| HS Code | 394423 |
| Product Name | Versalis Clearflex FG B0 Very Low Density Polyethylene |
| Manufacturer | Versalis |
| Polymer Type | Very Low Density Polyethylene (VLDPE) |
| Comonomer | Butene-1 |
| Density | 0.900 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Point | 115 °C |
| Vicat Softening Point | 80 °C |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Shore D Hardness | 45 |
| Haze | 10% |
| Gloss | 85 |
| Dart Drop Impact | 300 g |
| Seal Initiation Temperature | 90 °C |
As an accredited Versalis Clearflex® FG B0 Very Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex® FG B0 is supplied in 25 kg polyethylene bags, palletized; 1,000 kg bulk bags are also available. |
| Container Loading (20′ FCL) | Versalis Clearflex® FG B0 VLDPE is supplied in 25 kg bags, palletized and shrink-wrapped, for loading into 20′ FCL containers. |
| Shipping | Versalis Clearflex® FG B0 Very Low Density Polyethylene is a non-hazardous thermoplastic resin, typically shipped as free-flowing pellets in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk octabins/trucks. Transport in clean, dry conditions, away from direct sunlight, heat, moisture, and contamination. Ensure containers remain sealed and labeled. |
| Storage | Store Versalis Clearflex® FG B0 Very Low Density Polyethylene in original, sealed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, ignition sources, and oxidizing agents. Keep away from strong odors and contaminants. Stack pallets safely to prevent deformation. Maintain clean handling areas and follow local regulations for polymer storage. Keep bags closed until use. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored in original packaging, cool, dry, away from direct sunlight. |
Cast pallet stretch film can be produced with Clearflex® FG B0 as a partial replacement for a linear low density polyethylene carrier resin. The grade has a nominal density of 0.900 g/cm³ under ISO 1183-1 and a nominal melt flow rate of 1.0 g/10 min under ISO 1133-1:2022 at 190°C and 2.16 kg. Typical let-down on slot die lines ranges from 20 wt% to 35 wt% in the core layer of a two-layer or three-layer structure. A 90 mm single-screw extruder with a 32:1 L/D barrier screw and a 3.5 m slot die is usually zoned from 190°C near the feed throat to 260°C at the die adapter. Melt temperature at the die lip is held between 240°C and 255°C. If the melt drops below 230°C, the low-melt-tension curtain becomes sensitive to air-knife oscillation and forms transverse gauge bands at line speeds above 450 m/min. If the melt exceeds 265°C, oxidative degradation increases gel counts above 300 µm and the cling additive can volatilize. The chill roll surface is maintained at 22–28°C; lower surface temperatures below 18°C increase surface haze and reduce transverse tear resistance measured under ASTM D1922. Stretch wrap tensile set after 200% elongation is screened with ASTM D5459, puncture resistance with ASTM D5748, and film toughness with ASTM D882. Cling is not covered by an equivalent ISO or ASTM method; converters use tilt-table peel fixtures at 23°C and 50% RH with a controlled wrap tension. Blocking becomes severe when FG B0 exceeds 35 wt%, especially at roll storage temperatures above 35°C and winding pressures above 0.35 MPa. Finished rolls are typically wound at 12–18 N/m web tension to limit telescoping without embossing the low-modulus surface. Published stretch film data for this exact grade at 300% pre-stretch is limited; the operating window above reflects production practice for VLDPE grades with density near 0.900 g/cm³ rather than a single laboratory study.
Blown film lines producing stand-up pouch sealant layers place Clearflex® FG B0 in the inner web at 100 wt% or as a 30–50 wt% blend with a 0.916–0.918 g/cm³ metallocene C6-LLDPE. The sealant layer is coextruded against high-density polyethylene or oriented polyamide structural layers in a 3.2 m die with a 1.8 mm lip gap. Bubble geometry is limited by the low melt strength of the grade; blow-up ratios above 3.0 tend to destabilize the frost line unless internal bubble cooling and a high-stalk configuration are used. Frost line height is kept at 4–6 die diameters to balance quench rate and film clarity. Heat-seal performance is measured on 25 mm strips using ASTM F2029 with 0.275 MPa jaw pressure and 0.5 s dwell. A typical seal initiation temperature for a 30 µm sealant layer containing FG B0 falls between 88°C and 96°C, which is roughly 5–10°C below a comparable 0.918 g/cm³ C6-LLDPE sealant. Hot-tack strength is evaluated with ASTM F1921 at 0.5 s cooling time and 0.2 N/mm peel load, while seal strength is reported under ASTM F88 with a 300 mm/min crosshead speed. The lower density and higher comonomer content reduce the degree of crystallinity, but they also lower Vicat softening point, so the pouch cannot be hot-filled above 70°C without seal creep. Coextruded pouches with this sealant are used for frozen food, liquid condiment sachets, and stand-up snack packaging. Published comparative data for FG B0 against specific metallocene grades is limited; the seal-initiation delta above is typical for VLDPE sealants with density near 0.900 g/cm³ and should be confirmed by a sealing curve on the production line.
| Regulatory framework | Applicable requirement | Test or limit |
| EU food contact plastics | EU Regulation 10/2011 | Overall migration limit 10 mg/dm²; methods EN 1186-1, EN 13130-1 |
| US food contact | FDA 21 CFR 177.1520 | Olefin polymer specification; end-use testing applies |
| Good manufacturing practice | EC 2023/2006 | Food-contact manufacturing hygiene and documentation |
| Packaging heavy metals | EU Directive 94/62/EC | Sum of Pb, Cd, Hg, Cr(VI) ≤ 100 mg/kg |
| Medical device biocompatibility | ISO 10993-1 | Finished device testing required; raw polymer compliance alone is not sufficient |
| REACH | EC 1907/2006 | Candidate list SVHC ≤ 0.1% w/w; supplier confirmation required |
On woven polypropylene coating lines for flexible intermediate bulk containers, Clearflex® FG B0 can be used in the top sealing layer when it is blended with 20–30 wt% extrusion-coating LDPE. The VLDPE alone has insufficient melt tension across a 900 mm slot die, and neck-in becomes unmanageable at an air gap above 150 mm. A typical coating line uses a 120 mm single screw with a 30:1 L/D screw, a 1.6 mm die gap, and an air gap of 150–250 mm. Melt temperatures at the die are held between 285°C and 305°C. The high temperature promotes surface oxidation and adhesion to the corona-treated woven polypropylene fabric, but it also degrades the low-density component if residence time exceeds 15 min. Line speed is normally 100–180 m/min, with the chill roll at 15–20°C to freeze the melt curtain before orientation can relax. Peel adhesion between the polyethylene coating and the woven tape is tested under ISO 8510-1; values between 2.0 N/15 mm and 4.0 N/15 mm are generally accepted for FIBC seams, while adhesion below 1.5 N/15 mm risks delamination during filling. Because FG B0 has a low coefficient of friction at the coating surface, the finished fabric may require a slip agent in the outside layer to maintain handling on sack-stitching equipment. Coating weight is typically 20–30 g/m² for valve bags and 50–80 g/m² for FIBC inner liners. Published peel strength data for this specific grade on PP woven fabric is limited; the cited acceptance band is converter-specific and should be verified with a production trial.
Flexible medical liquid pouch film is a downstream segment where Clearflex® FG B0 can be used as the skin or seal layer in a polyolefin replacement for plasticized PVC. The film is produced on a cleanroom cast coextrusion line with a 1.5 m slot die and a 30:1 L/D screw. Melt temperatures are kept between 210°C and 240°C to limit additive degradation. The grade is blended with polyolefin elastomer or metallocene C8-LLDPE at 20–40 wt% in the sealant skin to reduce flexural modulus and prevent flex-crack failure at the pouch corner. Tensile properties are measured under ISO 527-3 on 15 mm wide strips. A film thickness of 150–250 µm is typical for liquid pouch applications. The heat-seal process is a two-side heated bar at 130–150°C for 1.5–2.5 s, and seal strength is verified with ASTM F88. The material does not contain ortho-phthalate plasticizers, so migration of plasticizer into the contained liquid is eliminated. Raw-material food-contact status is governed by FDA 21 CFR 177.1520 and EU Regulation 10/2011, while device-level biocompatibility is assessed on the finished pouch under ISO 10993-1. Steam sterilization at 121°C is outside the thermal resistance of this grade; the structure is more compatible with gamma or electron-beam sterilization at doses below 50 kGy, subject to oxidation control. Published data for FG B0 in Class II medical device pouch films is limited because medical film qualifications are proprietary. The grade should not be used where the pouch requires continuous service above 60°C or where the contained fluid is a strong oxidizing solution.
Three-layer agricultural silage film can incorporate Clearflex® FG B0 in the core layer at 10–30 wt% to improve impact resistance at low storage temperatures. The film is produced on a 2.5 m blown die with 2.2 mm lip gap and a blow-up ratio of 2.3–2.7. Melt temperature is held between 210°C and 230°C to retain the hindered amine light stabilizer package. The outer skins are formulated with a 0.918–0.924 g/cm³ LLDPE and carbon black or titanium dioxide to limit ultraviolet degradation. Dart impact is measured under ISO 7765-1 on 150 µm film; transverse tear resistance is measured under ISO 6383-1. The low-density core depresses the film flexural stiffness, which reduces stress concentration at the bale wrap edges where punctures from straw stems occur. At ambient temperature below 5°C, a film containing FG B0 in the core shows lower crack propagation than a standard 0.920 g/cm³ LLDPE control, although published grade-specific data is limited. Silage film mechanical requirements are specified in EN 13206. The film must be removed from the bale before ensiling is complete; the polyethylene is not biodegradable and can contaminate silage if shredded. Because the grade has a relatively low Vicat temperature, it is not suitable for greenhouse film exposed to sustained surface temperatures above 70°C in contact with metal profiles. UV and thermal stabilizer concentration must be increased when the film is used in sun-exposed applications longer than 12 months.
Frozen food packaging lines for vegetables, seafood, and portioned meat use Clearflex® FG B0 in the inner sealant layer of a three-layer or five-layer blown film. The seal layer is typically a 40–60 wt% blend of FG B0 with 0.916–0.920 g/cm³ C6-LLDPE, laid down at 15–20 µm in a total film thickness of 40–70 µm. The die is run at a 2.0 mm lip gap and a blow-up ratio of 2.2–2.6. Melt temperature is kept between 215°C and 230°C to prevent degradation of the heat-seal additives. Seals are made on a vertical form-fill-seal machine at 120–140°C with dwell times of 0.8–1.2 s. Seal strength is measured under ASTM F88 at 23°C and -20°C; the low-temperature value is the critical acceptance criterion because seals can fail by brittle fracture during handling in cold storage. The low density of FG B0 reduces the seal layer modulus and shifts the ductile-to-brittle transition to lower temperatures. Puncture resistance is screened by ASTM D5748 on flat film and by a filled-bag drop test at -18°C. The film structure must also maintain machine-direction modulus for high-speed web transport; if the FG B0 content is too high, the film exhibits lower tensile modulus under ASTM D882 and may wrinkle in the forming collar. A common correction is to add a high-density polyethylene core layer at 20–30 wt% to restore stiffness. Published data for FG B0 in frozen food structures is limited; the starting formulations given here are typical for VLDPE sealant grades with density near 0.900 g/cm³ and require production-line validation.
When post-consumer HDPE regrind is pelletized for transport packaging, Clearflex® FG B0 can be added at 5–15 wt% to restore some of the low-temperature impact lost after multiple heat histories. The two materials are dry-blended and then melt-compounded on a 75 mm co-rotating twin-screw extruder with a 36:1 L/D ratio and a strand pelletizing head. Barrel temperatures are set from 180°C in the feed zone to 220°C at the die plate, with screw speed at 400–600 rpm and throughput adjusted to maintain a melt temperature below 230°C. Charpy notched impact strength of the injection-moulded blend is measured under ISO 179-1 at -20°C, and tensile modulus is measured under ISO 527-2. The low-density component reduces flexural modulus by approximately 5–15% at the 15 wt% loading, which may be unacceptable in load-bearing rib designs. Injection moulding trials use a 1800 kN clamp force machine with a general-purpose screw and a cold runner; mould temperature is held at 20–40°C. The grade should not be added to mixed PP/HDPE regrind streams above 10 wt% because phase incompatibility with the polypropylene fraction can delaminate at knit lines. Published data for this exact grade in post-consumer HDPE regrind is limited; loading levels above are starting points derived from VLDPE impact-modification practice and must be confirmed on the target regrind batch.
Competitive Versalis Clearflex® FG B0 Very Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® FG B0 Very Low Density Polyethylene is a pelletized very low density ethylene copolymer intended for cast and blown film extrusion. The supplier’s published technical bulletin identifies a nominal density of 0.900 g/cm³ when tested according to ISO 1183-1 and a melt mass-flow rate of 0.80 g/10 min determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. Because the density is below the conventional linear low-density polyethylene range of 0.915–0.930 g/cm³, the resin has a lower crystalline weight fraction, a broader melting endotherm, and a more pronounced transition between elastic and plastic deformation in oriented film. These characteristics position the grade for sealing layers, stretch wrap, and flexible food-packaging structures where high elongation and progressive yielding are more important than stiffness.
In cast-film extrusion, the resin is normally run at melt temperatures of 180–210 °C, with the die lip held at the upper end of the range to reduce draw resonance. Blown-film lines typically require a die gap of 1.2–2.5 mm and a blow-up ratio between 2.0:1 and 3.5:1. At blow-up ratios above 3.5:1, bubble instability may develop because the lower crystallinity reduces melt tension. The melt is more shear-thinning than a conventional LDPE of density 0.923 g/cm³, which reduces screw torque at high screw speed but also reduces pressure sensitivity at the die. Processors on 30 L/D single-screw extruders observe that melt pressure is more dependent on die gap and output than on barrel temperature once the melt reaches 190 °C. Published data for this specific configuration is limited, so start-up should use a fixed die gap with output ramped in 10 % increments until internal bubble cooling stabilizes the frost line.
The shear-thinning behavior also means that energy input is dominated by motor screw speed rather than barrel set-point alone. On a 55 mm extruder with 30 L/D and a general-purpose barrier screw, screw speeds of 80–120 min⁻¹ are common for achieving a stable melt quality, but the actual operating envelope should be established by measuring melt temperature with a retractable immersion thermocouple rather than by relying on barrel set-points. Because the resin has a low density and limited thermal conductivity, a high-compression screw can generate local temperatures exceeding the set-point by 10–20 °C. In that case, the feed zone should be cooled and the compression ratio reduced to avoid gel formation.
Residence time above 230 °C should be kept below 10 min to limit thermal oxidation and gel formation. After storage at relative humidity above 60 %, predrying at 70–80 °C for 2–3 h is advisable because surface moisture can produce bubble pinholes and melt voids. Erucamide-based slip masterbatches are compatible at concentrations up to 1000 ppm; beyond this level, chill-roll plate-out may become visible on cast-film lines. For blown-film lines with internal bubble cooling, the frost line height is normally positioned between 1.5 and 3.0 die diameters. A high frost line combined with a low blow-up ratio increases transverse tensile strength but reduces impact. If the bubble oscillates during start-up, the first corrective action is to lower melt temperature by 5–10 °C and increase the die gap by 0.2–0.5 mm, because the low melt strength makes the bubble sensitive to high shear at the lip. A dual-lip air ring with a chilled lower lip is preferred for thickness uniformity.
Table 1 consolidates representative values from the supplier’s technical bulletin and equivalent converted film measurements. The values are not lot-specific guarantees; the certificate of analysis for the specific pellet lot governs production release. Mechanical data on film are influenced by gauge uniformity, draw ratio, and cooling rate, and therefore should be compared only under identical sample preparation.
| Property | Test method | Representative value |
|---|---|---|
| Nominal density | ISO 1183-1 | 0.900 g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 | 0.80 g/10 min at 190 °C / 2.16 kg |
| Melting peak | ISO 11357-3 | 117 °C |
| Vicat softening temperature | ISO 306 | 91 °C |
| Tensile yield stress, 25 µm cast film | ISO 527-3 | 7.0 MPa |
| Tensile elongation at break | ISO 527-3 | 700–800 % |
Optical performance is generally evaluated after film conditioning for 48 h at 23 °C and 50 % relative humidity. The low crystalline fraction reduces haze in thick gauges but can increase surface tack; therefore, an antiblock masterbatch based on synthetic silica or talc is used in the range of 500–1500 ppm. Excessive antiblock above 2000 ppm creates visible microdefects at film thicknesses below 25 µm and reduces dart impact. In coextruded structures, the additive is normally confined to the skin layer to preserve internal optics.
Heat-seal initiation in this resin is controlled by the low-temperature fraction of the melting distribution. Because the grade has a density of 0.900 g/cm³, its crystal lamellae are thinner than those of a typical LLDPE of 0.918 g/cm³, allowing fusion to begin at lower seal-bar temperatures. In a coextruded structure with a sealing layer of this product, the onset of a 4 N/15 mm seal strength may be observed near 85–95 °C on laboratory gradient sealers; the exact value depends on film gauge, dwell time, and sealing pressure. This temperature offset relative to LDPE is used to shorten dwell times or to reduce heat input on packaging machines with induction seal jaws.
The same low-density characteristic reduces hot tack onset but narrows the plateau between seal initiation and film distortion. At seal-bar temperatures above 120 °C, the sealing layer can thin and become prone to unoriented flow. This is the limiting factor in polyethylene-only laminates that are sealed through a polyester or oriented polyamide face stock. Seal strengths should be evaluated according to ASTM F88/F88M-21 for finished pouches and ISO 527-3 for film tensile properties. Users converting from EVA sealing layers should re-verify caulk depth and dwell time because the absence of vinyl acetate reduces low-temperature caulkability but improves organoleptic neutrality.
To establish a robust seal window on a vertical form-fill-seal machine, sealing temperature should be mapped in 5 °C increments over a dwell time range of 20–50 ms. The lower plateau of seal strength is determined by the resin, but the upper plateau is determined by the face stock and the jaw pressure profile. A seal strength of 4 N/15 mm is frequently used as the acceptance threshold in packaging specifications. Below the initiation temperature, hot tack failure occurs because chain interdiffusion across the seal interface is incomplete. At temperatures near 130 °C, seal thinning can occur in unsupported polyethylene laminates, so sealing cycles should be validated at the maximum line speed, not only at the nominal speed.
For direct food-contact applications in the European Union, the resin is intended for evaluation under Regulation (EU) No 10/2011 and its amendments. Compliance must be demonstrated on the finished packaging article using overall migration testing with food simulants assigned under Annex III. For applications in the United States, the base olefin copolymer can be considered under 21 CFR 177.1520(c) when the finished article meets the extractables and end-use limitations set by the regulation. The fabricator is responsible for verifying that processing aids, slip/antiblock concentrates, and printing inks do not shift overall migration or specific migration above the applicable limits. Where a food-contact declaration is required, the converter should request a declaration of compliance from the resin supplier and retain batch traceability data linking the pellet lot to the produced film.
Migration kinetics in thin film are controlled by film thickness, comonomer type, and the presence of migratory processing aids. Because the resin is supplied with a narrow molecular weight distribution, low-molecular-weight extractable fractions are generally limited; however, the final article may acquire migrants from slip agents, antistats, or printing inks. For fatty food simulants such as D2 or E5, overall migration must be tested on the finished laminate under the worst-case surface-to-volume ratio, typically 2 dm²/100 mL for packaging films. The resin supplier does not guarantee compliance of the converted article, because migration is dominated by downstream formulation and conversion.
| Framework | Relevant scope | Test or condition |
|---|---|---|
| EU Regulation 10/2011 | Plastic food-contact materials | Overall migration by simulant D1 or D2; specific migration for additives |
| FDA 21 CFR 177.1520(c) | Olefin polymers | Base polymer compliance subject to end-use condition and extractives |
| ISO 1133-1:2022 | Melt flow rate | Quality control at 190 °C / 2.16 kg |
| ISO 1183-1 | Density | Density gradient column or gas pycnometry |
A comparative evaluation against a standard LDPE film grade is often used when the specification requires impact resistance at freezer temperatures. The very low density ethylene copolymer retains ductile deformation at low temperatures more effectively than LDPE homopolymer because the amorphous phase is larger and the rubber-like plateau extends further. This does not mean unlimited low-temperature performance; notch sensitivity increases with high filler loadings, excessive slip additive concentrations, or severe gauge variation. For films intended for cold-chain transport or freezer packaging, the relevant test is often ISO 7765-1 dart impact at -20 °C or -40 °C, but published data for this specific product under those conditions is limited. Converters should generate internal data on a blown-film line with a fixed blow-up ratio of 2.5:1 and a minimum film gauge of 40 µm before setting a specification.
In stretch-wrap applications, the grade’s low modulus and high elongation combine to produce microclarity and puncture resistance. The puncture behavior should be measured using ASTM D5748-19 rather than low-rate tensile tests, because stretch-film puncture is a high-rate, biaxial deformation. Machine-direction extensibility of 200–350 % can be achieved in hand-wrap applications, depending on film gauge and tackifier addition.
For extrusion lamination and printed laminates, the surface energy of the film after corona treatment should be at least 38 mN/m for water-based inks and 36 mN/m for solvent-based inks. Because the resin has a low density and some low-molecular-weight species may migrate, corona treatment intensity should be limited to 2–4 W·min/m² to avoid surface crosslinking and reduce sealability on the reverse face. In adhesive lamination, the presence of amide slip additives can bloom to the surface and reduce adhesive wetting; the converter should conduct a dyne-level check after 24 h of roll ageing and before adhesive application.
The primary comparison points against a conventional LDPE of density 0.923 g/cm³ are lower tensile yield stress, lower seal initiation temperature, and lower elastic modulus. Against an EVA containing 18 wt% vinyl acetate, the product offers similar flexibility but lower seal caulkability at temperatures below 70 °C; however, it avoids acetic acid generation during high-temperature processing and reduces odor in low-taste packaging. Against a standard butene-based LLDPE of density 0.918 g/cm³, the product has lower stiffness and improved environmental stress-cracking resistance but may require more attention to bubble stability and melt pressure. In coextruded film structures, the grade is frequently placed as a skin layer over a polyethylene core or as a sealing layer against polypropylene or polyamide; compatibility with the adjacent layer must be confirmed by destructive peel testing and seal-integrity testing on the final laminate.
The material is not designed for injection molding or thermoforming applications where high flow under low pressure is the dominant process parameter. The low melt temperature and limited melt strength can result in warpage and dimensional instability in thick-walled parts. Thus, the specification should restrict use to film-extrusion processes unless a converter has developed validated tooling and processing protocols.