Versalis Clearflex H T Clh 150 Linear Low Density Polyethylene

Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 511337
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Density 0.915 g/cm³
    Meltflowrate 190c 2 16kg 1.5 g/10 min
    Meltingpoint 118 °C
    Vicatsofteningpoint 90 °C
    Tensilemodulus 170 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 700 %
    Hardnessshored 48
    Haze 6 %
    Gloss 45deg 90
    Dartdropimpact 100 g
    Elmendorftearstrength Md 200 g
    Elmendorftearstrength Td 350 g

    As an accredited Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® H&T CLH 150 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial storage and transport.
    Container Loading (20′ FCL) Versalis Clearflex H&T CLH 150 LLDPE loaded in 25 kg bags, palletized, shrink-wrapped, and secured inside a 20′ FCL container.
    Shipping Versalis Clearflex® H&T CLH 150 ships as non-hazardous, free-flowing linear low-density polyethylene pellets. Standard packaging is 25 kg polyethylene bags, palletized and stretch-wrapped, or bulk in clean, dry trucks, railcars, or containers. Store and transport away from moisture, direct sunlight, and excessive heat. No special hazardous transport requirements.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizing agents. Keep containers sealed, labeled, and in original packaging. Protect from moisture, contamination, and physical damage; stack safely to prevent deformation. Avoid dust generation and static discharge; use appropriate grounding. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging, dry, cool, and protected from direct sunlight.
    Application of Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene

    On a three-layer cast film line with a 1,500 mm die width and 0.9 mm die gap, Clearflex H&T CLH 150 is introduced at 30 wt% in the skin layers and 40 wt% in the core, with the balance comprising a C4-LLDPE of 3.0 g/10 min melt index (ISO 1133-1:2022). The die gap is maintained at 0.8–1.2 mm, chill roll surface temperature is held at 18–25 °C, the air gap is set at 50–100 mm, and melt temperature is maintained at 245–265 °C. At 600 m/min line speed, the blend suppresses draw resonance and maintains gauge variation below ±2% at 15 μm; the pre-stretch unit operates at 200–250% elongation with roller temperature 70 °C, and winding tension taper is 20–40% to prevent roll blocking. Cling force is generated by adding 1.5 wt% polyisobutylene-based cling masterbatch to the outer skin only; anti-block is omitted from the cling layer. Coefficient of friction against steel is 0.20–0.35 (ASTM D1894-14). Protrusion puncture resistance is measured by ASTM D5748-95(2019), peel cling by ASTM D5458-95(2020), and elastic recovery by ASTM D5459-95(2020). Food-contact grades meet EU No 10/2011 Annex I and FDA 21 CFR 177.1520; overall migration is controlled below 10 mg/dm². Finished product types are 12–15 μm pre-stretched hand film, 17–23 μm machine stretch film, and 20–25 μm power-stretch film on 500 mm rolls.

    What gauge-reduction limits arise in heavy-duty sack film?

    The lower gauge limit is set by dart impact resistance rather than tensile yield. In a three-layer blown film line with 250 mm die diameter, 2.8:1–3.2:1 blow-up ratio, 700–900 mm frost line height, and internal bubble cooling, the compound comprises 10–20 wt% LDPE of 0.2–0.3 g/10 min (ISO 1133-1:2022), 2.0–3.5 wt% carbon black/UV masterbatch, 0.5–1.0 wt% slip/process aid masterbatch, and the balance CLH 150. Melt temperature is 185–205 °C; screw speed is 80–100 rpm on 50 mm grooved-feed extruders with 30:1 L/D. At 80 μm film, dart impact must exceed 800 g by ASTM D1709-16a, and tensile break in MD/TD must exceed 40 MPa and 30 MPa respectively by ISO 527-3:2018. For FIBC inner liners, the film is tested to ISO 21898:2004, with REACH 1907/2006 Annex XVII PAH limits applied to carbon black concentrates. Where converter-specific dart impact curves for CLH 150 in the final sack laminate are required, published data for this specific configuration is limited; acceptance is therefore determined on pilot lines by ASTM D1709-16a. Terminal product types are FIBC inner liners, petrochemical heavy-duty sacks, and valve sacks for cement and resins.

    The five-layer asymmetric blown film structure for frozen food packaging uses CLH 150 in both outer skin layers at 45 wt% of the layer blend, combined with 10–15 wt% LDPE and 2–4 wt% slip/antiblock masterbatch; the 10 μm core is EVOH with 38 mol% ethylene, and the two tie layers are maleic anhydride-grafted LLDPE at 5–8 μm each. Die gap is 1.8 mm, die diameter 180 mm, blow-up ratio 2.2:1, and frost line height 450–600 mm; skin melt temperature is 190–210 °C, while EVOH is processed at 210–225 °C within a 45-minute maximum residence time to prevent gel specks. Heat seal initiation at 105–115 °C is confirmed by ASTM F88/F88M-21 on a 100 μm laminate; seal strength after 0.5 s at 140 °C exceeds 12 N/15 mm. Anti-fog concentrate at 1.5–2.5 wt% reduces water droplet surface tension to below 35 mN/m in storage at 4 °C. Compliance includes EU No 10/2011 Annex I and FDA 21 CFR 177.1520. The resulting rollstock is used for frozen vegetable bags, ice cream pouches, and frozen seafood flow wrap.

    Extrusion coating sealant skins for aluminium foil laminates

    On a 1,300 mm flat-die extrusion coating line, the grade is processed as the sealant layer at 12–20 g/m², either as 100% resin or as a blend containing 15–25 wt% LDPE to reduce neck-in; the extruder is a 90 mm single screw with 30:1 L/D, die gap 0.6–0.8 mm, air gap 150–250 mm, melt temperature 285–315 °C, and chill roll temperature 12–18 °C. A maleic anhydride-modified polyolefin tie resin is coextruded at 3–5 g/m² when direct adhesion to aluminium foil exceeds 5 N/15 mm at 180° peel. Heat seals are formed at 130–145 °C, 0.5 s dwell, 300 kPa; seal strength measured by ASTM F88/F88M-21 must exceed 15 N/15 mm for non-retort lidding. Corona treatment is held at 40–42 dyn/cm (ASTM D2578-09) before lamination. Food-contact compliance is FDA 21 CFR 177.1520 and EU No 10/2011. The converted laminate forms non-retort lidding films, dry food sachet laminates, and toothpaste laminate webs.

    When pallet loads require elastic recovery above 50% after 90 mm extension

    In blown stretch hood film, the gauge is 60–120 μm, and the formulation uses 70 wt% CLH 150, 20 wt% LDPE with 0.5 g/10 min melt index (ISO 1133-1:2022), and 10 wt% metallocene C6-LLDPE. Processing occurs on a three-layer blown film line with 250 mm die diameter, die gap 1.4–1.6 mm, blow-up ratio 1.8:1–2.2:1, frost line height 350–500 mm, melt temperature 210–220 °C, and output 350–450 kg/h. The low blow-up ratio maximizes machine-direction orientation and elastic recovery. Elastic recovery is tested after 90 mm extension per ASTM D5459-95(2020), with acceptance above 50%; puncture resistance per ASTM D5748-95(2019) should exceed 60 N. Additives are 0.5–1.0 wt% slip, 0.3–0.6 wt% synthetic silica anti-block, and 1.0–2.0 wt% UV/HALS masterbatch for outdoor storage. Compliance includes REACH 1907/2006 Annex XVII and, for food-contact pallet cover, EU No 10/2011. The film is converted into stretch hoods, stretch sleeves, and ventilated pallet covers.

    Agricultural tunnel cover film of 150–200 μm is manufactured on a three-layer blown line with 300 mm die diameter, 2.5:1 blow-up ratio, 600–800 mm frost line height, and 1.8 mm die gap. The compound comprises 60 wt% CLH 150, 20 wt% LDPE, and 20 wt% EVA with 18% vinyl acetate; UV stabilizer HALS is added at 1.5–2.0 wt%, anti-fog at 1.0–2.0 wt%, and an IR-absorber masterbatch at 0.5–1.0 wt%. Melt temperature is 190–210 °C, and output is 400–500 kg/h. The film is tested to EN 13206:2017 for agricultural covering film, with tensile properties by ISO 527-3:2018 and tear propagation by ASTM D1922-15(2021). The film meets REACH 1907/2006 Annex XVII; it is not intended for food-contact use. Rollstock is cut into greenhouse covers, low tunnel covers, and early-season soil warming mulch films.

    Free Quote

    Competitive Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex H&T CLH 150 Linear Low Density Polyethylene is a hexene-comonomer linear low density polyethylene supplied by Versalis S.p.A. in pelletized form for cast and blown film extrusion. The H&T designation identifies a high-toughness product within the Clearflex range, intended for film structures that require resistance to puncture, tear propagation, and high-strain wrapping. Incoming resin acceptance is normally based on melt flow rate measured under ISO 1133-1:2022 at 190 °C with a 2.16 kg dead weight, and density measured according to ISO 1183-1. The current manufacturer’s technical data sheet lists lot-specific nominal values, and those values should be used for incoming quality control because pellet melt flow rate alone does not fully predict film tear, draw, or optical performance.

    What Distinguishes Hexene-Based CLH 150 from Butene LLDPE and High-Pressure LDPE?

    The primary structural distinction is short-chain branch length. Hexene comonomer produces longer alpha-olefin short-chain branches than butene, which affects tie-molecule concentration and the distribution of lamellar thickness. Under ASTM D1709-16a dart impact testing and ASTM D1922 Elmendorf tear testing, hexene-based LLDPE film typically exhibits higher failure resistance at equivalent thickness and density than butene-based LLDPE. High-pressure LDPE differs further because it contains long-chain branching, which raises melt elasticity and improves bubble stability in blown film but reduces ultimate tensile strain and dart impact. The CLH 150 grade is therefore specified where converters require higher tear and puncture performance than LDPE without the narrow processing window associated with some metallocene-catalysed grades. The comparative numerical values for CLH 150, including typical dart drop, tear, and tensile properties, are provided in the current Versalis product datasheet; third-party published data for this specific product configuration is limited.

    Because the hexene comonomer modifies crystallinity and orientation behaviour, CLH 150 also differs from grades in the same family that are designed for low seal initiation or maximum stiffness. The high-toughness designation does not automatically imply improved seal strength; seal performance must be validated separately according to ASTM F88 or ISO 527-3-referenced film protocols.

    In cast film conversion on a 75 mm single-screw extruder with a 30:1 L/D barrier screw, initial processing trials often begin with barrel zone temperatures of 200 °C, 215 °C, 225 °C, 235 °C, and 240 °C, with a die temperature of 245 °C. The die gap is set between 0.6 mm and 0.8 mm. Chill-roll temperature is held between 18 °C and 24 °C in low-haze formulations; higher chill-roll temperatures can reduce condensation-related surface defects but may alter the bloom rate of cling additives. At line speeds above 250 m/min, gauge uniformity is influenced by air-knife pressure, vacuum box position, and melt temperature control. Operators have observed that shear heating in the metering zone can cause melt-temperature overshoot above the setpoint when screw speed is increased above 100 rpm; melt pressure and film appearance should therefore be monitored during start-up and grade changes. Published data for this specific formulation across all machine configurations is limited, so the described conditions are typical starting points for hexene LLDPE cast film rather than guaranteed specifications.

    Blown Film Bubble Stability and Frost Line Height

    For blown film, die gap typically ranges from 1.2 mm to 1.8 mm, with a blow-up ratio of 2.0:1 to 2.5:1. Frost-line height is controlled by external air-ring lip geometry and internal bubble cooling air flow. Hexene LLDPE grades exhibit lower melt tension than high-pressure LDPE, so bubble flutter at high secondary air flow can be a limiting constraint. The CLH 150 grade’s molecular weight distribution is broad enough to maintain backpressure and reasonable bubble stability on well-centred dies, but worn air rings or misaligned dies can produce gauge variation and uneven roll profile. Melt temperature at the die is usually maintained below 220 °C to limit oxidative degradation. When film thickness is below 25 µm, a higher frost line can reduce orientation-induced brittleness; above 80 µm, a lower frost line improves bubble cooling and output stability.

    When Pre-Stretch Ratios Exceed 250 % in Automatic Pallet Wrappers

    For power pre-stretch pallet wrapping, film elongation is typically set between 200 % and 300 %. At these ratios, transverse-direction tear propagation becomes the dominant failure mode, and converters commonly qualify film using ASTM D1922 Elmendorf tear and ASTM D5748 puncture resistance. The CLH 150 grade is selected for loads with sharp or irregular geometries because hexene comonomer reduces crack propagation relative to butene copolymers. In high-speed rotary arm wrapping trials, failure is usually first observed at the film edge or at pallet corner contact points. Edge trim quality, die-lip cleanliness, and unwind tension must be controlled to maintain stretch consistency. The grade should not be blended with high-density polyethylene without revalidating tear and pre-stretch performance, because increased stiffness can reduce ultimate stretch and cause catastrophic film break at high elongation.

    Mechanical Property Validation Under ISO 527 and ASTM D882 Protocols

    Tensile properties of cast film are commonly measured according to ASTM D882-18 at a test speed of 500 mm/min, with specimens conditioned at 23 °C and 50 % relative humidity for at least 40 h. For cast LLDPE stretch film, machine-direction tensile strength above 20 MPa and elongation at break above 300 % are common after pre-stretch, but the grade-specific values must be confirmed against manufacturer data. Puncture resistance is evaluated using ASTM D5748, and dart impact is measured according to ASTM D1709-16a Method A. The H&T designation indicates that the grade is optimized for high strain-at-break and tear resistance rather than maximum modulus or thermal stability. Comparative testing against CLH 120 or CLH 130 requires identical film gauge, draw ratio, and cooling history because post-extrusion cooling rate affects crystallinity and mechanical performance.

    Quality-control laboratories evaluate incoming CLH 150 by verifying the manufacturer’s lot certificate against ISO 1133-1:2022 melt flow rate and ISO 1183-1 density values. Film samples are checked for gauge uniformity with a micrometre and for haze per ISO 14782; gloss is measured at 60 ° according to ASTM D2457. Pellet melt flow rate alone should not be used to infer final film performance because molecular weight distribution, comonomer distribution, and thermal history also affect film properties.

    Regulatory Status and Compliance Checklist

    For food contact applications, the converter must validate end-use compliance on the finished article, not the resin pellet alone. Olefin homopolymers and copolymers produced under suitable conditions are referenced in the following framework:

    Regulation or standardDesignationRelevant measurement or condition
    EU Framework Regulation(EC) No 1935/2004Good manufacturing practice and food contact suitability
    EU Plastics Regulation(EU) No 10/2011Overall migration limit 10 mg/dm²; migration testing per EN 1186
    United States FDA21 CFR 177.1520Olefin polymers; conditions of use vary by film thickness and food type
    REACH(EC) No 1907/2006Substance registration and SVHC screening
    RoHSDirective 2011/65/EUHeavy metal restrictions at homogeneous material level

    Storage of pellets in a dry area below 50 °C is recommended. LLDPE is not hygroscopic, but condensation on cold pellet surfaces should be avoided when ambient storage is below 0 °C and the material is then introduced into a heated hopper. If surface moisture is present, a desiccant hopper dryer at 60 °C for 2 h may be used; prolonged drying is unnecessary and can accelerate oxidation of the stabilizer package. Regrind addition should be validated on the production line because higher regrind levels can increase gel counts and haze unless continuous melt filtration and a homogenizing screw are installed.

    Before dry blending with recycled LLDPE, incoming scrap should be characterized by melt flow rate and contamination level. The resin should be purged with a lower-viscosity polyolefin during shutdown to reduce carbonised deposits in high-shear zones. Failure to control die-lip buildup and air-ring condensation can produce edge tearing and variable cling performance in cast film, and can create bubble instability in blown film.

    Top