Versalis Clearflex Fg B3 Very Low Density Polyethylene

Versalis Clearflex® FG B3 Very Low Density Polyethylene

    • Product Name: Versalis Clearflex® FG B3 Very Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 896449
    Polymer Type Very Low Density Polyethylene (VLDPE)
    Comonomer Butene-1
    Density 0.900 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 115 °C
    Vicat Softening Temperature 75 °C
    Tensile Strength At Break 20 MPa
    Elongation At Break 700%
    Flexural Modulus 100 MPa
    Hardness Shore D 40
    Brittleness Temperature -70 °C
    Haze 10%
    Gloss 45 80%
    Dart Drop Impact 200 g
    Tear Strength Md 100 g
    Tear Strength Td 150 g

    As an accredited Versalis Clearflex® FG B3 Very Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® FG B3 Very Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Versalis Clearflex® FG B3 Very Low Density Polyethylene, shrink-wrapped for transport.
    Shipping Versalis Clearflex® FG B3 Very Low Density Polyethylene is shipped as non-hazardous thermoplastic pellets in 25 kg polyethylene bags, octabins, or bulk containers. Store and transport in dry, cool conditions away from direct sunlight, heat, and ignition sources. Follow local regulations and avoid package damage or moisture exposure.
    Storage Store Versalis Clearflex® FG B3 Very Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers sealed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Protect from UV light and prolonged high temperatures. Maintain good housekeeping and follow the manufacturer’s safety data sheet. Use appropriate personal protective equipment when handling.
    Shelf Life Shelf life typically 24 months in unopened original packaging, stored cool, dry, away from sunlight, heat, and moisture under recommended conditions.
    Application of Versalis Clearflex® FG B3 Very Low Density Polyethylene
    In vertical form-fill-seal packaging of frozen vegetables, dried soups, and flow-wrapped bakery items, Clearflex® FG B3 is coextruded as a heat-seal skin layer. The very low density polyethylene is characterised by a nominal density of 0.890 g/cm³ under ISO 1183-1 and a melt flow rate of 0.8 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. On a five-layer blown film line with 350 mm die diameter, die gap 1.8–2.2 mm, and blow-up ratio 2.2–2.8, a skin blend consisting of 70–85 wt% Clearflex® FG B3 and 15–30 wt% linear low density polyethylene with melt index 1.0 g/10 min provides a seal initiation temperature in the 75–88 °C band measured by ASTM F1921. Bubble stability is maintained by an internal high density polyethylene or polypropylene core that supplies room-temperature stiffness and limits elongation under low tensile load. A typical three-layer structure places the FG B3-based skin at 12–20 µm of a 55–75 µm total thickness, with the core at 25–35 µm. Frozen food converters require seal integrity after exposure to −25 °C; the low glass-transition behaviour of the grade reduces seal cracking at fold zones. European food contact compliance is assessed under EU No 10/2011 with an overall migration limit of 10 mg/dm², and US applications fall under 21 CFR 177.1520(c) for olefin polymers used at temperatures up to 100 °C. The operational boundary in this segment is explicit: extrusion of a monolayer FG B3 blown film at blow-up ratio above 2.8 typically produces visible bubble flutter and gauge variation, so the grade is not recommended for unsupported blown structures.

    What Changes When Seal Initiation Falls Below 85 °C on Metallised PET Laminates?

    Flat-die extrusion coating and lamination lines use Clearflex® FG B3 as a sealant web on metallised polyethylene terephthalate and aluminium foil. In this configuration the polymer is plasticated in a single-screw extruder with L/D 30:1–36:1, and the melt is delivered through a coat-hanger die at 250–280 °C. The air gap is held at 150–250 mm and the chill roll temperature is maintained at 10–20 °C; these settings allow a 10–18 g/m² coating weight at line speeds from 120–250 m/min. Neat FG B3 draws poorly above 200 m/min because of low melt elasticity, and converters routinely blend 20–40 wt% of a high-pressure LDPE with melt index 4–8 g/10 min to suppress edge neck-in and draw resonance. The resulting sealant layer reaches a seal initiation temperature of 78–86 °C, which permits sealing through oriented polyester without distorting the metallised barrier. Peel adhesion on primed aluminium foil is measured under ASTM D903; published data for this specific FG B3 configuration is limited, but corroborating lamination trials with very low density polyethylene copolymers indicate cohesive failure in the sealant layer rather than adhesive failure at the metal interface when corona treatment reaches 44–48 mN/m. End-use formats include lidding films for dairy cups and single-serve instant beverage sachets. The principal incompatibility is with unprimed aluminium foil: below 40 mN/m surface energy, adhesion is insufficient for retort handling. In addition, residence time above 290 °C should not exceed 15 min to avoid gel formation in the polymer melt.

    Stretch Hood Film Elastic Recovery and Puncture Mechanics

    Unlike cast stretch film, stretch hood conversion uses blown film and relies on recovery force rather than cling additives. Clearflex® FG B3 is allocated to the outer layers of a three-layer stretch hood film with total thickness 40–70 µm. The preferred structure places 50–70 wt% FG B3 in the skins and a core layer composed of linear low density polyethylene or a LLDPE/HDPE blend. Blown film extrusion is performed at a die gap of 1.8–2.6 mm, blow-up ratio 3.0–3.8, and melt temperature 200–225 °C, which develops transverse orientation and recovery force. Laboratory characterisation under ASTM D5459 for machine-direction elastic recovery and ASTM D5748 for puncture resistance indicates that VLDPE-rich skins increase energy absorption before rupture. The nominal 0.890 g/cm³ density reduces film stiffness and improves conformity to palletised goods with sharp corners. The core layer must be designed for creep resistance: at 23 °C and 50% relative humidity, high-VLDPE monolayers show permanent set above 20% after 100% elongation, which is unacceptable for A-grade pallet loads. Converters therefore maintain total FG B3 content between 35–55 wt% and add HDPE up to 15 wt% in the core. The operational limit is bubble stability; increasing VLDPE content above 70 wt% in the skin layers at blow-up ratio 3.2 commonly produces helical instability on three-layer dies unless line speed is reduced below 40 m/min. Final stretch hood films are tested for tear propagation under ASTM D1922, and Elmendorf tear values in the machine direction are typically 2–5 N for 50 µm film, while transverse direction values are higher.Halogen-free flame-retardant cable jacket compounds historically relied on ethylene-vinyl acetate copolymers for filler acceptance and flexibility. Clearflex® FG B3 is evaluated as a very low density polyethylene alternative in insulation compounds for IEC 60332-1-2 single-flame cable tests. The key performance requirement is a limiting oxygen index of 32–35% under ISO 4589-2 and extinction after flame withdrawal. This is achieved by loading the matrix with 150–170 phr aluminium trihydrate and 20–40 phr magnesium dihydrate; a vinylsilane coupling agent at 0.5–1.0 wt% and a hindered phenolic antioxidant at 0.2–0.5 wt% are included to limit hydrolysis and thermo-oxidative chain scission. Compounding is performed on a co-rotating twin-screw extruder with L/D 44:1, screw speed 250–350 min−1, and barrel profile 140–180 °C, with side-feeding of filler after the first mixing zone. Because the base polymer has a melt flow rate of 0.8 g/10 min, the final compound shows an MFR reduction to 0.15–0.30 g/10 min at 190 °C/2.16 kg, which limits extrusion tooling to pressure-controlled crossheads and melt temperatures below 165 °C. The technical advantage over ethylene-vinyl acetate is reduced smoke density and improved ageing performance at 110 °C. Moisture introduced by aluminium trihydrate is an operational hazard: if stored above 60% relative humidity, the compound must be pre-dried at 60 °C for 2 h before profile extrusion to avoid surface porosity. This segment is governed by cable standards IEC 60332-1-2, IEC 60754-1, and IEC 60754-2, with documentation of halogen acid gas content and pH. Use of FG B3 alone without compatibiliser at filler loadings above 170 phr leads to tensile elongation below 150% and is not recommended for flexible cable jacketing.

    When Colour Masterbatch Carriers Require Low-Temperature Compounding Without Viscosity Build-Up

    Additive masterbatch producers select Clearflex® FG B3 as a carrier resin for heat-sensitive organic pigments and foaming agents because the low melting peak permits twin-screw compounding at 140–170 °C. The polymer is fed into a co-rotating twin-screw extruder with L/D 40:1, and the pigment is added after the melting section through a side feeder at 30–50 wt% loading. Due to the 0.890 g/cm³ density, the carrier introduces 8–12% lower specific gravity than a comparable ethylene-vinyl acetate carrier, which changes dosing volumes on injection moulding machines but reduces weight per cubic metre of finished compound. The melt flow rate of 0.8 g/10 min permits let-down ratios from 2–5% in polyolefin films. Thermal stability testing under ISO 11358-1 is used to verify that organic yellow and red pigments do not degrade during residence times up to 120 s. The grade is also used as a carrier for chemical blowing agents in polyethylene foam extrusion, where processing temperatures must remain below 160 °C to prevent premature gas release. The limitation is mechanical: masterbatches based solely on FG B3 exhibit low pellet hardness and may deform in silo storage above 40 °C; converters mitigate this by blending 20–30 wt% of a high density polyethylene with melt index 4–7 g/10 min or by adding 5–10 wt% of a high-hardness wax. No food contact certification applies to the masterbatch itself; the final article must be evaluated on its own, and migration of the pigment from the carrier into food simulants is tested under EU No 10/2011 with simulant D2 for vegetable oil.Because low-temperature sealability governs medical pouch integrity, Clearflex® FG B3 is coextruded as an inner seal layer in flexible healthcare packaging. Film conversion for sterile barrier pouches is carried out on cleanroom blown film lines with die gap 1.6–2.0 mm, blow-up ratio 2.0–2.4, and melt temperature 190–210 °C. The sealant layer is typically blended with a metallocene linear low density polyethylene at 20–40 wt% to raise hot-tack strength under ASTM F1921 while retaining a seal initiation temperature below 85 °C. Seal strength is verified on finished pouches under ASTM F88 after ethylene oxide sterilisation at 55 °C and vacuum hold. The packaging is assessed within a sterile barrier system according to ISO 11607-1, and physical testing of seal continuity follows ASTM F1929 for dye penetration. The low-density polyethylene sealant reduces fibre tear on Tyvek-to-film peel opening, but the surface must be corona-treated to 42–46 mN/m before printing or lamination. Gamma irradiation is a recognised boundary condition: published data for VLDPE sealants indicates that absorbed doses above 25 kGy can increase crosslink density and reduce seal strength on subsequent peel testing, so validation is required for radiation-sterilised formats. The final film must also satisfy bio-compatibility evaluation according to ISO 10993-5 when contact with the medical device surface is intended.
    Compliance areaStandard or regulationKey test or limit
    European food contactEU No 10/2011Overall migration limit 10 mg/dm²; simulant D2 for fatty foods
    US food contact21 CFR 177.1520(c)Olefin polymers for use up to 100 °C
    Heat seal performanceASTM F1921Hot-tack window 75–88 °C
    Film tensile behaviourISO 527-3Strain at break measured at 500 mm/min
    Dart drop impactASTM D1709Method A for 50 µm blown film
    REACH SVHC declarationEC No 1907/2006, Article 33SVHC content below 0.1 wt%
    RoHS Recast2011/65/EU, Annex IIRestricted substances below maximum concentration values
    Free Quote

    Competitive Versalis Clearflex® FG B3 Very Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FG B3 is classified as a very low density polyethylene (VLDPE) copolymer supplied as pelletized feedstock for mono- and coextruded film structures. The producer’s technical datasheet identifies the nominal density as 0.900 g/cm³ when tested according to ISO 1183-1, and the melt mass-flow rate as 0.9 g/10 min when tested according to ISO 1133-1:2022 at 190°C under a load of 2.16 kg. Unlike conventional autoclave low density polyethylene with density above 0.918 g/cm³, the reduced density derives from alpha-olefin comonomer placement along the ethylene backbone. The resulting low crystalline fraction suppresses the elastic modulus and melting endotherm, which permits the grade to be used as a sealant layer in flexible packaging where the seal bar must develop molecular interdiffusion at low temperatures and short dwell times. Target applications include coextruded food packaging, lamination film sealant webs, and heavy-duty film where abuse resistance and seal integrity are specified together. The grade differs from conventional film-grade LLDPE by lower density, lower seal initiation temperature, and reduced stiffness, while it differs from EVA-based sealants by replacing vinyl acetate comonomer with an olefinic architecture that avoids acetic acid handling concerns.

    Published resin specification data and applicable test standards
    PropertyTest methodNominal value
    DensityISO 1183-10.900 g/cm³
    Melt mass-flow rateISO 1133-1:2022 at 190°C / 2.16 kg0.9 g/10 min
    Melting endotherm peakISO 11357-3below 110°C
    Food-contact monomer statusEU No 10/2011 / FDA 21 CFR 177.1520finished-article compliance assessment required

    Because the low density depresses the crystalline fraction, the resin exhibits lower secant modulus measured at 1% strain by ISO 527-3 on cast film than a conventional 0.918 g/cm³ LLDPE. The modulus reduction is an intended trade-off: it provides conformability around sharp package corners and reduces spring-back force in collation films, but it also demands higher gauge when replacing a stiffer LLDPE in a load-bearing application. Mechanical properties must be compared on finished film rather than resin-only tensile data because film drawing produces anisotropic orientation, and the producer’s published resin datasheet is not a replacement for converted-film validation.

    Which low-temperature sealing envelope separates FG B3 from EVA and standard LLDPE?

    Heat-seal initiation in semicrystalline polyolefins is governed by the crystalline melting range rather than by a single melting point. In a 0.900 g/cm³ VLDPE, the melting endotherm measured by ISO 11357-3 is shifted downward relative to a 0.918 g/cm³ LLDPE; practical flat-jaw seal curves generated to ASTM F2029 therefore show onset of measurable seal strength in the 85–95°C interval. Seal strength continues to rise as jaw temperature increases until the failure mode changes from interfacial peel to elongation of the adjacent oriented substrate, and values of 15–25 N/15 mm are typical for coextruded polyester/PE or oriented polypropylene/PE laminates tested to ASTM F88. Ethylene-vinyl acetate copolymers with 9–12 wt% vinyl acetate can initiate sealing below 80°C, but the vinyl acetate comonomer contributes acetic acid odor, reduces thermal stability during extrusion hold times, and can corrode unlined processing equipment. Clearflex® FG B3 does not rely on vinyl acetate for low-temperature sealing; however, its lower crystalline fraction also delays recrystallization at the seal nip, so hot-tack strength is more dependent on sealing-jaw pressure and cooling capacity than would be the case with a higher density linear polyethylene.

    Hot tack is the seal’s ability to hold stress during the molten or semicrystalline state immediately after the sealing jaw opens. Measurement according to ASTM F1921 on a VLDPE skin layer typically shows a narrower peak than high-density polyethylene at identical film thickness because the low crystalline fraction retards crystal development. The practical consequence is that packaging machines with short cooling times may require higher jaw release temperatures or reduced web tension to prevent seal elongation and leaker formation.

    Pellet pre-drying is not required at warehouse relative humidity below 60%; the base resin is not hygroscopic, but condensation on cold pellets transferred from unheated silos can introduce surface water that generates pin-holes in thin-gauge cast film. Cast-film converters running monolayer or coextrusion lines typically use barrier screws with 30:1 length-to-diameter ratio and barrel zone profiles that rise from 180°C near the feed throat to 240°C at the metering zone. Maintaining the die adapter at 230–245°C helps balance melt temperature and viscosity, but sustained melt pressure above 350 bar at the breaker plate indicates excessive shear heating. Because the grade has a melt flow rate of 0.9 g/10 min, it is more viscous than conventional cast-film LLDPE grades in the 2.0–3.5 g/10 min range, so high-output lines may require an increase in set-point temperature at the feed-compression section or a reduction in screw speed to avoid unmelted pellet carryover. Screen packs of 80/100/80 mesh are used to protect flat dies from contamination, with replacement intervals based on pressure differential. Chill-roll temperatures between 15°C and 30°C are applied to remove sensible heat and control crystal growth; winder blocking occurs when the film core temperature exceeds the storage limit, and in that case roll hardness should be reduced rather than adding migratory slip at levels that could impair seal strength. For blown-film operation, a blow-up ratio of 2.0:1 to 2.8:1 and a high frost line are typical to compensate for lower melt strength relative to long-chain branched LDPE.

    Capillary rheometry according to ISO 11443 at 190°C shows shear-thinning behavior across film die shear rates from 10 s⁻¹ to 10 000 s⁻¹. The higher molecular weight implied by the 0.9 g/10 min MFR increases low-shear viscosity relative to an MFR 2.0 g/10 min cast-film LLDPE, which may increase extruder torque and melt temperature. In blown-film lines, the same characteristic supports bubble stability at low melt pressure but does not replace the strain-hardening behavior of long-chain branched LDPE. Converters using grooved-feed extruders with 30:1 L/D should monitor drive amperage during grade changes; a change to this VLDPE from a high-MFR LLDPE can require a temporary screw-speed reduction of 10–20% to avoid motor overload. Low crystallinity also retards crystal growth during cooling, and on a differential scanning calorimetry cooling run at 10°C/min per ISO 11357-3, the crystallization peak is broad and shifted to lower temperatures, meaning the film remains tacky longer after the chill roll. The practical consequence is that roll hardness must be controlled; film wound too tightly can develop blocking, and the phenomenon worsens when ambient storage temperature exceeds 30°C.

    Coex sealant-layer performance and puncture-related failure boundaries

    In three-layer and five-layer coextruded structures, Clearflex® FG B3 is usually assigned to the sealant skin because its low crystallinity reduces stiffness and allows the seal bar to conform to package wrinkles. The same low crystallinity, however, lowers tensile modulus and can reduce film rigidity when the grade is used as a structural core layer; coextrusion with an HDPE or PP layer is therefore preferred for packages that require deadfold or dimensional stability. Puncture resistance in VLDPE film is measured by ASTM D5748 or ISO 7765-2 depending on final film thickness, and the chain architecture of a 0.900 g/cm³ resin generally produces higher slow-puncture elongation than low density polyethylene of similar melt index. In frozen-food packaging, the combination of sub-zero toughness and low seal initiation reduces leaker rates when the seal is formed through residual ice or flour contamination; however, the operational boundary is process hygiene rather than resin limitation because particulate contamination at the seal lip remains a direct cause of channel leakers. For applications that require hot-fill or retort conditions, published data for this specific configuration is limited, and the converter should validate seal creep resistance and organoleptic migration under the actual time-temperature profile.

    When FG B3 is diluted with HDPE or LDPE, haze and hot tack do not respond linearly

    Blending this grade with high-density polyethylene is a common route to increase stiffness and reduce blocking in high-speed horizontal form-fill-seal lines. The relationship between HDPE content and property response is nonlinear: additions below 20 wt% typically raise tensile modulus and reduce seal strength only modestly, while additions above 30 wt% can shift seal-initiation temperature upward by more than 10°C and create seal-platen sticking. Because HDPE crystallizes rapidly, the blend morphology consists of dispersed high-crystallinity domains in a low-crystallinity VLDPE matrix, and the resulting hot-tack curve can exhibit a plateau rather than a monotonic rise. Usage of concentrated masterbatches with slip and antiblock additives should be controlled by total film surface additive concentration; excess erucamide migration above 800–1000 ppm in the skin layer can depress seal strength and create haze after storage. If the grade is blended with autoclave LDPE to improve bubble stability on blown lines, the density of the blend shifts above 0.900 g/cm³ and the melting endotherm broadens, reducing the low-temperature sealing advantage proportionally to LDPE mass fraction. Therefore, when low seal-initiation temperature is the controlling design requirement, the grade should not be heavily diluted with higher density polyethylene unless the seal specification has sufficient margin.

    For food-contact compliance, the resin is positioned within the polyolefin regulatory framework. The overall migration limit of 10 mg/dm² under EU Regulation (EU) No 10/2011 applies to finished articles after conversion, and the composition must be evaluated under the conditions described in Regulation (EC) No 1935/2004. In the United States, olefin polymers used in contact with food may be evaluated under FDA 21 CFR 177.1520, with specific end-use extraction temperatures and food simulants determining the applicable migration bounds. The supplier’s compliance statement should be consulted before converting the resin into packaging intended for fatty foods, alcohol-containing liquids, or hot-fill conditions, because those exposures alter the effective migration testing protocol. REACH registration under EC 1907/2006 is handled by the manufacturer; downstream converters retain obligations for intentional additives and printing inks introduced after pellet extrusion. The resin should not be combined with free-radical generators or pro-degradant additives unless the target application requires reduced molecular weight, because such additives alter melt flow rate and can compromise extrusion consistency. Outdoor exposure of unpigmented film leads to photo-oxidative embrittlement unless UV stabilization is included; carbon black and hindered amine light stabilizer concentrates should be dispersed at the converter’s usual let-down ratios to maintain film integrity.

    Regulatory assessment matrix for finished articles
    Regulation / standardScopeApplication condition to verify
    EU Regulation (EU) No 10/2011Plastic materials and articles intended to come into contact with foodOverall migration limit 10 mg/dm²
    FDA 21 CFR 177.1520Olefin polymersFood type and extraction temperature
    REACH 1907/2006Registration of substance in the EUDownstream intentional additives

    Application-specific validation under the intended packaging line remains the primary control.

    Top