Versalis Clearflex Fgh B0 Film Grade Lldpe

Versalis Clearflex® FGH B0 Film Grade LLDPE

    • Product Name: Versalis Clearflex® FGH B0 Film Grade LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 629934
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Grade Film Grade
    Comonomer Butene-1
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break 30 MPa
    Elongation At Break 700 %
    Flexural Modulus 260 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Resistance Md 120 g
    Elmendorf Tear Resistance Td 200 g
    Haze 12 %
    Gloss 45 80 %

    As an accredited Versalis Clearflex® FGH B0 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg) for Versalis Clearflex® FGH B0 Film Grade LLDPE.
    Container Loading (20′ FCL) Palletized 25 kg bags of Versalis Clearflex® FGH B0 Film Grade LLDPE, shrink-wrapped and secured inside a 20′ FCL.
    Shipping Versalis Clearflex® FGH B0 Film Grade LLDPE is typically shipped in 25 kg polyethylene bags or octabins, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, protected from moisture, heat, and direct sunlight. It is non-hazardous under normal shipping conditions; follow supplier handling and storage guidelines.
    Storage Store Versalis Clearflex® FGH B0 Film Grade LLDPE in a dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging sealed, on pallets, protected from moisture, dust, oils, and UV light. Maintain moderate temperatures, avoid prolonged stacking pressure, and use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations. Do not smoke.
    Shelf Life Shelf life is 24 months from production date when stored in original, unopened packaging, dry, cool, and away from sunlight.
    Application of Versalis Clearflex® FGH B0 Film Grade LLDPE

    On high-speed cast stretch film lines running at 450–600 m/min with a 75 mm single-screw extruder and a 2.2 m T-die, the comonomer architecture of Clearflex® FGH B0 controls edge neck-in and draw resonance stability. The resin is supplied in the low-density linear low-density polyethylene band; melt flow rate measured per ISO 1133-1:2022 at 190 °C/2.16 kg and density measured per ISO 1183-1:2019 should be confirmed against the current technical data sheet before die selection. The resin is not pre-dried below 60% relative humidity; above that threshold, pre-drying at 70 °C for 2 h in a desiccant hopper is required to prevent screw surging and melt curtain instability. Melt temperature is held at 240–260 °C; a 1.0–1.2 mm die gap is preferred because narrower gaps raise shear heating and melt pressure, while wider gaps increase die swell and retard quench response. With a 20:1 draw ratio and an air-gap length of 90–120 mm, the film is quenched on a 30–35 °C chrome chill roll. Under these conditions, neck-in is typically confined to 4–8% per side; published pilot-line data for this specific die configuration remain limited, so pilot-scale confirmation is required before tooling changes.

    For one-sided cling or two-sided stretch film, the resin is dry-blended with a lower-crystallinity metallocene plastomer at 10–20 wt% and a polyisobutylene tackifier at 2–6 wt%. Tensile elongation at break measured per ISO 527-3 increases with plastomer addition, while secant modulus measured at 2% strain decreases by 20–30% relative to the neat LLDPE. Cling force is quantified per ASTM D5458 on a 200 mm wide specimen after 24 h aging at 23 °C. Processors must limit total tackifier loading above 6 wt% because low-molecular-weight PIB migrates to the film surface and produces roll blocking at storage temperatures above 30 °C. The outer cling layer is corona treated to 38–42 mN/m only when a printable surface is specified; for pre-stretch hand film, no corona is applied. Food contact compliance for the base resin is assigned under FDA 21 CFR 177.1520 and EU Regulation 10/2011; finished stretch film requires converter-specific migration testing because tackifier, plastomer, and processing aids are outside the resin certification.

    In coextruded cast stretch structures containing a core layer and two outer cling layers, the core layer is loaded with edge trim and reprocessed pellets at 10–20 wt%. Recycled content above 20 wt% raises gel counts and reduces optical clarity measured per ASTM D1003 by 1.5–2.0% absolute. Additive masterbatches are introduced through a side feeder to avoid screw slippage and inconsistent cling distribution. Film thickness variance across the web is controlled to ±3% at 20 µm using an automated die bolt system; excursions beyond that range produce transverse gauge bands that appear as alternating high-cling and low-cling areas after pre-stretching.

    What Determines Dart Impact Retention in Heavy-Duty Sack Extrusion?

    Heavy-duty shipping sacks produced from 100–150 µm blown film require a balance between machine-direction extensibility and impact energy absorption. A 90 mm extruder with an L/D of 30:1 and a 400 mm die is operated at a blow-up ratio of 2.2–2.8:1 and a frost line height of 8–10 die diameters. In blends of Clearflex® FGH B0 with LDPE at 20–40 wt%, the higher melt strength of the LDPE fraction stabilizes the bubble and broadens the processing window. Dart impact is measured per ASTM D1709 method A on a 38.1 mm tup; values in the 300–450 g range are typical for this thickness band when the film is conditioned for 40 h at 23 °C and 50% RH. Elmendorf tear is measured per ASTM D1922; MD tear values generally remain 30–40% lower than TD tear in high-stalk films because of orientation anisotropy.

    Die gap selection above 1.4 mm reduces melt fracture but depresses TD tear and increases thickness variation. A die gap of 1.2 mm combined with a 240 °C melt temperature minimizes gel particles and maintains tear balance. Use of recycled in-plant sack scrap above 15 wt% is not recommended without a melt filtration unit because gel counts measured on a 100 cm² film sample by optical scanning increase at a non-linear rate and reduce dart impact by 20–50% depending on feedstock cleanliness.

    Surface treatment for flexographic printing is set at 38–42 mN/m; untreated film retains 30–32 mN/m and causes ink adhesion loss during high-speed printing. The coefficient of friction is measured per ASTM D1894; a one-side slip package at 800–1200 ppm erucamide yields kinetic COF of 0.25–0.35 on the treated outer surface, while the inner surface remains untreated for stack stability. Avoid combining the resin with high-vinyl-acetate EVA above 10 wt% in this application because the resulting decrease in melting point increases blocking during roll storage.

    When Silage Film Requires UV Stabilization and Controlled Oxygen Transmission

    For black/white silage film coextruded on a three-layer line with a 1200 mm die and a 2.0:1 blow-up ratio, Clearflex® FGH B0 is used in the core layer at 60–70 wt% while the skin layers contain carbon black masterbatch and titanium dioxide. The core layer is formulated with hindered amine light stabilizers at 0.15–0.30 wt% and PE-based antiblock at 3000–5000 ppm; slip additive is omitted in the core because erucamide migration increases oxygen transmission at the film surface. Oxygen transmission rate is measured per ASTM D3985 at 23 °C and 0% RH; a 30 µm film typically maintains a barrier of 5000–8000 cm³/(m²·day·atm), which is sufficient for ensiling but not for modified-atmosphere packaging.

    Ultraviolet exposure is evaluated per ASTM G154 cycle 1 with UVA-340 lamps for 3000 h. Retention of dart impact after exposure is measured per ISO 7765-1; failure is defined when impact strength drops below 50% of the unexposed value. The white outer layer must be formulated with rutile TiO₂ at 4–6 wt% to prevent premature HALS consumption on the sun-exposed surface. Processors should avoid melt temperatures above 220 °C in the skin layers because carbon black and TiO₂ increase shear heating and can degrade the UV package.

    When the film is used on round bale wrappers, tackiness is generated by the outer skin composition rather than by a post-extrusion applied adhesive. The required cling level is tested per ASTM D4649 for stretch wrap load retention, with a minimum retained load of 50% after 1 h at 23 °C. Wet silage leachate contact reduces film toughness; converters should verify impact retention after immersion in lactic acid solution at pH 3.5–4.0 for 72 h before commercial use, because published field data for this specific exposure regime remain sparse.

    Extrusion lamination of a 20–30 µm melt web against printed BOPP and metallized PET uses a 65 mm extruder fitted with a 150 mm T-die and a 0.5–0.8 mm air gap. The melt temperature is held at 280–310 °C to promote adhesion to aluminium metallization and to oxidize the polyethylene surface. Clearflex® FGH B0 is run neat or blended with an adhesion-promoting anhydride-modified PE at 5–10 wt%; peel strength is tested per ASTM F88/F88M on 25 mm strips after 24 h conditioning at 23 °C and 50% RH. Values below 2 N/15 mm indicate insufficient oxidation or contamination, while values above 5 N/15 mm may indicate excessive melt temperature and polymer degradation.

    Hot tack during subsequent pouch forming is measured per ASTM F1921 at seal temperatures of 115–135 °C and a 0.5 s dwell. Heat seal initiation occurs at 95–105 °C; published hot-tack values for this exact lamination structure are limited and must be verified on the target packaging line. The substrate path must be preheated to 60–80 °C before the nip to avoid surface moisture flash-off and pinholes in the melt web. Haze of the laminated structure is measured per ASTM D1003; a haze increase above 3% absolute relative to the base film indicates poor melt curtain stability or excessive nip roll pressure. Contamination by polypropylene from shared silos results in gel streaks and delamination at the aluminium interface; dedicated resin handling is specified for high-barrier laminates. Migration testing under EU 10/2011 for fatty food simulant D2 at 40 °C for 10 days is required if the laminate contacts food directly; the anhydride-modified PE adhesion layer must have its own food-contact approval.

    Low-Temperature Puncture and Seal Integrity in Quick-Frozen Food Film

    A 70 µm frozen-food packaging film processed with a 50 mm extruder and a 150 mm die at a blow-up ratio below 2.0:1 exhibits higher MD tear orientation and low-temperature puncture resistance. Melt temperature is reduced to 200–220 °C to suppress oxidative gel formation; the die gap is set at 0.8–1.0 mm. Low-temperature impact is evaluated at -20 °C using a conditioned specimen chamber and ASTM D1709 method B, with the tup mass adjusted for the thinner film. Tear resistance at -20 °C is measured per ASTM D1922 after 40 h conditioning; MD tear values are typically 20–30% lower than at 23 °C because LLDPE undergoes ductile-to-brittle transition at low temperatures.

    Heat seal parameters are set at 115–135 °C, 0.4–0.8 s dwell, and 2.0 bar jaw pressure. Seal strength is measured per ASTM F88/F88M on 15 mm strips; retained seal strength after contact with frozen food at -18 °C must exceed 8 N/15 mm to survive rough handling. Slip additive concentration is limited to 500–800 ppm because higher erucamide levels migrate to the seal surface and reduce seal initiation temperature by 5–10 °C, increasing the risk of seal failure in high-speed vertical form-fill-seal machines.

    Clarity of frozen-food packaging is measured per ASTM D1003; haze values above 8% on a 70 µm film are rejected in retail display applications. The resin should not be blended with low-molecular-weight LDPE waxes exceeding 2 wt% in this application because wax bloom increases haze after cold storage and reduces ink adhesion on the reverse-printed web.

    Balancing MD/TD Shrink Tension in Printed Collation Film

    Printed collation shrink film produced on a 45 mm extruder with a 150 mm die is oriented by blown-film parameters that set the MD/TD shrink balance. A low blow-up ratio of 1.5–2.0:1 and a high frost line height of 12–15 die diameters produce MD free shrink of 55–65% at 120 °C and TD free shrink of 35–45% at 120 °C measured per ASTM D2732. The addition of Clearflex® FGH B0 at 70–80 wt% with an LDPE homopolymer fraction provides the required shrink tension and ink adhesion after corona treatment at 36–40 mN/m. Shrink tension is measured per ASTM D2838; values above 0.5 MPa at 120 °C produce curled edges on printed labels when ink coverage exceeds 30% of the surface.

    The film is wound with taper tension of 10–20 N per 100 cm roll width to prevent telescoping. Storage below 25 °C is mandatory because ambient temperatures above 30 °C initiate premature shrink in printed rolls. Processors should avoid film-to-film slip additive loadings above 1000 ppm because migration to the surface during storage reduces corona treatment stability and causes ink delamination. For shrink sleeves with a high TD shrink requirement, the film is annealed at 60–70 °C for 10–15 min to reduce residual stress and prevent label distortion before slitting.

    Seam welding of formed collation film is carried out at 120–140 °C with 0.3–0.6 s dwell; the seal area retains 70–80% of the original film tear strength when tested per ASTM D1922. Published data for this exact grade in printed collation configurations is limited; converters should validate shrink force and seal integrity on the target sleeve machine before high-volume production.

    Free Quote

    Competitive Versalis Clearflex® FGH B0 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FGH B0 is a film-grade linear low-density polyethylene supplied in pellet form for primary conversion on tubular blown film lines. The nominal density is 0.918 g/cm³ when measured under ISO 1183-1, and the nominal melt flow rate is 1.0 g/10 min at 190 °C with a 2.16 kg load under ISO 1133-1:2022. The grade carries a standard stabilisation system and a film-oriented additive package; exact slip and antiblock loadings are lot-specific and supplied in the certificate of analysis. Public summary literature does not disclose the comonomer identity or catalyst type in detail, so full mechanical and optical data must be obtained from the version-specific technical datasheet. Compared with high-pressure LDPE film grades of equivalent melt flow rate, the linear structure of this product is associated with higher tensile strength and puncture resistance at equal film thickness, although bubble stability at high blow-up ratio requires stricter control of cooling air and frost line.

    Molecular Architecture and Additive Package for Blown Film Line Stability

    The molecular architecture of this linear-low-density polyethylene is based on a predominantly linear backbone with short-chain branches distributed along the main chain. This structure differs from high-pressure LDPE, which contains long-chain branching and produces strain-hardening behaviour in the melt. The density of 0.918 g/cm³ places the product in a medium-comonomer LLDPE class intended to balance stiffness, dart impact, and optical clarity. The melt flow rate of 1.0 g/10 min corresponds to a moderate-viscosity window suitable for film thicknesses from 40 µm to 120 µm on conventional single-screw extruders without excessive motor load. Published data for comonomer distribution and molecular weight distribution for this specific grade is limited; converters requiring rheological curves should request the lot-specific technical datasheet.

    The commercial pellet includes a stabilisation system for thermal processing in air. Antioxidant loading is not disclosed in summary public documents. For LLDPE film grades with similar thermal requirements, primary phenolic antioxidants are commonly used at concentrations between 500 ppm and 1,200 ppm, often combined with phosphite secondary antioxidants at 600 ppm to 1,500 ppm. The B0 designation is associated in the supplier product range with a film additive package, but the specific silica, talc, or erucamide levels must be confirmed from the certificate of analysis because they influence coefficient of friction, blocking, and seal performance. The presence of slip and antiblock additives does not remove the need for corona treatment when printing or laminating; the required surface tension should be verified under ISO 1135 or equivalent before conversion.

    Production-scale blown film equipment processing this density and melt flow rate class typically uses grooved-feed extruders with 24:1 to 30:1 L/D and barrier or Maddock mixing screws. A die gap of 1.6 mm to 2.4 mm is used for LLDPE of this density; narrower gaps reduce haze but increase die pressure and shear heating. Melt temperature at the die should be maintained between 190 °C and 220 °C. Bubble stability is generally improved by setting the blow-up ratio between 2.0:1 and 3.0:1 and keeping the frost line height at 6 to 10 die diameters. Cooling air temperature and volume must be adjusted to avoid bubble flutter; internal bubble cooling is recommended when output exceeds 100 kg/h on a 160 mm die, although published data for this specific grade in that configuration is limited. Pre-drying is not normally required for LLDPE; if condensate has formed during cold storage, a warm-air dryer at 70 °C for 2 h is sufficient to remove surface moisture before extrusion.

    Die lip build-up from low-molecular-weight fractions can occur during extended campaigns. Periodic cleaning of the die lips is required to prevent gauge bands and optical defects. Extruder head pressure should be monitored; LLDPE film grades of similar melt flow rate typically produce pressures below 350 bar at the breaker plate with a 60/100/60 screen pack, but actual pressure depends on screw design, die gap, and output. Screw speed and backpressure settings should be adjusted so that melt temperature measured by an immersion thermocouple at the die adapter remains below 230 °C to avoid oxidative gel formation. Gauge variation measured by a capacitance gauge should be kept below ±10% to avoid weak spots in dart impact tests under ASTM D1709 method A.

    Only the nominal resin parameters that are consistently published for Clearflex FGH B0 are listed in the following table. Full mechanical and optical data must be obtained from the version-specific technical datasheet because values vary with film gauge, blow-up ratio, frost line height, and additive package lot.

    Parameter Published typical value Standard
    Density 0.918 g/cm³ ISO 1183-1
    Melt flow rate 1.0 g/10 min at 190 °C/2.16 kg ISO 1133-1:2022
    Primary conversion process Blown film extrusion —
    Additive package Stabiliser with slip/antiblock system —

    What Melt Temperature and Blow-Up Ratio Window Does the Grade Require?

    The processing window is defined by the interaction between melt viscosity, bubble stability, and film optics. At melt temperatures below 185 °C, the higher melt viscosity produces shear heating and increases motor load; at temperatures above 230 °C, oxidative degradation may generate gel particles and reduce dart impact. The optimum melt temperature for blown film is therefore generally between 190 °C and 220 °C. The blow-up ratio should be maintained within 2.0:1 to 3.0:1; below 1.8:1 transverse orientation is insufficient and film tear imbalance becomes severe, while above 3.5:1 the bubble is prone to flapping and gauge variation may exceed ±15%.

    Frost line height controls quench rate and crystalline size. A low frost line of 4 die diameters increases haze by accelerating crystallisation, while a high frost line of 12 die diameters lowers bubble stability. For this grade family, the practical control range is 6 to 10 die diameters. During film production at 40 µm, the relationship between frost line height and dart impact under ASTM D1709 method A is non-linear: excessively rapid cooling can reduce impact resistance by freezing in a less tie-molecule-rich amorphous phase. Published data for this specific Clearflex grade in this configuration is limited, but the effect is well documented for LLDPE film of equivalent density and melt flow rate.

    In frozen-food packaging, the film is evaluated after conditioning at -18 °C for 24 h. The relevant performance test is low-temperature dart impact under ASTM D1709 method A, because film brittleness at freezer temperatures is a common failure mode on vertical form-fill-seal machines. LLDPE film of 0.918 g/cm³ density and 40 µm thickness typically shows less brittle cracking than LDPE of the same thickness, but the actual value depends on frost line height and bubble cooling. Sealing on VFFS equipment is generally performed at 115 °C to 135 °C jaw temperature with 0.5 s to 1.0 s dwell; seal strength may be tested under ASTM F88 or ISO 527-3 after ageing.

    For heavy-duty shipping sacks, the conversion line usually targets a film thickness of 80 µm to 120 µm. The key property is Elmendorf tear resistance measured according to ISO 6383-2. In LLDPE blown films, tear resistance in the transverse direction is commonly higher than in the machine direction, and the MD/TD tear ratio is controlled by blow-up ratio and draw. Sack drop testing according to ISO 7965-1 after filling with 25 kg of granular material provides a production-scale validation of impact-toughness distribution, but published data for this specific Clearflex grade in heavy-duty sack structures is limited. Converters must evaluate filled-drop results on their own equipment because thread strength and seal geometry affect failure location.

    In transparent lamination films, the grade is assessed for haze and gloss. Haze is measured on a 40 µm film according to ISO 14782 or ASTM D1003. For clear-flex LLDPE films of this density class, haze values are typically below 10%, and 60° gloss under ASTM D2457 generally exceeds 100. These optical benchmarks are sensitive to die gap, melt temperature, and the concentration of antiblock agent. The slip/antiblock package reduces blocking during roll storage at pressures above 0.1 MPa, but the coefficient of friction must be verified under ISO 8295 after 24 h ageing at 60 °C because erucamide migration continues after extrusion.

    When Clearflex FGH B0 Replaces Conventional Butene LLDPE in Lamination Lines

    Replacement of a conventional butene-copolymer LLDPE of the same density and melt flow rate may alter the balance between optical clarity and impact resistance. If the Clearflex grade uses a higher alpha-olefin comonomer or a tighter comonomer distribution, the tie-molecule concentration in the amorphous phase increases, which improves dart impact and Elmendorf tear at equal density. This effect is most measurable at film thicknesses below 50 µm. However, the conversion may also reduce bubble stability because higher-comonomer LLDPE resins can display lower melt tension at low shear. On a 160 mm die with 2.5:1 blow-up ratio, the operator may need to increase frost line height from 6 to 8 die diameters and reduce cooling air velocity to maintain a stable bubble.

    Compared with a high-pressure LDPE film grade of equivalent melt flow rate, the LLDPE provides higher tensile strength at break and superior environmental stress-crack resistance, but the film is stiffer in the machine direction and is less forgiving to bubble instability during changes in line speed. Blending with LDPE at 10 wt% to 20 wt% is frequently used to improve bubble stability and increase melt extension; the blend may reduce dart impact only slightly while increasing haze. The specific blend ratio should be selected by measuring bubble stability, gauge variation, and Elmendorf tear under ISO 6383-2, not by melt flow rate alone.

    Relative to a metallocene-catalysed LLDPE of similar density, a broad molecular weight distribution typically improves processability by reducing extrusion pressure and may allow higher output, but it can also reduce hot-tack strength and final optical clarity. Sealing initiation temperature may be 5 °C to 10 °C higher than a metallocene grade of similar density. Converters should evaluate hot-tack under ASTM F1921 and seal initiation under ASTM F88 before substituting this product in high-speed form-fill-seal lines. Published data for FGH B0 hot-tack and seal-cold performance is limited; direct comparative trials are required.

    Regulatory suitability must be confirmed against the lot-specific extended safety data sheet. For food-contact use, the grade is typically referenced to EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c)(3.2a), but the converter must verify overall migration, specific migration, and sensory properties under the actual food simulant and time-temperature conditions. Under REACH Regulation (EC) No 1907/2006, substances of very high concern are not intentionally added above 0.1 wt% in the supplier product stewardship summaries. The grade is not formulated for medical or implant applications.

    Processing limitations include the risk of oxidative gel formation at prolonged melt residence times above 230 °C or at low purging rates. The grade is not recommended for exposure to strong oxidising agents, aromatic hydrocarbon solvents, or continuous contact with mineral oil at temperatures above 50 °C, because environmental stress cracking may occur in stressed film. Predrying is not required at relative humidity below 60%; above this threshold, surface condensation must be removed by drying at 70 °C for 2 h before extrusion.