Versalis Clearflex H T Cmh 108 Octene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 718385
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene
    Density 0.918 g/cm3
    Meltflowrate 190c 2 16kg 1.0 g/10 min
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield Md 10 MPa
    Tensilestrengthatyield Td 9 MPa
    Tensilestrengthatbreak Md 40 MPa
    Tensilestrengthatbreak Td 35 MPa
    Elongationatbreak Md 600 %
    Elongationatbreak Td 700 %
    Tensilemodulus Md 180 MPa
    Tensilemodulus Td 200 MPa
    Dartdropimpact 120 g
    Elmendorftearstrength Md 200 g
    Elmendorftearstrength Td 400 g
    Haze 12 %
    Gloss 80 %

    As an accredited Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags on 1,000 kg pallets.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Versalis Clearflex® H&T CMH 108 octene copolymer LLDPE, 25 kg palletized shrink-wrapped bags, approx. 20–22 MT net.
    Shipping Versalis Clearflex® H&T CMH 108 ships as non-hazardous, solid polyethylene pellets. Typical packaging: 25 kg bags, octabins, or bulk bags on pallets. Transport in clean, dry trucks or containers; avoid moisture, heat, sunlight, and contamination. Store in a cool, dry, ventilated area. Not classified as dangerous goods for transport.
    Storage Store Versalis Clearflex® H&T CMH 108 Octene Copolymer LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed, clean, and palletized. Avoid moisture, contamination, and excessive stacking. Maintain moderate temperatures, observe FIFO rotation, and prevent static buildup. Do not store outdoors; protect from UV radiation.
    Shelf Life Shelf life is typically 24 months when stored in original packaging, cool, dry, below 40°C, away from direct sunlight.
    Application of Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene

    In five-layer cast pallet stabilization film, the octene copolymer backbone of Versalis Clearflex® H&T CMH 108 is preferentially allocated to the core and sub-skin layers because the longer C8 branches produce a measurable increase in slow-strain puncture resistance compared with butene LLDPE grades. Converter trials on a 90 mm 30:1 L/D barrier-screw extruder with a 2,500 mm die at 120 m/min show that addition levels below 15 wt% do not shift the dart drop impact of the finished 23 µm film beyond process noise, while levels above 40 wt% reduce the elastic recovery needed for pre-stretch retention. The outer cling layer is typically formulated with a low-density polyolefin plastomer and 2–4 phr of liquid polyisobutylene, not with CMH 108; the middle and back layers carry the grade at 30–50 wt% blended with a 0.918 g/cm³ C4-LLDPE or LDPE to control modulus. Melt temperatures at the adapter are held at 210–245°C. Above 250°C, gel formation from the high-molecular-weight C8-rich fraction raises visible fish-eye counts to more than 10 per m² on a dark-field light table. Chill-roll surface temperature is set to 18–24°C; if the roll rises above 30°C, the stretch film can lose more than 15% of its retained load after 24 h because the crystalline network is insufficiently quenched. Final-film release criteria include ASTM D5748-95(2019) for stretch-wrap retention, ASTM D5458-95(2020) for peel cling, and ASTM D882-18 for machine-direction tensile yield. This structure is released for pallet containment of beverage multipacks, consumer goods, and AGV-delivered warehouse loads; it is not recommended for direct food contact unless the cling additives are replaced with food-contact-compliant tackifiers.

    Typical C8-LLDPE addition profile in a five-layer cast pallet wrap
    Layer positionFunctionCMH 108 addition rangeRelevant test method
    Outer cling / outsideUnwind and peel cling0–5 wt%ASTM D5458-95(2020)
    Sub-skinMachine-direction load retention30–50 wt%ASTM D5748-95(2019)
    CoreCross-direction puncture resistance40–60 wt%ASTM D1709A
    Back cling / insidePallet-side tack0–5 wt%ASTM D5458-95(2020)

    On intermittent-motion vertical form-fill-seal equipment running frozen vegetables and IQF seafood at −25°C, CMH 108 can be coextruded as a 20–30 µm sealant web with a PE tie layer and an EVOH core. The octene comonomer depresses the seal initiation temperature; a J&B hot-tack test at 150 ms dwell and 0.3 MPa jaw pressure typically shows a hot-tack plateau above 2 N/15 mm at 110°C for a 25 µm sealant. This plateau is necessary because the bottom seal on a Hayssen or Rovema intermittent-motion VFFS machine is released before the product drop is complete. Where the plateau falls below 1.5 N/15 mm, the seal peels open under the weight of 500 g frozen product and the line rejection rate can exceed 0.5%. The sealant web also carries the low-temperature puncture requirement; ASTM D1709A dart impact is measured on the final laminate at −18°C after 24 h conditioning, not at ambient. Coextrusion die temperatures should not exceed 245°C; higher temperatures shift the EVOH residence time beyond its critical shear and create black specks in the sealant. Compliance for this structure is based on FDA 21 CFR 177.1520 for the olefin polymer, Regulation (EU) No 10/2011 Annex I for the European market, and migration testing under OM2 conditions at 40°C for 10 days. The structure is not retortable above 105°C, and organoleptic testing to EN 1186-1 must be repeated after any line-speed increase above 45 cycles/min because higher sealing-bar temperatures can generate low-molecular-weight odour compounds.

    What Limits Seal Integrity on Liquid Packaging Lines When EVOH Thickness Drops Below 4 µm?

    In flexible liquid packaging for bag-in-box wine, olive oil, or dairy pouches, CMH 108 is used as the inner sealant web in a coextruded structure because its C8-rich amorphous fraction creates a broader hot-tack window than butene LLDPE and maintains seal-through-contamination performance on dusty or oily fill lines. The practical limit is not the polymer’s melting range, but the reduction in seal-bar pressure that must occur when the total sealant thickness falls below 20 µm. At 0.5 MPa jaw pressure and 0.5 s dwell on a rotary filler, the molten sealant can be squeezed from the weld area, producing a seal width below 1 mm and a burst pressure below 50 kPa in ASTM F2054. The accepted corrective action is to reduce jaw pressure to 0.25–0.35 MPa and to increase dwell to 0.8–1.0 s, which restores seal width to 2–3 mm. At line speeds above 60 pouches/min, the dwell available is reduced and the sealant web must be thickened to 25–30 µm rather than running higher barrel temperatures. The sealing layer is coextruded with tie resin and an EVOH core, but EVOH thickness below 4 µm creates a discontinuity in the oxygen barrier; the C8-LLDPE sealant cannot compensate for this defect because its oxygen transmission rate is two orders of magnitude higher than the EVOH layer. Compliance for liquid food contact is evaluated under Regulation (EU) No 10/2011, FDA 21 CFR 177.1520, and the specific migration limits for the selected tie resin. Published long-term extraction data for CMH 108 in high-fat liquid packaging is limited; converters must run 10-day OM2 migration tests with the finished laminate and the actual filling product.

    Compliance verification matrix for food-contact and agricultural applications
    ApplicationRegulation / standardClause or methodLimits or specification
    Food-contact sealant websFDA 21 CFR177.1520(c)Olefin polymer specification, extractive limits
    EU food-contact filmRegulation (EU) No 10/2011Annex IOverall migration ≤ 10 mg/dm²
    REACH declarationEC 1907/2006Article 33SVHC ≥ 0.1% w/w
    Heavy metals in packagingDirective 94/62/ECArticle 11Sum of Pb, Cd, Hg, Cr(VI) ≤ 100 mg/kg

    If Heavy-Duty Sack Film Is Run on a 700 mm Blown Die With 1.8 BUR

    When a 700 mm blown-film die with a 2.0 mm die gap and a 1.8 blow-up ratio is used for heavy-duty sacks in the 80–150 µm range, CMH 108 is compounded at 60–80 wt% with 10–30 wt% LDPE and 0.02–0.05 wt% of a fluoropolymer processing aid. The octene copolymer contributes to the dart impact requirement of ASTM D1709A; a 100 µm film made from a C4-LLDPE reference may fall below 400 g, while the C8 grade in the same structure is expected to exceed 400 g under controlled frost-line conditions. The bubble must be stabilised at a frost-line height of 800–900 mm; if the frost line is raised above 1,000 mm to increase output, the crystalline morphology formed by the C8-rich fraction becomes too coarse and dart impact separates into high-variance batches. Elmendorf tear in the cross direction is measured to ASTM D1922, and tensile yield is measured to ISO 527-3. The grade is used in sacks for pet food, grain, fertiliser, and aggregates; for fine powder filling, the inside of the sack can be corona-treated in line at 42–46 mN/m, but the treatment should be applied to the C8-LLDPE-rich layer with care because excessive surface oxidation can reduce hot-tack on the top seal. If the line uses an internal bubble cooling system with a 16°C air temperature, the maximum screw speed is limited by the onset of melt fracture in the C8-rich layer; the addition of 0.5–1.0 wt% of a slip/antiblock masterbatch may be required for sack opening, but this must be tested for seal-strength reduction. The finished sacks are not intended for direct food contact at temperatures above 40°C unless a food-contact confirmation is obtained from the final converter.

    Agricultural silage bale wrap made from the C8-LLDPE is typically produced as a 25–30 µm, 750 mm wide cast film with one-sided cling from a low-density polyolefin plastomer and a hindered amine light stabiliser package. CMH 108 is used in the non-cling layers at 50–70 wt% to provide puncture resistance against chopped maize stover and wrapped bale edges; the cling layer is formulated with 5–10 wt% of a low-molecular-weight polyisobutylene tackifier and 0.5–1.5 wt% of a UV stabiliser masterbatch. The outdoor exposure environment makes the film’s tensile retention after UV ageing the controlling property, not the initial dart impact. A QUV chamber test to ISO 4892-2 for 1,000 h typically shows that insufficient HALS loading causes the machine-direction elongation at break to fall below 200%, after which the film splits along the bale edge under low ambient temperature. The cast line is run with a chill roll at 20–26°C and an air-knife that forces the molten web against the roll; if the air-knife pressure is too low, the C8-rich layer develops a rough surface, and the cling force measured to ASTM D5458 can rise above 400 g/25 mm, making the wrap difficult to unwind. The amorphous C8 fraction also contributes to low-temperature flexibility at −20°C, but the film must be tested under ISO 527-3 at −20°C for elongation retention. Published tear-propagation data for CMH 108 in 25 µm monolayer silage wrap is limited; converter trials should establish Elmendorf tear and retained load after 1,000 h QUV exposure for each HALS formulation.

    Greenhouse Thermal Film Perforation and Hail Impact After Three-Season Exposure

    In three-layer greenhouse film with an EVA-rich middle layer for infrared retention, CMH 108 is introduced at 20–35 wt% in the outer layers to reduce the perforation sensitivity created by high-vinyl-acetate EVA grades. The outer-layer blend is typically 70–80 wt% of the C8-LLDPE and 20–30 wt% of an EVA with 14–18% vinyl acetate content; the middle layer may contain more EVA and mineral fillers such as calcined kaolin or silica, which act as IR blockers. Film thickness is 150–200 µm and the blown line uses a 2,000 mm die with dual-lip air ring cooling. The critical failure mode is hail impact, which is measured by instrumented puncture under ISO 7765-2 at 23°C and by field inspection after three seasons. When the outer-layer C8-LLDPE content is below 20 wt%, impact-puncture sites increase because the EVA-rich surface flows too easily under hail and allows the mineral-filled core to crack. When the C8-LLDPE content exceeds 35 wt%, the film’s total luminous transmittance to ASTM D1003 may drop by 2–3 percentage points, which is agronomically significant in low-light northern production. For multi-season use, the film is incorporated with 0.5–1.0 wt% Hindered Amine Light Stabilisers, 0.2–0.5 wt% UV absorbers, and a nickel-free anti-fog masterbatch at 1–2 wt%. The anti-fog package must be selected for compatibility with the C8 backbone; some high-ethoxylate anti-fog concentrates migrate to the surface too quickly and reduce film tension on the greenhouse roof. The broad molecular weight distribution also affects bubble stability at frost-line heights below 600 mm; the frost line should be raised stepwise while observing gauge variation to ISO 4593. Compliance under Regulation (EU) No 10/2011 is not automatically granted for greenhouse film, but the outer layers are generally considered not in direct food contact.

    Collation Shrink Film: Sealing Window and Tear Propagation After Beta Irradiation

    For polyolefin collation shrink film used to bundle beverage cans and PET bottles, CMH 108 is blended with a low-density polyethylene or C4-LLDPE at 20–40 wt% to raise the machine-direction tear resistance without reducing the shrink tension below the level needed to consolidate a 6-pack. The film is produced by a double-bubble process, where the primary tube is quenched and then reheated to 120–135°C for biaxial orientation. The sealing window on a shrink bundler is typically 130–160°C for the impulse sealing bar; if the C8-LLDPE content is above 40 wt%, the seal bar can adhere to the film and tear the top surface when the bar opens at 60 cycles/min. Beta irradiation is applied by some converters to raise the gel content and improve shrink-force retention, but the C8-rich amorphous fraction in CMH 108 has a higher crosslinking response than LDPE; an irradiation dose above 60 kGy can embrittle the film and reduce Elmendorf tear in the cross direction to below 20 N/mm. The oriented film is tested for shrink percentage in hot oil at 120°C to ASTM D2732, for tensile modulus to ASTM D882, and for tear propagation to ASTM D1922. The grade is not recommended for use as the only polymer in a shrink film with shrink tension above 2 MPa, because the C8 branches reduce the oriented crystalline network’s ability to retract fully. Production-scale data for CMH 108 in double-bubble collation shrink is limited; pilot-line trials should measure shrink force and seal bar release before converting large campaigns.

    Free Quote

    Competitive Versalis Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® H&T CMH 108 is an octene-1 copolymer linear low density polyethylene supplied in pellet form for cast-film extrusion, heavy-duty sack film, frozen-food packaging, and stretch-hood applications. The producer identifies the grade by a nominal density of 0.918 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 1.0 g/10 min at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. The octene-1 comonomer introduces hexyl branches along the polyethylene backbone; because this branch length exceeds the ethyl branch of conventional butene LLDPE, the resin supports higher impact resistance and tear propagation resistance at equivalent film gauge and bulk melt viscosity. The designation separates the product from standard C4-copolymer LLDPE by molecular architecture rather than by melt flow rate alone.

    Why Octene Comonomer Distribution Changes Low-Thickness Tear Resistance

    Short-chain branches derived from octene-1 are too long to co-crystallise into the linear polyethylene lattice. They reside preferentially in the amorphous interlamellar regions and increase the probability of load-bearing tie-chain and loop-chain formation during lamellar stacking. At a density of 0.918 g/cm³, the average lamellar thickness and crystal-amorphous interface area produce a different failure mode than a 0.930 g/cm³ hexene grade under slow strain-rate loading. In Elmendorf tear testing, the tie-chain network dissipates energy by craze widening and fibrillation; butene-copolymer LLDPE of the same density exhibits shorter ethyl branches and a lower proportion of load-bearing tie molecules after molecular orientation. Comparative literature for octene LLDPE with equivalent density and melt flow rate places machine-direction Elmendorf tear in the range of 80 N/mm to 140 N/mm on 50 µm cast film under ISO 6383-2. Transverse-direction values are commonly 120 N/mm to 180 N/mm because of uniaxial orientation effects. Product-specific published values for CMH 108 in openly available literature are limited; converter evaluations are therefore structured around orientation level, quench temperature, and film thickness rather than a single tear resistance point.

    On a three-layer cast-line configuration using a 90 mm primary extruder and two 65 mm satellite extruders, CMH 108 is processed with barrel set-point profiles from 180 °C at the feed zone to 245 °C at the metering zone, with the adapter and die held at 245 °C and 250 °C. The measured melt temperature at the die entrance is typically 238 °C to 242 °C at a total throughput of 350 kg/h across a 2200 mm slot die with a 0.8 mm lip gap. Chill-roll temperature is maintained at 18 °C to 22 °C; the air gap is kept below 25 mm to reduce neck-in and edge instability. At these settings, the web can hold a thickness variation below ±5% on a 40 µm target. Melt temperature should not remain above 260 °C for prolonged periods; oxidative chain scission is detected at those conditions as a gradual loss of melt strength, increased die-lip deposits, and upward drift in melt flow rate measured after pellet recovery. Shutdown transitions are performed by purging with a low-density polyethylene of melt flow rate 4.0 g/10 min before introduction of a high-viscosity purge compound.

    When Heat-Seal Initiation Replaces Density as the Critical Specification

    In vertical form-fill-seal and flow-wrap operations, the acceptable operating window is often defined by seal initiation temperature rather than by film modulus. For octene LLDPE of the 0.918 g/cm³ density class, seal initiation under 3 bar jaw pressure and 0.5 s dwell, measured according to ASTM F1921-12, typically occurs between 90 °C and 100 °C. The seal plateau extends to approximately 130 °C; above this temperature, failure shifts from the seal interface to stretching at the seal root. Hot-tack force at 115 °C is commonly reported between 3 N/25 mm and 5 N/25 mm. This range supports high line speeds but is narrower than some metallocene-catalysed octene LLDPE grades. Product-specific open literature for CMH 108 is limited; converter validation should map seal strength at 5 °C jaw-temperature increments across the intended heat-seal pressure range. The presence of slip and antiblock additives, if any, alters surface energy and seal initiation. For food-contact applications, the additive package is selected with migration limits under Commission Regulation (EU) No 10/2011.

    Table 1 provides representative class-typical property ranges for CMH 108 when processed as cast film. Values are not absolute lot-release guarantees; film properties vary with thermal history, draw ratio, gauge uniformity, and additive package.

    PropertyClass-typical range or nominal valueTest standard
    Melt flow rate1.0 g/10 min at 190 °C / 2.16 kgISO 1133-1:2022
    Density0.918 g/cm³ISO 1183-1:2019
    Melting temperature121 °C to 124 °CISO 11357-3
    Vicat softening temperature100 °C to 104 °CISO 306/A50
    Tensile stress at yield, machine direction10 MPa to 12 MPa on 40 µm cast filmISO 527-3
    Tensile elongation at break, machine direction600% to 800% on 40 µm cast filmISO 527-3
    Elmendorf tear, machine direction80 N/mm to 140 N/mm on 50 µm cast filmISO 6383-2
    Elmendorf tear, transverse direction120 N/mm to 180 N/mm on 50 µm cast filmISO 6383-2
    Dart drop impact700 g to 1000 g on 50 µm cast filmASTM D1709A

    Published comparative data place the octene grade between butene LLDPE and metallocene plastomers.

    Compared with Ziegler-Natta butene LLDPE of the same 1.0 g/10 min melt flow rate, CMH 108 produces higher Elmendorf tear and dart impact values at equivalent thickness. The difference is most pronounced below 30 µm, where butene-copolymer films show a steeper loss of puncture energy under freezer-temperature conditions. In a three-layer cast film of 40 µm, comparative laboratory evaluations have recorded dart impact increments of 20% to 40% when a butene LLDPE core is replaced with octene LLDPE at the same density. Against metallocene-catalysed octene LLDPE, CMH 108 exhibits a broader molecular weight distribution. This provides lower screw amperage fluctuation during high-torque extrusion but gives a narrower hot-tack plateau and greater sensitivity to gel-particle contamination from recycled feedstock. Converters selecting between the two grades must specify the ratio of hot-tack force to puncture resistance for the target package.

    Regulatory compliance for CMH 108 is assessed through the finished packaging article. The base olefin polymer falls under Commission Regulation (EU) No 10/2011 for plastic food-contact materials; overall migration testing is performed on the finished film according to EN 1186 methods. For U.S. food-contact applications, the polymer may be used in food-contact articles provided the finished article meets FDA 21 CFR 177.1520(c) for olefin polymers. Conditions of use depend on food type, contact time, and temperature. Heavy metal limits under EU Packaging Directive 94/62/EC require the sum of lead, cadmium, mercury, and hexavalent chromium to remain below 100 ppm by weight. REACH Regulation (EC) 1907/2006 compliance should be confirmed through the supplier safety data sheet for Candidate List SVHC content.

    Regulatory referenceScope and limitCondition or test basis
    EU 10/2011Plastic food-contact material; overall migration < 10 mg/dm²EN 1186 total immersion or food simulant
    FDA 21 CFR 177.1520Olefin polymers; final article suitabilityCondition of use dependent on food type and temperature
    EU Packaging Directive 94/62/ECSum of Pb, Cd, Hg, Cr(VI) < 100 ppmPackaging heavy metal testing
    REACH Regulation (EC) 1907/2006Candidate List SVHC content < 0.1% w/w per articleSupplier declaration or chemical analysis

    Storage conditions affect processing stability. Pellets should be protected from surface moisture when ambient relative humidity exceeds 60%; although polyethylene has low hygroscopicity, surface moisture introduced during outdoor silo storage can increase pinhole and bubble defects at die lip temperatures above 240 °C. The recommended storage temperature is below 50 °C, away from direct ultraviolet exposure. Resin oxidation during prolonged storage is indicated by a melt flow rate increase above 1.3 g/10 min or visible yellowing of pellets. The material is incompatible with polypropylene-based purge compounds under high-shear conditions because phase separation and layer delamination can persist into the final film. The grade is recyclable in polyethylene recovery streams; multilayer structures containing EVOH, polyamide, or tie resins require dedicated compatibilisation and should not be introduced into standard LDPE/LLDPE mechanical recycling without separation.

    Top