Versalis Clearflex Fg 336 Hexene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 522080
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.918 g/cm³
    Meltflowrate 190c 2 16kg 0.9 g/10 min
    Melttemperature 122 °C
    Vicatsofteningtemperature 100 °C
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 600 %
    Flexuralmodulus 250 MPa
    Shoredhardness 50
    Brittlenesstemperature < -70 °C
    Haze 12 %
    Gloss 45deg 70
    Dartdropimpact F50 150 g
    Elmendorftearstrength Md 150 g
    Elmendorftearstrength Td 300 g
    Sealinitiationtemperature 105 °C
    Coefficientoffriction 0.2

    As an accredited Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex FG 336 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped, with 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL: 18 pallets (55 × 25 kg bags); 24.75 MT net Versalis Clearflex® FG 336 Hexene Copolymer LLDPE.
    Shipping Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene is shipped as non-hazardous solid resin pellets, typically in 25 kg polyethylene bags or bulk containers, palletized and stretch-wrapped. Transport in dry trucks or containers. Store cool, dry, well-ventilated; avoid heat, sunlight, moisture, and contamination. Follow SDS and local regulations.
    Storage Store Versalis Clearflex® FG 336 Hexene Copolymer LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep original bags or containers closed, palletized, and protected from contamination. Avoid excessive stacking and prolonged UV exposure. Maintain normal ambient temperatures and follow supplier/local regulations. Clean up spills promptly, as pellets can create slippery surfaces.
    Shelf Life Shelf life: 24 months when stored in unopened original packaging, cool, dry, below 40°C, and away from direct sunlight.
    Application of Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene

    On single-layer and coextrusion blown film lines, Versalis Clearflex® FG 336 is processed as a 1-hexene comonomer linear low density polyethylene film resin. The grade is blended at 70–85 wt% with 10–25 wt% LDPE having a melt index of 0.3–0.5 g/10 min and 5–10 wt% metallocene hexene LLDPE to adjust shrink force and optics. Blown film extrusion uses a 75 mm grooved-feed extruder with 30:1 L/D, a 250 mm spiral mandrel die, die gap 1.8–2.4 mm, blow-up ratio 2.6–3.2:1, frost line height 5–8 die diameters, and melt temperature 195–225 °C. Under these conditions output ranges from 180–250 kg/h depending on screw speed and backpressure. Slip additive erucamide is dosed at 500–1500 ppm and silica antiblock at 1000–3000 ppm. Antiblock loading above 3000 ppm causes a measurable reduction in dart impact and increased haze. The resulting collation shrink film is tested under ASTM D1709-16A for dart impact, ASTM D882 for tensile properties, and ASTM D2732 for free shrink. Food-contact formulations comply with EU 10/2011 and FDA 21 CFR 177.1520(c) when overall migration is tested under EN 1186-1. Finished goods include printed and unprinted collation shrink film for beverage multipacks, can bundles, and hygiene product packs. In ambient humidity above 60% RH, additive masterbatches must be pre-dried at 70 °C for 4 h before dosing to prevent surface streaking and seal contamination.

    Compliance AttributeStandardCondition / Limit
    Olefin polymer food contactFDA 21 CFR 177.1520(c)Density range 0.930–0.940 g/cm³
    EU plastic food contactEU 10/2011Overall migration 10 mg/dm² or 60 mg/kg
    Dart impactASTM D1709-16A38 mm dart, 660 mm drop height
    Tensile propertiesASTM D88223 °C, 50% RH, 500 mm/min
    Elmendorf tearASTM D1922-1550 N pendulum
    Melt indexISO 1133-1:2022190 °C, 2.16 kg

    What Limits Low-Temperature Seal Integrity in Vertical Form-Fill-Seal Packaging?

    Vertical form-fill-seal lines impose seal initiation demands that cannot be met by butene-rich LLDPE sealant webs at high cycle speeds. Clearflex® FG 336 lowers the seal initiation temperature relative to butene LLDPE because the 1-hexene branches reduce the melting endotherm without sacrificing heat-seal strength. The sealant layer is blended at 65–80 wt% with 15–25 wt% LDPE and 5–10 wt% metallocene LLDPE in a 40–80 µm web. Coextrusion is conducted on a 7-layer blown film line with a 400 mm die, die gap 2.0 mm, blow-up ratio 2.2–2.6:1, and melt temperature 195–215 °C. The film is sealed on vertical FFS equipment with seal bar temperature 110–135 °C, jaw pressure 0.3–0.6 N/mm², and dwell 0.5–1.0 s. Hot-tack force is measured under ASTM F1921-12 and seal strength under ASTM F88/F88M-15 after 24 h conditioning at 23 °C and 50% RH. If seal bar temperature exceeds 140 °C, the metallocene-rich portion can contaminate sealing jaws. If temperature drops below 105 °C, seal failure occurs during high-speed horizontal transfer. The finished film is used for frozen vegetable pouches, coffee bags, snack packs, and powder beverage sachets. Food-contact compliance follows EU 10/2011, FDA 21 CFR 177.1520(c), and specific migration testing under EN 1186-14 for fatty food simulants.

    When Hexene LLDPE Replaces Butene LLDPE in Heavy-Duty Sack Films

    When replacing butene LLDPE with Clearflex® FG 336 in heavy-duty sack film, the extrusion line must be reassessed for melt pressure and motor load because the hexene copolymer has a narrower molecular weight distribution and higher shear viscosity at low melt temperatures. The formulation is 75–85 wt% Clearflex® FG 336, 10–20 wt% LDPE, and 3–5 wt% carbon black masterbatch for UV resistance. Extrusion on a 90 mm grooved-feed blown film extruder with 30:1 L/D, 300 mm die, die gap 2.0–2.4 mm, blow-up ratio 2.0–2.8:1, and melt temperature 205–230 °C is typically operated with melt pressure monitored against a maximum of 450 bar. If pressure exceeds 400 bar, screw speed is reduced or die gap is increased by 0.2 mm. Film gauge ranges from 80 µm to 200 µm. The resulting sack film is tested for Elmendorf tear under ASTM D1922-15, dart impact under ASTM D1709-16A, and tensile strength under ISO 527-3. Finished articles include heavy-duty sacks for polymer resin pellets, fertilizer, and mineral fillers. Carbon black masterbatch must not exceed 5 wt% because higher loading reduces heat-seal strength in bottom gusset seals. Compliance is required under REACH and RoHS for industrial packaging. Published data for this specific configuration is limited; therefore, line trials should confirm pressure and output limits.

    Three-layer agricultural coextrusion uses Clearflex® FG 336 in the core layer to provide tear resistance and dart impact strength in greenhouse and silage films. The outer layers contain 0.3–0.8 wt% hindered amine light stabiliser, 0.2–0.5 wt% UV absorber, and 0.5–1.5 wt% anti-fog additive. The core layer consists of 60–75 wt% Clearflex® FG 336, 10–20 wt% LDPE, and 10–15 wt% EVA with vinyl acetate content 14–18%. Coextrusion is performed on a three-layer blown film line equipped with 55 mm, 70 mm, and 55 mm extruders, a 350 mm die, die gap 2.0–2.2 mm, blow-up ratio 2.0–2.4:1, and melt temperatures 185–205 °C. Film thickness ranges from 100 µm to 200 µm. The film is tested under ISO 527-3 for tensile properties, ISO 6383-2 for tear resistance, and ASTM D1709-16A for dart impact. Accelerated weathering is assessed under ISO 4892-3 with UVA-340 lamps for 2000 h. Finished products include greenhouse covers, low tunnels, silage clamp covers, and ensiling bags. Anti-fog additive migration must be controlled by limiting film storage temperature to 30 °C maximum; above this temperature, surface bloom accelerates and reduces film clarity. The grade is not recommended for direct contact with high-acid silage leachate unless an inner EVA layer is used. Agricultural film specifications are aligned with EN 13206 where applicable.

    Cling Additive Partitioning Changes with Chill Roll Temperature and Haul-Off Speed

    Cast stretch film production requires precise control of chill roll temperature because cling additive partitioning shifts with thermal history and haul-off speed. Clearflex® FG 336 is used as the base resin in the core and cling layers. The formulation includes 80–95 wt% Clearflex® FG 336, 2–5 wt% polyisobutylene cling additive, 500–1200 ppm erucamide slip, and 0.5–1.5 wt% metallocene LLDPE to improve puncture. Cast film extrusion is performed on a 75 mm extruder with 30:1 L/D, a 2000 mm flat die, die gap 0.5–0.8 mm, chill roll temperature 18–22 °C, air gap 100–150 mm, and line speed 300–600 m/min. At line speeds above 450 m/min, cling additive can migrate unevenly toward the film surface if chill roll temperature exceeds 22 °C, reducing cling force and increasing unwind noise. Cling force is measured under ASTM D5458-95, puncture resistance under ASTM D5748-95(2012), and Elmendorf tear under ASTM D1922-15. Finished products include manual pallet wrap, machine stretch film, and pre-stretched hand film. For food-contact pallet wrap used with packaged food, the formulation must comply with EU 10/2011 and FDA 21 CFR 177.1520(c); the cling additive must have food-contact status under relevant national additive regulations. In high-ambient-temperature warehouses above 30 °C, the film should be stored for no longer than 6 months before use to prevent additive bloom from blocking the film surface.

    Coextruded Barrier Film Sealant Layer and Tie-Resin Dilution Effects

    Within five-layer and seven-layer barrier film structures, Clearflex® FG 336 functions as the sealant skin for processed meat and cheese packaging. The sealant layer consists of 65–85 wt% Clearflex® FG 336, 10–20 wt% metallocene LLDPE, and 5–12 wt% maleic anhydride grafted polyethylene tie resin. The tie resin is required for adhesion to the polyamide or EVOH core, but levels above 12 wt% reduce dart impact and increase gel counts in the sealant layer. Blown film coextrusion uses a 7-layer line with a 350 mm die, die gap 1.8–2.2 mm, blow-up ratio 2.0–2.6:1, and melt temperatures 195–220 °C. The sealant web thickness is 20–40 µm within a total structure of 70–120 µm. Barrier performance of the full structure is measured under ASTM D3985-17 for oxygen transmission rate and ASTM F1249-13 for water vapour transmission rate. Seal strength is tested under ASTM F88/F88M-15 and package integrity under ASTM F1929-15 using dye penetration. Finished products include vacuum pouches for processed meat, cheese packs, and stand-up pouches for dry snacks. Food-contact compliance is governed by EU 10/2011, FDA 21 CFR 177.1520(c), and 21 CFR 177.1395 for laminate structures where applicable. The structure is not recommended for retort conditions above 121 °C because the sealant layer softens and seal creep failure may occur under 0.5 bar overpressure differential.

    Free Quote

    Competitive Versalis Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FG 336 is a pelletized 1-hexene comonomer linear low-density polyethylene intended for blown film extrusion. The 1-hexene comonomer inserts butyl short-chain branches along the predominantly linear ethylene backbone, whereas a 1-butene comonomer inserts ethyl branches. That difference is directly relevant to the film failure sequence: the longer butyl branch can generate a more effective tie-molecule network between crystalline lamellae, raising dart impact and tear propagation resistance relative to a butene-based LLDPE of similar density and melt flow rate. The product identity includes not only the polymer composition but also the additive package, because slip and antiblock levels are order-dependent. The material is not marketed as a general-purpose injection-moulding feedstock; its rheological behaviour and bubble-stability envelope are optimized for high-stalk or in-pocket blown film lines. The nominal density is 0.918 g/cm³ under ISO 1183-1:2019, and the nominal melt mass-flow rate is 0.35 g/10 min at 190 °C under 2.16 kg load under ISO 1133-1:2022. The certificate of analysis is the controlling lot-release document; general technical datasheets cannot substitute for batch-specific verification.

    Nominal specification and regulatory compliance envelope

    The primary specification parameters are density and melt mass-flow rate. Density controls stiffness, barrier properties, and tensile yield; melt mass-flow rate controls extruder output, motor load, melt temperature rise, and bubble stability. The typical crystalline melting peak under ISO 11357-3 is near 124 °C, and the Vicat softening temperature A50 under ISO 306 is near 105 °C. These thermal values are informative for drying and sealing but are not always lot-release parameters. The product is supplied with a thermal stabilizer; if downstream handling or final use requires lower friction, the converter should specify a slip or antiblock package because both additives change film surface performance. Film haze is testable under ISO 14782, and coefficient of friction under ISO 8295. Regulatory compliance is not a resin property alone; it is an end-article property that includes the polymer, additives, pigments, printing inks, adhesives, and processing history.

    Specification, thermal, and regulatory matrix for Clearflex® FG 336
    ParameterStandard or regulationControl basis
    Melt mass-flow rateISO 1133-1:2022 at 190 °C/2.16 kgnominal 0.35 g/10 min; batch certificate controls
    DensityISO 1183-1:2019nominal 0.918 g/cm³; batch certificate controls
    Crystalline melting peakISO 11357-3typical 124 °C; informative
    Vicat softening temperature A50ISO 306typical 105 °C; informative
    Food-contact articlesEU 10/2011, FDA 21 CFR §177.1520final article compliance required
    REACHRegulation (EC) No 1907/2006SVHC below 0.1 wt%

    How does 1-hexene comonomer architecture shift film tear and impact balance?

    At constant melt index and density, a hexene-based LLDPE generally offers higher dart impact strength under ASTM D1709 and higher Elmendorf tear resistance under ISO 6383-2 than a butene-based LLDPE of equivalent comonomer mole fraction. The improvement is not the result of average density alone; it derives from a shift in the solid-state tie-molecule concentration and from a broader distribution of lamellar thickness that alters crack arrest. Butene-based LLDPE can show better optical clarity in some processing regimes because the shorter ethyl branches co-crystallize more readily and produce smaller crystalline domains. Compared with high-pressure LDPE, Clearflex FG 336 has a linear backbone and lower melt tension at a given melt mass-flow rate; high blow-up-ratio applications often require blending with LDPE or a processing aid to sustain bubble stability. Compared with many metallocene-catalysed hexene LLDPE grades, the present grade generally has a broader processing window but may exhibit higher seal initiation temperature; hot-tack and seal-strength comparisons must be measured by ASTM F1921 and ASTM F88 on the final coextruded structure, not on resin plaques. The choice between Clearflex FG 336 and other Clearflex grades is therefore governed less by density alone than by the required balance between puncture resistance, optics, seal performance, and line speed.

    At a target film thickness of 25 µm, the dart impact strength of hexene LLDPE can be significantly higher than that of a butene-based grade with the same nominal density, but the absolute value depends on frost-line height and blow-up ratio. A higher frost line generally increases machine-direction orientation and may reduce dart impact; therefore, comparisons between resin types are meaningful only when the same line geometry and bubble cooling conditions are used. When downgauging from 80 µm to 50 µm, puncture resistance under ASTM D5748 is a better predictor for heavy-duty sack service than tensile yield alone. Because hexene LLDPE has a broader tie-molecule distribution, the gauge reduction may be implemented with less loss of Elmendorf tear strength under ISO 6383-2 than would be observed with butene LLDPE; however, film haze may increase if the frost line is not adjusted.

    Within the Clearflex family, FG 336 is selected over lower-density or higher-melt-flow grades when the film must retain tear resistance at low gauge. A higher melt-flow grade will reduce extruder motor load but may sacrifice dart impact and bubble stability because molecular weight distribution and low-shear viscosity shift. The choice is not a linear function of melt index; low-shear viscosity measured by dynamic rheometry under ISO 6721-10 is more useful than melt mass-flow rate alone for judging bubble stability.

    During blown film conversion, the interaction of melt temperature, blow-up ratio, and frost-line height determines crystallite orientation and film gauge uniformity. On a conventional single-layer line with a grooved-feed extruder of L/D 30:1 to 36:1, barrel temperatures from 175 °C in the feed zone to 220 °C in the metering zone are common starting points. Die temperature is typically set at 220–230 °C, and the melt temperature should remain below 240 °C to avoid gel generation. A die gap of 1.2–2.5 mm and blow-up ratios of 2.0–3.0 are practical for structural films; on high-stalk processes, frost-line heights of 8–10 die diameters provide a balance between machine-direction and transverse-direction tensile strength. Internal bubble cooling shifts the freeze line upward and can increase throughput, but it also alters the thermal profile of the bubble and therefore the crystalline orientation. Capillary rheometry at 190 °C between 10 s⁻¹ and 1000 s⁻¹ shows strong shear-thinning; the apparent viscosity at 100 s⁻¹ is not linearly extrapolated from low-shear data, and screw speed-output curves are nonlinear. On lines with melt pumps, the pump should be controlled by inlet pressure rather than screw speed alone to prevent overfeeding the die and creating thickness oscillation. Published data for this specific grade on high-output internal bubble cooling lines is limited, so these settings should be treated as starting points and verified on the target equipment.

    When melt temperature and residence time exceed critical limits

    Thermal degradation of Clearflex FG 336 is primarily a thermo-oxidative process, not a hydrolytic process; drying is not required under normal indoor storage unless pellet surfaces have condensed moisture. If condensation occurs, predrying at 50–60 °C for 2 h with dehumidified air can remove surface moisture without pellet agglomeration. Residence time from the feed throat to die exit should normally be kept below 15 min, and melt temperature should not exceed 240 °C. Dead zones in adapters, screen packs, and die manifolds are common sources of gel particles; the extruder should be purged with an LDPE of similar melt mass-flow rate before shutdown or after colour changes. The grade should not be dry-blended with polypropylene or high-density polyethylene of widely divergent viscosity without evaluating layer stability, because incompatible domains can disturb bubble symmetry and create optical streaks. Avoid combinations with halogenated flame retardants, strong oxidizers, or amines that may accelerate radical-mediated chain scission at processing temperatures. If the melt pressure before the screen changer rises above 350 bar at a constant screw speed, the screen pack should be checked for gel accumulation or foreign material. The product is not recommended for prolonged outdoor exposure unless a UV stabilizer package is added by the converter; unstabilized polyethylene will embrittle under ASTM D4329 weathering.

    In multi-layer heavy-duty sacks and industrial liners, Clearflex FG 336 is used as the core layer to provide puncture resistance under ASTM D5748, while LDPE skins control bubble stability, heat sealing, and coefficient of friction. In collation shrink film, machine-direction shrink behaviour must be characterized under ISO 14616 because the orientation and relaxation response of hexene LLDPE differs from LDPE-based shrink formulations. For food-contact packaging, the converter must demonstrate compliance of the finished article under EU 10/2011 and FDA 21 CFR §177.1520; migration testing must include inks, coatings, and adhesives because the overall migration limit applies to the whole structure, not to the base resin alone. When the product replaces a butene-based LLDPE of similar nominal density, the processor may need to adjust die gap and frost-line height to compensate for differences in crystalline orientation and melt tension. The final choice of screw, die, and downstream nipping conditions should be confirmed by surface energy measurements under ISO 8296 if the film is printed or metallized, because hexene comonomer distribution affects oxidation treatment response.

    At start-up, the extruder and die should be preheated to the lower end of the processing range before rotation begins to avoid shear heating of unmelted pellets. The screw should be started at low speed, typically 10–15 min⁻¹, and flood-fed only after melt pressure stabilizes. A purge with an LDPE of similar melt mass-flow rate should be used when transitioning from a higher-viscosity polyolefin, because the low-viscosity Clearflex FG 336 stream may bypass residual high-viscosity material in the compression zone and produce localized gel streaks. At shutdown, the die should be kept at temperature until the melt flow stops and then cooled while closed, to minimize oxidative degradation on internal surfaces.

    The grade is not formulated for rotational moulding, injection stretch-blow moulding, or pipe extrusion. Published data for this specific grade under ISO 12162 for pressure pipe design is limited, and use in pressurized pipe systems is outside the intended application envelope. For stretch film, if a high-tack additive is not specified, surface cling must be provided by another layer or post-treatment. These limitations are part of the grade selection process and should not be inferred from LLDPE generic literature.

    Because the additive package influences processing and performance, low-slip and antiblock selections require converter-specific verification. A low-slip additive raises the coefficient of friction under ISO 8295, which may improve stack stability but reduce performance in automated bagging machines. An antiblock package may reduce haze under ISO 14782 but can increase die lip buildup. The converter should specify the target coefficient of friction and haze because these cannot be corrected by extrusion alone.

    For industrial hygiene, the polymer is not classified as dangerous under CLP Regulation (EC) No 1272/2008. During extrusion, thermal decomposition can release aliphatic hydrocarbons and carbon monoxide if the material is overheated; local exhaust ventilation should be maintained near the die and screen changer. Standard housekeeping for pellet spills should be observed to prevent slipperiness and dust generation. Any pigment or masterbatch added by the processor must be evaluated separately for food-contact and REACH status, because the base resin certification does not extend to additive concentrates or physical mixtures made downstream.

    Top