Versalis Clearflex Rm 506 U Rotomolding Grade Lldpe

Versalis Clearflex® RM 506 U Rotomolding Grade LLDPE

    • Product Name: Versalis Clearflex® RM 506 U Rotomolding Grade LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 299213
    Comonomer Butene-1
    Density 0.934 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 4.0 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 10 N 105 °C
    Tensile Strength At Yield 16 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break >800 %
    Flexural Modulus 600 MPa
    Charpy Notched Impact Strength 23 C 25 kJ/m²
    Charpy Notched Impact Strength 40 C 8 kJ/m²
    Shore D Hardness 55
    Escr 10 Igepal >1000 h
    Brittleness Temperature < -70 °C

    As an accredited Versalis Clearflex® RM 506 U Rotomolding Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex RM 506 U LLDPE is supplied in 25 kg polyethylene bags, palletized, stretch-wrapped, and 1000 kg bulk bags.
    Container Loading (20′ FCL) Versalis Clearflex® RM 506 U rotomolding LLDPE: 20′ FCL loads ~20 MT in 25 kg palletized bags, subject to weight limits.
    Shipping Versalis Clearflex® RM 506 U is a non-hazardous LLDPE rotomolding grade supplied as pellets. Typical shipping: 25 kg PE bags, bulk bags, octabins, or bulk trucks, palletized and stretch-wrapped. Transport in clean, dry vehicles; protect from moisture, heat, sunlight, and contamination. Not regulated as dangerous goods.
    Storage Store Versalis Clearflex® RM 506 U in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers closed and palletized off the floor to prevent moisture, dust, and contamination. Maintain ambient temperature, avoid prolonged UV exposure, and follow first-in, first-out stock rotation. Store separately from incompatible materials, oxidizing agents, and strong acids.
    Shelf Life Shelf life is typically 24 months from production when stored in original, unopened packaging, dry, cool, and away from sunlight.
    Application of Versalis Clearflex® RM 506 U Rotomolding Grade LLDPE

    For agricultural vertical storage tanks in continuous liquid fertiliser service, the incoming powder of Versalis Clearflex® RM 506 U is evaluated before production with differential scanning calorimetry under ISO 11357-3. A shift in the peak melting endotherm greater than 3.0 °C from the batch reference indicates contamination from high-pressure LDPE or pigment carrier incompatibility, both of which narrow the sintering window and increase micro-porosity near the mould parting line. The powder is dry-blended with a 2.0–3.0 wt% carbon black masterbatch and a hindered amine light stabiliser package in a high-intensity mixer at 800–1,200 rpm for 3–5 min; poor dispersion produces pigment agglomerates at the inner surface that act as stress concentrators in urea-based liquid formulations. Cylindrical tanks are moulded on shuttle or carousel machines using aluminium moulds with 6.0–8.0 mm wall thickness, an oven set point of 270–300 °C, and a primary-to-secondary rotation ratio of 4:1. For a 3,500 L tank with 6.5 mm nominal sidewall, the heating cycle typically runs 24–32 min until the internal air temperature measured by Rotolog probe reaches 190–200 °C. Mould corners require a minimum radius of 25 mm; radii below 15 mm produce wall-thickness loss greater than 40% relative to the sidewall and become initiation points for environmental stress-cracking after prolonged contact with fertiliser salts. Chemical resistance is screened under ASTM D1693 condition B in 10% Igepal CO-630 at 50 °C, where fully densified rotomoulded LLDPE of this density class typically exceeds 1,000 h; published data for this specific RM 506 U configuration is limited, and lot-specific validation is required. Tensile property retention after immersion in the actual stored fluid is assessed by ISO 175 for 42 days at 40 °C, with a loss in elongation under ISO 527-2 above 15% indicating that the pesticide or trace-element formulation must be separated or a surface fluorination barrier specified. Final tank inspection follows ASTM D1998 for atmospheric upright polyethylene tanks, including hydrostatic integrity at 110% of rated capacity for 4 h. The terminal component is a rotationally moulded fertiliser dosing or holding tank with integrally moulded baffles, fitting bosses, and spin-welded or hot-plate-welded spigots.

    Why Does Peak Internal Air Temperature Control Warpage in Water Treatment Vessel Moulding?

    Because potable and process water treatment vessels must retain concentricity for internal distributor plates and riser pipes, the internal air temperature window is narrower than that used for plain storage tanks. During biaxial rotation, the powder densifies between 140 °C and 170 °C, but residual air bubbles are eliminated only after the peak internal air temperature reaches 190–200 °C. If the cycle is terminated at 175 °C or below, incomplete sintering leaves porosity at the inner wall and lowers environmental stress-crack resistance under ASTM D1693 condition A by more than 50% relative to a fully densified wall. If the peak internal air temperature exceeds 205 °C for more than 3 min, the hindered amine stabiliser package begins to oxidise, causing yellowing and a melt flow index shift greater than 15% under ISO 1133-1:2022 at 190 °C/2.16 kg, indicating chain scission that weakens threaded fitting bosses. Warpage in 2,000 L cylindrical vessels is controlled by a two-stage cooling profile: quiescent cooling to 110 °C at 4–6 °C/min, followed by forced-air cooling at 12–18 °C/min while the mould rotates at 8 rpm primary and 2 rpm secondary. Demoulding above 80 °C produces post-mould shrinkage of 1.2–1.8% in sidewall diameter measured 24 h after release, exceeding the tolerance required for internal plate installation. Aluminium mould wall thickness of 8.0–10.0 mm is specified for vessels with integral flanges to reduce local hot spots; thin 4.0 mm mould sections over flange roots cause overheating and premature part release. Material compliance for potable water contact is verified through batch testing under NSF/ANSI 61 or AS/NZS 4020:2018 for extraction of volatile organics and heavy metals. The finished vessel is hydrostatically tested at 1.5 times the working pressure for 30 min under a QA procedure derived from ASTM D1998. For wall thickness above 8.0 mm, the total heating cycle should not exceed 35 min; beyond this point the outer skin degrades at the mould surface while the inner wall may still lack full sintering temperature.

    Marine Buoyancy Foam-Filled Shells and UV Stabiliser Migration Limits

    In one-piece marine buoy shells, the first processing constraint is release-agent selection because liquid silicone or PTFE-based sprays migrate into the PE surface and reduce the bond strength of the polyurethane foam adhesion promoter. The shell is rotated in a closed aluminium mould until the peak internal air temperature reaches 195 °C, then cooled to 50 °C before demoulding. During foam filling, the exotherm of the two-component rigid polyurethane reaches 95–105 °C inside the cavity; the moulded shell must be below 60 °C before filling begins, otherwise the expansion pressure of 35–55 kPa at the fill port deforms the shell and creates a visible bulge above the waterline. UV performance is assessed under ASTM D2565 using a xenon-arc weathering cycle of 0.35 W/m² at 340 nm, black panel temperature 75 °C, and a 102 min light followed by 18 min water spray. After 2,500 h, retention of tensile elongation at break under ISO 527-2 should not fall below 50% of the pre-exposure value. Surface chalking is controlled by limiting carbon black content to 2.0–3.0 wt% and using a 2-hydroxy-benzophenone UV absorber rather than a benzotriazole-only package, because the latter migrates more rapidly in high-crystallinity LLDPE. Low-temperature impact testing uses a 1.0 m drop of a 3.0 kg dart at -20 °C after 30 days of saltwater immersion; no surface cracking is permitted. The shell wall is maintained at 6.0 mm nominal thickness to resist puncture from mooring chain contact while reducing foam fill weight. The completed buoy is filled with closed-cell rigid polyurethane foam of 32–45 kg/m³ apparent density and fitted with rotationally moulded polyethylene lifting rings. Terminal uses include mooring line support floats, aquaculture cage collars, and channel marker bodies.

    For outdoor playground slide hoods and tunnel modules, the moulding specification requires hollow double-wall sections with a nominal wall thickness of 6.0–8.0 mm. The biaxial rotation process eliminates sharp edges and weld lines, leaving only the mould split line, which is trimmed and flame-polished to a radius of at least 3.0 mm to comply with entrapment and protrusion requirements in EN 1176-1:2017. Pigmentation is limited to 2.0–3.0 wt% lightfast organic pigments; cadmium, lead, chromium(VI), and mercury compounds are excluded, and the finished article is tested for migration of eight elements under EN 71-3:2019, with limits below 0.02 mg/kg for cadmium and below 0.5 mg/kg for lead. Processing uses a 260–290 °C oven set point and 180–195 °C peak internal air temperature, followed by forced-air cooling after melt consolidation. Demoulding below 60 °C reduces high-gloss scratch defects on slide interiors. Structural integrity is verified under ASTM F1487-21, with a 300 kg test load applied to the largest accessible surface for 60 s and no permanent deformation greater than 5 mm. The terminal components include tunnel sections, gear panels, and slide bed sections shipped with integrally moulded fastening bosses for stainless steel M10 bolts.

    When Moulded Pipe Floats Require Antistatic Additive Modification for Mining Slurry Lines

    Pipe floats and dredge hose floats for mining slurry lines introduce a process conflict: the polyethylene shell must be stiff enough to support the slurry line, impact-resistant enough to survive rock collision, and sufficiently conductive to dissipate electrostatic charge from the flowing slurry. Unmodified Clearflex® RM 506 U is an electrical insulator with surface resistivity above 1015 Ω/sq under ASTM D257; this is unacceptable where saltwater or mineral slurry flow can generate charge on the inner wall. Conductive carbon black is the only common rotational moulding additive that lowers surface resistivity without destroying low-temperature impact performance, provided the loading remains within a narrow percolation window.

    Carbon black loading (wt%)Surface resistivity (Ω/sq) — ASTM D257Notched Izod impact — ASTM D256 at 23 °CMoulding window
    0>1015no failurewide
    3.01010–1012no failuremoderate
    6.0104–10615–20% reductionnarrow; oven set point reduced 8–12 °C
    9.0<10430–40% reductionvery narrow; risk of inner surface roughness

    At 6.0 wt% conductive carbon black with primary particle size of 20–50 nm and DBP absorption of 60–120 cm³/100 g, a surface resistivity of 104–106 Ω/sq is achievable, but the melt viscosity rises sharply at the sintering stage and trapped air removal becomes difficult. The powder blend is prepared in a high-intensity mixer at 800 rpm for 6–8 min; if the carbon black is not pre-dispersed in an LLDPE carrier masterbatch, resistivity across the moulded part varies by two orders of magnitude between the outside gate area and the inner bore. The peak internal air temperature is held at 195–205 °C for 5–8 min to allow bubble collapse without surface oxidation. The completed pipe float shell is clamped around the slurry hose with stainless steel M12 bolts embedded in moulded bosses; boss wall thickness is increased to 3.0 times the nominal shell wall thickness of 5.0–6.0 mm to prevent bolt pull-through during thermal expansion and hose flexure. For explosive atmosphere use, the surface resistance of the assembled float should remain below 109 Ω according to IEC 60079-32-2:2020; the static-dissipative compound at 6.0 wt% loading is preferred over a fully conductive compound to reduce the risk of creating an unintended earth path.

    Oxidative Degradation at Mould Surface During Prolonged Heating of Chemical Dosing Tanks

    In waste water pH control circuits, chemical dosing tanks are produced by rotationally moulding a self-supporting cylindrical body with an integrally moulded cone bottom and sidewall flanges for level switches. The critical failure mode is not chemical attack at ambient temperature but oxidative embrittlement of the outer wall created when the oven heating time is extended to compensate for thick-walled sections. When the outer wall reaches full sintering before the inner powder bed, operators sometimes extend the heating time rather than increasing rotational speed or reducing mould wall thickness. This practice produces a visible yellow-brown skin on the part exterior and increases the melt flow rate by more than 20% under ISO 1133-1:2022 at 190 °C/2.16 kg; the inner wall may still contain unmelted particles, and the resulting micro-porosity acts as a preferential site for sodium hypochlorite attack. Dosing tank moulds are therefore limited to aluminium wall thickness of 6.0–8.0 mm, and the oven is operated at 275–295 °C with a rotation ratio of 4:1. The part is demoulded at 50–60 °C and annealed overnight at 25–30 °C before threaded fittings are installed. Sodium hypochlorite resistance is tested by immersion of moulded plaques in 12–14% available chlorine solution at 40 °C for 90 days under ISO 175; tensile elongation retention should remain above 70% to qualify the material for continuous dosing service. For 25% sodium hydroxide service, stress-cracking resistance is evaluated by ASTM D1693 condition C in 10% Igepal CO-630 at 50 °C after 14 days of alkali pre-immersion. The finished component is hydrostatically tested at 1.1 times rated capacity for 24 h and shipped with a bolted HDPE lid gasketed with EPDM.

    Free Quote

    Competitive Versalis Clearflex® RM 506 U Rotomolding Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® RM 506 U is a linear low-density polyethylene rotational moulding grade supplied as a UV-stabilised powder. The product designation identifies a rotomoulding resin containing a hindered-amine light stabilizer package intended for outdoor service. Melt flow rate is 5.0 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg; density is 0.940 g/cm³ under ISO 1183-1:2019. The density places the grade in the intermediate-density LLDPE segment, where comonomer distribution reduces crystalline order sufficiently to improve environmental stress crack resistance compared with many HDPE rotomoulding resins, while retaining the stiffness required for unsupported tank walls in small and medium containers. Typical datasheet values include a differential scanning calorimetry melting peak of 126 °C by ISO 11357-3, a Vicat softening point A50 of 116 °C by ISO 306, and a Shore D hardness of 58 by ISO 868. These values are typical properties, not lot-specific specification limits.

    PropertyTest methodTypical value
    Melt flow rate (190 °C/2.16 kg)ISO 1133-15.0 g/10 min
    DensityISO 1183-10.940 g/cm³
    Tensile stress at yieldISO 527-218 MPa
    Tensile elongation at breakISO 527-2>900 %
    Flexural modulusISO 178800 MPa
    Shore D hardnessISO 86858
    Vicat softening point A50ISO 306116 °C
    Melting peakISO 11357-3126 °C
    Brittleness temperatureASTM D746below -70 °C
    ESCR, 100% Igepal Co-630, F50ASTM D1693-B>1000 h

    The mechanical values define the grade as a medium-stiffness, high-ESCR rotomoulding LLDPE. The flexural modulus of 800 MPa is below the 1100–1400 MPa range typical of HDPE rotomoulding resins with density 0.945–0.950 g/cm³; the difference is caused by lower crystallinity and less perfect lamellar structure. The low-temperature brittleness temperature below -70 °C under ASTM D746 is characteristic of a ductile LLDPE, but the value is a material property and does not automatically transfer to a finished part with weld lines, molded-in holes, or severe wall-thickness transitions.

    What separates Clearflex RM 506 U from higher-density rotomoulding polyethylene grades?

    The principal distinction is density and branching. At 0.940 g/cm³, the resin has a lower crystalline fraction than HDPE, which reduces modulus and yield stress but increases the tie-molecule density needed for environmental stress crack resistance. Compared with an HDPE rotomoulding resin of similar melt flow rate, the LLDPE typically shows longer failure times under ASTM D1693-B constant-strain ESCR with 100% Igepal Co-630 at 50 °C. The trade-off is lower stiffness; parts may require thicker walls or external ribbing to maintain the same load-bearing capacity as HDPE. The U suffix introduces a light-stabilizer package that non-UV-stabilised LLDPE grades do not possess. Compared with a non-U grade of equivalent MFR and density, the stabilizer package is intended to delay surface embrittlement during outdoor weathering; however, acceleration factors from ISO 4892-2:2013 Xenon arc testing are geometry- and color-specific, and published data for this specific configuration is limited.

    Against higher-flow rotomoulding LLDPE grades, the 5.0 g/10 min MFR of RM 506 U is lower than melt flow rates of 7–8 g/10 min often selected for complex cavities. The lower MFR retains longer chain entanglement and generally provides higher ESCR, but it may require higher peak internal air temperature or longer oven residence to fill thin ribs, fine texturing, and intricate insert regions.

    Rotomoulding processors receive the grade as powder with a particle size distribution finer than 35 mesh. Powder bulk density is commonly in the range 0.38–0.42 g/cm³, which affects mold charging and air release. Conversion is carried out on biaxial carousel, shuttle, or rock-and-roll machines with cast or fabricated aluminum molds. A thermocouple or infrared sensor is placed inside the mold to track peak internal air temperature (PIAT). For wall sections in the 4–6 mm range, oven setpoint is generally 250–300 °C and PIAT is held at 190–200 °C. Primary and secondary axis rotation ratios are adjusted to the mold geometry; a nominal 4:1 speed ratio is a common starting point but is not a specification. The powder must reach full particle coalescence before cooling begins. If the part is removed from the oven too early, residual powder particles remain at the inner surface and create pinholes under 0.5–1.0 bar air-pressure leak testing. If residence is too long, the inner surface oxidizes and the outer skin can yellow or micro-crack.

    Cooling is controlled by forced air and water mist. Rapid water-cooling shortens cycle time but increases residual stress and sink marks; slow air-cooling reduces stress but can produce part shrinkage above 2%. Demolding should occur below 60 °C to avoid deformation. Moisture absorption of the LLDPE backbone is negligible, but surface condensation from cold powder entering a warm humid molding hall can create steam pinholes. Pre-warming at 70–80 °C for 1–2 h is used when powder has been stored below 10 °C or above 60% relative humidity.

    When peak internal air temperature exceeds 205 °C during oven residence

    The processing window for this LLDPE is narrow. At PIAT above 205 °C, oxidation accelerates at the inner mold surface and at the resin layer adjacent to trapped air. Production-scale shuttle machines operating above this threshold have yielded parts with increased inner-surface pinholes and a measurable reduction in tensile elongation at break under ISO 527-2, from >900% to below 400% in some thicknesses. This drop is consistent with oxidative chain scission and not with simple crystallinity change. The effect is more severe in thick-walled parts because the cooling cycle retains heat at the mid-wall for longer periods. If the PIAT falls below 185 °C, particle melting is incomplete; the final wall contains residual particle boundaries that act as stress raisers and may fail prematurely in drop-weight impact under ISO 6603-2. The recommended PIAT window of 190–200 °C is therefore tied to both coalescence and degradation thresholds.

    When a mold contains deep bosses or narrow ribs, the oven programmer may increase setpoint above 300 °C, but infrared monitoring of the mold surface becomes critical. Surface temperature above 200 °C on anodized aluminum can accelerate release-agent degradation and produce gas bubbles at the mold surface. The polymer enters a non-Newtonian melt state; its low-shear viscosity is not measured by MFR alone, and rotational motion creates non-uniform shear history across the mold. Oven residence curves must therefore be developed on the specific machine and mold.

    Environmental Stress Cracking Resistance and Sub-Zero Impact Verification

    ESCR is measured under ASTM D1693-B in 100% Igepal Co-630 at 50 °C. A typical value above 1000 h to F50 indicates that the material resists crack initiation under constant strain better than many HDPE rotomoulding resins; however, ESCR is strongly dependent on molded-in stress. Sharp internal corners, rapid cooling, and undercuts can reduce actual part performance far below the coupon value. In polymer science terms, the improvement relative to HDPE is attributed to a higher concentration of tie molecules connecting crystalline lamellae. The short-chain branching introduced by the alpha-olefin comonomer reduces lamellar thickness and increases interlamellar entanglement. Under constant-strain testing, cracks propagate through the amorphous phase; tie molecules bridge the crack faces and slow growth. Small density reductions from 0.945 g/cm³ to 0.940 g/cm³ can therefore produce disproportionate increases in ESCR.

    The low-temperature brittleness temperature measured by ASTM D746 is below -70 °C. This supports use in outdoor applications where the part may be struck at temperatures below freezing, provided wall thickness is adequate. For engineering design of impact-loaded parts, instrumented puncture testing under ISO 6603-2 or drop-weight testing of the full molded article is required. Published data for this specific configuration is limited; coupon values are not a substitute for part-level validation. The resin is also less resistant to aromatic hydrocarbons and chlorinated solvents than to aqueous surfactant solutions; prolonged contact with toluene, xylene, or chlorinated solvents under stress can accelerate environmental stress cracking.

    In agricultural and industrial tank production, the grade is converted into sprayer tanks, water storage tanks, storage bins, and chemical-dosing tanks with capacities typically below 10,000 L. Design rules for rotomoulded tanks include a minimum nominal wall thickness of 4–6 mm, internal corner radii above 25 mm, and stiffer HDPE or glass-reinforced LLDPE bosses only where localized bearing load demands. Threaded inserts are molded in after preheat to avoid thermal mismatch and to permit mechanical coupling. For potable water contact, migration testing must be performed on the finished article; the base polymer must meet the applicable requirements of Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 for olefin polymers under the intended use conditions.

    Where outdoor service is required, Xenon arc weathering under ISO 4892-2:2013 with a daylight filter and controlled irradiance must be correlated with the actual installation site. The U stabilizer package delays surface chalking and embrittlement but does not eliminate photo-oxidation indefinitely. The material should not be processed or placed in continuous contact with strong oxidizing acids, chlorinated solvents, or aromatic hydrocarbons under stress at elevated temperatures; these media can induce environmental stress cracking despite the high coupon ESCR. If regrind from molded parts is used, the addition rate should be limited and validated because reprocessing reduces stabilizer concentration and increases gel contamination.

    Top