| HS Code | 468956 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.922 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Temperature | 98 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | ≥600% |
| Dart Drop Impact F50 | 110 g |
| Haze | 12% |
| Gloss 45 | 70 |
| Coefficient Of Friction | >0.5 |
| Blocking | 40 g |
| Antioxidant | Present |
As an accredited Versalis Clearflex® FG 336 A Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packaged in 25 kg polyethylene bags, palletized, or 1,000 kg bulk bags for safe transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL loading: Versalis Clearflex® FG 336 A Film Grade LLDPE, 25 kg bags, palletized, securely stowed for ocean shipment. |
| Shipping | Versalis Clearflex® FG 336 A Film Grade LLDPE is supplied as free-flowing pellets in 25 kg PE bags, stacked on pallets and stretch-wrapped, or in bulk containers/octabins. It ships by truck or container as non-hazardous cargo. Keep dry, away from heat, sunlight, and ignition sources; no special transport class required. |
| Storage | Store Versalis Clearflex® FG 336 A Film Grade LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original packaging sealed on pallets, off the floor, to protect from moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Rotate stock first-in, first-out; follow supplier guidance. |
| Shelf Life | Store in original unopened packaging, dry, well-ventilated area, below 40°C, away from sunlight. Shelf life: 24 months from production date. |
Cast film conversion of Clearflex FG 336A at 23 µm nominal thickness exposes two process conflicts. The first is edge neck-in at the die-to-chill-roll interface. The second is draw resonance when the film is drafted above 250 m/min. The grade has a nominal melt flow rate of 3.5 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022 and a nominal density of 0.922 g/cm³ per ISO 1183-1:2019.
On a 75 mm grooved-feed single-screw extruder with 30:1 L/D and a double-flight barrier section, barrel zone set points are 190°C, 210°C, 225°C, 235°C, and 240°C. The adapter and the 1,500 mm slot die are held at 240°C to 246°C. The die gap is 0.45 mm. The air gap is maintained between 38 mm and 50 mm. The primary chill roll runs at 18°C. The secondary roll runs at 22°C. Vacuum-box pressure is set from 25 mbar to 40 mbar. Air-knife pressure is adjusted until edge weave ceases.
Formulation for machine-grade pallet wrap uses 76 wt% Clearflex FG 336A, 15 wt% metallocene LLDPE with a melt flow rate of 1.0 g/10 min, and 2 wt% LDPE carrier masterbatch containing 50 wt% polyisobutylene tackifier. Slip/antiblock masterbatch at 1.0 wt% to 1.5 wt% is introduced to bring the outside coefficient of friction to 0.30–0.45 under ISO 8295. For a 23 µm machine film, stretch puncture resistance is tested under ASTM D5748. Industrial wrap lines often set an acceptance gate of 0.6 J/µm or higher. Where published datasheet data for this exact formulation is limited, incoming resin lot qualification should include a reference sample obtained under the same cast-line conditions. Neck-in increases above 250°C melt temperature. Die-lip temperature profiling may be used to compensate for edge quench. At melt temperatures above 255°C, oxidation-induced gel formation becomes visible as transparent specks in the final film.
Moisture on the pellet surface is not absorbed by the resin, but condensation on pellets stored in outdoor silos can create feed-throat melt-pressure oscillation. Pellets should be brought above dew point before conveying. The terminal product is machine pallet wrap supplied in 450 mm to 500 mm roll widths, calendered onto 76 mm paper cores. For EU export, the finished stretch film is within the scope of 94/62/EC for heavy metals. The sum of lead, cadmium, mercury, and hexavalent chromium must not exceed 100 mg/kg by acid digestion and ICP-OES.
At 70 µm film thickness, heavy-duty sack production on three-layer blown-film equipment demands a balance between dart impact, Elmendorf tear, and bubble stability. A form-fill-seal sack structure commonly uses 30 wt% Clearflex FG 336A in the outer layer, 40 wt% in the core, and 30 wt% in the inner layer. LDPE with a melt flow rate of 0.3 g/10 min is added at 20 wt% to improve melt strength. High-density polyethylene with a melt flow rate of 0.1 g/10 min is added at 10 wt% for stiffness and downgauging. A post-industrial recycled LLDPE fraction in the core layer should not exceed 15 wt%. Its melt flow rate should not deviate by more than ±20% from the virgin Clearflex FG 336A value.
On an 80 mm grooved-feed extruder with 30:1 L/D and a 250 mm spiral mandrel die, the die gap is set at 2.2 mm. The blow-up ratio is held between 2.5:1 and 2.8:1. The frost-line height is maintained at 7 to 9 die diameters. Melt temperature at the die is kept between 200°C and 210°C. Screen-changer melt pressure is typically observed in the 350 bar to 420 bar range before the gear pump. A pressure rise greater than 25% at constant output signals gel build-up and requires a screen change.
Bubble stability is the principal conflict. Linear low-density polyethylene has lower melt tension than the LDPE fraction. Setting the frost-line height too high produces a soft bubble that sways. Setting it too low reduces machine-direction tear. A lay-flat width variation greater than ±5 mm across the bubble circumference indicates uneven cooling. Dual-lip air rings with lower-lip velocity 25% higher than upper-lip velocity are used on high-output lines. At these conditions, the 70 µm heavy-duty sack should meet a dart-drop F50 value of at least 500 g under ASTM D1709. Elmendorf tear is measured under ISO 6383-2. Machine-direction tear is limiting in form-fill-seal service. Increasing blow-up ratio above 2.8:1 improves transverse-direction tear but reduces machine-direction tear and destabilises the bubble. Do not pre-dry below 60% relative humidity. At higher humidity, condensation on the pellet surface must be eliminated with hopper-carrier air above dew point. The terminal product is a 70 µm heavy-duty sack for 50 kg polymer granule packaging.
Agricultural bale wrap produced at 25 µm thickness from Clearflex FG 336A is typically run as a cast coextruded structure. The outer layer is formulated at 12 wt% of total thickness. The core layer is 68 wt%. The inner layer is 20 wt%. The outer layer contains 4 wt% of a UV masterbatch based on 20 wt% hindered amine light stabiliser and 10 wt% carbon black in LDPE. The outer layer also contains 2 wt% polyisobutylene masterbatch for cling. The inner layer contains 1.5 wt% of a slip/antiblock masterbatch to control blocking on the unwind path.
On a 70 mm 24:1 L/D cast-line extruder with a 1,200 mm slot die, the die gap is set at 0.35 mm. Melt temperature is 235°C. Chill roll temperature is 20°C. Line speed is held near 600 m/min. Edge trim is kept below 8% of web width. Ageing resistance is evaluated under ISO 4892-2 using a UVA-340 lamp. A common silage-wrap acceptance target is retention of at least 50% tensile elongation after 2,000 h. Tensile elongation is measured under ISO 527-3. Tear propagation resistance is measured under ISO 6383-2. The product must satisfy EN 13206 for thermoplastic stretch films used to wrap silage bales. Published data for this specific three-layer structure is limited. Resin lots with a melt flow rate outside ±10% of nominal can shift cling uniformity and should be controlled. The terminal product is a 750 mm wide, 1,500 m long roll of 25 µm silage bale wrap.
Five-layer coextruded barrier packaging for processed meat makes the sealant web the controlling factor for both heat-seal integrity and migration compliance. The structure is typically 20 µm LDPE / 3 µm maleic anhydride grafted tie / 5 µm EVOH / 3 µm tie / 40 µm sealant. The sealant layer is compounded from 75 wt% Clearflex FG 336A and 25 wt% LDPE with a melt flow rate of 0.3 g/10 min. A slip/antiblock masterbatch is added at 1.5 wt%. The sealant melt temperature at the die is held at 205°C to 215°C. The die gap is 1.8 mm. The blow-up ratio is 2.0:1. The frost-line height is 4 to 5 die diameters. EVOH degradation is avoided by keeping the barrier-layer melt below 230°C.
Differential scanning calorimetry of Clearflex FG 336A per ISO 11357-3 shows a melting peak in the 121°C to 126°C range. Heat-seal strength is tested under ASTM F88 with a 25 mm wide specimen, 0.28 MPa jaw pressure, and 0.5 s dwell. At a seal bar temperature of 130°C, the sealant web should exceed 12 N/25 mm on a 40 µm sealant layer. For migration compliance, the finished structure is tested under EU No 10/2011. Overall migration must remain below 10 mg/dm² in food simulant A, B, or D2 depending on intended food type. The resin must comply with FDA 21 CFR 177.1520 paragraph 3.1a for olefin polymers. Additives must be verified against the positive lists in EU No 10/2011 Annex I.
| Regulatory area | Standard / directive | Test method / clause | Limit or condition |
|---|---|---|---|
| EU food contact | EU No 10/2011 | EN 1186-1 gravimetric; simulants A, B, D2 | Overall migration < 10 mg/dm² |
| US food contact | FDA 21 CFR 177.1520 | Paragraph 3.1a; extraction tests | Net chloroform-soluble extractables per regulation |
| REACH | 1907/2006 | Article 33, Annex XVII | SVHC ≤ 0.1 wt%; no restricted phthalates |
| Export packaging metals | 2011/65/EU | IEC 62321 series | Pb 1,000 mg/kg, Hg 1,000 mg/kg, Cd 100 mg/kg, Cr(VI) 1,000 mg/kg |
The terminal product is a 40 µm sealant web used in form-fill-seal pouches for processed meat and cheese. Corona treatment of the outer LDPE side to 42 mN/m is performed in-line for lamination adhesion.
Producing e-commerce mailer film at 55 µm monolayer thickness from Clearflex FG 336A requires simultaneous control of puncture resistance during sortation and tear initiation during manual opening. The formulation comprises 70 wt% Clearflex FG 336A, 20 wt% LDPE with a melt flow rate of 0.30 g/10 min, and 10 wt% white masterbatch containing 60 wt% titanium dioxide in LDPE. Erucamide slip active is added at 300 ppm to 600 ppm. Synthetic silica antiblock is added at 1,500 ppm. On a 65 mm 28:1 L/D single-screw extruder with a 150 mm die, the die gap is set at 1.5 mm. The blow-up ratio is held at 2.8:1. The frost-line height is 5 die diameters. Melt temperature is maintained between 190°C and 205°C.
Dart-drop impact is tested under ASTM D1709. Industrial acceptance for a 55 µm e-commerce mailer often requires F50 ≥ 250 g. Puncture propagation is screened by ASTM D5748. Seal strength is measured under ASTM F88 at 0.28 MPa and 0.5 s. The seal should reach 10 N/25 mm at 130°C. If seal strength exceeds 15 N/25 mm, the mailer may fail opening-preference tests because tear initiation at the laser score becomes inconsistent. Corona treatment for printing is set to 40 mN/m. The terminal product is a tamper-evident mailer bag with a pressure-sensitive closure tape.
Frozen-food lamination web at 40 µm is produced as a monolayer blown film with 20 wt% LDPE to reduce heat-seal initiation. Pre-drying is not required below 60% relative humidity. Corona treatment to 42 mN/m is applied before lamination with solventless polyurethane adhesives.
Competitive Versalis Clearflex® FG 336 A Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® FG 336 A is a linear low-density polyethylene film extrusion grade produced by Versalis within the Clearflex family. The resin is manufactured on a gas-phase Spherilene platform and is supplied as pellets for blown film and cast film conversion where improved impact strength and tear resistance at reduced gauge are required relative to high-pressure LDPE. Manufacturer-documented nominal values for density and melt mass-flow rate are 0.918 g/cm³ per ISO 1183-1 and 1.0 g/10 min at 190 °C under 2.16 kg per ISO 1133-1:2022, respectively. These values place FG 336 A in the standard film-grade LLDPE class for general-purpose and heavy-duty packaging, with a balance between melt viscosity and bubble stability on conventional air-quenched blown film equipment. Published comonomer disclosure for this specific grade is limited, and catalyst residue and short-chain branch distribution are not specified in accessible technical literature.
The primary differentiation from high-pressure low-density polyethylene is the largely linear microstructure of the LLDPE backbone, with short-chain branches contributed by an alpha-olefin comonomer rather than long-chain branching generated by the autoclave or tubular polymerisation mechanism. This structural difference lowers extensional viscosity at typical film-blowing elongation rates, so bubble stability is more dependent on internal bubble cooling and air-ring configuration. By comparison, high-pressure LDPE possesses long-chain branching that confers strain hardening and broader bubble stability at high take-up ratios. At equivalent density and film thickness, the LLDPE class provides higher dart impact resistance and Elmendorf tear resistance, but lower clarity and lower melt strength. Relative to metallocene-catalysed hexene-LLDPE of the same nominal density and melt flow rate, FG 336 A is expected to show a broader composition distribution, lower gloss, lower dart impact, and higher seal initiation temperature; the offset is typically more stable head pressure, lower gel sensitivity, and a wider extrusion torque window. This comparison is drawn from the general behaviour of density 0.918 g/cm³ Ziegler-Natta LLDPE film resins; published film property data for FG 336 A specifically is limited.
The melt index of 1.0 g/10 min corresponds to a comparatively high molecular weight grade for film, which supports bubble strength but increases back pressure on shallow-metering screws. In rotational rheometry at 190 °C, the complex viscosity at 0.1 rad/s for density 0.918 g/cm³ LLDPE is typically in the range 8,000–15,000 Pa·s; the shear-thinning exponent over the frequency range 1–100 rad/s is lower than that of high-pressure LDPE because of reduced long-chain branching. This means melt pressure responds more strongly to throughput increases, and die lip shear rate must be monitored when line speed is raised. Published data for this specific grade is limited; the cited values are class-typical for Ziegler-Natta film LLDPE.
Low-temperature solid-state performance is also relevant for frozen food packaging. The brittleness temperature for density 0.918 g/cm³ LLDPE measured by ISO 974 is typically below -70 °C, whereas high-pressure LDPE values may fall near -60 °C. This provides a technical basis for specifying FG 336 A in cold-chain sacks where film flex cracking at freezer temperatures is a failure mode. Actual values depend on molecular weight, comonomer type, and thermal history; published data for this specific grade is limited.
Processing of FG 336 A on monolayer or coextruded blown film lines requires a single-screw extruder with L/D of at least 24:1 and a barrier or Maddock mixing section. Barrel temperatures are typically set from 170 °C at the feed throat to 200 °C in the metering zone; die and adapter temperatures are usually maintained between 210 °C and 225 °C. Melt temperature measured at the die exit should remain below 230 °C to limit oxidative gel formation and to avoid bubble temperature instability. A die gap of 1.4 mm to 2.5 mm is recommended for conventional LLDPE film production; die gaps below 1.0 mm raise wall shear rate at the die lip and can induce sharkskin melt fracture. Blow-up ratios between 2.0:1 and 3.0:1 are common for this density class, with frost line heights of 4 to 8 die diameters for air-quenched bubbles. Internal bubble cooling moves the frost line lower and permits higher throughput at constant film gauge, but too low a frost line at high output can quench the film before biaxial orientation is established and reduce dart impact resistance by more than 15% compared with a frost line of 6–8 die diameters.
Melt pressure on a grooved-feed extruder with a 30:1 L/D barrier screw and 120 mm die diameter is typically observed in the range 25–40 MPa at output rates of 1.5–2.5 kg/h per millimetre of die circumference; this is a field range from production-scale lines and not a supplier guarantee for every die geometry. The linear structure lowers melt fracture resistance compared with LDPE-rich formulations. When sharkskin appears at higher output, a fluoropolymer-based polymer processing aid can be added at 200–500 mg/kg; the die lip should be chromium-plated and free of rough oxidation deposits. Pre-drying is not required for pellet storage at ambient conditions, but condensation on pellets stored below the dew point can introduce moisture into the feed hopper and create pinholes in the bubble. Sacks should be allowed to reach ambient temperature before opening when stored in unheated warehouses.
Dry blending with high-pressure LDPE at 15–30 wt% improves bubble stability, reduces melt fracture, and widens the air-ring tolerance. At LDPE fractions above 30 wt%, dart impact and Elmendorf tear values begin to shift toward LDPE performance. Conversely, adding FG 336 A to LDPE at similar ratios improves seal strength and downgauging capability in heavy-duty sack film. The optimal blend ratio is not fixed by the resin specification and must be confirmed by film property tests on the target line.
Typical test-method alignment for film-grade LLDPE of this density class is reported in the table below. The values are not batch-release limits unless specified in the manufacturer’s certificate of analysis; published data for this specific configuration is limited.
| Property | Method | Typical value |
|---|---|---|
| Nominal density | ISO 1183-1 | 0.918 g/cm³ |
| Melt mass-flow rate (190 °C/2.16 kg) | ISO 1133-1:2022 | 1.0 g/10 min |
| Melting temperature (DSC, 10 °C/min) | ISO 11357-3 | 122–124 °C for density 0.918 LLDPE class |
| Vicat softening temperature A50 | ISO 306 | 98 °C (published data for FG 336 A limited) |
| Film tensile yield stress | ISO 527-3 | MD 11 MPa / TD 11 MPa typical class range |
Mechanical performance in film conversion is not derived solely from resin density. For a 40 µm monolayer film produced at a blow-up ratio of 2.5:1, dart drop impact per ISO 7765-1 typically falls within 120–200 g for this density class; however, published data for FG 336 A run under controlled air-quench conditions is limited. Elmendorf tear resistance per ISO 6383-2 after conditioning at 23 °C and 50% RH commonly shows transverse-direction tear values of 10–25 N/mm and machine-direction values of 8–18 N/mm. Tensile elongation at break per ISO 527-3 is usually above 600%. Optical haze per ISO 14782 may range from 8–14%; the grade is not intended for high-clarity metallocene film applications. Oxygen transmission rate for 25 µm film measured at 23 °C and 0% RH per ASTM D3985 is approximately 3500–4500 cm³/m²·day·atm, indicating that barrier properties are not differentiated and must be supplied by coextruded barrier layers.
Cast film conversion of FG 336 A does not require bubble stability control but does require edge pinning and rapid quench to minimise neck-in. On a 1,000 mm wide cast line with a slot die gap of 0.4–0.8 mm, melt temperature at the die lip is typically held at 230–250 °C to reduce draw resonance; chill roll temperatures of 20–30 °C are used to develop low haze and balanced tear. Higher chill roll temperatures increase crystallinity and lower tack to the roll. Edge trim can be recycled in-line but the high molecular weight of the resin may increase trim handling energy; grinders with 5–10 mm screen size are used for trim fluff.
In coextruded polyethylene-based food packaging, FG 336 A can be used in the sealant layer because the density of 0.918 g/cm³ provides a lower seal initiation temperature than MDPE or HDPE skins. Seal strength measured according to ASTM F88 on a 40 µm blown film commonly exceeds 8 N/15 mm above 120 °C sealing temperature; the exact seal initiation temperature depends on dwell time, film thickness, and surface additive migration. Hot-tack performance per ASTM F1921 is governed by crystallisation rate and can be impaired by excessive slip or antiblock masterbatch. The grade is generally supplied with a formulation for low blocking and controlled slip; the converter must verify that the additive package does not exceed the migration limits of the food-contact legislation applicable to the final structure.
For structures requiring low-temperature sealing at line speeds above 40 packs/min, verification on horizontal form-fill-seal equipment with a jaw temperature profile of 120–140 °C and dwell times of 0.2–0.5 s is required, because seal initiation data measured on laboratory hot-tack testers does not transfer linearly to production machinery. Published data for this specific configuration is limited; converters should record heat-seal strength as a function of jaw temperature for each layer ratio.
Compliance documentation for polyolefin food-contact use should reference Regulation (EU) No 10/2011 and its amendments, including the overall migration limit of 10 mg/dm² for standard testing under the relevant test conditions. For the United States market, the base olefin polymer may fall under FDA 21 CFR §177.1520(c) when used as a food-contact article component, subject to density and extractable fraction limits; the film converter is responsible for confirming that the finished article meets any applicable temperature and food-type use limitations. The grade should not be used in applications requiring long-term UV exposure or high-temperature sterilisation without additional stabiliser or crosslinkable additive validation.
| Requirement | Reference | Typical status |
|---|---|---|
| Food contact plastic migration | Regulation (EU) No 10/2011 | Base polymer subject to overall migration limit 10 mg/dm²; compliance depends on final article |
| Olefin polymers food contact | FDA 21 CFR §177.1520(c) | Base olefin polymer eligibility subject to condition of use |
| REACH registration | Regulation (EC) No 1907/2006 | Monomer and polymer registration obligations apply at placed-on-market stage |
| RoHS hazardous substances | Directive 2011/65/EU | Not normally applicable to uncured PE packaging but trace-metal content should be confirmed by supplier documentation |
Published data for the specific clear grade and for high-speed cast film conversion of FG 336 A is limited. Converters performing downgauged stretch film trials should verify film tensile, puncture, and cling performance on the actual line configuration, because coextruded layer ratios and die lip shear history alter the crystalline orientation and post-extrusion property development. Blown film trials should include gauge tension mapping and bubble stability logging to establish whether the selected die gap, blow-up ratio, and processing aid concentration maintain film thickness variability below ±5% at target output.