Versalis Flexirene Cl 10 Butene Copolymer Linear Low Density Polyethylene

Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 915899
    Polymertype Linear Low Density Polyethylene
    Comonomertype Butene-1
    Density 0.920 g/cm³
    Meltflowrate 3.5 g/10 min (190°C/2.16 kg)
    Meltingpoint 120 °C
    Vicatsofteningtemperature 95 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 700%
    Flexuralmodulus 200 MPa
    Hardnessshored 50
    Haze 8%
    Gloss 85%
    Dartdropimpact 120 g

    As an accredited Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Flexirene® CL 10 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe industrial storage and transport.
    Container Loading (20′ FCL) Versalis Flexirene® CL 10 butene copolymer LLDPE loaded in 20′ FCL: 25 kg bags, palletized, stretch-wrapped, secured for ocean transport.
    Shipping Versalis Flexirene® CL 10 Butene Copolymer LLDPE is shipped as non-hazardous solid polyethylene pellets in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers dry, closed, and away from heat, sunlight, and moisture. No dangerous-goods placarding is normally required; follow local transport and handling regulations.
    Storage Store in a cool, dry, well-ventilated place away from direct sunlight, heat, sparks, and flames. Keep in original, closed containers/packages, palletized, and off the floor. Protect from moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Keep away from strong oxidizing agents. Maintain good housekeeping to prevent pellet spills/slipping hazards. Ensure containers are closed when not in use.
    Shelf Life Shelf life is approximately 24 months when stored in original, unopened packaging under cool, dry conditions, away from direct sunlight and heat.
    Application of Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene

    On high-stalk blown film lines fitted with internal bubble cooling and dual-lip air rings, Flexirene CL 10 butene copolymer linear low density polyethylene is processed at a melt temperature set between 190 °C and 230 °C and a die-zone temperature no higher than 240 °C to suppress gel formation from localized oxidation. The nominal density of 0.918 g/cm³, determined per ASTM D792-20, and the melt flow rate of 1.0 g/10 min, determined at 190 °C/2.16 kg per ISO 1133-1:2022, place the resin in the low-melt-index sector of butene LLDPE. On 45 mm to 120 mm grooved-feed extruders with length-to-diameter ratios of 24:1 to 30:1, stable bubble operation is obtained at blow-up ratios of 2.2:1 to 3.0:1 and frost-line heights of 6 to 10 die diameters. Dart impact resistance, measured according to ASTM D1709-15a Method A, generally increases as the frost line is raised, provided the bubble remains centred and the film temperature at the frost line does not drop below the crystalline solidification onset. Tensile yield and elongation at break are assessed with ASTM D882-18 at a jaw separation rate of 500 mm/min; tear resistance is routinely measured by ASTM D1922-15 for machine-direction and transverse-direction propagation. On production lines, die-lip build-up is minimised by maintaining the lower die gap at 1.8 mm to 2.4 mm; when sharkskin or melt fracture appears on the outer bubble surface, a fluoropolymer-based processing aid is added at 200 mg/kg to 800 mg/kg to condition the die lip and reduce shear stress at the metal-melt boundary. Film blocking is addressed with silica antiblock masterbatch at a typical loading of 2 wt% to 5 wt%, while slip performance is obtained with erucamide or oleamide concentrates at converter-specified migration rates. The low-density butene backbone permits downstream conversion on form-fill-seal equipment running at jaw speeds above 40 cycles/min; however, hot-tack strength must be validated on the specific packaging machine because seal-bar pressure and dwell time alter the heat-seal response.

    Compliance for food packaging contact rests on the converter, not on the raw resin certificate alone. The relevant olefin polymer provisions in the United States are 21 CFR 177.1520, including the extractable fraction limitations referenced therein; in the European Union, multilayer films are evaluated against Regulation (EU) No 10/2011 with the overall migration limit of 10 mg/dm². Corona treatment for lamination or printing is usually set between 38 mN/m and 44 mN/m wetting tension, measured with dyne solutions per ASTM D2578-23, but excessive treatment can oxidise the surface and increase seal initiation temperature on reverse-printed laminates.

    Test standardMeasured parameterApplication relevance
    ISO 1133-1:2022Melt flow rate at 190 °C/2.16 kgExtruder throughput and melt pressure estimation
    ASTM D792-20Solid densityPackage weight and yield calculations per tonne
    ASTM D1709-15aDart impact resistanceSack and liner puncture tolerance
    ASTM D882-18Tensile yield, elongation at break, secant modulusFilm handling and load retention
    ASTM F88/F88M-23Heat-seal strengthForm-fill-seal pack integrity
    21 CFR 177.1520 / EU No 10/2011Migration limitsFood-contact compliance verification

    Why Does Chill-Roll Haze in Cast Film Track the Oxidation Layer Formed in the Air Gap?

    The relationship between chill-roll haze and oxidation layer thickness in cast film is observed on flat-die lines where the molten web exits the die at 230 °C to 260 °C and remains airborne for 15 mm to 30 mm before contacting the polished roll. In this interval, the surface of the butene copolymer oxidises sufficiently to alter the refractive index of the quenched skin layer; the resulting haze is measured by ASTM D1003-21 and is influenced more by air-gap residence time than by bulk resin density. Chill-roll temperature is commonly held between 18 °C and 30 °C depending on line speed and film thickness. When gauge drops below 20 µm, the melt curtain must be pinned to the chill roll within 30 mm to 60 mm of the die exit to suppress draw resonance. In practice, cast film converters use a vacuum box or air knife positioned above the chill roll to induce rapid contact; without such positioning, edge-curl and transverse gauge variation become visible at speeds above 120 m/min. Seal initiation temperature is evaluated from gradient-bar laboratory sealers and subsequent peel tests per ASTM F88/F88M-23; thin cast webs from butene LLDPE can exhibit seal initiation below 105 °C when the quench rate is high and the chill-roll temperature is kept low, but published data for this specific configuration is limited and must be established on the actual line.

    Cast film lines running at 150 m/min to 350 m/min use a screw with a barrier flight and a Maddock mixing section to even out the melt temperature. A die gap of 0.5 mm to 0.8 mm and a die-to-roll air gap of 15 mm to 30 mm are typical for thin-gauge packaging webs. Haze values below 3 % are not determined by the butene copolymer alone; they depend on polish roll surface roughness, oxidation layer thickness, and the absence of additive plate-out at the die lip. Fluoropolymer processing aid at 400 mg/kg reduces die build-up but can reduce surface tension before corona treatment. Corona treatment is therefore delayed until after the primary chill roll, and where lamination is intended, wetting tension above 38 mN/m is verified per ASTM D2578-23 before dry-bond or extrusion lamination.

    When a Butene Copolymer Replaces C4 LDPE in Extrusion Coating of Kraft and Aluminium Foil

    Extrusion coating of paperboard, kraft, and aluminium foil imposes demands on melt strength, neck-in, and adhesion that differ from film extrusion. Flexirene CL 10 is not used as the sole extrusion-coating resin at high line speeds because its butene-based linear architecture yields a broader molecular weight distribution than autoclave LDPE but lower melt strength than high-pressure LDPE. The practical solution is compounding with LDPE before coating; blends with 20 wt% to 40 wt% Flexirene CL 10 are processed through a single-screw extruder with a length-to-diameter ratio of 30:1 to 36:1 and a flat die with internal deckles. Melt temperature at the die is typically set between 280 °C and 310 °C to promote adhesion to aluminium foil and paperboard, but residence time at these temperatures must be limited because butene LLDPE oxidises more readily than high-pressure LDPE at the same temperature. Neck-in measured on a pilot line at 200 m/min is generally higher for the butene copolymer blend than for LDPE homopolymer; coating weight uniformity is maintained by adjusting the die deckle width and by increasing the air-gap distance to 200 mm to 350 mm. The coated substrate adhesion is quantified with peel tests after conditioning at 23 °C and 50 % relative humidity for at least 24 h; values are sensitive to ozone treatment of the melt curtain, which is applied at 0.5 kW/m² to 1.5 kW/m² depending on line speed and substrate.

    Adhesion to aluminium foil is evaluated by T-peel per ASTM D1876-08(2023), while coating thickness down to 10 µm is verified by cross-sectional microscopy or infrared absorption. Where liquid packaging lines exceed 300 m/min, the LLDPE blend fraction is kept at or below 20 wt% to avoid edge weave and web breaks. The same blend rule is applied when coating photographic-grade paper and sterilizable medical packaging stock, because the lower branch of the melt strength curve is the controlling limit rather than extruder output.

    Interlayer Adhesion Failure Modes in Three-Layer Silage Wrap Containing Butene LLDPE

    Three-layer silage wrap produced by coextrusion poses a specific interlayer adhesion risk when Flexirene CL 10 is assigned to the core or backing layer. The outer cling layer is usually based on an ultra-low-density or metallocene-catalysed copolymer with a tackifier package, not on butene LLDPE. In the core, the 0.918 g/cm³ density lowers the bending stiffness of the cast film and allows pre-stretch on agricultural wrappers from 55 % to 75 % before the film enters the bale chamber. Interlayer adhesion is measured by peel testing after 24 h of wound roll ageing; a recorded loss of more than 50 % relative to the 1 h value indicates migration of low-molecular-weight tackifier from the cling skin into the core, which is accelerated by storage temperatures above 35 °C. Surface cling is quantified by ASTM D5458-95(2020), puncture resistance by ASTM D5748-95(2019), and tensile properties of the film by ISO 527-3:2018. The required balance is control of machine-direction elongation after pre-stretch, which should not exceed the wrapper load-cell limit; excessive machine-direction elongation causes bale retention force to decay within the first 24 h after wrapping.

    Ultraviolet stabilization in silage wrap is critical because the film is stored outdoors for 6 to 12 months. Hindered amine light stabilizers are added at 0.10 wt% to 0.30 wt% depending on geographic UV exposure, with UV absorbers added for surface protection. The converter must measure additive dispersion by ISO 18553:2002 and confirm that no agglomerates above 10 µm remain in the core layer; agglomerates act as stress concentrators and reduce puncture resistance. Failure mode analysis on wrapped bales shows that splitting initiates at the fold line of the bale edge or at the clamp point where the film is cut; these zones require the highest notched tear resistance. Notched tear propagation is assessed by the Elmendorf tear method ASTM D1922-15; values improve with bubble orientation in blown silage wrap but remain lower in cast constructions unless the core is coextruded with sufficient molecular orientation.

    On form-fill-seal lines converting heavy-duty sacks for fertilizer, resin pellets, and petrochemical products, Flexirene CL 10 is coextruded as the outer or inner ply in tubular film with HDPE or MDPE in the core. The objective is to balance creep resistance under stacking with a low-temperature seal that closes reliably through dusty valve-sack openings. Blown film lines in this segment run die diameters from 200 mm to 400 mm and output rates of 150 kg/h to 450 kg/h depending on extruder size. A melt flow rate of 1.0 g/10 min keeps melt pressure high enough to maintain bubble stability with high-molecular-weight HDPE in the core, while the lower-density outer ply contributes to dart impact and improves seal behaviour through contamination layers. Dart impact tests per ASTM D1709-15a Method B at film thicknesses of 150 µm to 200 µm show that the outer LLDPE-rich layer contributes more to puncture tolerance than the HDPE core. Filled-sack drop resistance is assessed by ISO 7965-2:2013 after conditioning at 23 °C and 50 % relative humidity; repeated drop cycles expose shortcomings in seal integrity rather than in film tensile strength. Creep under load is screened with ASTM D2990-17; however, full pallet compression testing on the converted sack is the production-scale method. When recycled LDPE is introduced at 15 wt% to 30 wt% in the core or outer layer, the melt pressure oscillates more widely across the screen changer; screens of 120 µm to 200 µm mesh must be used with automatic screen changers to avoid gel accumulation at the breaker plate.

    Twin-Screw Compounding of Butene LLDPE Carriers Does Not Tolerate Low Intake Zone Temperatures

    Co-rotating twin-screw compounding with Flexirene CL 10 as a masterbatch carrier is constrained by torque at the feed throat. The melt flow rate of 1.0 g/10 min, measured per ISO 1133-1:2022, means the polymer enters the plastification section as a high-viscosity melt; if the intake zone barrel temperature is below 170 °C, the specific energy input can exceed 0.25 kWh/kg and the screw safety coupling may disengage. Calendering and pelletising on a strand line require a die pressure below 10 MPa to prevent die swell from producing out-of-round pellets; strand bath water temperature is held at 15 °C to 25 °C to quench the filled compound. Mineral filler loadings of 30 wt% to 60 wt% calcium carbonate are dispersed at screw speeds of 400 min⁻¹ to 800 min⁻¹, depending on filler particle size and coating. Dispersion quality is assessed by ISO 18553:2002; agglomerate counts at 10 µm to 30 µm are compared against the converter internal specification. Letdown in final film at 3 wt% masterbatch dilution is verified by ash content per ISO 3451-1:2019 and by tensile elongation retained at more than 80 % of the uncompounded control when tested per ISO 527-3:2018.

    Free Quote

    Competitive Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Flexirene® CL 10 is a butene-1 copolymer linear low-density polyethylene supplied as a pelletized cast film resin. The typical density is 0.918 g/cm³ when measured according to ISO 1183-1, and the nominal melt flow rate is 1.0 g/10 min at 190 °C under a 2.16 kg piston load according to ISO 1133-1. The comonomer is butene-1, which introduces short ethyl branches into the otherwise linear polyethylene backbone; this structural feature separates the grade from hexene- or octene-based linear low-density polyethylene resins that use longer α-olefin branches. The grade is intended for mono-layer and coextruded cast stretch film, lamination film, and agricultural film. Because the nominal melt flow rate is moderate, the resin retains more melt elasticity than a high-melt-flow cast film grade, which influences neck-in and draw resonance behavior on flat-die lines. Typical differential scanning calorimetry data according to ISO 11357-3 indicate a peak melting temperature of 121 °C to 123 °C, and the Vicat softening temperature by ISO 306/A50 is typically reported at 98 °C to 100 °C. The product is stabilized for normal melt processing; however, residence time and melt temperature must still be controlled to limit gel formation and optical specks in thin film.

    How Butene Comonomer Length Changes Film Toughness Relative to Octene Grades

    Comonomer length controls the architecture of the amorphous tie chains. Butene-1 incorporation creates ethyl branches, which are shorter than the butyl branches from hexene-1 or the hexyl branches from octene-1. Under tensile testing to ISO 527-2, a butene-based LLDPE of 0.918 g/cm³ generally develops lower tensile yield stress than an octene-based LLDPE of the same density, and dart impact strength measured to ASTM D1709 is typically lower. The reduced branch length depresses the probability of forming tie molecules between adjacent lamellae, which lowers puncture resistance and slow crack growth resistance. The shorter branch length also lowers the melting point and can reduce haze in cast film when the chill roll is operated at 20 °C to 30 °C. In machine-direction stretch wrap, the moderate 1.0 g/10 min melt flow rate of Flexirene CL 10 supports higher extensional viscosity than a 2.0 g/10 min high-speed cast film grade, which can reduce web breaks in the draw gap. Published direct comparative data for Flexirene CL 10 against specific octene-based commercial grades is limited; the mechanical distinction is based on the general butene versus higher α-olefin LLDPE class, not on a single competitor data sheet.

    The following typical values are representative for initial die and chill roll calculations and should not be read as contractual lot specifications.

    PropertyMethodTypical value
    DensityISO 1183-10.918 g/cm³
    Melt flow rateISO 1133-11.0 g/10 min
    Peak melting temperatureISO 11357-3121–123 °C
    Vicat softening temperatureISO 306/A5098–100 °C
    Tensile stress at yieldISO 527-211 MPa
    Tensile strain at breakISO 527-2>800%

    Melting, Shear Viscosity, and Die-Exit Stability in Cast Film Conversion

    On single-screw cast film extruders of L/D 30:1 to 35:1, Flexirene CL 10 is processed with a barrel profile that rises from 170 °C to 190 °C in the feed and compression zones to 230 °C to 250 °C in the metering and die zones. A flat die with a die gap between 0.6 mm and 0.8 mm is common for films from 12 μm to 50 μm. Melt temperature should remain below 280 °C; prolonged operation above this threshold initiates thermal-oxidative chain scission and crosslinking, evidenced by yellowed gels, die-lip deposit, and melt pressure drift. Below 210 °C, the viscosity of the 1.0 g/10 min melt flow grade limits output on shallow-channel screws and raises backpressure at the screen pack, particularly when using 120 μm polished screen packs.

    The die-to-chill-roll gap is typically held between 10 mm and 25 mm; excessive gap increases neck-in, while a very short gap can trap air and produce pockmarked film edges. Chill roll set points of 20 °C to 30 °C are conventional. In coextrusion with high-density polyethylene skins, the lower melting point of CL 10 tends to widen the process window for interlayer bonding at 240 °C to 250 °C die temperature. At the die exit, draw ratios are typically held between 40:1 and 80:1; above this range, draw resonance can appear as periodic thickness bands unless the die gap is widened or the melt temperature is raised by 5 °C to 10 °C.

    Because the machine-direction tensile strain at break of the resin is typically above 800% under ISO 527-2, the material is used in machine-film pre-stretch operations on power-driven roller systems. In a 17 μm monolayer cast stretch film processed at a line speed of 600 m/min, web tension is usually maintained below 2.5 N/cm width at the winder to avoid blocking and stretch-force drift; published data for this specific configuration is limited. The butene branch structure reduces the melting point to 121–123 °C, allowing lower heat-seal initiation temperatures than high-density polyethylene layers in lamination structures. In cast lamination film for book covers or printed graphics, the resin is often placed as the seal layer because its low modulus reduces spring-back and permits clean guillotine cutting without edge cracking. Converters should verify the coefficient of friction and blocking force at 40 °C and 30% relative humidity because butene-based grades can exhibit higher blocking tendency after repeated winder traverses.

    Corona treatment of cast film produced from Flexirene CL 10 is usually required before printing or lamination. A surface energy target of 38 mN/m to 42 mN/m is recommended under ASTM D2578; treatment levels above 46 mN/m can increase blocking and reduce heat-seal strength. The resin responds to standard corona discharge units placed before the winder. Because antioxidant and processing stabilizer packages can affect wetting decay, treated film should be printed or laminated within 24 h or re-verified before use.

    Extrusion coating of lightweight papers and boards with the resin produces a higher melt curtain stability than high-fluidity grades, but line speed may be limited to 150 m/min to 250 m/min on flat-die coaters with 0.5 mm to 0.7 mm die gaps. Adhesion to paper is typically improved by ozone or corona pretreatment; without surface oxidation, peel strength measured to ISO 8510-2 may fall below the converter’s target, particularly when using clay-coated boards. Published data for this specific configuration is limited.

    When Heavy-Duty Inner Plies Demand Puncture Energy Above Butene LLDPE Limits

    In woven polypropylene sack inner liners, the film must withstand puncture during filling and flexural fatigue during stacking. Under film puncture testing by ASTM D5748, a butene-based LLDPE of 0.918 g/cm³ may show lower puncture energy than an octene-based LLDPE of equal density because short ethyl branches do not generate the same tie-molecule density. If the liner specification requires puncture energy above the typical butene LLDPE threshold, Flexirene CL 10 should be blended with an octene-based LLDPE or high-pressure LDPE at 15 wt% to 30 wt% to improve dart impact and slow crack growth. The resulting blend must be pre-evaluated on the production line with a temperature profile not exceeding 250 °C. In blown film coextrusion of heavy-duty liners, the grade may be less suitable because its cast film orientation has lower bubble stability; published data for this specific configuration is limited.

    Carrier resin selection in masterbatch and dry-blend operations should be controlled to avoid melt pressure variance. The carrier resin of a cling agent, polymer processing aid, or pigmented concentrate should have a melt flow rate within 0.7 g/10 min and 1.3 g/10 min; a carrier melt flow rate above 4.0 g/10 min can lower local viscosity and create film thickness fluctuations at the die lip. Regrind from edge trim can be recycled into the extruder at 10 wt% to 20 wt% without significant gel increase if the trim is clean and the melt filtration system has a 120 μm screen pack. Higher regrind ratios magnify contamination from labels, adhesive residues, or oxidized film; if gel count measured by camera detection on a 2 m film path exceeds 5 ppm of the web area, the regrind fraction should be reduced or the screen pack changed. At relative humidity above 70%, pellet surface condensation is possible during cold storage; polyethylene does not require predrying, but free water must be removed with dry air at 60 °C for 2 h before the hopper.

    Regulatory Limits Define Downstream Addition and Testing Boundaries

    For food-contact articles, the converter must establish compliance under Commission Regulation (EU) No 10/2011 and, where applicable, FDA 21 CFR 177.1520 for olefin polymers. Overall migration testing under the EN 1186 series and specific migration testing for additives must be completed on the final laminate or coated article because the polymer alone does not guarantee a food-contact declaration. The grade is supplied with antioxidant and processing stabilizer packages; downstream converters should avoid combining the resin with high levels of free radical initiator masterbatches used for vis-breaking because uncontrolled rheology modification can generate low-molecular-weight extractables and alter the 1.0 g/10 min melt flow rate in the final film. No halogenated flame-retardant or lead-based pigment should be added where RoHS Directive 2011/65/EU compliance is claimed. Under REACH, the ethylene and butene-1 monomers must be registered; the polymer itself is exempt from registration but not from authorization or restriction of contained monomers and additives.

    For silage wrap and agricultural tunnel film, the low density and high elongation of CL 10 allow film to follow irregular bale surfaces. In agricultural film trials, a 25 μm single-layer film on a 1.5 m cast line has been drawn to 150% elongation in the machine direction without brittle failure when the chill roll is kept at 22 °C; published data for this specific configuration is limited. The material is not intended for applications requiring long-term outdoor UV resistance unless a suitable hindered amine light stabilizer masterbatch is incorporated by the converter. UV-stabilized films should be tested to ISO 4892-2 for weathering or ASTM G154 for accelerated UV exposure before batch release.

    Top