| HS Code | 389958 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer Type | 1-Octene |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Temperature | 124 °C |
| Vicat Softening Temperature | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 240 MPa |
| Hardness Shore D | 50 |
| Dart Impact Strength | 250 g |
| Elmendorf Tear Strength Md | 120 N/mm |
| Elmendorf Tear Strength Td | 200 N/mm |
| Haze | 12% |
| Gloss 45 | 50% |
As an accredited Versalis Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe handling, transport, and storage. |
| Container Loading (20′ FCL) | 20′ FCL: Versalis Clearflex® H&T LFH 208 octene copolymer LLDPE in 25 kg bags, palletized, shrink-wrapped, secured, and evenly distributed. |
| Shipping | Versalis Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene is shipped as non-hazardous, free-flowing pellets in 25 kg PE bags or 1 MT octabins, palletized and stretch-wrapped. Transport in clean, dry trucks/containers; avoid moisture, heat, UV, and contamination. No special hazard placards required. |
| Storage | Store indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep original bags or containers tightly closed, clean, and palletized off the floor to prevent moisture pickup and contamination. Avoid prolonged UV exposure, extreme temperatures, and excessive stacking. Rotate stock and follow the supplier’s safety data sheet for additional guidance. |
| Shelf Life | Shelf life is approximately 24 months when stored in original, unopened packaging under dry, cool conditions, away from direct sunlight. |
In blown film extrusion of octene-copolymer linear low-density polyethylene of the Clearflex H&T LFH 208 class, bubble stability is governed by the ratio of melt relaxation time to transient extensional strain rate at the die lip. The polymer is processed on single-screw extruders with barrier screw geometry, typically 45 mm to 60 mm diameter and 30:1 L/D ratio, fitted with Maddock mixing sections to homogenise the melt prior to the annular die. Die gap is set between 1.8 mm and 2.4 mm, narrower than the 2.5 mm to 3.5 mm typical for low-density polyethylene, to compensate for the lower melt strength of the octene copolymer. Blow-up ratios are maintained between 2.2:1 and 3.0:1. At blow-up ratios below 2.0:1, transverse direction tensile properties and dart impact deteriorate measurably. At ratios above 3.2:1, bubble flutter and gauge variation exceed acceptable conversion tolerances. The frost line is positioned 300 mm to 700 mm above the die face. A frost line below 300 mm causes elevated film haze and residual orientation stress. A frost line above 700 mm increases susceptibility to bubble breathing and web wander. Melt temperature is controlled between 190°C and 215°C. Below 185°C, the elevated viscosity of the octene copolymer produces melt fracture at die output above 20 kg/h. Above 220°C, oxidative degradation initiates, evidenced by gel formation and progressive loss of dart impact. Output rates on a 45 mm extruder typically range from 15 kg/h to 35 kg/h, limited by available torque at screw speeds of 90 rpm to 120 rpm. Film at 50 μm gauge exhibits dart impact of 400 g to 900 g per ASTM D1709 Method A, Elmendorf tear of 100 g to 220 g machine direction and 300 g to 500 g transverse direction per ASTM D1922, tensile strength of 35 MPa to 50 MPa machine direction per ISO 527-3, and elongation at break of 600% to 800% machine direction and 700% to 900% transverse direction. Haze ranges from 8% to 15% per ASTM D1003, with 45° gloss of 50 to 80 per ASTM D2457. Heavy-duty sack applications at 60 μm to 80 μm gauge, designed for 25 kg to 50 kg powder or granulate fill, require minimum dart impact of 600 g to survive drop testing per ISTA 3A.
Blending with autoclave LDPE at 10 wt% to 20 wt% increases bubble stability and permits a wider die gap of 2.2 mm to 2.8 mm. The trade-off is a reduction in dart impact of approximately 15% to 25% per 10 wt% LDPE addition and a proportional loss of Elmendorf tear resistance. The rheological basis for this behaviour is the higher long-chain branching density of autoclave LDPE, which elevates the zero-shear viscosity and strain-hardening modulus of the blend, but dilutes the tie-chain fraction contributed by the octene comonomer. Published data for the specific LFH 208 designation is limited; the values stated represent the documented performance envelope of octene-copolymer LLDPE film grades with melt flow rate 0.8 g/10 min to 1.0 g/10 min at 190°C and 2.16 kg per ISO 1133-1:2022.
| Blend Composition (wt%) | Dart Impact ASTM D1709 Method A (g, 50 μm) | MD Elmendorf Tear ASTM D1922 (g) | 45° Gloss ASTM D2457 |
|---|---|---|---|
| 100/0 LLDPE/LDPE | 500–900 | 120–220 | 50–70 |
| 85/15 | 400–700 | 100–180 | 45–65 |
| 70/30 | 300–500 | 80–140 | 40–55 |
| 50/50 | 180–300 | 60–100 | 30–45 |
When octene-copolymer LLDPE displaces butene-copolymer grades in multilayer sealant webs, the seal initiation temperature shifts downward by approximately 10°C to 20°C, while the hot tack window broadens. The sealant layer in a coextruded structure is typically 15% to 30% of total film thickness, ranging from 10 μm to 25 μm within an 80 μm to 120 μm total structure. Seal initiation temperature for optimised octene sealant grades is recorded at 85°C to 95°C versus 95°C to 110°C for equivalent butene-copolymer LLDPE, measured by differential scanning calorimetry per ISO 11357 and seal testing per ASTM F88. Hot tack strength per ASTM F1921 at 115°C typically exceeds 3.5 N/15 mm for octene sealant layers, a value not reliably achieved by butene grades at equivalent gauge. Seal strength after 24 h conditioning at 23°C and 50% relative humidity is measured at 15 N/15 mm to 25 N/15 mm per ASTM F88. The sealing window extends from 90°C to 140°C without burn-through on rotary jaw equipment. This performance supports packaging line speeds of 60 to 120 pouches per minute on horizontal form-fill-seal machines used for coffee, snack and dried food formats. Tie layers in five-layer structures are typically maleic anhydride-grafted LLDPE at 4 wt% to 6 wt% of total structure, bonding the octene sealant layer to EVOH or polyamide barrier layers.
| Regulatory Reference | Test Method / Clause | Compliance Parameter | Acceptance Criterion |
|---|---|---|---|
| FDA 21 CFR | §177.1520(c) | Polyolefin for food contact | Density 0.915–0.925 g/cm³ |
| EU Regulation 10/2011 | Annex I, Table 1 | Overall migration | <10 mg/dm² |
| EU Regulation 10/2011 | Annex I, Table 2 | Specific migration limit (1-octene) | <15 mg/kg food simulant |
| REACH | Regulation (EC) 1907/2006 | SVHC screening | <0.1 wt% per SVHC |
| ISO 1133-1:2022 | Method A | Melt flow rate | 0.8–1.0 g/10 min |
Anti-fog surfactant retention in multi-season tunnel greenhouse film is constrained by the rate of surface migration relative to surfactant loss through condensate wash-off. A three-layer covering film at 150 μm to 200 μm total thickness incorporates glycerol monooleate or sorbitan ester anti-fog agents at 0.5 wt% to 1.5 wt% in the inner layer only, with the core layer reserved for structural LLDPE and the outer layer formulated for UV resistance. Migration kinetics follow Fickian diffusion with effective diffusion coefficients of 10⁻¹² m²/s to 10⁻¹⁴ m²/s at 25°C; the inner-layer reservoir is calculated to replenish surface-active molecules for 24 to 48 months under Mediterranean solar flux. UV stabilisation uses hindered amine light stabilisers at 0.3 wt% to 0.7 wt% combined with a benzophenone absorber at 0.2 wt% to 0.4 wt% in the outer layer. Haze after 500 h accelerated weathering per ISO 4892-2 remains below 30% for correctly stabilised octene LLDPE. Extrusion temperature is held at 180°C to 195°C to prevent thermal degradation of the anti-fog surfactant; exceeding 200°C for more than 5 min residence time volatilises the glycerol ester and irreversibly reduces the internal reservoir. Film mechanical compliance is tested per EN 13206 for covering films intended for permanent greenhouses, with specific clauses covering tensile, tear, and dart impact after accelerated weathering.
After exiting a 400 mm annular die at a blow-up ratio of 2.8:1, collation shrink film produced from octene-copolymer LLDPE is oriented in the machine direction at 3:1 to 7:1 draw ratios and in the transverse direction at 4:1 to 8:1 on a simultaneous or sequential stenter frame. Final film thickness is 40 μm to 80 μm. Residual shrink performance at 160°C is measured at 50% to 75% machine direction and 55% to 75% transverse direction per ISO 14616. Shrink force at 160°C is typically 4 N/15 mm to 8 N/15 mm per ISO 14616, sufficient to immobilise a six-pack of 330 ml beverage cans without collapsing corrugate fibreboard trays. The octene comonomer provides higher elongation at break during the orientation step, reducing web breaks when compared to butene-copolymer LLDPE at equivalent draw ratios. Shrink tunnel operation at 130°C to 160°C requires residual solvent-free formulation and a slip package that does not volatilise at oven temperatures, with erucamide at 500 ppm to 1,000 ppm maintaining final-film coefficient of friction below 0.35 per ASTM D1894.In hygiene converting lines, backsheet embossing on octene-copolymer LLDPE film requires a polymer matrix that maintains dimensional stability under calendar roll temperatures of 70°C to 95°C while preserving the embossed pattern under downstream lamination tension. The film is extruded at 15 μm to 25 μm gauge and embossed with heated steel rolls at pattern depths of 40 μm to 200 μm. Pattern depth retention after 24 h at 40°C is typically above 70% of initial depth when the polymer crystallisation temperature is sufficiently low to permit rapid quench on the embossing roll. Lamination to polypropylene spunbond nonwoven is achieved by adhesive bonding with hot-melt adhesive coat weights of 1.5 g/m² to 3.0 g/m² or by extrusion lamination with a tie layer of maleic anhydride-grafted polypropylene. Peel strength of the laminate is measured at 2 N/25 mm to 5 N/25 mm per a modified peel test derived from ISO 527-3. Compliance for skin contact applications references ISO 10993 biocompatibility screening where the film is incorporated into finished medical or hygiene devices. The absence of butene comonomer branching irregularities in octene-copolymer LLDPE contributes to a smoother embossed surface with reduced die-lip streaking, which is quantified by surface roughness measurement below 0.8 μm Ra on the embossed film face.
After sealing jaws release on a vertical form-fill-seal machine running free-flowing granulate at 80 to 120 bags/min, the still-molten seal must bear the product drop load without peel-back failure. Octene-copolymer LLDPE of the Clearflex H&T LFH 208 class provides hot tack strength per ASTM F1921 in the range of 3.0 N/15 mm to 4.5 N/15 mm at 110°C, surpassing the minimum 2.5 N/15 mm required for drop-weight survival on high-speed vertical fill machines. The film is prepared at 50 μm to 90 μm gauge with a slip package of erucamide at 500 ppm to 1,000 ppm to achieve machine-direction kinetic coefficient of friction 0.15 to 0.25 per ASTM D1894 after 72 h migration at 23°C. Machine-direction Elmendorf tear per ASTM D1922 is retained at 100 g to 250 g, enabling clean propagation from laser-scored perforations without diagonal tear-out. Seal integrity after 24 h is measured at 15 N/15 mm to 22 N/15 mm per ASTM F88. The absence of excessively high seal plateau modulus prevents jaw-sticking on hot-bar sealing surfaces operated at 140°C to 160°C, a failure mode commonly observed with lower-MFI butene grades.At -30°C, the ductile-to-brittle transition of packaging films determines whether a frozen vegetable bag survives pallet handling or fractures at the fold crease. Octene-copolymer LLDPE of the LFH 208 class maintains an embrittlement temperature below -70°C per ASTM D746, a direct consequence of the longer C8 comonomer chain reducing crystallisable main-chain segment length compared to butene copolymers. Frozen food packaging structures are routinely extruded at 30 μm to 70 μm gauge, with dart impact at -20°C retaining 70% to 85% of room-temperature values per ASTM D1709. Distribution testing per ISTA 3A involves 10 to 12 drop cycles onto concrete from 1.2 m, conditions under which films with embrittlement temperatures above -40°C consistently fail at seal-fold intersections. Environmental stress crack resistance per ASTM D1693 exceeds 1,000 h without failure in 10% Igepal surfactant at 50°C, confirming suitability for high-fat frozen seafood packaging where surface oils contact the film over extended storage periods. The frozen food laminate commonly pairs the octene LLDPE as a sealant and outer abuse layer with a metallised PET or BOPP core, with the sealant gauge fixed at 15 μm to 25 μm to retain machine-direction tensile modulus above 200 MPa per ISO 527-3 during high-speed pouch converting.
Competitive Versalis Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® H&T LFH 208 is supplied as a pelletized octene-1 copolymer linear low density polyethylene for blown and cast film conversion. The model designation places the grade within the manufacturer’s high-toughness linear film range, with 1-octene rather than 1-butene or 1-hexene as the principal α-olefin comonomer. The octene-derived branch contains 6 carbon atoms, which increases tie-chain formation in the quenched film morphology and lowers the brittle-to-ductile transition temperature relative to C4-based grades at equivalent density and melt mass-flow rate. Lot-release characterization relies on ISO 1183-1:2019 for density, ISO 1133-1:2022 for melt mass-flow rate at 190 °C/2.16 kg, ISO 11357-3:2018 for melting peak temperature, and ISO 306:2022 for Vicat softening temperature. The supplier does not disclose the complete molecular architecture, additive package, or catalyst system in abbreviated public literature; the certificate of analysis remains the authoritative document for lot-specific values.
Class-level values for octene-copolymer film resins place density in the 0.918–0.922 g/cm³ band and melt mass-flow rate in the 0.8–1.0 g/10 min band. These ranges are not a certified lot-release specification for Clearflex H&T LFH 208, but they define the production window into which high-toughness film grades of this type are generally formulated. Exact grade-specific values should be read from the current Versalis technical datasheet or certificate of analysis.
| Property | Reference Method | Specimen/Condition | Reported Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 / ASTM D1505-18 | Compression moulded plaque, 23 °C | g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-20 | 190 °C, 2.16 kg | g/10 min |
| Melting peak | ISO 11357-3:2018 | Second heating at 10 °C/min | °C |
| Vicat softening | ISO 306:2022 A50 | 10 N, 50 °C/h | °C |
| Film tensile | ISO 527-3:2018 / ASTM D882-18 | 25 µm film, 500 mm/min | MPa, % |
| Dart impact | ASTM D1709-22 Method A | 25 µm film | g |
| Elmendorf tear | ASTM D1922-23 | 25 µm film, MD/TD | N/mm or gf |
| Haze | ASTM D1003-21 | 25 µm film | % |
| Gloss 60° | ASTM D2457-21 | 25 µm film | Gloss units |
Because 1-butene contributes a branch of 2 carbon atoms, 1-hexene contributes 4 carbon atoms, and 1-octene contributes 6 carbon atoms, short-chain branch length is the primary structural difference between these copolymers. Longer branches disrupt polyethylene chain folding more effectively and increase the number of interlamellar tie chains after quenching. The mechanical consequence is that an octene-based grade evaluated at the same density and melt index generally shows higher dart impact by ASTM D1709-22 and higher Elmendorf tear by ASTM D1922-23 than a butene-based grade; yield stress may be slightly lower because the longer branches reduce crystalline order.
Processability also differs from C4 and C6 grades in shear heating and backpressure. On a 30:1 L/D single-screw extruder, the octene grade tends to build higher melt pressure at equivalent screw speed when the molecular weight distribution is narrow. If the grade has a broader distribution, a melt flow ratio MFR21.6/MFR2.16 in the range 14–18 typically provides sufficient shear thinning for high-output blown film. The resin is linear and lacks long-chain branching, so bubble stability is not equivalent to high-pressure low-density polyethylene; it relies on molecular weight distribution, comonomer distribution, and quench rate.
| Parameter | 1-Butene LLDPE | 1-Hexene LLDPE | 1-Octene LLDPE |
|---|---|---|---|
| Short-chain branch length | 2 carbon atoms | 4 carbon atoms | 6 carbon atoms |
| Tie-chain population in quenched film | Lower | Intermediate | Higher |
| Dart impact at 25 µm, ASTM D1709-22 | Baseline | Intermediate | Higher |
| Elmendorf tear resistance, ASTM D1922-23 | Baseline | Intermediate | Higher |
| Yield stress at equivalent density, ISO 527-3:2018 | Slightly higher | Intermediate | Slightly lower |
| Screw backpressure at equivalent melt index | Lower | Intermediate | Higher |
On a production-scale blown-film line equipped with a 45 mm barrier screw extruder at 30:1 L/D, a starting profile is 190 °C in the feed zones, 200–210 °C in the compression and metering zones, 210 °C at the adapter, and 210–215 °C at the die. A die gap of 1.6–2.0 mm is used with a blow-up ratio of 2.2:1–2.8:1; the frost line is held at 8–12 die diameters above the air ring to control optical haze and tear balance. These are class-level parameters for high-toughness octene LLDPE film extrusion and must be trimmed on the target line because die diameter, air ring design, and tower height change the quench rate.
Recycle addition of edge trim and startup film up to 20 wt% is often tolerated without pre-drying, provided pellets are stored below 60% RH and are not transferred from cold silos into a warm production hall without condensation control. Melt temperature should remain below 260 °C; extended residence time above this threshold consumes the antioxidant package and produces gel particles and off-spec odour. When transitioning from a butene LLDPE to Clearflex H&T LFH 208, purging with the new resin for 8–10 extruder volumes is recommended; otherwise die-lip deposits and interfacial haze bands can persist.
When cast stretch film is down-gauged to 12–17 µm, the resin is processed on a 75 mm T-slot die line with a die gap of 0.45–0.55 mm, chill roll temperature of 15–20 °C, and air gap of 10–20 cm. The higher tie-chain population from octene comonomer supports down-gauging without the same loss in puncture energy observed with C4 grades. Puncture resistance is evaluated by ASTM D5748-18; a higher dart impact value by ASTM D1709-22 does not automatically predict cast-film puncture energy, so both tests are used. The resin may be placed in core layers of coextruded stretch films where the skin layers provide cling and slip.
In heavy-duty sacks and agricultural silage film, Clearflex H&T LFH 208 can serve as a core or sub-skin layer in a coextruded structure with a total thickness of 80–120 µm. Tear propagation resistance is measured by ASTM D1922-23 in both machine and transverse directions after 48 h conditioning at 23 °C/50% RH. Published data for this specific product configuration is limited in abbreviated public literature; therefore, pilot-line verification on the intended film structure is required before conversion.
The bubble stability of Clearflex H&T LFH 208 in blown film is not controlled by long-chain branching, because the resin is linear; it is controlled by the combination of melt temperature, frost line height, air ring flow, and die gap. At a 2.5:1 blow-up ratio and 1.8 mm die gap, a frost line height above 12 die diameters tends to increase transverse direction tear by ASTM D1922-23 but may raise haze above 8%; a frost line below 8 die diameters can improve clarity but reduce bubble stability and increase film blocking if the antiblock package is not adjusted.
Temperature profile asymmetry should be avoided. If the die lip temperature varies by more than ±3 °C around the circumference, gauge variation and curled film edges are typical failure modes on a 200 mm air ring. Internal bubble cooling can increase output by 15–30% relative to external air ring only, but the higher quench rate shifts the dart impact value; optimum internal bubble cooling flow is established by measuring bubble pressure and frost line height.
Because the sealing response of octene-copolymer LLDPE is broader than that of high-pressure LDPE and often shifted to a lower seal initiation temperature at equivalent density, seal testing is required for converter qualification. Seal initiation is measured on a laboratory heat sealer with 0.5 s dwell time, 0.275 MPa jaw pressure, and peel speed of 300 mm/min; the temperature at which a seal strength of 2.0 N/25.4 mm is obtained is reported as seal initiation. For a nominal 0.920 g/cm³ octene film grade, this commonly falls between 100 °C and 110 °C, but the exact value for Clearflex H&T LFH 208 must be confirmed on the supplier datasheet.
Hot-tack strength is measured with a J&B hot-tack tester at 0.5 s dwell and 0.275 MPa jaw pressure; the hot-tack plateau typically extends from 110 °C to 130 °C and declines above 140 °C as the melt no longer resists peel force. Vicat softening temperature by ISO 306:2022 Method A50 is not a sealing parameter but provides a thermal resistance comparison; class-level Vicat values for 0.920 g/cm³ octene LLDPE are typically between 95 °C and 105 °C.
For food-contact applications, the resin is typically covered under Commission Regulation (EU) No 10/2011 when the final article complies with the relevant overall migration limit and specific migration limits, and under FDA 21 CFR 177.1520 for olefin polymers in the United States. The converter must verify that the grade’s lot-specific additive package, regrind content, and coextruded layer structure satisfy the applicable conditions of use. REACH Regulation (EC) No 1907/2006 requires registration of imported monomers; the polymer itself may be exempt from registration. RoHS Directive 2011/65/EU applies only to electrical and electronic equipment and does not govern bulk packaging film; however, converted film supplied into such equipment must comply with homogeneous material concentration limits for restricted substances. Storage should be in closed packaging below 60% RH and below 40 °C to avoid additive migration and pellet caking.
Agricultural silage film structures with a total thickness of 120 µm use Clearflex H&T LFH 208 as a core layer at 60–70% of the film cross-section, with polyamide or EVOH barrier skins where oxygen transmission must be reduced. Film is produced on a 65 mm three-layer blown-film line at 210 °C die temperature and a 2.0 mm die gap. Tear resistance is reported by ASTM D1922-23 after 24 h conditioning at 23 °C/50% RH; dart impact by ASTM D1709-22 Method B is typically specified for the structure because Method A underestimates failure energy for heavier films. Processing tolerances are narrower for this structure: bubble diameter variation above ±2% causes gauge nonuniformity that reduces tear resistance at the fold edges.