| HS Code | 982691 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 118 °C |
| Vicat Softening Temperature | 95 °C |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Shore D Hardness | 50 |
| Film Haze | 10% |
| Film Gloss | 80% |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 250 g |
As an accredited Versalis Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex® FG 368 comes in 25 kg polyethylene bags, palletized to 1,000 kg per pallet for bulk industrial supply. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags, palletized, shrink-wrapped; approximately 18–20 MT Versalis Clearflex® FG 368 Octene Comonomer LLDPE per container. |
| Shipping | Versalis Clearflex® FG 368 is shipped as non-hazardous, food-grade polyethylene pellets in sealed bags, octabins, or bulk containers. Store and transport in a clean, dry, covered environment away from moisture, odors, and contaminants. Avoid excessive heat, direct sunlight, and puncturing. Follow local regulations and keep packaging intact. |
| Storage | Store Versalis Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers, and use clean handling equipment. Follow supplier SDS and local regulations. |
| Shelf Life | Shelf life is approximately 24 months when stored in original, unopened packaging under cool, dry conditions, away from direct sunlight. |
In heavy-duty form-fill-seal packaging for bulk resins, fertilizers, and petrochemical granules, Clearflex FG 368 is processed as the load-bearing outer layer because octene comonomer incorporation produces longer short-chain branches than butene-based LLDPE. Longer linear segments between branch points increase the concentration of tie molecules in the amorphous phase during blown film cooling; the result is a measurable increase in Elmendorf tear and dart impact at equivalent film gauge, which becomes critical when sack walls are subjected to snagging on conveyor spirals or pallet corners. On a 3-layer Windmöller & Hölscher Varex II line with 70 mm grooved-feed extruders (L/D 30) and a 350 mm annular die, a typical construction uses 40 wt% FG 368 in the outer layer, 30 wt% FG 368 in the inner seal layer, and 30 wt% LDPE or trim in the core. Melt temperature is held between 210 °C and 235 °C, die lip gap is 2.4 mm, blow-up ratio is 2.8:1, and frost line height is set to 800 mm under IBC control. At these settings, films in the 120 µm to 160 µm range are run at line speeds of 45 m/min; bubble instability becomes measurable above BUR 3.2:1 and is visible as hunting of the frost line if the internal air temperature exceeds 35 °C. Seal initiation is evaluated according to ASTM F88 with a heat-seal bar at 120 °C and 0.3 MPa pressure; production-scale specification for 25 kg chemical sacks typically requires seal strength above 10 N/25 mm at 130 °C. Dart impact comparative data are collected using ASTM D1709 Method A; 100 µm monolayer blown film produced from 100% FG 368 can sustain puncture energies in the range of 350 g to 500 g depending on cooling rate, while coextruded 150 µm film with outer FG 368 layers regularly passes 1,000 g minimum customer specifications. The end product includes FFS sacks of 25 kg and 50 kg rated for petrochemical pellet packaging, where the film must also meet ASTM D1922 tear requirements above 15 N/mm in machine direction and 18 N/mm in transverse direction. Edge trim regranulate addition up to 20 wt% is common, but film output can drop by 6% if the trim contains surface condensation after storage above 60% RH; pre-drying or vented compounding is required to maintain stable melt delivery. Published data for the exact grade in high-BUR FFS structures remains limited; process settings cited are typical for octene-copolymer LLDPE film extrusion on the equipment described.
Greenhouse films produced from octene LLDPE fail in service less from tensile loss than from the interaction between light stabilizers and anti-fog surfactants when both are loaded into the same skin layer. The recommended construction separates functions by layer: external skin contains 0.6 wt% of a high-molecular-weight HALS, 0.2 wt% of a benzotriazole UV absorber, and 100% FG 368; the core may be a metallocene-catalyzed ethylene-octene plastomer; the internal skin contains 8 wt% anti-fog masterbatch and 100% FG 368. Total film thickness is controlled to 180 µm with a thickness tolerance of ±5 µm measured under ISO 4593. Multi-layer blown film is run on a 3-layer line with 60 mm extruders and 250 mm die, melt temperature 200 °C to 215 °C, blow-up ratio 2.2:1, and frost line height below 450 mm. Lower frost line height preserves the anti-fog additive in the inner layer by reducing dwell time in the melt and suppressing thermal degradation below the decomposition onset near 240 °C; this is the primary processing boundary. Retention of light transmission is measured according to ISO 4892-2 under Xenon arc exposure for 1,000 h; acceptable films retain more than 85% of initial tensile strength at break when tested under ISO 527-3. Haze is measured under ASTM D1003, and the anti-fog rating is assessed using a cold-water condensation chamber. The internal anti-drip layer must not be combined with sulfur-containing thioester heat stabilizers; published degradation studies indicate that thioester oxidation products can quench the nitroxyl radicals that HALS relies upon, reducing UV retention by as much as 30%. The end product is a 180 µm thermal greenhouse cover with 12-month to 24-month service life in southern Europe; the film also meets REACH Article 33 communication requirements for substances in candidate list above 0.1 wt%, but no SVHC is intentionally added. Processing bottlenecks appear during summer runs when cooling air temperature exceeds 25 °C, causing bubble flapping at BUR 2.2; the correction is to reduce die gap to 1.8 mm and increase IBC pressure by 0.2 kPa, but this narrows the total processing window to approximately ±5 °C.
Because reverse-printed laminates require the innermost web to seal through residual ink solvents and laminating adhesive without compromising seal strength or hot tack, FG 368 is converted into a 30 µm blown or cast sealant film and laminated to reverse-printed polyester or biaxially oriented polypropylene under a solventless adhesive at 1.5 g/m²; the substrate is 12 µm PET or 20 µm BOPP. Seal initiation temperature is determined on a JIS Z 0238 test apparatus, and hot tack is measured under ASTM F1921. For high-speed vertical form-fill-seal, sealant layer blends use 85 wt% FG 368 with 15 wt% ethylene-octene plastomer with melt index 2.5 g/10 min (ISO 1133-1:2022, 190 °C, 2.16 kg). The plastomer lowers seal initiation to 92 °C but reduces stiffness; the ratio is not increased above 20 wt% because the sealant web becomes tacky and blocking occurs on rewind. Film is produced on a single-screw cast line with a 1,000 mm flexible lip die, melt temperature 220 °C, chill roll temperature 18 °C, and line speed 120 m/min. Heat seal strength is tested under ASTM F88 at 115 °C and 0.2 MPa for 0.5 s; target seal strength exceeds 6 N/15 mm. Hot tack is assessed under ASTM F1921 with 200 N/min jaw separation; minimum required hot tack at 100 °C is 2.5 N/25 mm. Compliance for food contact is established under FDA 21 CFR §177.1520(c) for olefin polymers and EU Regulation 10/2011 Annex I with overall migration below 10 mg/dm² using simulant D2, while specific migration of octene-1 is below detection limits in standard test protocols. Additives must be limited: erucamide slip agent above 1,200 mg/kg can reduce seal strength by more than 25% after 14 days of storage at 40 °C because migration to the seal interface creates a low-molecular-weight boundary layer. The end products include coffee pouches, dried food laminates, and meat snack packs. This segment is intentionally shorter because the established practice is well characterized.
Cast stretch line throughput for pallet wrap is limited less by extruder output than by the onset of draw resonance when octene LLDPE film is drawn beyond a critical ratio. A 5-layer cast stretch line with 2,500 mm slot die and mechanical winding at 3,000 m/min running FG 368 in the three middle layers at a combined 80 wt% produces 17 µm to 23 µm film with machine-direction tensile strength above 40 MPa under ASTM D882. The outer cling layers are typically 10 wt% each of a metallocene ethylene-octene plastomer containing 3–5 wt% polyisobutylene tackifier. Die gap is 0.8 mm, melt temperature 245 °C, chill roll temperature 22 °C, vacuum box pressure 12 kPa, and air knife velocity 6 m/s. Draw resonance is observed when the draw ratio, defined as film take-up speed divided by die exit velocity, exceeds 12:1 under the selected die gap; melt fracture becomes visible when shear stress at the die lip exceeds 0.14 MPa, corrected by increasing die gap or reducing throughput. Puncture resistance is measured using ASTM D5748; a 20 µm cast film from FG 368 shows puncture force in the range of 1.8 N to 2.2 N. Cling force is measured using ASTM D5458; target cling for pallet wrap is between 0.8 N and 1.5 N. Pre-stretch on machine is set to 250%; above 300% film neck-in under load causes overlap failure at the pallet corners. Blocking on unwind occurs when tackifier content in the core exceeds 0.5 wt%; therefore the core is formulated without tackifier and the film requires corona treatment of the cling layer to 42 mN/m surface tension.
| Layer | FG 368 content (wt%) | Additive | Thickness (µm) | Test standard |
|---|---|---|---|---|
| Top cling | 0% | 4 wt% polyisobutylene in metallocene plastomer | 2 µm | ASTM D5458 |
| Sub-skin | 100% | None | 4 µm | ASTM D882 |
| Core | 100% | None | 8 µm | ASTM D5748 |
| Sub-skin | 100% | None | 4 µm | ASTM D882 |
| Bottom cling | 0% | 4 wt% polyisobutylene in metallocene plastomer | 2 µm | ASTM D5458 |
End products include 17 µm and 20 µm hand wrap and 23 µm machine wrap for pallet stabilization. Published data for FG 368 in 5-layer cast structures is limited; the process parameters shown are standard for octene LLDPE stretch film grades on the specified equipment.
Silage bale wrap produced from octene LLDPE is designed for multi-layer anaerobic food preservation, not for barrier in the classic gas-barrier sense. Oxygen transmission rate of each 25 µm layer is typically 8,000 cm³/m²·day·atm measured at 23 °C and 0% RH under ASTM D3985, so the barrier is achieved through applied layers and pre-stretch film tension rather than the polymer itself. A five-layer cast line with 1,500 mm dies runs FG 368 at 80 wt% in the middle layers; the external layers contain 0.25 wt% high-molecular-weight HALS and 0.15 wt% UV absorber, while the cling layer contains 5 wt% polyisobutylene in a metallocene plastomer carrier. Recommended film thickness per layer is 25 µm, applied with six to eight wraps of 70% pre-stretch around a 1.2 m diameter bale. Tear propagation resistance is measured using ASTM D1922; machine direction values below 8 N/mm are rejected because tears start at cut edges and propagate under bale handling. Puncture resistance under ASTM D5748 is specified above 2.0 N; elongation at break must exceed 500% under ASTM D882 to permit the pre-stretch ratio without local thinning. The processing boundary is the cling layer additive: adding polyisobutylene directly into FG 368 at more than 2 wt% leads to migration to the core within days, causing blocking and stretching unevenness. The end product is a 750 mm x 1,800 m roll of green or white silage wrap. Published data for FG 368 in silage wrap is limited; the process window cited is from standard octene LLDPE agricultural stretch film practice.
In air cushion packaging, two coextruded LLDPE plies are heat-sealed into discrete cells and inflated with compressed air; the critical test is not tensile strength but burst pressure and the propagation of pin-hole leaks. FG 368 is extruded into a 50 µm monolayer web on a 1,000 mm blown film line with 70 mm single screw, die gap 1.8 mm, BUR 3.0:1, melt temperature 215 °C. The film is sealed on a rotary air-cushion machine at 135 °C jaw temperature and 0.35 MPa pressure; seal failure occurs when the seal bar temperature drops below 125 °C, producing weak spots. Burst strength is measured by inflating a cell to failure; production film made from 100% FG 368 fails in the range of 0.12 MPa to 0.16 MPa, sufficient for void-fill but not for load-bearing air pillows. Melt index is controlled to 1.0 g/10 min under ISO 1133-1; lower melt index improves dart impact but increases extruder backpressure above 28 MPa at 70 rpm in a 30 L/D screw. Surface treatment is not required; slip and anti-block masterbatches are limited to 500 mg/kg each because higher loadings reduce seal strength under ASTM F88 below 5 N/15 mm. End products include void-fill pillows and EPE replacement for small parcel shipping. This segment is shallow because the process is well established.
Competitive Versalis Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® FG 368 is an octene-1 comonomer linear low density polyethylene supplied for blown and cast film conversion. The grade belongs to the Clearflex® family produced with single-site catalyst technology; the incorporation of octene-1 creates hexyl short-chain branches along the ethylene backbone. Melt mass-flow rate is determined under ISO 1133-1:2022 at 190°C with 2.16 kg load, and density is determined under ISO 1183-1:2019. Commercial film-grade octene LLDPE resins of this subtype are typically controlled within 0.8 g/10 min to 1.2 g/10 min and 0.916 g/cm³ to 0.920 g/cm³; the Versalis certificate of analysis defines the acceptance interval for Clearflex® FG 368. Primary uses include coextruded collation shrink film, frozen food packaging, and sealant webs for form-fill-seal pouches. The material is distinguished from butene- and hexene-comonomer grades by longer short-chain branching, which reduces crystallite thickness distribution and increases tie-chain probability at equivalent density.
Compared with butene-1 LLDPE of equal density and melt flow rate, octene-1 grades present longer hexyl branches that are less efficiently incorporated into the orthorhombic polyethylene unit cell. This structural effect lowers the temperature at which the crystalline network begins to melt and shifts heat-seal initiation toward lower platen temperatures when measured under ASTM F2029 or ASTM F88/F88M. Because long-chain branching is not present in the primary architecture, shear viscosity remains controlled, yet the tie-chain population at fast crack propagation is generally higher than in butene grades; the result is higher Dart drop impact at fixed thickness measured under ASTM D1709, Method A, and higher slow-puncture energy under ASTM D5748. Published data for this specific configuration is limited to datasheet summaries; comparative studies on metallocene octene LLDPE films report dart impact values in the range of 500 g to 1200 g for 50 µm monolayer film, while butene grades of identical density frequently fall below the lower bound. Seal initiation temperature for octene blends can range from 85°C to 105°C depending on density and coextruded layer structure. Direct substitution into a previously qualified butene extrusion line therefore requires re-verification of seal dwell conditions.
On high-output blown film towers equipped with internal bubble cooling and external gauge control, Clearflex® FG 368 is processed at barrel temperatures typical for metallocene LLDPE; flat temperature profiles from feed throat to adapter are preferred to avoid melt-pressure fluctuations. Extruder lengths of 24:1 to 30:1 L/D, barrier screws with Maddock mixing sections, and die gaps between 1.4 mm and 2.0 mm are used to manage melt temperature and output stability. The bubble expansion ratio may be set between 2.2:1 and 3.0:1, with frost-line height adjusted to maintain strain hardening before film collapsing. Observed production-scale failure modes include melt-pressure surging caused by pellet bridging in the feed throat when ambient humidity exceeds 70%, and unstable bubble geometry when die lip temperatures deviate by more than 5°C across quadrants. These conditions are process requirements from polyethylene film extrusion practice; they do not replace the converter’s start-up procedure.
Seal integrity on vertical and horizontal form-fill-seal equipment is governed by dwell time, platen pressure, and the thermal conductivity of the sealant layer. For octene LLDPE such as Clearflex® FG 368, hot-tack force is commonly evaluated under ASTM F1921 with a seal pressure of 0.275 MPa, a dwell time of 0.5 s, and cooling time of 0.1 s. Values above 2.0 N/25 mm across the 95°C to 120°C seal-temperature window are regarded as sufficient for high-shelf-speed pouch lines, whereas loss of hot-tack below 1.5 N/25 mm can induce seal peel and product rejects during film transport. Haze measurements under ASTM D1003 and gloss at 45° under ASTM D2457 are used to control the aesthetic quality of multi-layer collation shrink films; octene-based LLDPE typically exhibits haze below 12% and gloss above 60 GU in monolayer blown film. The final optical response is matrix-dependent: coextrusion with high-density polyethylene skins or the addition of slip and antiblock masterbatch in the outer layers modifies surface topography and should be evaluated at production-scale frost-line heights.
Because octene comonomer alone does not define the thermal or mechanical window, differentiation from flexomer and plastomer grades is necessary. Plastomers with density below 0.905 g/cm³ display elastic recovery and tack that are undesirable in high-speed packaging; Clearflex® FG 368 remains in the LLDPE density region where tensile yield strength, secant modulus, and Elmendorf tear propagation follow film orientation rather than elastomeric extension. Tensile properties are measured under ISO 527-3 or ASTM D882, tear properties under ASTM D1922, and puncture energy under ASTM D5748. In coextruded structures, the octene grade is typically placed in the core or sealant layer to increase dart impact without sacrificing outer-layer stiffness; the higher melt strength of LDPE skin layers stabilizes the bubble when internal bubble cooling is unavailable. Comparative datasets from blown-film converters indicate that replacement of a butene-grade core with an octene grade at constant thickness can raise dart impact by 20% to 60%, although published data for this specific configuration is limited to machine-scale studies.
Severe screw-channel temperatures are undesirable because they promote additive volatilization and can degrade the organoleptic profile required in food packaging. The melt temperature is typically held between 190°C and 230°C, with adapters and melt pipes set no more than 10°C above the final zone. Pressure-rise curves through a spiral mandrel die become unstable when melt fracture initiates at insufficient die-lip shear stress; purge protocols therefore shift from low-viscosity LDPE to the octene grade in controlled steps to avoid residual gels and die-lip build-up. On cast film lines, the chill-roll temperature between 20°C and 35°C is maintained to freeze the film before crystalline growth can create surface haze; vacuum box and air-knife settings are adjusted to avoid draw resonance. Process engineers record back-pressure and filter pressure drop at 40 MPa to 60 MPa as early indicators of screen-pack blinding. The grade-specific rheological curve should be taken from the Versalis datasheet because lot-to-lot molecular-weight distribution differences can alter pressure-flow relationships, with Rheological data obtained under ISO 11443.
Because food-contact status depends on the complete article, Clearflex® FG 368 is evaluated under the regulatory framework relevant to the final packaging structure. In the European Union, compliance is assessed under Commission Regulation (EU) No 10/2011 and its amendments, including overall migration limits under EN 1186 test conditions. In the United States, the grade is expected to meet 21 CFR 177.1520(c) for olefin polymers when used under specified conditions. REACH registration data are available through the Versalis supply chain; RoHS limits for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE are below the 0.1 wt% threshold in homogeneous material when relevant. These statements are regulatory framework descriptors, not direct certifications for all end uses; multi-layer laminates and printed film remain subject to the specific migration limits of the complete article.
| Regulatory area | Reference standard or clause | Verification requirement |
|---|---|---|
| European food-contact plastics | Commission Regulation (EU) No 10/2011, EN 1186 migration protocols | Supplier declaration of conformity for the specific grade; overall migration limits apply to the finished article |
| United States food contact | 21 CFR 177.1520(c) | Conditions of use specified by the resin supplier; end-use migration evaluation if barrier composition changes |
| REACH | Regulation (EC) No 1907/2006 | Registration by Versalis; Substances of Very High Concern not present above 0.1 wt% |
| RoHS | Directive 2011/65/EU, IEC 62321 methods | Lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE below 0.1 wt% in homogeneous film material |
Batch-to-batch variation in octene incorporation is monitored by the converter through gel-permeation chromatography, but common film lines rely on melt flow rate, density, and differential scanning calorimetry. Melting peak and crystallization temperatures measured under ISO 11357-3 are sensitive to the short-chain branching distribution; a shift of more than 2°C in the main melting endotherm may indicate lot-to-lot drift and should prompt a check of extrusion settings. Blocking force in wound film is evaluated under ASTM D3354; values above 20 g/cm at 35°C aging for 24 h are often associated with inadequate antiblock or excessive surface tack. Because octene LLDPE can have lower surface hardness than HDPE, storage below 50°C and below 60% relative humidity is recommended to prevent pellet softening and hopper bridging. The material should not be pre-dried unless exposed to moisture ingress; if pre-drying is used, desiccant-bed settings below 70°C for 4 h are common for polyolefins but should be confirmed from the supplier’s lot certificate.
When total film thickness is reduced from 60 µm to 40 µm, the converter re-validates machine-direction tear and transverse-direction tensile stress because sealant performance is cooling-rate dependent. Final roll geometry is checked for camber and gauge profile using an on-line beta gauge or capacitance thickness measurement under ISO 4593. The octene grade can retain sealant performance at reduced thickness if the heat-seal curve remains within the packager’s specified upper and lower limits. This is not an unconditional property of the resin class; it depends on frost-line height, film orientation, and the thermal history of the coextruded structure.