a 2.0:1 to 2.5:1 blow-up ratio. At these conditions, the resin displays ductile yielding and high elongation at break, but published data for this specific configuration is limited because film performance shifts with minor changes in die temperature and cooling air velocity.
Dart drop impact testing by ASTM D1709 is a threshold-type measurement, not an intrinsic material property. The measured F50 value depends on film gauge, test specimen diameter, clamp geometry, and pole diameter. For a butene-based LLDPE of density 0.918 g/cm³, impact resistance is controlled by the balance between lamellar thickness and tie-chain density. Lower film blow-up ratios increase machine-direction orientation and can lower transverse-direction tear; higher blow-up ratios improve transverse-direction strength but may destabilize the bubble. Therefore, property optimization requires adjustment of the blow-up ratio within the stable processing window rather than reliance solely on resin selection.
Film tear resistance is evaluated by ISO 6383-2 or ASTM D1922 using trouser-tear or Elmendorf tear geometries. Butene-1 LLDPE films exhibit lower initial tear resistance than hexene- or octene-based LLDPE films at equal density because ethyl branches are less effective in distributing stress across tie chains. The effect is measurable at equivalent film gauge and is especially pronounced in machine-direction tear. For applications requiring high tear propagation resistance, blending with LDPE or adding a hexene-based LLDPE may be required, but the addition changes both melt rheology and film optics. Any blend should be validated on the actual film line because die lip build-up and bubble respiration can shift with blend composition.
In low-temperature impact service, the ductile-to-brittle transition is influenced by density rather than melt flow rate. A density of 0.918 g/cm³ provides low-temperature toughness superior to a 0.926 g/cm³ LLDPE but lower stiffness. The product is therefore selected for frozen-food packaging and outdoor agricultural film where low-temperature flexibility is more important than top-load rigidity. Materials with higher density would increase modulus but reduce impact at sub-zero temperatures; the reverse trade-off is observed when density is lowered below 0.915 g/cm³, where stiffness and yield stress decline further.
For incoming resin acceptance, the melt flow rate should be measured with a capillary melt flow indexer conforming to ISO 1133-1:2022, using a 2.095 mm die bore and 8.0 mm cylinder bore. Calibration of the temperature controller at 190°C should be verified because a ±1°C deviation can produce a measurable shift in flow rate. Density specimens should be prepared by compression molding or from extruded strand and conditioned by ISO 291 before testing by ISO 1183-1. Disputes between producer and converter are typically resolved by testing the same pellet lot with the primary method specified by the supplier, with the secondary standard used only for referee purposes.
Production-scale conversion of Flexirene® CL 10 is typically performed on single-screw extruders with screw length-to-diameter ratios of 24:1 to 30:1. A high-shear barrier screw with a spiral Maddock mixing section is commonly used to homogenize melt temperature and disperse thermal additives. Low-shear screws designed for high-pressure LDPE may not provide sufficient melting homogeneity at high output, particularly when the grade is run neat without LDPE blending. Screw speed and barrel set temperatures must be matched to avoid unmelts in the film; typical barrel profile ranges are 160–180°C in the feed zone, 190–210°C in the compression zone, and 210–225°C in the metering zone. Melt temperature at the adapter is normally held between 210°C and 240°C.
The die gap for 25–40 µm blown film is usually set between 1.0 mm and 1.5 mm. Narrower die gaps below 0.8 mm can raise die pressure and induce melt fracture at high screw speeds, while wider die gaps above 2.0 mm may increase frost line height and reduce bubble stability. The optimum gap depends on film gauge and output; for a 25 µm film on a 90 mm grooved-feed extruder, stable operation is often achieved with a 1.2 mm die gap and a 2.2:1 to 2.5:1 blow-up ratio. Bubble instability may appear as draw resonance, bubble breathing, or helical instabilities when the frost line is raised above a critical height or when cooling air velocity is unbalanced around the circumference. Adjusting the lower nip and air ring can reduce gauge variation, but if the resin is run at low melt temperature, the material may show elevated die pressure and reduced melt elasticity.
Thermal degradation becomes significant above 260°C. Extended residence time at high melt temperature can generate carbonyl oxidation products, increase gel formation, and reduce tear resistance. Start-up and shutdown sequences should minimize hold-up time in the die and adapter. When switching from polar resins such as nylon, EVOH, or PVC, purging with a linear low-density polyethylene or a dedicated purging compound is required because residual polar polymer domains can cause film defects and delamination. The use of a melt pump is acceptable but not mandatory; if a melt pump is used, the inlet pressure should be controlled to avoid excessive shear heating.
Moisture absorption of the pellet is negligible under normal storage; bulk water absorption is below 0.01% at 23°C and 50% RH. However, when pellets are transferred from cold storage into a warm, humid hopper area, condensation can form on the pellet surface. Surface moisture introduced into the extruder feed throat can appear as bubbles or specks in the film. In such cases, a hopper dryer set at 60–70°C for 1–2 h is sufficient. Extended drying above 90°C is unnecessary and may cause pellet agglomeration in the hopper.
The selection between Flexirene® CL 10 and other linear low-density polyethylene grades involves a comparison of comonomer length, molecular weight distribution, and resulting film performance. Butene-1 comonomer produces ethyl branches of two carbon atoms; hexene-1 produces butyl branches of four carbon atoms; octene-1 produces hexyl branches of six carbon atoms. Longer branches are more effective at reducing crystallinity and increasing tie-chain concentration at a fixed density. Because tie-chain concentration is one of the primary controls of impact and tear resistance, hexene- and octene-based LLDPE grades generally outperform butene-based LLDPE in high-abuse film applications. However, butene-based grades often provide a broader processing window than metallocene grades because the Ziegler-Natta molecular weight distribution is wider than the narrow distribution of metallocene-catalyzed LLDPE.
| Resin Type | Short-Chain Branch Length | Molecular Weight Distribution | Bubble Stability Rank | Film Impact Rank at Equal Density |
|---|---|---|---|---|
| Flexirene® CL 10 butene-1 LLDPE | Ethyl branch, 2 carbon atoms | Broader, Ziegler-Natta | Moderate to high | Moderate |
| Hexene-1 LLDPE | Butyl branch, 4 carbon atoms | Broader or narrow | Moderate | Higher |
| Octene-1 LLDPE | Hexyl branch, 6 carbon atoms | Broader or narrow | Moderate | Highest |
| Metallocene-catalyzed LLDPE | Usually hexene or octene | Narrow | Lower without modification | Highest |
The broader molecular weight distribution of Flexirene® CL 10 contributes to shear thinning, which reduces apparent viscosity at extrusion shear rates and can lower die pressure compared with a metallocene grade of similar melt flow rate. The same broad distribution also provides higher low-shear melt strength, which supports bubble stability during start-up and at high blow-up ratios. Metallocene grades, by contrast, may require LDPE blending or processing aids to achieve equivalent bubble stability, but they usually provide improved dart impact, tear resistance, and optical clarity when film gauge is held constant.
Differences from high-pressure LDPE are also significant. LDPE has high long-chain branching, lower melting point, lower tensile strength, and higher melt elasticity than LLDPE. A film containing Flexirene® CL 10 at 0.918 g/cm³ density will generally show higher tensile yield stress, higher elongation at break, and better puncture resistance than an LDPE film of similar melt index. However, the lower long-chain branching of LLDPE reduces bubble stability in some old air-cooled lines; blending 10–20 wt% LDPE is a common practice to increase melt strength. The blend reduces dart impact and tear resistance relative to the neat butene-1 LLDPE and should be evaluated at the intended film gauge.
Within the Flexirene film-grade product family, the numerical suffix is not a reliable indicator of density or comonomer type; suffix values often distinguish melt flow index or additive package. Therefore, substitution of one grade for another should be based on the supplier’s current technical data sheet and not on product name alone. If a converter requires a higher-output grade, a product with a melt flow rate of 2.0 g/10 min may reduce melt pressure, but it may also reduce dart drop impact and bubble stability because lower melt viscosity reduces melt strength. If a toughener is required, a move to a hexene- or octene-based LLDPE at the same density may improve impact without changing gauge, but the extrusion pressure and film optics may shift.
Flexirene® CL 10 is not a stand-alone solution for all film structures. In coextruded barrier films, it is typically used in the sealant or bulk layers rather than the outer abuse layer when the outer layer must carry printing ink or withstand abrasion. In multilayer structures with polyamide or EVOH, the tie-layer selection and the processing of the polyethylene layer must be matched to avoid melt instability and layer non-uniformity. The butene-1 grade can be combined with LDPE in the same layer to improve bubble stability, but the addition of LDPE raises the melting range and changes heat-seal initiation temperature. Heat-seal performance should be evaluated by ASTM F2029 or ASTM F88 because seal strength is a function of density, comonomer type, and seal bar temperature, not melt flow rate alone.
Regulatory compliance for food-contact applications should be confirmed against FDA 21 CFR 177.1520 for olefin polymers and against EU Regulation 10/2011 for plastic materials intended for food contact. The applicable status depends on the finished film formulation, including any added slip, antiblock, or processing aid. REACH and RoHS conformity should be verified from the supplier’s latest certificate because additive packages may change between production campaigns. The base polyethylene is hydrophobic and insoluble in water, but the film may not be considered biodegradable or compostable under ASTM D6400 or EN 13432.
In storage and handling, the pellet should be kept away from direct sunlight and strong oxidizing agents. Prolonged storage at temperatures above 40°C can increase the rate of antioxidant depletion and shift the oxidation induction time measured by ISO 11357-6. The product is not hygroscopic, but surface moisture must be avoided. When regrind is used, the addition of more than 20 wt% clean edge trim can alter film optics and bubble stability; the regrind should be of known origin and free of polar polymer contamination. Any final film property verification should be performed on production-scale film, not on pellet-compression molded specimens, because back-pressure, screw speed, and draw down affect orientation and residual stress.