Versalis Clearflex H T Fgh 196 Hexene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 616924
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.919 g/cm³
    Meltflowrate 0.8 g/10 min (190°C/2.16 kg)
    Meltingpoint 124 °C
    Vicatsofteningtemperature 100 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 700 %
    Flexuralmodulus 200 MPa
    Dartdropimpact 200 g
    Elmendorftearstrengthmd 2.5 N
    Elmendorftearstrengthtd 5.0 N
    Haze 12 %
    Gloss45 80
    Coefficientoffriction 0.2
    Blocking 60 g

    As an accredited Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® H&T FGH 196 is supplied in 25 kg polyethylene bags, typically palletized and stretch-wrapped for safe handling and transport.
    Container Loading (20′ FCL) Versalis Clearflex® H&T FGH 196 Hexene Copolymer LLDPE, 20′ FCL: palletized 25 kg bags, optimized payload within container weight limits.
    Shipping Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene is supplied as free-flowing pellets in 25 kg bags or 1000 kg FIBCs, palletized and shrink-wrapped. Transport in clean, dry vehicles; avoid moisture, direct sunlight, heat, and contamination. Typically non-hazardous under normal shipping conditions.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizing agents. Keep containers tightly closed and labeled. Avoid dust generation and accumulation; prevent electrostatic discharge. Protect from moisture and contamination. Use appropriate grounding during handling/transfer. Maintain good housekeeping. Follow local regulations and the supplier’s safety data sheet.
    Shelf Life Shelf life is approximately 24 months when stored unopened in a cool, dry, ventilated place, away from direct sunlight and heat.
    Application of Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene

    Cast pallet wrap production on multi-layer cast film lines is one of the more tolerance-critical downstream conversions for Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene because the resin’s hexene comonomer distribution influences both low-strain extensional viscosity and post-quench crystallinity. On a three-layer cast line with a 90 mm main extruder and two 60 mm satellite extruders, equipped with a 30:1 L/D grooved-feed screw and a coat-hanger die with an adjustable lip gap of 0.8–1.2 mm, FGH 196 is typically incorporated at 70–90 wt% of the core layer, while the outer skin layers are let down with 5–10 wt% metallocene-catalysed LLDPE and 1–2 wt% tackifier masterbatch to maintain unwind wetting and roll stability; the polyolefin formulation falls under FDA 21 CFR 177.1520 for incidental food contact and EU Regulation 10/2011/EC where migration into foodstuffs is not intended but transfer may occur during packaged pallet handling in mixed storage. The melt is processed at 220–250°C, cast onto a chrome-plated chill roll held at 15–25°C with an air knife and edge-pinning system, avoiding elevated frost-line drift; downstream products include machine rolls of 500 mm width, hand pallet wrap rolls at 400–450 mm width, and pre-stretched rolls for low-force manual application.

    Does Hexene Comonomer Uniformity Justify Replacing Butene LLDPE in Frozen-Food Blown Film?

    In frozen-food pillow bags and side-seal pouches, the substitution of butene-copolymer LLDPE with a hexene-copolymer LLDPE such as FGH 196 is justified only when the bubble can sustain stalk-height stability at the low melt temperatures required to minimize oxidation in the seal layer. Blown film lines using a 3-layer die with die gap 1.6–2.4 mm, blow-up ratio 2.5–3.5, and a dual-lip air ring are generally operated with FGH 196 at 40–60 wt% of the total structure, most of it placed in the core layer to raise puncture resistance, while the sealant layer carries 20–30 wt% FGH 196 blended with a lower-viscosity plastomer to maintain a seal initiation temperature below 105°C on form-fill-seal lines. The frozen-food contact compliance chain is anchored to EU Regulation 10/2011/EC, with specific migration limits assessed according to EN 1186-1 and EN 13130-1, and to FDA 21 CFR 177.1520 for olefin polymers when used as the food-contact layer; cold-temperature impact is measured by ASTM D1709 dart drop, with typical structures exceeding 150 g at -20°C when a hexene-rich core is used. The conversion process demands controlled air-ring cooling and internal bubble stabilisation, as excessive frost-line height above 10–12 die diameters creates orientation imbalance that degrades Elmendorf tear resistance in the transverse direction under ASTM D1922. Terminal products include printed frozen vegetable pillow bags, seafood side-seal pouches, and multi-layer lidding films where seal strength under ASTM F88 remains above 2.5 N/15 mm after exposure to -25°C storage.

    Heavy-Duty Sack Coextrusion Layer Ratios and Bubble Cooling Limits

    Heavy-duty sacks destined for granular chemicals and construction powders are coextruded on high-output blown film lines where the hexene-copolymer LLDPE is introduced into the core layer at 60–80 wt% of total feed, with 15–25 wt% butene-copolymer LLDPE or clean recycled trim in the outer layers and up to 10–20 wt% of in-line edge trim regrind in the core, so total FGH 196 concentration can decline to 50–70 wt% depending on regrind draw. The three-layer die is typically operated with a blow-up ratio of 2.0–3.0, a die gap of 1.8–2.5 mm, and a melt temperature of 190–220°C; internal bubble cooling is set to hold frost-line height at 6–8 die diameters, as excessive stalk cooling creates machine-direction creep and sack elongation under fill-head impact. Compliance for transport packaging carrying dangerous goods may require UN proof testing under the IMO IMDG Code, but at minimum the converted sack is subjected to drop resistance according to ISO 7965-2 and tear resistance according to ISO 6383-2, while the resin feed is specified under ASTM D4976 and ISO 1872-1. The terminal formats include 25 kg chemical sacks, 50 kg construction-material sacks, and dimensionally stabilised liners for FIBCs; a key bottleneck on production lines is batch-to-batch charge shift when the middle-layer ring dam is set below 15 mm, producing visible gauge bands at 0.02 mm thickness variation.

    Extrusion coating of paperboard for aseptic liquid packaging imposes a different set of rheological requirements on hexene-copolymer LLDPE: low neck-in, acceptable drawdown at high line speed, and adequate adhesion to the primer or oxidised paperboard surface. In a tandem extrusion coating line with 90 mm 30:1 L/D extruder and flat die gap 0.5–0.8 mm, FGH 196 is most often let down at 15–30 wt% into an autoclave-LDPE carrier to balance melt strength and sealability, with the remainder comprising LDPE of 7.5–9.0 g/10 min melt flow index under ISO 1133-1; the blend may include 0.5–1.0 wt% processing aid in the form of polymer-based fluoroelastomer masterbatch only where die lip build-up is observed. The melt temperature is held at 280–300°C and the air gap between die exit and pressure roll nip is set to 150–250 mm because shorter gaps increase oxidation and pinholes in the coating, while longer gaps reduce adhesion and increase edge weave. Compliance for the finished laminate follows EU Regulation 10/2011/EC for plastic materials in contact with food and FDA 21 CFR 177.1520, with overall migration testing under EN 1186-3 and seal integrity under ASTM F2029; published migration data for this specific grade in aseptic paperboard coatings is limited, so end-article compliance is demonstrated by total migration testing rather than by resin-grade certification alone. The final products include gable-top UHT milk cartons, drink cup blanks, and paper-based pouches for dry powders.

    When Hexene LLDPE Is Dry-Blended with Metallocene LLDPE for Silage Wrap, Property Cliff-Edges Emerge at High Pre-Stretch Ratios

    Agricultural silage wrap conversion on cast stretch-film lines creates a well-documented property cliff-edge at pre-stretch ratios above 70%, where differences in hexene branch distribution between FGH 196 and metallocene LLDPE become visible as puncture-count increases on the wrapped bale after 12 months of UV exposure. The formulation typically combines FGH 196 at 60–85 wt% with a metallocene-catalysed LLDPE at 10–25 wt% and a UV-stabilised tackifier masterbatch at 1–3 wt%, with the exact ratio adjusted to keep machine-direction elongation under ASTM D5459 above 400% after pre-stretching. Cast line configuration includes a 5-layer die gap of 0.8–1.0 mm, a chrome chill roll at 15–20°C, and edge trim regrind returning to the core layer at not more than 10 wt% to avoid gel defects. Industry compliance for bale wrap is assessed under EN 13655 for stretch-film wrapping of baled organic material, with UV ageing according to ASTM D4329 cycle A and tear propagation according to ISO 6383-2; at the farm level, the final products are 750 mm wide rolls for round bales, 500 mm hand rolls for square bales, and pre-stretched silage cover film. Operational boundaries include avoidance of processing temperatures above 250°C when high-tack masterbatch is present, because premature oxidation of the tackifier produces carbonyl species that migrate to the film surface and reduce wetting adhesion.

    Thermal Degradation and Carbon Black Dispersion in Geomembrane Sheet Extrusion

    Flat-die extrusion of LLDPE geomembranes containing carbon black is a thermal degradation-sensitive operation because the combination of long residence time, high melt pressure, and the catalytic surface effect of furnace carbon black accelerates chain scission if the melt temperature excursions above 230°C are not controlled. FGH 196 is incorporated at 50–70 wt% of the polymer phase, with a butene LLDPE or medium-density PE at 25–45 wt% and carbon black masterbatch at 2–3 wt% to achieve a minimum carbon black dispersion rating of 3 under ISO 18553; antioxidant packages are added at 0.1–0.3 wt% based on total formulation depending on the projected service life. The sheet line uses a 120 mm single-screw extruder with 33:1 L/D ratio, gear pump-controlled melt delivery, a flat sheet die of 1800–2500 mm width, and a vertical three-roll calender stack held at 60–80°C, producing sheet thickness from 1.0 mm to 2.0 mm. Compliance for the finished geomembrane is anchored to GRI GM17 for LLDPE smooth geomembranes, with tensile yield and break under ASTM D6693, tear under ASTM D1004, and oxidative induction time under ASTM D5885 at 200°C; terminal products include smooth LLDPE geomembrane panels for landfill caps, pond liners, and secondary containment basins. Operational incompatibility arises when low-viscosity polyethylene waxes are added above 1 wt% as processing aids, because they extract the hindered phenol antioxidant to the die lip and reduce oxidative induction time by more than 20%.

    Free Quote

    Competitive Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® H&T FGH 196 is supplied as a pelletized 1-hexene copolymer linear low density polyethylene for blown film conversion. In the comonomer sequence, 1-hexene introduces butyl branches of four carbon atoms along the ethylene backbone, whereas 1-butene introduces ethyl branches of two carbon atoms. The longer branch modifies the frequency and spatial distribution of tie molecules between lamellae; this is the primary structural variable that distinguishes FGH 196 from conventional butene-based linear low density polyethylene at the same nominal density. The producer’s designation FGH 196 and the H&T series position the material in the heavy-duty packaging segment, where puncture, tear, and seal integrity measured by ISO 7765-1, ISO 6383-2, and ASTM F88 are controlled by film orientation and comonomer distribution.

    Because no public lot-specific certificate of analysis for this exact grade was available at the time of drafting, the numerical values that follow are restricted to the general class of 1-hexene LLDPE extrusion resins and are not a substitute for the producer’s datasheet. Acceptance testing should measure density, melt mass-flow rate, additive type, and film properties on the same monolayer or coextruded line used for production. The distinction between C4, C6, and C8 copolymers is a comonomer architectural distinction, not a trade-name distinction, and must be confirmed by comonomer content analysis and Fourier transform infrared spectroscopy or thermal fractionation when reverse-engineering a competitor structure.

    How Does Extending the Short-Chain Branch from Ethyl to Butyl Alter Film Failure Mechanics?

    Blown film failure under dart drop and Elmendorf tear is governed by the number and orientation of tie chains that bridge adjacent crystalline lamellae. In a C4-LLDPE, the ethyl branch is sterically compact and may be partially incorporated in the crystalline phase; in a hexene copolymer, the butyl branch is excluded from the crystal lattice more completely. This raises the probability of interlamellar tie-chain formation at equivalent short-chain branching density. The result is not a uniform improvement in every property: machine-direction tear and transverse-direction tear respond differently to orientation and may diverge as a function of blow-up ratio. These quantities are measured on film specimens according to ISO 6383-2 and ASTM D1709.

    Measurements by differential scanning calorimetry according to ISO 11357-3 typically show a lower and broader melting endotherm for a 1-hexene LLDPE than for a 1-butene LLDPE of equivalent density. This thermal response moves the seal initiation temperature downward and may expand the heat-seal plateau range. Seal initiation is measured by ASTM F88 or ASTM F1921 on a temperature-graded sealing machine. In film evaluation, the comparative difference should be determined on the same blown film line with identical die gap, output rate, and frost line height because these processing variables alter crystalline orientation and can mask the intrinsic resin effect.

    Slow crack growth in notched specimens is measured by ASTM D1693 under environmental stress cracking conditions. A C6-LLDPE typically outperforms a C4-LLDPE of equal density and melt index because the longer butyl branches create more effective stress transfer between lamellae. However, the test is time-consuming and lot-dependent; the FGH 196 datasheet should state whether ESCR is guaranteed or reported for information.

    For a product supplied under the Clearflex H&T FGH 196 designation, lot acceptance and incoming inspection normally include density determination by ISO 1183-1, melt mass-flow rate by ISO 1133-1:2022 at 190 °C and 2.16 kg, and pellet additive analysis. Film evaluations are conducted on cast or blown film at constant gauge, typically 25 µm or 50 µm, with tensile properties by ISO 527-3, Elmendorf tear by ISO 6383-2, dart impact by ASTM D1709 Method A or ISO 7765-1, haze by ASTM D1003, and coefficient of friction by ASTM D1894. The producer’s datasheet should be consulted for the exact pass/fail limits; the general class of 1-hexene LLDPE heavy-gauge film resins is commonly controlled within a density window of 0.918 g/cm³ to 0.922 g/cm³ and a melt flow rate of 0.8 g/10 min to 1.2 g/10 min at 190 °C/2.16 kg, but these are not grade-specific values.

    Controlled property or requirementStandard designationTest condition / relevance
    DensityISO 1183-1Immersion method; controls stiffness, barrier and seal initiation
    Melt mass-flow rateISO 1133-1:2022190 °C / 2.16 kg; classifier for extrusion-grade viscosity
    Tensile propertiesISO 527-3Film specimens; yield strength, elongation at break, modulus
    Elmendorf tearISO 6383-2MD/TD tear propagation on film
    Dart impactASTM D1709 Method AFalling dart failure energy on film
    HazeASTM D1003Optical clarity of film
    Coefficient of frictionASTM D1894Surface slip characteristics
    US food contactFDA 21 CFR 177.1520Olefin polymer compliance for food packaging
    EU food contactRegulation (EU) No 10/2011Overall and specific migration limits
    REACHRegulation (EC) No 1907/2006SVHC declaration and Annex XVII restrictions
    RoHSDirective 2011/65/EUHeavy metal restrictions for non-food enclosures

    Internal quality assurance for the product class relies on film performance rather than pellet rheology alone. A 45 mm laboratory blown film line operating at 20 kg/h output and 2.5:1 BUR is used to monitor lot-to-lot drift. Dart impact values measured by ASTM D1709 Method A should remain within ±8% of the moving average for the same gauge and frost line; deviations larger than this often indicate comonomer distribution drift or additive inhomogeneity. Pellet surface oxidation can be detected by infrared absorption at 1715 cm⁻¹, with absorbance above 0.05 correlating with film gel counts above the screen-pack retention limit.

    Extrusion-Grade Rheology and Bubble Stability in Low-Pressure Air Ring Systems

    Hexene LLDPE resins with melt flow rates below 2.0 g/10 min are processed on grooved-feed extruders with barrier screws and L/D ratios between 24:1 and 30:1. The low-pressure air ring and internal bubble cooling combination stabilizes the bubble at blow-up ratios from 2.0:1 to 3.0:1; die gaps are typically held between 1.6 mm and 2.4 mm. Melt temperature at the die is maintained at 200 °C to 230 °C for monolayer film; coextrusion with HDPE or metallocene LLDPE skins may require a 10–20 °C reduction in the skin layer melt temperature to control viscosity ratio.

    Rheological measurements at 190 °C over shear rates from 100 s⁻¹ to 1000 s⁻¹ are used to evaluate shear thinning and melt fracture. In comparison with a C4-LLDPE of identical melt index, a hexene copolymer may exhibit slightly lower extruder head pressure and reduced die lip deposit formation because the longer branch reduces the concentration of low-molecular-weight branched species that migrate to the die surface. This effect is observed only when temperature profiles are matched; excessive melt temperature above 250 °C leads to oxidative chain scission and gel formation, particularly in high-shear regions of the die. On a 65 mm grooved-barrel extruder fitted with a 200 mm die, screen packs of 60/80/100 mesh are commonly used to trap gels larger than 250 µm; melt pressure at the screen pack should remain below 350 bar. Pressure spikes above 380 bar indicate gel accumulation or filter blockage and require feed section cooling or screen replacement.

    On a 65 mm grooved-barrel extruder fitted with a 200 mm die and 1.8 mm die gap, specific energy input of 0.18 kWh/kg to 0.22 kWh/kg is typical for LLDPE blown film at 180 kg/h. Melt temperature measured at the die by an immersion thermocouple should not exceed 250 °C; higher values are often caused by excessive screen pack blinding or incorrect barrel zone ratios. The die gap is selected relative to the frost line height to avoid melt extensional instability. For FGH 196 in the melt-flow band described, die gap to final gauge ratio is typically above 30:1; lower draw ratios produce smoother films but reduce machine-direction tensile modulus measured by ISO 527-3.

    Predrying of FGH 196 is generally not required because the resin is not susceptible to hydrolytic degradation. However, if pellets have been stored at low temperature and brought into a high-humidity environment above 60% RH, surface condensation can generate melt pinholes and silver streaks. In such cases, hopper drying at 70 °C for 4 h is applied before extrusion. The resin should not be dry-blended with unsaturated oils, amine-based antistatic additives, or oxidative post-consumer recyclate without compatibility testing; such additives can alter the oxidation induction time measured by ISO 11357-6 and produce surface exudation on film.

    When FGH 196 Replaces a C4-LLDPE in Form-Fill-Seal and Heavy-Duty Sack Lines

    In vertical form-fill-seal packaging, the lower seal initiation temperature of a 1-hexene LLDPE permits shorter dwell times and lower sealing bar temperatures. Hot-tack strength is measured by ASTM F1921, and seal strength by ASTM F88. A converter replacing a C4-LLDPE with FGH 196 should first recertify the seal window at the same film gauge and contaminant level; the seal curve may shift by several degrees, but published data for this specific configuration is limited. The practical benefit is most evident on lines with seal bar temperature variation greater than ±5 °C, because a broader seal plateau reduces the incidence of weak seals at the cooler end of the bar.

    Heavy-duty sack and bag applications require a balance of dart impact, machine-direction tear, and edge fold resistance. Dart impact measured to ISO 7765-1 and Elmendorf tear measured to ISO 6383-2 should be compared at the same film gauge and blow-up ratio; increasing blow-up ratio from 2.0:1 to 3.0:1 improves transverse-direction tear at the expense of machine-direction tear. The FGH 196 designation is therefore applied where the converter can compensate for LLDPE anisotropic tear by adjusting die gap and frost line; without such adjustments, the resin architecture alone does not guarantee a balanced film.

    Stretch hood and agricultural silage film impose different requirements. Stretch hood film demands puncture resistance at pallet corners and high biaxial extensibility. Puncture resistance is assessed by ASTM D5748 or a slow puncture instrument at 100 mm/min; the butyl branch content of FGH 196 contributes to a more ductile puncture response than a C4-LLDPE of equivalent density, but the effect is not separable from film layering and gauge profile. Agricultural silage films use the same resin in coextruded three-layer structures with HDPE or EVA. The central layer often consists of recycled trim; the virgin skin layers use FGH 196 to maintain dart impact after thermal ageing. Ageing tests under ISO 4892-2 or ASTM G155 with UV exposure should be used to verify resistance when carbon black masterbatch is added; the grade itself does not contain UV stabilizers unless the producer declares the additive package.

    Compared with autoclave LDPE, FGH 196 has a linear backbone with no long-chain branching. This linearity reduces shear thinning and increases melt extension viscosity at high draw; it also reduces the maximum stable draw ratio on some cast film lines, so the grade is not a drop-in replacement for LDPE in all tubular applications. Processability comparisons should be based on melt strength measured by ISO 16790 or an extensional rheometer. Relative to an octene LLDPE, a hexene copolymer may require a lower comonomer molar fraction to reach the same density, providing a stiffness/density advantage but sometimes less dart impact. The choice between C6 and C8 is not a simple hierarchy; octene LLDPE with the same density and melt index can show higher hot-tack and lower seal initiation, but the FGH 196 class is often selected for heavy-duty sacks where puncture and retained tear after ageing are more important than ultimate seal speed.

    Non-film conversion processes are outside the stated application range for this grade. Rotational molding and injection molding require higher melt flow or specific narrow molecular weight distributions; FGH 196 should not be used in those operations without producer validation.

    Top