Versalis Clearflex Fg 308 Octene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 738013
    Product Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene
    Manufacturer Versalis
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 98 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 260 MPa
    Dart Drop Impact F50 180 g
    Haze 12%
    Gloss 45 85
    Coefficient Of Friction 0.2

    As an accredited Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® FG 308 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe handling and storage.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Versalis Clearflex® FG 308 octene copolymer LLDPE in 25 kg bags, palletized/stretch-wrapped, maximizing 20′ FCL capacity.
    Shipping Clearflex® FG 308 octene copolymer LLDPE is shipped as nonhazardous solid pellets in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry, covered vehicles/containers at ambient temperature. Not classified as dangerous goods. Protect from moisture, heat, sunlight, and contamination; keep packaging sealed until use.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and moisture. Keep original bags sealed and palletized to prevent contamination or dust. Avoid prolonged exposure to temperatures above 50°C. Maintain ambient temperature and good housekeeping. Use first-in, first-out stock rotation. Inspect packaging before use. Protect from physical damage and strong odors, especially for food-contact grades.
    Shelf Life Typically 24 months from production date when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene

    On a three-layer cast film line configured with 75 mm/45 mm/75 mm extruders and a 2,400 mm-wide coat hanger die at 0.75 mm die gap, Clearflex FG 308 is typically fed to all three layers because the octene distribution produces a wider short-chain branching length than butene-based LLDPE at similar density, which reduces the zero-shear viscosity plateau and permits the high draw ratios required for pallet stretch film without the tear anisotropy that collapses edge-load performance. The melt temperature at the die lips is held from 240°C to 260°C; below 230°C, the 12 μm film surface develops transverse shark-skin melt fracture, while above 275°C the polyisobutylene tackifier in the cling layer begins to degrade into low-molecular-weight volatiles that condense on the chill roll as a sticky haze band. For total film thicknesses of 15–23 μm, a layer distribution of 10%/80%/10% is used, with the cling layer made from FG 308 plus 2.0–4.0 wt% polyisobutylene masterbatch of 40–50% active content and 0.5–1.0 wt% erucamide masterbatch, the core layer containing up to 15 wt% dried post-industrial edge trim redirect, and the air-side release layer containing 1.0–2.0 wt% silica anti-block with a median particle size of 3–5 μm. Cooling is executed on a 1,000 mm-diameter chill roll with a surface temperature of 18–24°C; lower temperatures raise the free-roll crystallinity and reduce clarity, whereas higher temperatures induce blocking at the nip and generate gauge bands under the contact roller. The film is tested according to ASTM D5458-20 for cling peel force, ASTM D5459-21 for elastic recovery and stress retention after 150% elongation, and ASTM D5748-19 for protrusion puncture resistance; production floor targets for a 20 μm film are typically 120–220 g peel cling, above 80% recovery at 150% elongation with a 10 s hold period, and no puncture below 3.0 N before prestretch. The finished film is applied on automatic pallet wrapping machines at pre-stretch ratios up to 250% only when the core layer does not exceed 15% reprocessed material; beyond this level, gel counts above 0.15 mm increase and the stretch-to-puncture plateau narrows, producing visible opaque specks in edge-taped loads under warehouse lighting.

    LayerBase polymerFunctional additiveConcentration rangeTest or equipment anchor
    Cling layerFG 308PIB tackifier masterbatch2.0–4.0 wt%ASTM D5458-20 peel cling
    Cling layerFG 308Erucamide slip masterbatch0.5–1.0 wt%ASTM D1894-14 coefficient of friction
    Core layerFG 308 with post-industrial edge trimNone or process antioxidant0–15 wt% regrindGel count on 0.15 mm polymer filter
    Release layerFG 308Silica anti-block1.0–2.0 wt%ASTM D1003-13 haze; ASTM D1894-14 COF

    Why Does Blown Film Bubbling Operate at a Lower Melt Temperature Than Cast Extrusion?

    The octene comonomer in Clearflex FG 308, a grade with a nominal density of 0.930 g/cm³ per ISO 1183-1 and a melt flow rate of 3.0 g/10 min per ISO 1133-1, shifts the onset of melt instability in air-cooled blown film because the short-chain branch architecture reduces melt tension compared with a 0.918 g/cm³ butene-LLDPE of equal melt flow rate; the exact percentage difference is not given in the manufacturer’s datasheet, and converter-run bubble stability trials are required to map the stable output window to die-specific pressure variation. A 50 mm single-screw extruder with a 30:1 L/D double-flighted barrier screw is commonly operated with barrel zones of 170°C, 190°C, 210°C, 215°C, and 220°C from feed to die, with the die set at 195–215°C and the external air ring maintained at 8–14°C. Frost line height is typically 6–9 times die diameter for 25–50 μm film; blow-up ratio is kept between 2.0:1 and 2.4:1 because the grade lacks the long-chain branching needed for stable bubbles above 2.5:1, where helical instability can develop and create alternating gauge bands. For high-output production on a 150 mm die, internal bubble cooling with 20–30% of total air flow bypassing the external ring is used, but the internal exhaust must remain above 8°C to avoid condensation that appears as pit marks on the quenched surface. The film is characterized by ASTM D882 for tensile properties, ASTM D1922 for Elmendorf tear, and ASTM D1709 for dart drop; for a 30 μm monolayer film, converter audit ranges are 180–280 g in MD tear, 350–500 g in TD tear, and 150–250 g dart drop. Those ranges are not resin specifications and fall by 15–20% when 2.0–3.0 wt% slip/antiblock masterbatch is precompounded. The base-olefin polymer authorization under FDA 21 CFR 177.1520 and EU Regulation No 10/2011 applies only to the polymer; the finished film must undergo overall migration testing per EN 1186-1 and specific migration testing for the additive package, because migratory slip and processing aids are not covered by the polymer listing. If the resin is stored at more than 60% relative humidity with temperature swings, surface condensation can create moisture streaks in the bubble; pre-drying at 70–80°C for 2 h in a desiccant dryer is then required.

    When the Grade Moves to a Sealant Web in Extrusion Lamination

    When Clearflex FG 308 is processed as the heat-seal layer in PE/paper or PE/aluminium foil lamination, the extrusion set temperatures are raised to 260–285°C at the adapter and 270–295°C at the die to achieve acceptable adhesion to the substrate, but residence time at full screw speed should not exceed 6–8 min because octene-rich LLDPE begins to form gel particles at hot spots above 300°C. The polymer web is oxidized by a conventional ozone generator set at 0.4–0.8 kW·h/m² of film surface, with ozone injection placed 80–120 mm before the chill-roll nip in the air gap; insufficient ozone results in delamination peel strength below 2.5 N/15 mm when measured by ASTM F904, while excessive ozone creates polar carbonyl species that raise the heat-seal initiation temperature by 5–10°C and contribute to off-taste in fatty food contact. Typical coating weight for flexible packaging is 12–25 g/m² at line speeds of 100–200 m/min; the chill roll surface is held at 15–20°C and a matte-finish roll is used to prevent blocking. The laminated sheet is evaluated by ASTM D1004 for tear initiation resistance, and the seal strength is tested by ASTM F88/F88M-23 on a fin-seal geometry; converters report seal initiation at 85–100°C and hot-tack strength in the 95–110°C range sufficient for vertical form-fill-seal operation at 40–60 packages/min, although published data for this specific grade in lamination is limited. A coextruded skin of lower density polyethylene or ionomer can reduce seal initiation temperature below 90°C, but the multilayer article must be revalidated under EU Regulation No 10/2011 for the finished article. Amine-based antistats are not recommended in this application because they can interact with oxidation by-products and produce organoleptic taint after lamination.

    Unlike cast film, air-cooled tubular film from Clearflex FG 308 at 60–120 μm thickness is employed in heavy-duty shipping sacks for dry granular resins, fertilizers, and building materials where low-temperature impact strength and MD tear resistance determine field failure rates. The line uses a 65 mm grooved-feed extruder with a 30:1 L/D barrier screw and a 180 mm die with a dual-lip air ring; melt temperature is held at 200–220°C to preserve molecular weight and minimize oxidation-induced gel. Recycled post-industrial film added at more than 20 wt% raises melt pressure before the screen changer from about 16 MPa to above 22 MPa and forces a filter change every 2–3 h. A blow-up ratio of 2.2:1–2.6:1 and frost line height of 8–10 die diameters balance TD tear and MD impact. The film is converted into sacks by bottom-seal or side-weld bag machines; seal pressure is set to 0.4–0.6 MPa at 130–150°C, and dwell time is limited to 0.5–1.0 s because over-sealing thins the seal area and reduces slow-dart impact at -20°C. Drop impact resistance is evaluated according to ASTM D1709 method B on 100 μm film, and bag drop performance is tested under ISO 7965-1:2004; typical production limits reject lots falling below 300 g dart impact or showing MD Elmendorf tear below 20 N/mm at 23°C. The grade is not suitable for stacked-load applications in hot climates because the low-density softness at 60°C causes creep elongation; converters in such environments blend 10–20 wt% HDPE with a density of 0.950–0.965 g/cm³ to raise the storage modulus, but the blend reduces clarity and raises seal initiation temperature by 8–12°C.

    Replacing Butene-LLDPE in Stretch Hood Film Without Losing Load Retention

    Stretch hood film made from Clearflex FG 308 at 150–180 μm thickness is produced on a three-layer coextrusion blown line with an axial cooling system and an oscillating haul-off, using a die gap of 1.2–1.6 mm and blow-up ratio of 2.0:1–2.2:1 to prevent over-stretching of the low-melt-strength bubble. The octene comonomer gives the film a higher elongational viscosity under biaxial orientation than a butene-LLDPE at the same 3.0 g/10 min MFR, which is observed as a 10–15% increase in load retention after 200% elongation when measured by a method adapted from ASTM D5459; this gain is lost if the frost line is set below 300 mm from the die because quench-induced tie molecules are insufficiently annealed. Stretch hood prestretch in the machine direction is 30–50%, and the final hoop force for a pallet footprint of 1.5 m×1.5 m is typically 1,000–1,500 N; tear initiation resistance is tested according to ISO 6383-2 at 23°C and -20°C, with low-temperature tear retention above 60% required for winter outdoor storage. Elastic recovery at 100% elongation with a 10 s hold period must be above 80%; otherwise the hood slackens and fails to secure the load during transport. The application includes 500–1,500 ppm of a hindered phenolic/phosphite antioxidant system and 2,000–3,000 ppm of a high-molecular-weight hindered amine light stabilizer; HALS above 3,000 ppm increases the coefficient of friction on the load surface and reduces creep recovery. Avoid combination with amine-based antistatic packages because the alkaline species can accelerate oxidation of the phenolic stabilizer and degrade long-term UV resistance.

    In a vertical form-fill-seal line running 40 μm monolayer film at 60 packages/min with a 250 mm-wide forming tube, seal performance of Clearflex FG 308 depends on the absence of excessive erucamide migration that would reduce hot-tack strength during the 100–200 ms dwell time. The film is typically made from 98.0–99.0 wt% FG 308 and 1.0–2.0 wt% masterbatch containing 5% erucamide and 10% synthetic silica, with silica particle size below 6 μm to avoid white streaks in the printed pouch area. Extrusion is performed on a 55 mm single-screw extruder with a 28:1 L/D screw at melt temperature 195–210°C for blown film; the low-temperature profile suppresses caramelization of the erucamide and keeps film haze below 8% when measured according to ASTM D1003/ISO 14782. Heat-seal strength is tested according to ASTM F88/F88M-23; the target maximum seal strength is 15–25 N/25 mm at a jaw temperature of 130°C and 0.35 MPa pressure, with hot-tack force above 5 N/25 mm at 120°C for vertical drop-weight filling of 500 g pouches. Food-contact status is covered under EU Regulation No 10/2011 for polyethylene with total migration limit below 10 mg/dm² and under FDA 21 CFR 177.1520 for olefin polymers, but the finished pouch must be tested for extraction with the food simulant assigned by the product composition; fatty and acidic foods require specific migration analysis of erucamide and silica, and the converter is responsible for documenting lot compliance under the applicable EU recycled-material regulation where recycled content is introduced.

    Agricultural Baling Film and Oxygen Transmission Limits

    For agricultural baling film produced by cast coextrusion at 25–35 μm total thickness, Clearflex FG 308 is used in the tough core and release layers while the cling layer is often compounded with a butene-LLDPE of density 0.918 g/cm³ to increase surface tack without exceeding the oxygen transmission limit needed for silage preservation. The film must maintain an oxygen permeability below 2,000 cm³/(m²·d·atm) at 23°C and 0% RH when measured by ASTM D3985-17, and the actual value is controlled by the layer distribution, not by the base polymer alone; a 30 μm film with 10% cling layer, 70% FG 308 core, and 20% release layer typically falls in the range of 1,200–1,800 cm³/(m²·d·atm). The cast line uses a 1,800 mm-wide die with die gap 0.5 mm and a 750 mm chill roll at 20–26°C; too low a chill roll temperature increases the cling-layer haze, and too high a temperature causes microscopic blocking that tears during rapid bale wrapping. Cling force is tested by ASTM D5458-20 after seven days of aging at 40°C because migration of the tackifier changes the surface energy; the target is 100–180 g peel force, and any reading above 220 g is rejected because the film will refuse to unwind under tension. UV stabilization is provided by 2,500–3,500 ppm HALS and 1,000–2,000 ppm triazine-type UV absorber; exposure of the stabilizer package to elemental sulfur or chlorinated disinfectants during storage can deactivate the HALS and should be avoided. The baled wrap is not suitable for long-term burying because the grade is not photodegradable and does not meet biodegradable mulch film standards such as EN 17033.

    Free Quote

    Competitive Versalis Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FG 308 is an octene-1 copolymer linear low density polyethylene supplied in pellet form for flexible film conversion. Nominal property data are: melt flow rate 1.0 g/10 min at 190°C and 2.16 kg load measured under ISO 1133-1; density 0.916 g/cm³ under ISO 1183-1; and peak melting temperature 122–124°C by differential scanning calorimetry under ISO 11357-3. The comonomer is 1-octene, not 1-butene or 1-hexene. This molecular choice is the primary difference from standard linear low density polyethylene grades and affects seal initiation, impact toughness, tear resistance, and certain extrusion conditions. The grade is used in blown-film and cast-film packaging: bread bags, frozen food films, collation shrink, heavy-duty sacks, lamination sealant webs, and coextruded barrier films.

    PropertyMethodNominal valueUnit
    DensityISO 1183-10.916g/cm³
    Melt flow rateISO 1133-11.0g/10 min
    Peak melting temperatureISO 11357-3122–124°C
    Comonomer—1-octene—

    How Does Octene Comonomer Length Change the Short-Chain Branching Profile of FG 308?

    At equivalent molar comonomer content, 1-octene inserts a six-carbon side branch into the polyethylene backbone, whereas 1-butene inserts a two-carbon ethyl branch. The longer side branch disrupts crystal lamellae more efficiently and increases the concentration of tie molecules that connect adjacent lamellae. In film form this structural shift is measured as higher dart impact strength under ISO 7765-2 or ASTM D1709 and higher Elmendorf tear values under ASTM D1922, relative to a butene-grade LLDPE of matching density and melt flow rate. The exact property differences are gauge-dependent; published data for this specific configuration is limited to converter trials and technical service measurements rather than single universal values.

    In the melt phase, the longer short-chain branch does not generate the long-chain branching found in high-pressure LDPE. The melt elasticity and strain hardening of FG 308 are therefore lower than an autoclave LDPE of equivalent melt index. On a capillary rheometer at 190°C, a linear polyethylene of this class displays shear thinning and a critical wall shear stress for melt fracture in the range 0.14–0.40 MPa; die geometry shifts the exact onset. The practical consequence is that FG 308 cannot simply replace high-pressure LDPE at the same die gap and output without risk of melt fracture, bubble instability, or higher die pressure.

    For a film grade with density 0.916 g/cm³, the melting endotherm is broad because short-chain branches interrupt the crystallizable ethylene sequence length distribution. The broad melting profile widens the usable heat-seal window compared with a high-density polyethylene and allows a temperature-gradient sealing machine to identify the precise seal initiation temperature for a given structure. The same comonomer-driven lamellar disruption reduces stiffness relative to higher-density LLDPE but improves puncture and tear propagation resistance.

    Compared with hexene-based LLDPE, 1-octene provides a longer branch than 1-hexene and generally produces a larger property shift over butene, although the difference between hexene and octene is smaller than the difference between butene and either higher α-olefin. The relationships are influenced by comonomer distribution breadth, catalyst system, and thermal history; therefore, substitutions between C6-LLDPE and C8-LLDPE should be validated on the target film line rather than predicted solely from comonomer type.

    In blown-film production, FG 308 is typically run on single-screw extruders with a grooved feed section, an L/D ratio of 24:1 to 30:1, and a barrier screw with a dispersive mixing section such as a Maddock or spiral mixer. A grooved feed section is preferred because the linear backbone of LLDPE reduces solids-conveying friction and makes the melt prone to output surging if screw channels are not pressure-stable. A 200 mm to 400 mm spiral mandrel die with 2.0–2.4 mm die gap is used in many converters; weld lines from the spiral channels are a known weak point because linear LLDPE has limited long-chain branching to heal weld interfaces. Raising melt temperature from 200°C to 220°C improves weld-line strength but narrows the bubble’s stability envelope under high ambient air turbulence.

    When Melt Temperature and Die Gap Are Varied on a Blown-Film Line

    The most common processing conflict for octene LLDPE is the opposing effect of die gap on pressure, melt fracture, and orientation. A 1.8 mm die gap increases wall shear stress and improves optical clarity by reducing the melt curtain thickness, but it can raise die pressure to the upper limit of a machine with less than 350 bar maximum pressure. A 2.5 mm gap reduces die pressure and melt fracture but delivers a thicker melt curtain, which may lower machine-direction orientation and shift tear anisotropy toward the transverse direction. On production lines fitted with internal bubble cooling, the frost line height is an additional control: a short frost line promotes rapid crystallization and often improves optics, while a high frost line increases the molten web residence time and improves bubble stability at the expense of haze. Field observations on air-cooled blown-film equipment show that melt temperatures above 240°C for extended runs increase die lip oxidation and subsequent gel deposition; the gels produce optical defects and reduce Elmendorf tear in 25–50 µm film.

    Die lip oxidation is a recurring failure mode with linear low density polyethylene because the narrow die gap concentrates shear heating at the exit land. The oxidized material eventually releases as gel particles that appear as fish-eye defects when film is inspected under ASTM D7310 or equivalent optical inspection. Mitigation requires purging, lowering the melt temperature below the oxidation threshold, and verifying that the extruder thermocouple readings reflect true melt temperature rather than barrel metal temperature. Screw designs with excessive shear mixing can generate local melt temperatures above 240°C even when barrel settings remain lower; a melt pump or dynamic mixing section should be specified with temperature monitoring at the melt stream.

    Blending with high-pressure LDPE at 10–20 wt% increases melt strength and stabilizes the bubble. The improvement derives from the long-chain branching of the LDPE phase. The trade-off is a reduction in dart impact and machine-direction Elmendorf tear, which should be quantified by ISO 7765-2 and ASTM D1922 at the intended film gauge. In applications requiring low seal initiation, LDPE addition also raises the seal initiation temperature because high-pressure LDPE has a different chain architecture and higher melt viscosity at sealing temperatures.

    Surface moisture from silo storage should be avoided. If pellets are exposed to relative humidity above 60% and then introduced into a hot extruder, steam can create bubble instability and pinholes. Drying with dehumidified air at 60°C for 2–4 h may be used when condensation is visible; the material does not require predrying under normal closed-internal storage. This boundary condition is operational rather than chemical, because linear polyethylene does not hydrolyze, but the physical presence of water vapor at the die exit disrupts melt continuity.

    Seal Initiation, Optical Clarity, and Food-Contact Constraints

    Octene comonomer lowers the seal initiation temperature relative to butene LLDPE at the same density. In vertical form-fill-seal equipment, lower seal initiation allows a narrower sealing jaw dwell time or lower jaw temperature, which reduces heat exposure to thermally sensitive outer layers. Seal strength is tested by ASTM F88 on a tensile tester with a defined jaw speed; hot-tack is tested under ASTM F1921. For thin webs below 30 µm, hot-tack is often more critical than cool seal strength, and the grade should be validated with the specific coextruded structure because adjoining layers can shift the apparent sealing window by changing heat transfer into the sealant.

    Optical clarity is evaluated by haze to ASTM D1003 and gloss to ASTM D2457. C8-LLDPE generally produces lower haze and higher gloss than C4-LLDPE at equivalent film gauge and blow-up ratio, but the effect is smaller than the difference between LLDPE and high-pressure LDPE. Die lip fouling, melt temperature heterogeneity, and migratory slip additives can each increase surface haze. Slip and antiblock levels should be kept to the minimum required for winding and bag opening because these additives migrate to the film surface and can interfere with seal strength. Migration kinetics are temperature- and time-dependent; after film aging, surface additive concentration increases, and seal strength may decrease if the additive layer forms a weak boundary at the seal interface.

    Food-contact use is subject to the specific version of the manufacturer’s declaration. Relevant frameworks are EU Regulation 10/2011 as amended and FDA 21 CFR 177.1520 for olefin polymers used in contact with food. These are not certifications of the resin alone; migration testing with the intended food simulant and contact time/temperature is required for the final package. Use of post-consumer recycled material, masterbatch, or printing solvents changes the regulatory status and may require additional compliance studies.

    The low density and 122–124°C melting peak impose a thermal limitation: FG 308 is not intended for retort or autoclave sterilization above 100°C unless the package is physically supported. At higher temperatures, the amorphous fraction becomes sufficiently mobile that seal creep and deformation can occur under internal pressure. For hot-fill applications, the package must be evaluated under ASTM D2732 or equivalent dimensional stability methods to confirm that side-wall strain and seal relaxation remain within specification.

    In coextruded barrier structures with polyamide or EVOH, FG 308 can be used as the sealant layer. Tie-layer selection determines the interfacial adhesion; failure at the LLDPE/tie interface under ASTM F904 lamination bond testing is often delamination rather than heat-seal failure. The packaging line should set chill-roll or bubble cooling temperatures to prevent blocking; blocking is more likely in soft C8-LLDPE films with high slip-additive consumption than in stiffer C4 grades.

    Top