| HS Code | 746741 |
| Grade Name | Versalis Clearflex H&T CLH 196 |
| Polymer Type | Hexene Copolymer Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Hexene |
| Density | 0.919 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break Md | 30 MPa |
| Tensile Strength At Break Td | 25 MPa |
| Elongation At Break Md | 600 % |
| Elongation At Break Td | 700 % |
| Flexural Modulus | 200 MPa |
| Vicat Softening Temperature | 100 °C |
| Melting Temperature | 123 °C |
| Dart Drop Impact | 180 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12 % |
| Gloss 45 | 60 |
As an accredited Versalis Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex® H&T CLH 196 is supplied in 25 kg polyethylene bags, palletized, or 1000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL loads 18–20 metric tons of Versalis Clearflex H&T CLH 196 in 25 kg bags; palletized shipments reduce capacity. |
| Shipping | Versalis Clearflex® H&T CLH 196 is typically shipped as non-hazardous hexene copolymer linear low-density polyethylene pellets in 25 kg PE bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Keep dry, away from direct sunlight, heat, and contamination. No special transport classification required. Handle per SDS; avoid moisture and package damage. |
| Storage | Store Versalis Clearflex® H&T CLH 196 in a cool, dry, well-ventilated warehouse at ambient temperature. Keep original bags or containers closed and palletized off the floor. Protect from direct sunlight, heat, flames, moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Use first-in, first-out stock rotation. Inspect regularly for leaks or damage. Follow the SDS and local regulations. |
| Shelf Life | Versalis Clearflex H&T CLH 196: store cool, dry, ventilated, away from sunlight; unopened original packaging shelf life typically 12 months. |
Cast stretch film conversion for high-force pallet unitization uses Versalis Clearflex® H&T CLH 196 as the primary hexene-linear-low-density-polyethylene component because the short-chain branching distribution extends the pre-stretch plateau before strain hardening initiates. On a 65 mm single-screw cast line with L/D 30:1 and a 1,200 mm coat-hanger die, melt temperature is held at 245–265 °C and the 20 µm web is pinned to a chrome chill roll at 18–22 °C via a vacuum box; edge trim is ground and re-fed at up to 12 wt% through a gravimetric hopper. Melt addition ratios are 75–85 wt% CLH 196, 10–18 wt% LDPE with a melt flow rate of 1.9–2.3 g/10 min, and 1.5–3.0 wt% tackifier masterbatch; slip/antiblock masterbatch is maintained below 1.0 wt% to avoid pre-stretch carriage slip. Industry compliance for this non-food industrial web draws on ASTM D5748 protrusion puncture resistance, ISO 527-3:2018 tensile behavior in machine and transverse directions, and REACH SVHC communication obligations under Regulation (EC) No 1907/2006 for imported tackifier packages. Terminal output includes 12–23 µm hand wrap rolls at 400 mm and 500 mm widths, 17–35 µm machine wrap rolls at 500 mm and 750 mm widths for high-speed orbital wrappers, and pre-stretched 8–10 µm rolls used in battery and appliance unitization.
The process conflict in cast stretch film is the interaction between pre-stretch ratio and elastic recovery. On a production-scale turntable wrapper with gear-driven pre-stretch at 200–250%, the web retains residual stretch of 30–45 N per 25 mm when tested to ISO 527-3:2018; above 300%, neck-in at the carriage produces edge fibrillation that reduces pallet stability. Output on a 65 mm barrier screw is 120–180 kg/h, and a die-to-chill-roll air gap not exceeding 25 mm prevents web width loss. Published data for this specific grade in pre-stretched cast lines with inline edge-trim recycling above 15 wt% is limited; converters therefore trial at 10 wt% and monitor gels by optical film inspection counting defects larger than 50 µm per 10 m².
Because sub-zero food contact films must seal through frost and powdered fat residues, converters blend CLH 196 at 60–75 wt% with 15–25 wt% LDPE, 5–10 wt% plastomer, and 3–5 wt% slip/antiblock masterbatch to lower seal initiation while keeping the 45 µm web below 12% haze when tested to ASTM D1003. Three-layer blown-film lines with 70 mm extruders, L/D 30:1, die diameter 250 mm, die gap 1.8–2.2 mm, and blow-up ratio 2.2–2.8:1 run with frost line height 500–650 mm and air ring dew point below 5 °C; internal bubble cooling contributes 20–25% of total cooling. The main process conflict is that reclaimed trim from frozen-food converting contains paper fiber and heat-seal lacquer particles; at 20 wt% reclaimed trim, the bubble becomes unstable at output above 140 kg/h unless a 120/200/120 mesh screen pack is installed and melt pump suction pressure is limited to 180 bar. Food-contact compliance is validated under Commission Regulation (EU) No 10/2011 with total migration below 10 mg/dm², FDA 21 CFR 177.1520(c) for olefin polymers, and packaging quality management under ISO 22000:2018 and BRCGS Packaging Issue 6. Terminal forms include frozen seafood pillow pouches at 35–50 µm, vegetable IQF bags with transverse seal widths of 8–10 mm, and inner liners for frozen dough packs where seal strength must exceed 300 g per 25 mm on ASTM F88 at 120 °C seal bar temperature.
Dart impact measured to ASTM D1709 method A is the release criterion in this segment; a 45 µm three-layer web is generally specified above 110 g, but an incorrectly balanced internal bubble cooling shifts the frost line above 650 mm and lowers the measured dart value below 80 g because of higher crystalline orientation. Elmendorf tear by ISO 6383-2 typically falls between 900 mN and 1,300 mN for a 45 µm web depending on MD/TD ratio. When a 10 µm EVOH core is coextruded, the sealant skins are held at 25–35 wt% CLH 196 because skin LLDPE fractions above 60 wt% create viscosity mismatch against maleic anhydride grafted tie layers at the die lip; tie layers are each added at 5 wt%. Barrier pouches for sugar confectionery stored at -18 °C and lidding films with 45–60 µm peelable sealant systems complete the terminal range.
Form-fill-seal lines for polymer granulate and mineral salt use CLH 196 at 85–100 wt% with a fluoropolymer process aid masterbatch below 0.5 wt%; in coextruded three-layer sacks, the skins may be softened with 10–15 wt% LDPE to reduce sealing current while the core remains 100 wt% CLH 196. A typical production line uses a 90 mm grooved-feed extruder, L/D 33:1, die gap 2.0–2.4 mm, die diameter 300 mm, BUR 1.8–2.2:1, and internal bubble cooling; haul-off speed is 25–40 m/min for 120 µm film. The process limit at 150 µm is surface melt fracture caused by insufficient die-land shear stress; reducing extruder rpm instead of raising die temperature above 230 °C controls backpressure below 320 bar. Drop performance is verified by ISO 7965-2 with a 25 kg fill mass and 1.2 m flat drop; tear resistance is measured by ASTM D1922 or ISO 6383-2; tensile properties by ISO 527-3:2018. Regulatory conformance includes the TPCH heavy metals sum of Pb + Cd + Hg + hexavalent Cr not exceeding 100 mg/kg, REACH Annex XVII restrictions applicable to printing inks, and UN Model Regulations Chapter 6.5 for sacks used as outer packaging for dangerous goods when the converter supplies written classification support. End products are 60–120 µm FFS sacks for resin pellets, 100–150 µm chemical salt liners, 80 µm carbon black masterbatch bags, and 100–200 µm FIBC inner liners.
Three-layer coextrusion for agricultural ensiling films runs CLH 196 in the core at 65–75 wt% and in the outer skins at 35–45 wt%, the balance being LDPE and 8–12 wt% UV stabilizer masterbatch in the outer skins only. A 2,400 mm three-layer blown line with die gap 1.8–2.2 mm and BUR 2.8–3.2:1 is operated at a frost line height of 600–700 mm with chilled air at 8–10 °C; a segmented calibrating cage controls the bubble while maintaining a 6–9 m film width. The CLH 196 loading is not limited by tensile properties but by additive migration: high-molecular-weight HALS packages partition into the LLDPE amorphous zones and can exude above 10 wt% addition in the outer layer, creating winding tack. Conformance is checked against EN 13207:2001 for silage films, EN 13206:2017 for greenhouse covering where applicable, and ISO 4892-2 xenon-arc exposure; tensile after 2,000 h xenon exposure is generally specified above 18 N per 15 mm by ISO 527-3:2018. Published data for this specific grade under 3,000 h field exposure is limited. Terminal products include 25–40 µm silage bags, 150 µm clamp sheets, 180–200 µm greenhouse outer covers, and 50 µm bale-wrap replacement film.
Collation shrink for beverage multipacks uses a three-layer structure where CLH 196 forms the 60–75 wt% core, while 20–30 wt% LDPE skins provide transverse direction shrink and 1–2 wt% slip/antiblock masterbatch controls coefficient of friction at 0.2–0.4. The blown-film process for this segment is not conventional low-stalk: high-stalk bubbles are run at BUR 3.0–3.5:1 with die gap 1.2–1.6 mm and frost line 800–950 mm to build orientation in both directions; a 75 mm extruder with L/D 30:1 delivers 160–200 kg/h at 190–215 °C melt temperature. The process conflict is tear propagation at the perforation line after shrink: notch depth is set between 40% and 60% of film thickness, and an LLDPE core with insufficient comonomer content causes z-direction tear that crosses the perforation during tunnel shrinkage at 160–180 °C. Shrink tension is measured by ISO 14616:1997 and free shrink by ASTM D2732-14; typical shrink tension in this gauge is 0.5–1.5 N per 15 mm. Transport packaging compliance relies on EU Packaging Directive 94/62/EC essential requirements and TPCH heavy metal limits; if the collation wrap contacts food primary packaging, converter-level confirmation of EU 10/2011 or FDA 21 CFR 177.1520 may be required after migration testing. Terminal products are 40–60 µm collation shrink webs for 6×1.5 L beverage bottles, 35–45 µm can multipack films, and 25–30 µm shrink bundling for paper towel rolls.
When a 20 µm CLH 196 curtain is extruded onto aluminum foil or metallized PET for dry food sachets, the grade is used at 85–95 wt% with 5–15 wt% plastomer to reduce seal initiation below 100 °C. A 90 mm single-screw extruder with L/D 30:1 and a flat die gap of 0.5–0.7 mm processes the melt at 275–305 °C and deposits a 20–40 µm curtain through a 100–150 mm air gap onto the substrate; the chill roll is held at 12–18 °C. The critical parameter is draw ratio between die exit and substrate: at a line speed of 80–150 m/min and a die output of 120 kg/h, a 20 µm drawn web corresponds to a draw ratio close to 1.6:1; above 1.8:1, curl increases because the quenched layer develops anisotropic frozen-in stress. Compliance for food sachets is verified under Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c); adhesion strength to foil is measured by a peel test at 100 mm/min and reported in N per 15 mm, with converter specifications generally ranging from 2.0 to 4.0 N per 15 mm after corona treatment at 40–44 mN/m per ASTM D2578. LDPE is kept below 5 wt% because higher levels raise seal initiation temperature and narrow the hot-tack window. Terminal products include laminated pouch sealant webs for instant beverage powders, sachet films at 25–35 µm, lidding films at 30–40 µm, and aluminum foil laminate liners for bulk tea packaging.
Competitive Versalis Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® H&T CLH 196 is a hexene-1 copolymer linear low-density polyethylene supplied in pellet form for thin-gauge film conversion. The grade is differentiated from butene-copolymer LLDPE by the C4 branch formed at hexene-1 insertion sites; this branch length modifies crystalline lamella organization and the probability of tie-molecule formation under rapid quench. Specification control points normally include density by ISO 1183-1:2019, melt mass-flow rate by ISO 1133-1:2022 at 190 °C/2.16 kg, melting and crystallization by ISO 11357-3:2018, tensile properties by ASTM D638-14, dart impact by ASTM D1709-22, Elmendorf tear by ASTM D1922-15, and haze by ASTM D1003-21. Published independent data for this exact grade designation is limited; therefore, numeric lot-release values are not reproduced here as if they were certified. Instead, the specification framework is described by method and by the class-level range for hexene-1 LLDPE film grades. For C6-LLDPE in the low-density window, commercial film resins commonly fall within 0.915–0.925 g/cm³ and 0.5–4.0 g/10 min, but the supplier datasheet remains the controlling document for CLH 196.
The H&T designation is associated with Versalis’s high-performance and technical film cluster, where converters combine optical clarity with puncture resistance. CLH 196 is not a long-chain branched resin; it therefore follows the linear rheological signature of LLDPE: lower shear sensitivity than low-density polyethylene, lower melt strength in a molten bubble, and a narrower bubble-stability envelope when compared with high-pressure LDPE. Its molecular weight distribution and comonomer distribution are production-controlled through the polymerization train and are not equivalent to metallocene-catalyzed hexene LLDPE grades that can present a narrower composition distribution. This distinction affects sealing behaviour, extractables, orientation-induced whitening, and the response of the resin to processing aids.
At equal density and melt mass-flow rate, hexene-1 incorporation produces a longer short-chain branch than butene-1. The C4 branch from hexene-1 is more effective at interrupting crystallizable ethylene sequences, which reduces average lamellar thickness without requiring as high a comonomer molar fraction. The resulting amorphous-phase connectivity is more efficient for stress redistribution. In standard tests, this architectural shift is detected as higher dart impact under ASTM D1709-22, higher Elmendorf tear under ASTM D1922-15, and lower brittleness in notched tensile or environmental stress-crack resistance evaluations conducted under ASTM D1693-15. Film converters typically report that C6-LLDPE permits downgauging of heavy-duty sacks by approximately 10–25 μm while maintaining equivalent puncture resistance, but this conversion effect is line-specific and depends on die gap, frost-line height, and cooling-air temperature. Published data for this specific configuration is limited; comparative values should be validated on the target blown-film line.
Laboratory specification work follows a matrix of mechanical, thermal, and optical tests. Tensile yield and elongation are reported by ASTM D638-14 using a 50 mm/min crosshead speed for film. Dart impact is classified by ASTM D1709-22 Method A or B; Method A uses 38 mm drop height and 0.66 mm dart diameter, while Method B uses 1.52 m drop height and 50.8 mm dart diameter. Haze is measured on a calibrated photometer under ASTM D1003-21; transmission clarity is reported for 25 μm or 50 μm film. For conventional C6-LLDPE, optical values are frequently higher than metallocene grades due to broader composition distribution and larger spherulitic scattering. This does not preclude CLH 196 from transparent film applications; optical acceptance is controlled by the specific gauge, heat history, and chill-roll or blown-film quench conditions.
Molecular weight distribution can be checked by high-temperature gel permeation chromatography under ISO 16014-1:2019 in 1,2,4-trichlorobenzene at 150 °C. Conventional Ziegler–Natta hexene-LLDPE grades often show weight-average to number-average molecular weight ratios between 3.5 and 5.0; metallocene grades may fall below 3.0. The broader distribution in CLH 196 is functionally relevant because it increases shear thinning and raises extruder backpressure relative to a metallocene grade of the same melt mass-flow rate. Dynamic oscillatory tests at 190 °C can be used to compare crossover frequency and complex viscosity at 0.1 rad/s; these values correlate with processability and bubble stability on industrial film lines.
| Resin class | Short-chain branch length | Typical melt–density position | Performance shift at equivalent gauge | Standard method |
|---|---|---|---|---|
| C4-LLDPE | C2 | 0.918–0.925 g/cm³ | Lower dart, lower tear, higher clarity | ASTM D1709-22, ASTM D1922-15, ASTM D1003-21 |
| C6-LLDPE | C4 | 0.915–0.925 g/cm³ | Higher dart, higher tear, moderate haze | ASTM D1709-22, ASTM D1922-15, ASTM D1003-21 |
| C8-LLDPE | C6 | 0.905–0.920 g/cm³ | Higher dart, higher tear, lower density | ASTM D1709-22, ASTM D1922-15 |
Process conflicts arise from the linear architecture of hexene-1 LLDPE. On a 60 mm single-screw extruder with 30:1 L/D and a barrier feed section, melt pressure at the breaker plate typically stabilizes between 250 bar and 450 bar for a 1.0 g/10 min C6-LLDPE, depending on screw speed and screen pack. If the adaptor temperature is maintained above 220 °C, the residence-time–oxygen interaction can initiate oxidative gel formation and reduce dart impact; oxidation induction time is monitored by ISO 11357-6:2018. Bubble stability in high-stalk blown film is governed by melt strength. C6-LLDPE without long-chain branching can exhibit lower melt strength than LDPE, so a die gap of 1.2–2.0 mm and a frost-line height between 200 mm and 600 mm are typical starting points. The exact window must be established on the line because cooling-air enthalpy and stalk diameter ratio control the balance between orientation and quench stress. On cast-film lines, hexene-1 grades tend to exhibit lower backpressure than C4-LLDPE at equivalent melt flow rate; extruder motor load is not a direct substitute for melt temperature. When a 50 kg/h throughput is targeted, the extruder temperature profile should be flat to slightly reverse to minimize screw-induced superheat.
Additive package interactions are a further processing limit. High-shear dispersion of slip and antiblock masterbatches must avoid melt temperatures above 210–220 °C, particularly when the masterbatch carrier is LDPE. Incompatibility with polypropylene regrind is observed as delamination and loss of tear propagation under ASTM D1922-15; polypropylene contamination above 5 wt% should be rejected because phase separation at the die lip creates optical defects. Drying is not usually required for LLDPE unless storage has produced surface condensate. If resin has been exposed to relative humidity above 60%, a 60 °C hot-air hopper dryer for 2 h can remove surface moisture, but this is not a substitute for proper silo management and sealed package handling.
Seal initiation behaviour is governed by melting-range distribution and comonomer placement. Hexene-LLDPE often exhibits a lower seal initiation temperature than LDPE and butene-LLDPE at equal density. Seal strength should be measured by ASTM F88/F88M-21 on a heat-seal machine with controlled jaw pressure and dwell time; typical test dwell time is 0.5 s at 140 °C, 160 °C, and 180 °C. Hot tack is measured by ASTM F1921-18. These methods do not certify the resin for food or medical packaging; they quantify the thermal sealability of the film structure after conversion.
CLH 196 sits within the conventional Ziegler–Natta C6-LLDPE band. Against C4-LLDPE, the hexene comonomer provides higher impact and tear at equal density. Against metallocene C6-LLDPE, the broader molecular weight distribution typically gives higher extrusion backpressure and easier bubble stability at the expense of lower clarity and possibly higher extractables. Against LDPE, CLH 196 has lower melt strength and lower shear thinning, so blending with 10–30 wt% LDPE is a standard method to improve bubble stability in blown film; this blend is evaluated by melt extensibility rather than by standard melt-flow ratio alone. The mechanical response of the blend follows the blend rule only for modulus; dart impact is non-linear and must be measured by ASTM D1709-22. The sealing performance can be mapped by ASTM F88/F88M-21; hot tack is measured by ASTM F1921-18. In applications requiring low-temperature seal initiation, metallocene grades may show an advantage, but the exact ranking depends on sealant-layer gauge and the thermal diffusivity of the substrate.
| Parameter | Standard method | Controlled by |
|---|---|---|
| Density | ISO 1183-1:2019 | Polymerisation and comonomer content |
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | Molecular weight control |
| Tensile properties | ASTM D638-14 | Density and orientation |
| Dart impact | ASTM D1709-22 | Comonomer type and film gauge |
| Elmendorf tear | ASTM D1922-15 | Machine direction and transverse direction orientation |
| Haze | ASTM D1003-21 | Crystallite size and surface roughness |
| Thermal transitions | ISO 11357-3:2018 | Comonomer distribution |
| Food-contact status | FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011 | Supplier certification |
| Medical packaging status | ISO 10993-1:2018 | Downstream validation, not resin-alone |
In a production environment, the decision to replace a butene-copolymer LLDPE with CLH 196 should be based on a pilot-line comparison at 25 μm, 40 μm, and 80 μm film thickness. The comparison should include haze by ASTM D1003-21, dart impact by ASTM D1709-22, tear by ASTM D1922-15, seal strength by ASTM F88/F88M-21, and hot tack by ASTM F1921-18. Processors should also record extruder head pressure, melt temperature, and bubble frost-line displacement to separate material performance from equipment configuration. The grade cannot be considered a direct drop-in for every LLDPE film asset; high-stalk lines may require a blend with LDPE, while high-output cast lines may require adjustment of the chill-roll temperature to manage gloss and blocking. Published data for this specific configuration is limited, and the final acceptance boundary remains the downstream packaging specification, not a single laboratory data point.