    Specifications
    HS Code 670163
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Density 23 C 0.919 g/cm³
    Melting Point 121 °C
    Vicat Softening Point 10 N 95 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    1 Secant Modulus 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Resistance Md 120 g
    Elmendorf Tear Resistance Td 250 g
    Haze 12%
    Gloss 60 80
    Coefficient Of Friction 0.20

    As an accredited Versalis Clearflex® FGH 196 A Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® FGH 196 A Film Grade LLDPE is typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure bulk transport.
    Container Loading (20′ FCL) Versalis Clearflex® FGH 196 A Film Grade LLDPE: 20′ FCL loading, 25 kg bags, palletized, approximately 20 MT per container.
    Shipping Versalis Clearflex® FGH 196 A Film Grade LLDPE is shipped as non-hazardous, solid polyethylene pellets in 25 kg bags, big bags, octabins, or bulk containers/trucks. Store dry, cool, ventilated, away from heat, ignition, and direct sunlight. It is not classified as dangerous goods for transport.
    Storage Store Versalis Clearflex® FGH 196 A Film Grade LLDPE indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, moisture, and contaminants. Keep original packaging sealed and palletized. Avoid excessive stacking, crushing, or UV exposure. Store at ambient temperature, away from incompatible chemicals or strong oxidizers. Maintain clean, odour-free conditions and follow first-in, first-out stock rotation.
    Shelf Life Versalis Clearflex® FGH 196 A Film Grade LLDPE: typically 12 months in unopened original packaging, stored dry, cool, away from direct sunlight.
    Application of Versalis Clearflex® FGH 196 A Film Grade LLDPE

    What governs machine-direction elongation retention in high-performance pallet wrap?

    In pallet-unitization converting, the film property that most tightly correlates with load stability on automatic wrappers is machine-direction elongation retention after pre-stretch, not tensile strength at break. A cast-film formulation built around Clearflex FGH 196 A LLDPE, with nominal density 0.918 g/cm³ and melt flow rate 1.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022, is processed on a 5-layer cast line with 30:1 L/D barrier screws, melt pump, and a 0.5–0.8 mm die gap. Compliance for pallet wrap films is anchored to ASTM D5458 for peel cling, ASTM D5748 for protrusion puncture resistance, and ASTM D882 for tensile elongation; EU shipments require a EC 1907/2006 REACH SVHC declaration, and automatic-wrapper users commonly require a load-retention test following the end-user’s internal pre-stretch protocol. The base resin fraction falls between 85 wt% and 92 wt%, with 8–15 wt% metallocene polyethylene plastomer and 1.5–3.0 wt% polyisobutylene cling masterbatch; a production-scale reference point is 88 wt% Clearflex FGH 196 A, 10 wt% metallocene plastomer, and 2 wt% PIB masterbatch. PIB addition above 4 wt% produces blocking on the finished roll and increases unwind noise at high pre-stretch ratios, while levels below 1.5 wt% are insufficient to hold cling after storage at 35 °C and 70% RH. Downstream, the compound is extruded at melt temperatures between 245 °C and 270 °C; die temperature is held below 270 °C to limit gel formation in C6-LLDPE. The melt curtain crosses an air gap of 80–150 mm before contacting a chill roll maintained at 15–25 °C. On-line pre-stretch is typically 200–250% for machine film; converters monitor gauge bands across the web because die lip buildup from low-molecular-weight cling additive can create ±3 µm thickness oscillation after 2–3 h of continuous operation. On cast film lines, the limiting failure mode at high line speeds is draw resonance and web sag in the air gap. When the air gap exceeds 150 mm, film width variation can exceed ±2 mm and the cling additive may bloom unevenly. Process engineers therefore set the edge-pinning system to stabilize the edges; the melt curtain temperature at the die exit is measured by infrared pyrometry and held at 260–270 °C. The rheological response of the 1.0 g/10 min resin at typical cast-film shear rates of 100–500 s⁻¹ gives stable output on 90 mm extruders, but at output rates above 350 kg/h melt fracture may appear on the skin layer if no fluoropolymer processing aid is used. A fluoropolymer PPA masterbatch at 0.05–0.10 wt% is introduced during start-up and then reduced to maintenance level after 20–30 min. Finished terminal product types include hand-applied stretch film on 300–500 mm rolls, machine-grade film for rotating-ring wrappers, and power pre-stretched film sold as jumbo rolls for automatic pallet wrappers. The material is not recommended for unsupported food contact unless an overpack or functional barrier is present; direct food contact requires a specific migration test under Commission Regulation (EU) No 10/2011 or 21 CFR 177.1520, which is not part of the standard industrial stretch-film approval profile.

    A three-layer blown-film structure for frozen-food lamination can be run on a 400 mm die with a die gap of 1.4–2.2 mm and a blow-up ratio of 2.0–2.5. The sealant skin is formulated with 65–75 wt% Clearflex FGH 196 A, 20–30 wt% high-pressure LDPE for bubble stability, and 3–5 wt% slip-antiblock masterbatch; the core layer uses 80–90 wt% Clearflex FGH 196 A with 10–20 wt% LDPE. This structure falls under Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² and 21 CFR 177.1520 for olefin polymers, provided that all slip and antiblock additives are listed in the appropriate positive list. Converter seal curves for C6-LLDPE of similar density and melt index exhibit seal initiation between 95 °C and 105 °C at a dwell time of 0.5 s and a bar pressure of 0.3 N/mm²; below 95 °C peel strength drops below 5 N/15 mm, which is insufficient for frozen-food VFFS operation. Production experience on blown-film lines indicates that the frost line should be held at 4–8 die diameters to prevent excessive crystallinity in the sealant skin, which increases low-temperature seal brittleness. Corona treatment is set to 36–42 mN/m; surface energy above 50 mN/m causes z-axis oxidation that interferes with seal strength and can increase odor in frozen-food packaging. On VFFS lines, cold-seal pack failures occur when the sealant skin has been over-treated or when slip agent bloom saturates the sealing interface during long dwells; the slip-antiblock masterbatch should not be increased beyond 5 wt% without re-verifying hot-tack strength at 120 °C and 0.5 s dwell. Terminal product types include IQF vegetable pouches, frozen seafood bags, pre-formed side-gusset pouches, and pillow packs produced on vertical form-fill-seal lines. Regrind should be limited to 10 wt% because higher levels introduce gel specks that open pinholes in ≤40 µm sealant skins.

    When tear-propagation resistance governs gauge reduction in industrial sack webs

    Under conditions of repeated mechanical shock and side-impact compression, industrial sack webs produced on heavy-duty blown-film lines are specified less by tensile yield than by dart impact and Elmendorf tear propagation. A gauge-reduction trial on an 80 mm extruder with a 200–300 mm annular die and high-stalk bubble stability runs the resin at 75–85 wt% Clearflex FGH 196 A, 10–20 wt% high-pressure LDPE, and 3–5 wt% carbon black masterbatch for opacity and UV shielding; where post-industrial regrind is used, the recycle fraction is held below 25 wt% because higher levels reduce bubble stability and increase melt pressure fluctuation. The compliance envelope for heavy-gauge PE film includes ASTM D1709 method A for falling-dart impact, ASTM D1922 for Elmendorf tear, ASTM D882 for tensile properties, and ISO 527-3 for film and sheet tensile testing; export shipments may require EC 1907/2006 REACH declarations. Down-gauging from 180 µm to 140 µm is accepted only when the dart impact remains above 500 g and machine-direction Elmendorf tear remains above 100 g in batch release testing; if the sealant or print layer is laminated, interlaminar bond strength must exceed 2 N/15 mm after 24 h adhesive cure. The high-stalk process is run with a frost line height of 6–9 die diameters and a collapsing frame fitted with low-friction slats; excessive frost line height above 9 die diameters can induce bubble oscillation that changes film width by ±5 mm and reduces dart impact consistency. Terminal product types include heavy-duty industrial liners, non-UN bulk sacks, e-commerce mailers, and shrouds for palletized chemical bags. The material is not rated for UN dangerous goods packaging unless separately certified under the relevant UN packaging test procedure; published data for this specific configuration is limited and must be generated on the converter’s line.

    Field-aged silage cover film in continental European agriculture tends to fail by splitting along the fold creases rather than by uniform tensile yielding, which moves the resin selection criterion toward low-temperature dart impact and fold-crack resistance. In three-layer agricultural film structures, the core is typically compounded with 70–80 wt% Clearflex FGH 196 A, 15–25 wt% EVA or VLDPE in the skin layers, and 5–8 wt% hindered-amine light stabilizer masterbatch; the film is produced on blown-film lines with internal bubble cooling, a blow-up ratio of 2.5–3.0, and a layflat width in the range of 8–12 m. Compliance is assessed under EN 13206:2017 for thermoplastic covering films used in agriculture and horticulture, with mechanical properties tested under ISO 527-3. The process requires a high-stalk bubble and an upper collapsing frame with low friction to avoid transverse creasing; die lip temperature is maintained below 230 °C to protect the HALS package. Terminal product types include silage pile covers, bale-wrap covers, and greenhouse side curtains. The formulation is not recommended for multi-season greenhouse roofs in locations exceeding 140 kLy/year solar radiation unless a coextruded UV-barrier layer or increased HALS loading is validated by xenon-arc exposure to EN ISO 4892-2.

    Lamination sealant webs coextruded for solventless adhesive converting

    Because seal initiation and hot-tack strength determine converter speed on solventless adhesive lamination lines, the sealant skin is formulated with 80–90 wt% Clearflex FGH 196 A, 10–20 wt% high-pressure LDPE, and 1–2 wt% slip-antiblock masterbatch; the film is coextruded as a three-layer web on a blown-film line with a die gap of 1.5–2.0 mm and a blow-up ratio of 2.0–2.2. Compliance for food-contact lamination structures is governed by Commission Regulation (EU) No 10/2011 and 21 CFR 177.1520, with heat-seal quality tested under ASTM F2029 and seal strength measured under ASTM F88. After film production, the sealant web is corona-treated to 38–42 mN/m and laminated to PET, BOPP, or oriented nylon with a solventless adhesive coat weight of 1.5–2.0 g/m²; the converter must verify that the polyurethane adhesive cure is not inhibited by oxidized surface species formed when corona treatment exceeds 50 mN/m. Terminal product types include stand-up pouches, sachets, pillow packs for dry foods, and wet-wipe overwrap lamination. In-line delamination checks are performed after 24 h adhesive aging; a bond strength below 2 N/15 mm indicates either adhesive under-cure, excessive slip migration, or insufficient treatment below 38 mN/m. The sealant web should not be used in retort applications above 100 °C because the C6-LLDPE sealant softens and may lose pouch integrity under sustained steam pressure.

    Free Quote

    Competitive Versalis Clearflex® FGH 196 A Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FGH 196 A enters the film extrusion market as a film-grade linear low-density polyethylene positioned for blown-film and cast-film conversion where the required balance involves draw-down, dart impact retention, and machine-direction/transverse-direction tear strength. The grade is supplied in pellet form with a stabilisation package; the exact additive composition is lot-specific and must be checked on the certificate of analysis before release. The designation “FGH 196 A” contains the film-grade identifier and the approximate flow/density position: the 196 designation is used in the Clearflex range for materials that combine a density around 0.918 g/cm³ with a melt flow rate around 1.0 g/10 min. This flow class is selected by converters who need to run high-output lines without the high melt viscosity that causes excessive motor load and melt-pressure instability on extruders with L/D ratios of 24:1 or higher. In blown-film operation, the material is typically processed on single-screw extruders using barrier screws and mixing sections; in cast-film operation, it is extruded through a flat die onto chill rolls. Because the grade is a linear low-density polyethylene, it does not have the long-chain branching of low-density polyethylene, so melt strength is lower; this difference appears as reduced bubble stability at high blow-up ratios and must be controlled through die gap, air ring, and frost line adjustments.

    The “H” suffix in the Clearflex film nomenclature is commonly associated with hexene-modified chemistry in Versalis polyolefin film grades. Hexene-1 incorporation creates short-chain branches with a branch length of four carbon atoms, which alters the spatial distribution of tie molecules during quench and changes the tear/dart impact balance relative to butene-based LLDPE grades. The practical consequence is that converters can down-gauge heavy-duty sacks and industrial liners while maintaining puncture resistance, provided the film is tested according to the methods discussed below. Published data for the exact comonomer distribution of Clearflex FGH 196 A is limited; however, the property envelope and processing behaviour are consistent with a hexene-based linear low-density polyethylene film grade. A converter should verify the comonomer declaration on the technical datasheet and on the lot certificate before finalising formulation.

    Which property limits define the Clearflex FGH 196 A specification?

    The specification of Clearflex FGH 196 A is controlled by the resin manufacturer through density and melt flow rate, and by the converter through film properties measured on laboratory-scale blown film. Density is determined by immersion or gas pycnometry according to ISO 1183-1:2019 or ASTM D1505; the value is typically reported in the 0.917–0.921 g/cm³ range for base resin. The melt flow rate is determined at 190 °C under a 2.16 kg load using ISO 1133-1:2022 or ASTM D1238-20, with a typical range of 0.8–1.2 g/10 min. These two parameters define the average molecular weight and crystallinity that govern processability. A higher density would raise stiffness but reduce puncture and dart impact retention; a lower melt flow rate would improve toughness but increase extruder motor load. The following table summarises the property envelope commonly cited for Clearflex FGH 196 A in film applications. The values are not release limits and should be replaced by the certificate of analysis for the specific lot.

    PropertyTest methodTypical range/value
    Density (base resin)ISO 1183-1:2019 / ASTM D15050.917–0.921 g/cm³
    Melt flow rate (190 °C, 2.16 kg)ISO 1133-1:2022 / ASTM D1238-200.8–1.2 g/10 min
    Tensile stress at break, MDISO 527-3:2018 / ASTM D882-1834–42 MPa
    Tensile stress at break, TDISO 527-3:2018 / ASTM D882-1828–36 MPa
    Elongation at break, MDISO 527-3:2018 / ASTM D882-18800–950%
    Elongation at break, TDISO 527-3:2018 / ASTM D882-18850–1000%
    Dart impact (50 µm, Method A)ASTM D1709-22110–150 g
    Elmendorf tear, MDISO 6383-2:198360–90 N/mm
    Elmendorf tear, TDISO 6383-2:198380–120 N/mm
    Haze (50 µm)ASTM D1003-218–15%
    Gloss (60°)ASTM D2457-1350–70
    Vicat softening point (A50)ISO 306:202296–102 °C
    Melting peak temperatureISO 11357-3:2018120–126 °C

    The density range of 0.917–0.921 g/cm³ corresponds to a crystalline fraction that keeps secant modulus moderate while preserving puncture resistance. In thin films, haze values are sensitive to die gap, chill-roll finish, and antiblocking agents; a converter should not compare haze values across laboratories unless the sample preparation follows the same extrusion conditions and film thickness. The melt flow rate of 0.8–1.2 g/10 min is low enough to retain molecular weight for toughness but high enough to allow cast-film line speeds above 150 m/min on lines with a 75 mm barrier screw and a die gap of 0.5–1.0 mm. The coefficient of friction is not an inherent resin property in this grade; it is adjusted with slip and antiblock masterbatches, so film-to-seal-jaw behaviour should be evaluated according to ISO 8295:1995 or ASTM D1894-14 on the final formulation.

    On blown-film lines, the recommended starting conditions for Clearflex FGH 196 A are a temperature profile of 170–200 °C in the barrel, 200–230 °C in the adapter and die, and a melt temperature below 240 °C. A 60 mm single-screw extruder with a 30:1 L/D barrier screw and a 250 mm die can process this grade at die gaps between 1.4 mm and 2.0 mm. At blow-up ratios of 2.0:1–3.0:1, bubble stability is generally sufficient when the frost line is maintained at 6–10 die diameters; if the frost line is too low, quench stress raises the MD/TD tear ratio and may create film flatness defects. The air ring should be operated with a venturi and chilled air at 10–18 °C; the cooling-air velocity must be adjusted when ambient humidity exceeds 60% because surface condensation on the bubble leads to blocking and uneven gauge. On cast-film lines, the melt temperature is usually set between 230 °C and 250 °C, the die gap between 0.5 mm and 1.0 mm, and the primary chill-roll temperature between 18 °C and 30 °C. Higher chill-roll temperatures reduce crystallinity and improve tear retention but increase blocking tendency; the appropriate setting depends on the final film thickness and line speed. At regrind levels above 30%, the flake should be dry-surface conditioned if stored at relative humidity above 60%, because surface moisture can produce pinholes and reduce output stability. Production-scale observations show that the limiting factor in high-output operation is often melt-pressure variability rather than melt temperature; when pressure fluctuation exceeds 10% of the setpoint, gauge control deteriorates and screw speed must be reduced until the feed section is refilled.

    Published data for this specific configuration is limited for lines above 90 mm screw diameter and for dies above 450 mm; the starting points above are not a substitute for a designed experiment on the target line. A process capability study should record melt temperature before the screen changer, barrel pressures in the metering section, die pressure, and film gauge at 10-point transverse profiles. The grade does not require pre-drying of dry virgin pellets; moisture-related defects are attributed to recycled flake wetting rather than to pellet moisture. When switching from a butene LLDPE to Clearflex FGH 196 A, the line should be purged with a transitional melt-flow LLDPE or LDPE until die pressure and melt temperature return to the established setpoints; direct resin-to-resin changeover without a purge can leave incompatible melt fractions in the die lips and produce uneven film edges.

    Tear and dart impact differences versus butene LLDPE and metallocene LLDPE.

    When Clearflex FGH 196 A is compared with a butene-based LLDPE of the same melt flow rate, the most prominent differences appear in dart impact and Elmendorf tear. A butene-based LLDPE film at 50 µm commonly exhibits a dart impact of 80–120 g under ASTM D1709-22 Method A, while the Clearflex FGH 196 A envelope is shifted to 110–150 g. Elmendorf tear values in the machine direction are often 40–70 N/mm for the butene comparitor and 60–90 N/mm for the Clearflex FGH 196 A grade when measured according to ISO 6383-2:1983. The reason is not simply total comonomer content; the length and placement of short-chain branches change the tie-chain concentration formed during film quenching. Hexene-derived branches create a greater probability of stress-transmitting tie molecules across lamellae, which improves dart impact and tear resistance without a proportional increase in density. The effect is less visible in tensile yield but becomes measurable in puncture resistance tested by ASTM D5748-19.

    ParameterClearflex FGH 196 AButene LLDPE comparitorMetallocene LLDPE comparitor
    Dart impact (50 µm)110–150 g80–120 g150–250 g
    Elmendorf tear, MD/TD60–90 / 80–120 N/mm40–70 / 60–100 N/mm80–130 / 100–160 N/mm
    Haze (50 µm)8–15%12–20%2–6%
    Bubble stability on 60 mm extruderModerate-highModerateLower at same melt temperature
    Melt pressure at equivalent outputLower than metalloceneLower than metalloceneHigher, especially at high shear

    The comparison to metallocene LLDPE is equally important for film converters. Metallocene grades typically deliver dart impact values above 150 g and haze below 6% at 50 µm, but they often require higher melt temperatures and produce higher die pressure on the same screw. On a 60 mm extruder running 100 kg/h, the specific energy input can be 10–20% higher with a narrow-molecular-weight metallocene LLDPE, and the bubble is more sensitive to air-ring turbulence. Clearflex FGH 196 A is positioned between conventional butene LLDPE and metallocene LLDPE in optics and toughness; the trade-off is selected when the converter needs stable high-output bubble operation without sacrificing the dart impact gain available from hexene chemistry. Against low-density polyethylene, the grade has higher tensile stress at break and puncture resistance but lower melt strength; as a result, LDPE is often blended to increase melt strength in high blow-up-ratio lines, while FGH 196 A contributes toughness and down-gauging potential.

    Blending with LDPE at 10–20 wt% improves bubble stability and increases melt strength, but reduces dart impact and tensile strength. The blend ratio should be evaluated in a cast-film or blown-film trial; otherwise the converter risks losing the property advantage of the hexene chemistry. If optical clarity is the primary requirement, a metallocene LLDPE or LDPE-rich blend is typically used, but this shifts the tear/dart impact balance and may require a different die gap and frost line setting.

    Heavy-duty sacks and industrial liners are the main packaging applications where Clearflex FGH 196 A is evaluated. Sacks made from 80–150 µm film are typically tested for puncture resistance according to ASTM D5748-19 or ISO 7765-1:1988; the grade is selected when puncture values need to exceed those obtained with butene LLDPE at the same gauge without moving to a full metallocene formulation. Stretch-film formulations can use this grade in core layers where tear and load retention are necessary, but the surface cling and unwind force are not inherent properties and must be supplied by coextruded adhesive layers or cling masterbatches. The film can be down-gauged when the converter validates that dart impact and tear resistance remain above the end-use minimum; downgauging trials should follow a design-of-experiments protocol that records film gauge, line speed, melt temperature, die pressure, and ambient relative humidity. In agricultural film, the grade is suitable only with adequate UV stabilisation; the weathering performance should be verified by ISO 4892-2:2021 for the specific exposure and film thickness, because the base resin has no intrinsic long-term outdoor weathering resistance. Food-contact applications require confirmation that the finished packaging complies with EU Regulation (EC) No 1935/2004, Commission Regulation (EU) No 10/2011, and FDA 21 CFR 177.1520 as applicable; the converter is responsible for migration testing on the final structure, including laminating adhesives, printing inks, and recycled content. The resin should not be processed above 250 °C, because oxidative degradation leads to gel formation and surface defects. Contact with strong oxidising agents and chlorinated solvents at temperatures above 40 °C should be avoided, as swelling and loss of mechanical properties can occur.

    Incoming resin quality is usually assessed by density and melt flow rate on the pelletised lot, combined with a film screening trial when the final application is a high-tenacity sack or stretch film. The pelletised grade should be sampled according to ISO 1133-1:2022 and ISO 1183-1:2019; certificates of analysis typically report the polymerisation lot, the stabiliser package, and the nominal melt flow rate. Converters should retain a retained sample from each silo discharge and correlate it with film properties, because batch-to-batch variance in comonomer distribution can shift the MD/TD tear balance even when density and melt flow rate remain within the specification band. This variance is addressed by process adjustments, particularly screw speed and frost line height, rather than by reformulating the resin.