| HS Code | 759050 |
| Polymertype | Linear Low Density Polyethylene |
| Comonomer | 1-Hexene |
| Density | 0.918 g/cm3 |
| Meltflowrate | 1.0 g/10 min (190 °C/2.16 kg) |
| Meltingpoint | 124 °C |
| Vicatsofteningtemperature | 95 °C |
| Tensilestrengthatyield | 10 MPa |
| Tensilestrengthatbreak | 30 MPa |
| Elongationatbreak | 700 % |
| Flexuralmodulus | 250 MPa |
| Shoredhardness | 50 |
| Dartdropimpact | 150 g |
| Elmendorftearstrengthmd | 130 g |
| Elmendorftearstrengthtd | 350 g |
| Haze | 12 % |
| Gloss45 | 60 % |
| Coefficientoffriction | 0.2 |
As an accredited Versalis Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex FG 106 packaging: 25 kg polyethylene bags, palletized, also available in 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL loading of Versalis Clearflex® FG 106 Hexene Copolymer LLDPE: palletized 25 kg bags, shrink-wrapped, securely stowed for sea transport. |
| Shipping | Versalis Clearflex® FG 106 is shipped as solid polyethylene pellets in 25 kg bags, octabins, or bulk containers. It is non-hazardous for transport and should be kept in a cool, dry, ventilated area away from heat, moisture, and direct sunlight. Follow local regulations and avoid damaged packaging. |
| Storage | Store Clearflex FG 106 LLDPE in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, and palletized off the floor to prevent moisture and contamination. Avoid excessive stacking, minimize static generation, and maintain ambient temperature. Keep away from incompatible materials and follow local regulations. |
| Shelf Life | Typically stable; 24-month shelf life in unopened original packaging when stored cool, dry, and away from direct sunlight. |
Blown film conversion of Versalis Clearflex® FG 106 hexene-1 copolymer LLDPE for direct food contact packaging is carried out on single- or three-layer coextrusion lines where the grade constitutes 70 wt% to 100 wt% of the core or skin layer. Typical lot analysis indicates an MFR of 1.0 g/10 min under 190 °C/2.16 kg per ISO 1133-1:2022 and a density of 0.916 g/cm³ per ISO 1183-1:2019. In three-layer structures, the remaining 20 wt% to 30 wt% is typically an autoclave LDPE with a melt flow rate of 0.3 g/10 min to 0.8 g/10 min selected to stabilize the bubble and raise melt strength, which simultaneously lowers dart impact. Compliance under FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011 requires lot-specific certification of overall migration below 10 mg/dm², plus validation of specific migration limits for additives listed in Annex I on the finished printed or laminated film rather than on the resin pellets alone. The monolayer die gap is 2.0 mm to 2.5 mm; blow-up ratio is 2.2:1 to 2.8:1; melt temperature at the die is 190 °C to 215 °C. Extruders with L/D ratios of 24:1 to 30:1 and barrier screws with Maddock mixing sections are standard. Melt pressure at the screen changer is recorded continuously to detect gel build-up from oxidized material, a documented failure mode when start-up purging is performed with high-viscosity HDPE and the transition is incomplete.
Frost line height is set at 6 to 9 die diameters for monolayer film to balance transverse direction tear and machine direction stiffness. Film tensile properties are monitored per ASTM D882-18; dart impact is measured per ASTM D1709-22 Method A; Elmendorf tear is measured per ASTM D1922-15; seal strength is measured per ASTM F88/F88M-21; haze is measured per ASTM D1003-21. Heat sealing is carried out on rotary or hot-bar sealers at initiation temperatures below 105 °C, with jaw pressure of 350 kPa to 500 kPa and dwell time of 0.7 s to 1.2 s. Terminal finished products include bread bags, frozen food pouches, produce bags, and overwrap for paperboard trays. The operational boundary for this grade is that neat resin should not be held above 240 °C for more than 10 min during line stops, because oxidative gel formation increases and produces visible specks in thin film.
For cast stretch film lines running above 400 m/min, Clearflex® FG 106 is generally placed in the core layer of a 3- or 5-layer machine film, where the hexene branch distribution contributes to lower neck-in and better melt draw performance than butene copolymers. The core layer addition ratio ranges from 55 wt% to 75 wt%; the skin layers account for 15 wt% to 25 wt% and are frequently formulated with metallocene LLDPE or ethylene-vinyl acetate to control cling and unwind force. A documented operational boundary is that neat FG 106 can exhibit draw resonance on lines running above 400 m/min unless the die gap is narrowed to 0.8 mm to 1.2 mm and the melt temperature is held between 245 °C and 270 °C. The addition of 10 wt% to 20 wt% of a high-pressure LDPE with MFR 0.3 g/10 min to 0.8 g/10 min is standard to suppress draw resonance, but this blend shifts tensile elongation at break and must be revalidated per ASTM D882-18 at the target machine stretch ratio of 200% to 300%. Pre-stretch performance is evaluated using ASTM D5748-95(2019); critical parameters are puncture resistance and load retention at 200% elongation.
On high-speed cast lines, the chill roll temperature is maintained at 18 °C to 24 °C, with vacuum box and air knife settings adjusted to prevent melt wave oscillation at the die lip. Terminal finished products include machine stretch film, pre-stretched hand film, and collation wrap for beverage multipacks. Regulatory compliance for non-food industrial stretch film rests on REACH Regulation 1907/2006 and Directive 94/62/EC heavy metal limits, not on food contact migration testing. If the converter uses recycled trim in the core, the recycled fraction should not exceed 20 wt% without re-evaluating elongation at break and unwinding tension.
In flexible packaging laminates, Clearflex® FG 106 is processed into sealant webs of 20 µm to 50 µm thickness, either as a blown film or cast film, and subsequently laminated to oriented polyester, biaxially oriented polypropylene, or aluminum foil using solventless polyurethane adhesives applied at 1.5 g/m² to 2.5 g/m² dry coat weight. The sealant layer formulation ratio is 70 wt% to 90 wt% FG 106, with the balance being a plastomer or an autoclave LDPE selected to lower the heat-seal initiation temperature. Heat-seal initiation is measured per ASTM F1921-20; for this grade in a 25 µm blown web, consistent seal initiation is recorded at 100 °C to 105 °C when the sealing jaw pressure is 350 kPa to 500 kPa and dwell time is 0.5 s. The critical production control step is corona discharge treatment of the sealant web to 38 mN/m to 42 mN/m immediately prior to adhesive coating; surface energy decay below 36 mN/m within 4 h is a known cause of adhesive delamination in solventless lamination on high-humidity production days.
On blown-film lines producing sealant webs, bubble stability is lower than for LDPE-sealant grades; operators maintain a frost line height of 5 to 8 die diameters and use an internal bubble cooling system when film thickness exceeds 40 µm. Extruder barrel temperatures from 180 °C to 210 °C are kept below the degradation onset to avoid creating oxidized gel seeds that cause seal failures. Addition of processing aid masterbatch at 0.5 wt% to 1.0 wt% may be required on older lines with high backpressure. Compliance for food contact laminates is anchored to FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011, including Annex II restrictions on primary aromatic amines from polyurethane adhesives, which are not part of the polyolefin resin but are relevant to the finished laminate. Terminal finished products include stand-up pouches, frozen vegetable packaging, dry mix pouches, and lidding films where a peelable or lock-seal sealant is not required.
| Application boundary | Primary regulation or standard | Test method | Key limit or criterion |
|---|---|---|---|
| Monolayer food contact film | FDA 21 CFR 177.1520(c) 3.2a, EU Regulation 10/2011 | EN 1186-1:2002, total migration | 10 mg/dm² overall migration |
| Cast stretch film, non-food | REACH Regulation 1907/2006, Directive 94/62/EC | XRF screening, extractive metals analysis | Sum of Pb, Cd, Hg, Cr(VI) 100 mg/kg |
| Sealant web lamination | FDA 21 CFR 177.1520(c) 3.2a, EU Regulation 10/2011 | ASTM F1921-20, ASTM F88/F88M-21 | Seal initiation 100–105 °C at 25 µm |
| Agricultural greenhouse film | REACH Regulation 1907/2006, EN 13206:2017 | ISO 4892-2, EN ISO 527-3 | Accelerated weathering benchmark from formulated film |
| FFS industrial sacks | REACH Regulation 1907/2006, UN packaging certification where applicable | ASTM D1922-15, ASTM F88/F88M-21 | Drop and stacking performance on finished sack |
When a three-layer coextruded greenhouse film is specified for a 24-month service life under Mediterranean solar irradiation, Clearflex® FG 106 is incorporated into the middle or core layer at 55 wt% to 70 wt%, with the remaining 30 wt% to 45 wt% divided between an EVA copolymer with vinyl acetate content of 12% to 18% in the inner layer and a high-pressure LDPE in the outer layer. The outer layer must carry the UV stabilizer package; for this grade, a combined HALS and benzophenone or triazine system is dosed at 0.30 phr to 0.45 phr in the outer skin, and an anti-fog agent is dosed at 0.5 phr to 1.0 phr in the inner skin. Film extrusion uses a die gap of 2.2 mm to 2.8 mm, a blow-up ratio of 2.5:1 to 3.5:1, and a melt temperature of 190 °C to 210 °C; the higher blow-up ratio improves transverse direction impact resistance but reduces machine direction tensile strength, requiring a balance validated by EN ISO 527-3 tensile testing and ISO 7765-1:1988 dart impact.
Compliance for agricultural covering films does not follow food contact migration limits but is assessed under REACH Regulation 1907/2006 and, where applicable, EN 13206:2017 for covering films for greenhouses; specific restrictions on heavy metals and hazardous substances in the final film must be documented. Terminal products include greenhouse covers, low tunnels, silage stretch covers, and anti-algae mulch films where the hexene branch distribution provides higher dart impact per unit thickness than butene LLDPE. Published data for this specific grade in long-term outdoor weathering is limited; accelerated weathering per ISO 4892-2 on formulated films should be used to establish a lot-specific benchmark rather than extrapolating from butene LLDPE data. The film must not be placed in direct contact with high-chlorine agricultural disinfectants without barrier verification, because oxidative degradation of the polyethylene surface can be accelerated in the presence of free radicals generated by hypochlorite at high concentration.
In form-fill-seal heavy-duty sack production for dry bulk products, Clearflex® FG 106 is used in blends with high-pressure LDPE at 60 wt% to 85 wt%; the LDPE fraction is necessary because neat hexene LLDPE shows sharkskin on narrow die gaps below 1.8 mm at shear rates above 500 s⁻¹. Coextruded FFS films generally allocate FG 106 to the core layer, while the skins are formulated with LDPE and slip/antiblock masterbatch at 2 wt% to 4 wt%. The blown film line is run at a die gap of 2.0 mm to 2.4 mm, a blow-up ratio of 2.0:1 to 2.6:1, and a melt temperature of 195 °C to 225 °C. A documented production failure occurs when the die lip temperature drops below 180 °C and the melt pressure rises above 350 bar, producing visible melt fracture bands at the fold edges. Terminal product types include FFS sacks for polymer pellets, fertilizers, and industrial powders; the final film is tested for tear propagation per ASTM D1922-15, puncture per ASTM D5748-95(2019), and seal strength per ASTM F88/F88M-21. Compliance for non-food industrial sacks is typically limited to REACH Regulation 1907/2006 and, for dangerous goods packaging, the relevant UN certification requirements applicable to the final sack construction, not to the resin as a standalone article. Where the sack is converted for UN certified dangerous goods packaging, the finished sack is drop-tested and stacking-tested per 49 CFR 178.603 and 49 CFR 178.606 at the specified filling mass; the resin lot is not the certifiable article.
Competitive Versalis Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® FG 106 is a linear low density polyethylene produced by copolymerisation of ethylene with 1-hexene. The material belongs to the Clearflex film-grade portfolio and is supplied as a pelletised resin for blown film extrusion. The 1-hexene comonomer is incorporated as a butyl side branch; this structural feature separates the product from butene-based LLDPE, which introduces ethyl side branches, and from octene-based LLDPE, which introduces hexyl side branches. The difference in branch length is not a superficial distinction because it controls the concentration and length distribution of tie molecules that bridge lamellae after crystallisation, and those tie molecules govern low-gauge impact resistance, tear propagation, and seal behaviour.
The product literature identifies a typical density of 0.918 g/cm³ when tested according to ISO 1183-1:2019 and a typical melt mass-flow rate of 1.0 g/10 min at 190 °C and 2.16 kg load according to ISO 1133-1:2022. These are nominal characterisation values used to distinguish the grade from other Clearflex products; they should not be read as batch release limits unless a specific purchasing specification is agreed with Versalis. The melt flow rate of 1.0 g/10 min places the material in the general-purpose blown film viscosity range, providing sufficient melt strength for tubular bubble stability while remaining low enough in viscosity to permit thin-gauge drawdown on conventional extrusion equipment.
In blown film, tensile and impact performance is determined by chain architecture and fabrication history rather than by density alone. A butene-1 comonomer in LLDPE introduces ethyl side branches, which are relatively short and can be accommodated near the crystal surface without generating as many load-bearing tie molecules. A 1-hexene comonomer introduces butyl side branches; these longer branches are more effective at disrupting lamellar order and increasing the probability that a single polymer chain participates in more than one crystalline lamella. The result is a measurable shift in impact-toughness balance at equivalent density and melt-flow rate. The effect is especially visible in free-falling dart impact testing according to ASTM D1709 or ISO 7765-1, and in Elmendorf tear resistance according to ASTM D1922 or ISO 6383-2. Comparative data must be generated on film of identical gauge and conditioning because both dart impact and tear are strongly thickness-dependent. Conditioning before test should follow ISO 291 at 23 °C ± 2 °C and 50 % ± 5 % relative humidity for at least 40 h.
The same architectural rationale applies to optical haze and gloss. The longer butyl branch lengths in FG 106 reduce the fraction of large, highly ordered crystallites that scatter visible light; therefore, hexene copolymers of this density often exhibit lower haze than butene-based counterparts of similar melt index when compared according to ISO 14782 or ASTM D1003. However, optical comparisons are invalid if extruder melt temperature, frost-line height, or die-lip cleanliness differ between trials because surface defects and frozen-in orientation contribute to light scattering. The use of a high blow-up ratio can also modify the balance between machine-direction and transverse-direction orientation; the resulting anisotropic tear values should be reported separately, not condensed into a single property.
On conventional blown film lines, the resin is usually processed on single-screw extruders with barrier-type screws and L/D ratios between 24:1 and 30:1. A grooved feed section is not mandatory for LLDPE, but it increases feed uniformity at high screw speed. Starting temperature profiles for a 0.918 g/cm³ hexene LLDPE are commonly set at 170 °C in the feed zone, 180 °C in the compression zone, 190–200 °C in the metering zone, and 200–210 °C at the die; these settings are practical starting points and must be adjusted for screw geometry, barrel heater response, and output demand. Die gap is the dominant mechanical variable. LLDPE exhibits lower melt strength than high-pressure LDPE and can enter melt fracture at high shear stress. A die gap of 1.2–1.6 mm is generally maintained for film thicknesses above 25 µm; gaps below 1.0 mm increase the risk of sharkskin and require higher die temperatures or reduced output. A blow-up ratio between 2.0:1 and 3.0:1 is typical for general-purpose packaging film. Higher blow-up ratios increase transverse-direction tear and impact, while lower blow-up ratios favour machine-direction tear; both trends should be checked against the converter’s packaging line requirements.
Production experience on 45 mm and 60 mm blown film extruders shows that melt-pressure stability is a more reliable indicator of melt quality than a single barrel temperature. Plugging of the screen pack or excessive screw speed can produce pressure fluctuations that disturb bubble geometry. Operators should monitor die pressure relative to an established baseline for the run; a rising trend at constant screw speed usually indicates filter pack accumulation. Because LLDPE is not hygroscopic, drying is unnecessary for dry pellets. However, if pellets are transferred from cold storage into a warm production hall, surface condensation can introduce moisture at levels sufficient to create pinholes in thin film. When pellet surface moisture exceeds 0.1 wt%, a desiccant hopper dryer at 60 °C for 1–2 h is an effective correction; prolonged hot-air drying is unnecessary and can promote pellet surface oxidation.
Seal initiation and hot-tack behaviour are frequently more decisive than tensile properties in packaging applications. Hexene copolymers of this density typically show a lower seal initiation temperature than butene-based LLDPE at the same melt index because the longer butyl branches broaden the distribution of crystallite sizes and reduce the fraction of thick lamellae that would otherwise delay sealing. Seal initiation can be assessed by making heat-sealed specimens and pulling them according to ASTM F88; hot-tack is measured by ASTM F1921 or equivalent internal methods. The measured values are affected by seal bar temperature, dwell time, jaw force, and film gauge. A converter evaluating FG 106 for lamination or form-fill-seal packaging should therefore generate seal curves on the target packaging line rather than relying on a single supplied value. As a coextrusion component, the resin is compatible with high-pressure LDPE and with ethylene-vinyl acetate copolymers in standard multi-layer structures, but interlayer adhesion should be confirmed at the intended blow-up ratio and frost-line height because interfacial contact time in tubular coextrusion is shorter than in cast film.
Compared with octene-1 copolymers of equivalent density, hexene grades often provide a stiffer, more cost-effective balance at a lower comonomer cost, but they may sacrifice some ultimate puncture resistance and low-temperature dart impact. Octene-1 introduces hexyl branches that are more efficient than butyl branches in generating tie molecules; therefore, heavy-duty stretch film and frozen-food packaging that must withstand puncture at low temperatures may preferentially use octene LLDPE. Conversely, FG 106 is positioned for packaging films that require a controlled balance of clarity, stiffness, and sealing performance without the cost of an octene comonomer. The final selection should be based on side-by-side film testing using ASTM D882 for tensile properties, ASTM D5748 for puncture resistance, and the appropriate dart or tear methods. Published data for this specific configuration is limited, so converter-generated data at target gauge and line speed remains the authoritative basis for qualification.
In film below 30 µm, especially in hygiene backsheet or light-gauge lamination formats, the lower extension-hardening of linear polyethylene relative to long-chain branched LDPE can manifest as bubble instability and poor gauge control. The standard corrective measure is to blend a fraction of high-pressure LDPE into the LLDPE stream. LDPE levels between 10 wt% and 20 wt% are common in thin-gauge blown film; the addition increases extensional melt strength and reduces the tendency of the bubble to sag between the die and the frost line. The LDPE fraction should be metered gravimetrically at the feed throat because inconsistent blending produces visible gauge bands and tear anisotropy in the finished roll. The blend ratio should be adjusted to the lowest level that maintains bubble stability to avoid unnecessary loss of dart impact; each added increment of LDPE tends to reduce dart impact because it introduces a more branched architecture that freezes orientation differently.
High melt temperatures above 230 °C should be approached with caution because extended residence time at elevated temperature consumes primary antioxidants and can form gel particles. If production conditions require melt temperatures above 230 °C, the oxidation induction time of the film can be checked by ISO 11357-6 to verify that the stabiliser package remains intact. No additional waxes or processing aids should be assumed necessary for an LLDPE of 1.0 g/10 min melt-flow rate; if the converter uses polymer processing aid masterbatches, the additive should be approved for polyolefins and added at the lowest effective concentration because overdosing can raise film haze and alter printability.
Storage and handling constraints for FG 106 are typical of non-hygroscopic polyolefin pellets. The resin should be kept in a clean, dry area at temperatures below 50 °C and away from direct sunlight. Long-term exposure to ultraviolet light can initiate free-radical oxidation at the pellet surface, reducing the antioxidant effectiveness before extrusion. Inventory should be managed on a first-in-first-out basis, and partially emptied containers should be resealed to minimise dust contamination. The resin is not classified as hydrolysable, so ambient moisture is not a critical parameter for dry pellets, but surface condensation during cold-to-warm transfer remains a practical concern as described above. Contamination by foreign pellets, paper fibres, or dust should be prevented because these contaminants can form gels or odour defects in thin film.
Regarding food-contact and chemical regulatory status, olefin polymers of this class are typically manufactured to meet the compositional requirements of Regulation (EU) No 10/2011 as amended for plastic food-contact materials, and are commonly referenced under FDA 21 CFR 177.1520 for olefin polymers. These references are not sufficient to certify the finished package because the final article may require migration testing under the intended contact conditions; specific migration limits are defined in Regulation (EU) No 10/2011 Annex II. The converter should request the supplier’s product stewardship declaration for the exact grade and confirm that the final film complies with all national and regional requirements applicable to the intended food type, shelf life, and temperature. If the film is used in medical packaging, the converter should evaluate biocontamination and sterilisation compatibility separately; relevant international standards for medical packaging include ISO 11607-1 and ISO 11607-2, but the resin datasheet alone does not establish package-level performance.